Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CEMENTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Micrometer-scale 3-D shape characterization of eight cements: Particle shape and cement chemistry, and the effect of particle shape on laser diffraction particle size measurement

Eight different portland cements were imaged on a synchrotron beam line at Brookhaven National Laboratory using X-ray microcomputed tomography at a voxel size of about 1 mum per cubic voxel edge. The particles ranged in size roughly between 10 mum and 100 mum. The shape and size of individual particles were computationally analyzed using spherical harmonic analysis. The particle shape difference between cements was small but significant, as judged by several different quantitative shape measures, including the particle length, width, and thickness distributions. It was found that the average shape of cement particles was closely correlated with the volume fraction of C{sub 3}S (alite) and C{sub 2}S (belite) making up the cement powder. It is shown that the non-spherical particle shape of the cements strongly influence laser diffraction results, at least in the sieve size range of 20 mum to 38 mum. Since laser diffraction particle size measurement is being increasingly used by the cement industry, while cement chemistry is always a main factor in cement production, these results could have important implications for how this kind of particle size measurement should be understood and used in the cement industry.

36 MATERIALS SCIENCE↗

Graphene nanoplatelets reinforced cement as a solution to leaky wellbores reinforcing weak points in hydrated Portland cement with graphene nanoparticles improves mechanical and chemical durability of wellbore cements

In this work, to improve the performance of wellbore cement under subsurface environments, graphene nanoplatelets (GNPs) were added in various percentages to Class-H cement slurry. Microstructural characterization of cement slurries cured at 90 °C and 95% RH indicates that GNP modifies the microstructure of hydrated cement by reinforcing pore spaces. As a result, the mechanical properties, such as Young's modulus and axial peak stress, obtained from high temperature triaxial compression tests are significantly improved based on different percentages of added GNPs. Furthermore, the hydrated 1 × 2 inch GNP- Portland cement cores tested under simulated deep wellbore conditions of high-temperature and high pressure (HTHP), appear to have a ductile-like behavior, when compared to a typical brittle nature of Portland cement pastes. From our observations and published data on graphene resistance to fracture, GNP addition to cement is evidently enhancing the flexibility of cement. These improvements would reduce the risks associated with wellbore cement deterioration and a consequent leakage in fossil fuel production, geothermal energy production, CO 2 storage as well as long-term sealing materials in plugging and abandonment of all wellbores at the end of their service life.

36 MATERIALS SCIENCE↗

Determining the water-cement ratio, cement content, water content and degree of hydration of hardened cement paste: Method development and validation on paste samples

We propose a new method to estimate the initial cement content, water content and free water/cement ratio (w/c) of hardened cement-based materials made with Portland cements that have unknown mixture proportions and degree of hydration. This method first quantifies the composition of the hardened cement paste, i.e. the volumetric fractions of capillary pores, hydration products and unreacted cement, using high-resolution field emission scanning electron microscopy (FE-SEM) in the backscattered electron (BSE) mode and image analysis. From the obtained data and the volumetric increase of solids during cement hydration, we compute the initial free water content and cement content, hence the free w/c ratio. The same method can also be used to calculate the degree of hydration. The proposed method has the advantage that it is quantitative and does not require comparison with calibration graphs or reference samples made with the same materials and cured to the same degree of hydration as the tested sample. This paper reports the development, assumptions and limitations of the proposed method, and preliminary results from Portland cement pastes with a range of w/c ratios (0.25-0.50) and curing ages (3-90 days). We also discuss the extension of the technique to mortars and concretes, and samples made with blended cements.

36 MATERIALS SCIENCE↗

Bone Marrow Nails Created by Percutaneous Osteoplasty for Long Bone Fracture: Comparisons Among Acrylic Cement Alone, Acrylic-Cement-Filled Bare Metallic Stent, and Acrylic-Cement-Filled Covered Metallic Stent

Purpose: This study was designed to compare the strength among bone marrow nails created to treat long bone fractures using interventional procedures. Methods: Twelve resected intact tibiae of healthy swine were used. A circumferential bone fracture was made in nine tibiae and restored with the following created bone marrow nails: acrylic cement alone (ACA) (n = 3), acrylic-cement-filled bare metallic stent (AC-FBMS) (n = 3), and acrylic-cement-filled covered metallic (AC-FCMS) stent (n = 3). The remaining intact tibiae (n = 3) were used as controls. Results: A bone marrow nail was successfully achieved within 30 min in all swine. The maximum injection volume of acrylic cement for creating ACA, AC-FBMS, and AC-FCMS was 1.7 {+-} 0.3, 3.2 {+-} 0.4, and 2.9 {+-} 0.4 mL, respectively. The thickness of bone marrow nail created in the ACA, AC-FBMS, and AC-FCMS groups was 3.6 {+-} 1.0, 10.3 {+-} 0.26, and 9.6 {+-} 0.32 mm, respectively (AC-FBMS group versus AC-FCMS group, p = 0.038), probably because of leakage of acrylic cement surrounding the interstices. The maximum bending power (kilonewton) and bending strength (newton/mm{sup 2}) in the normal long bone, ACA, AC-FBMS, and AC-FCMS groups were: 1.70 {+-} 0.25 and 79.2 {+-} 16.1; 0.21 {+-} 0.11 and 8.8 {+-} 2.8; 0.46 {+-} 0.06 and 18.2 {+-} 1.6; and 0.18 {+-} 0.04 and 7.8 {+-} 2.7, respectively. Conclusions: Although the maximum bending power and bending strength of AC-FBMS were not satisfactory, it was the most robust of the three marrow nails for restoring fractured long bone.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

Intrinsic differences in atomic ordering of calcium (alumino)silicate hydrates in conventional and alkali-activated cements

The atomic structures of calcium silicate hydrate (C–S–H) and calcium (–sodium) aluminosilicate hydrate (C–(N)–A–S–H) gels, and their presence in conventional and blended cement systems, have been the topic of significant debate over recent decades. Previous investigations have revealed that synthetic C–S–H gel is nanocrystalline and due to the chemical similarities between ordinary Portland cement (OPC)-based systems and low-CO{sub 2} alkali-activated slags, researchers have inferred that the atomic ordering in alkali-activated slag is the same as in OPC–slag cements. Here, X-ray total scattering is used to determine the local bonding environment and nanostructure of C(–A)–S–H gels present in hydrated tricalcium silicate (C{sub 3}S), blended C{sub 3}S–slag and alkali-activated slag, revealing the large intrinsic differences in the extent of nanoscale ordering between C–S–H derived from C{sub 3}S and alkali-activated slag systems, which may have a significant influence on thermodynamic stability, and material properties at higher length scales, including long term durability of alkali-activated cements.

36 MATERIALS SCIENCE↗

Influence of multi-species solute transport on modeling of hydrated Portland cement leaching in strong nitrate solutions

The differences between the predictions of Fickian diffusion and Nernst-Planck electro-diffusion based reactive transport models are investigated in the context of an important practical problem – leaching of Portland cement in strong nitrate porewater solutions under saturated conditions. Numerical results are presented for three distinct porewater solutions: deionized water, ammonium nitrate solution, and diluted porewater from a cementitious low-activity nuclear waste form. Solute concentrations predicted by the two transport models show significant differences: as much as a factor of two for ammonium nitrate leaching and as much as a factor of four for waste form leaching; whereas, negligible differences are observed for deionized water leaching. The major conclusion is that Fickian diffusion may be accurate enough for deionized water leaching, but electro-diffusion should be considered in the reactive solute transport modeling of ammonium nitrate decalcification and in the degradation modeling of cementitious materials exposed to nuclear waste form solutions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Insights into the physical and chemical properties of a cement-polymer composite developed for geothermal wellbore applications

To isolate injection and production zones from overlying formations and aquifers during geothermal operations, cement is placed in the annulus between well casing and formations. Wellbore cement can fracture due to chemical and physical stress. A polymer-cement (composite) with self-healing properties, stable at high temperatures, was recently developed by our group. Here we present data on the elemental distribution, mineral composition, internal microstructure, and tensile elasticity of this composite and how it compares to cement without polymer (control cement). Entrapped air porosity was similar between control cement (0.44% by volume) and composite (0.22% by volume). Total voids increased with polymer content in the cement (10% and 25% composite), and polymer was found to fill most of these voids. Polymer appears to act as a (cement hydration) retarder increasing the amount of unhydrated silicate minerals in the matrix. Tensile elasticity was improved for composites as compared to control cement, suggesting that the composite materials perform better under mechanical stress. Density-functional calculations reproduce the drop in Young’s modulus by about 60% observed experimentally when polymer is added to the cement. In addition, calculations indicate that the bonding interactions between the cement and polymer remain stable over the range of strain studied.

Rod, Kenton A. (ORCID:0000000318189094)↗

Hydrated Ordinary Portland Cement as a Carbonic Cement: The Mechanisms, Dynamics, and Implications of Self-Sealing and CO 2 Resistance in Wellbore Cements

This report analyzes the dynamics and mechanisms of the interactions of carbonated brine with hydrated Portland cement. The analysis is based on a recent set of comprehensive reactive-transport simulations, and it relies heavily on the synthesis of the body of work on wellbore integrity that we have conducted for the Carbon Storage Program over the past decade.

54 ENVIRONMENTAL SCIENCES↗

CO{sub 2} reaction with hydrated class H well cement under geologic sequestration conditions: effects of flyash admixtures

The rate and mechanism of reaction of pozzolan-amended Class H cement exposed to both supercritical CO{sub 2} and CO{sub 2}-saturated brine were determined under geologic sequestration conditions to assess the potential impact of cement degradation in existing wells on CO{sub 2} storage integrity. The pozzolan additive chosen, Type F flyash, a by-product of coal combustion, is the most common additive used in cements for well sealing in oil-gas field operations. The 35:65 and 65:35 (v/v) pozzolan-cement blends were exposed to supercritical CO{sub 2} and CO{sub 2}-saturated brine and underwent cement carbonation. Extrapolation of the carbonation rate for the 35:65 case suggests a penetration depth of 170-180 mm for both the CO{sub 2}-saturated brine and supercritical CO{sub 2} after 30 years. Despite alteration in both pozzolan systems, the reacted cement remained relatively impermeable to fluid flow after exposure to brine solution saturated with CO{sub 2}, with values well below the American Petroleum Institute recommended maximum well cement permeability of 200 {mu}D. Analyses of 50:50 pozzolan-cement cores from a production well in a sandstone reservoir exhibited carbonation and low permeability to brine solution saturated with CO{sub 2}, which are consistent with our laboratory findings. 16 refs., 4 figs., 1 tab.

01 COAL, LIGNITE, AND PEAT↗

Structural and chemical changes from CO2 exposure to self-healing polymer cement composites for geothermal wellbores

Wellbore cement is subjected to a number of mechanical, thermal and chemical stress regimes over its lifetime. Therefore, next generation wellbore cement formulations need to be evaluated in conditions relevant to these environments. In this work, we investigate the mechanism of the alteration of a novel self-healing polymer-cement composite recently reported by our group after exposure to a CO2-rich environment by using synchrotron based X-ray Fluorescence (XRF) and X-ray absorption near edge structure (XANES) and scanning electron microscopy coupled with energy dispersive spectroscopy. Results showed that chemical alteration of the polymer-cement follows the rim carbonation mechanism, similar to conventional cement although carbonation takes place to a lesser extent in polymer-cements despite the higher porosity. Along with detailed mechanistic insights on carbonation in polymer-cement composite, the performance of these in CO2-rich environment is further studied using standard compressive strength analysis.

Elbakhshwan, Mohamed↗

Oil-Well Cement and C[subscript 3]S Hydration Under High Pressure as Seen by In Situ X-Ray Diffraction, Temperatures 80[degrees]C with No Additives

The hydration kinetics of a white cement and batches of both Class G and H oil-well cements were examined between 0 and 60 MPa, at {le}80 C, using in situ synchrotron X-ray diffraction. This gives a continuous measure of the C{sub 3}S (Ca{sub 3}SiO{sub 5}), CH (Ca(OH){sub 2}), C{sub 4}AF (Ca{sub 2}FeAlO{sub 5}), ettringite, and other phases in the hydrating slurries. Slurries prepared from single-phase C{sub 3}S; synthetic C{sub 4}AF, and gypsum; and white cement, synthetic C{sub 4}AF and gypsum were also examined. An increasing pressure enhanced the rate of hydration for all slurries. Analysis of the data, using a kinetic model, provided rate constants that were used to obtain activation volumes for C{sub 3}S hydration. For all the cement and C{sub 3}S slurries studied, similar activation volumes were obtained (average {Delta}{double_dagger}{approx}-35 cm{sup 3}/mol), indicating that the presence of cement phases other than C{sub 3}S has a modest influence on the pressure dependence of C{sub 3}S hydration. An alternative analysis, using the time at which 90% of the initial C{sub 3}S remained, gave similar activation volumes. Pressure accelerated the formation of ettringite from synthetic C{sub 4}AF in the presence of gypsum. However, in slurries containing cement, the pressure dependence of C{sub 3}S hydration plays a major role in determining the pressure dependence of ettringite formation.

36 MATERIALS SCIENCE↗

Alkali-activated Class F Fly Ash-rich Portland Cement Blends as Alternative Thermal Shock Resistant Cements

This study focused on evaluating the resistance of 300°C-autocalved alkali-activing Class F fly ash (FAF)-rich Type II Ordinary Portland Cement (OPC) blends with 80/20 and 90/10 FAF/OPC ratios to five thermal-shock (TS) fatigue cycles (one cycle, 600°C heat – 25°C water quenching). The factors to be evaluated included the hydration behaviors, crystalline/ amorphous phaseidentifications, -compositions and -transformations, and microstructural-developments andalterations for blended cements assembled by three different alkaline activators, sodium metasilicate (SMS), soda ash (SA), and sodium sulfate (SS). All factors were related directory to the changes in compressive strength after TS testing. The setting time of cement slurries at 25° and 85°C depended on the alkaline activators; SMS and SA contributing to a strong alkalinity hastened setting, while SS with moderate alkalinity extended the setting time. A more prolonged setting time was observed from non-activated cement. In this case, there were two separated hydration reactions: The first reaction was the hydration of OPC; the second one was associated with the dissolution and pozzolanic activity of FAF. In contrast, all alkali- activated cements engendered the concomitant hydration of OPC and FAF, thereby conferring a higher compressive strength on them than that of the non-activator one. The principal contributor to the development of strength of both the non-activated and activated cements at 300°C was the amorphous NaO 2 - or CaO-Al 2 O 3 - SiO 2 -H 2 O (N,C-A-S-H) phase formed by the interactions between alkaline activator, OPC, and FAF. This phase played an important role in minimizing the loss in strength after TS. On the other hand, adding SMS and SA introduced the mixed crystalline FAF-OPC hydrates, such as garranite and wairakite, as the major phases, into the autoclaved cement bodies. Also, these activators induced the formation of two FAF-related crystalline hydrates, analcime as the major phase and riversidelite (0.9 nm tobermorite) as the minor one. However, these identified phases were sensitive to TS, so converting the major phases into minor phases or vanishment. In contrast, three crystalline phases including calcite and anhydrous sodium sulfate as the major ones and 1.1 nm tobermorite as the minor one, that formed in non-activated and activated cements remained unchanged after TS. Additionally, SAactivated cement revealed porous microstructure created by the incorporation of copious amount of carbonate reaction products into the cement, raising concerns that cements might enhance the rate of water transportation and reduce compressive strength. Nevertheless, TS-insensitive amorphous N,C-A-S-H phase as the major cementitions structure coexisting with TS-insensitive crystalline products were responsible for sustaining the integrity of alkali-activated FAF-rich OPC cement systems in such harsh heat-cooling fatigue environments.

15 GEOTHERMAL ENERGY↗

Guidebook for Using the Tool BEST Cement: Benchmarking and Energy Savings Tool for the Cement Industry

The Benchmarking and Energy Savings Tool (BEST) Cement is a process-based tool based on commercially available efficiency technologies used anywhere in the world applicable to the cement industry. This version has been designed for use in China. No actual cement facility with every single efficiency measure included in the benchmark will likely exist; however, the benchmark sets a reasonable standard by which to compare for plants striving to be the best. The energy consumption of the benchmark facility differs due to differences in processing at a given cement facility. The tool accounts for most of these variables and allows the user to adapt the model to operational variables specific for his/her cement facility. Figure 1 shows the boundaries included in a plant modeled by BEST Cement. In order to model the benchmark, i.e., the most energy efficient cement facility, so that it represents a facility similar to the user's cement facility, the user is first required to input production variables in the input sheet (see Section 6 for more information on how to input variables). These variables allow the tool to estimate a benchmark facility that is similar to the user's cement plant, giving a better picture of the potential for that particular facility, rather than benchmarking against a generic one. The input variables required include the following: (1) the amount of raw materials used in tonnes per year (limestone, gypsum, clay minerals, iron ore, blast furnace slag, fly ash, slag from other industries, natural pozzolans, limestone powder (used post-clinker stage), municipal wastes and others); the amount of raw materials that are preblended (prehomogenized and proportioned) and crushed (in tonnes per year); (2) the amount of additives that are dried and ground (in tonnes per year); (3) the production of clinker (in tonnes per year) from each kiln by kiln type; (4) the amount of raw materials, coal and clinker that is ground by mill type (in tonnes per year); (5) the amount of production of cement by type and grade (in tonnes per year); (6) the electricity generated onsite; and, (7) the energy used by fuel type; and, the amount (in RMB per year) spent on energy. The tool offers the user the opportunity to do a quick assessment or a more detailed assessment--this choice will determine the level of detail of the energy input. The detailed assessment will require energy data for each stage of production while the quick assessment will require only total energy used at the entire facility (see Section 6 for more details on quick versus detailed assessments). The benchmarking tool provides two benchmarks--one for Chinese best practices and one for international best practices. Section 2 describes the differences between these two and how each benchmark was calculated. The tool also asks for a target input by the user for the user to set goals for the facility.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Wellbore cement fracture evolution at the cement–basalt caprock interface during geologic carbon sequestration

Composite Portland cement-basalt caprock cores with fractures, as well as neat Portland cement columns, were prepared to understand the geochemical and geomechanical effects on the integrity of wellbores with defects during geologic carbon sequestration. The samples were reacted with CO2-saturated groundwater at 50 ºC and 10 MPa for 3 months under static conditions, while one cement-basalt core was subjected to mechanical stress at 2.7 MPa before the CO2 reaction. Micro-XRD and SEM-EDS data collected along the cement-basalt interface after 3-month reaction with CO2-saturated groundwater indicate that carbonation of cement matrix was extensive with the precipitation of calcite, aragonite, and vaterite, whereas the alteration of basalt caprock was minor. X-ray microtomography (XMT) provided three-dimensional (3-D) visualization of the opening and interconnection of cement fractures due to mechanical stress. Computational fluid dynamics (CFD) modeling further revealed that this stress led to the increase in fluid flow and hence permeability. After the CO2-reaction, XMT images displayed that calcium carbonate precipitation occurred extensively within the fractures in the cement matrix, but only partially along the fracture located at the cement-basalt interface. The 3-D visualization and CFD modeling also showed that the precipitation of calcium carbonate within the cement fractures after the CO2-reaction resulted in the disconnection of cement fractures and permeability decrease. The permeability calculated based on CFD modeling was in agreement with the experimentally determined permeability. This study demonstrates that XMT imaging coupled with CFD modeling represent a powerful tool to visualize and quantify fracture evolution and permeability change in geologic materials and to predict their behavior during geologic carbon sequestration or hydraulic fracturing for shale gas production and enhanced geothermal systems.

basalt↗

Cement stress and microstructure evolution during curing in semi-rigid high-pressure environments

The process of cement slurry curing into a solid has a direct effect on the initial state of stress in a composite concrete and steel structure. Failure models for critical infrastructure and wellbores could benefit from measurements of this initial stress because it greatly influences structural performance. Here, we present measurements of the initial stress state (total stress, effective stress, and pore pressure) of multiple cement formulations cured under a high-pressure of 40 MPa within a semi-rigid steel pipe. Our results show that cements cured in this restrained environment exhibit dense microstructures with low permeability (nano-Darcy), develop an anisotropic stress state greater than zero and less than the curing pressure, and undergo a staged curing process where hydration and mechanical behaviors evolve from a slurry into a pre-stressed porous medium. Both drained and undrained scenarios were investigated, revealing a feedback from the semi-rigid boundary towards improved cement performance.

36 MATERIALS SCIENCE↗

{sup 13}C chemical shift anisotropies for carbonate ions in cement minerals and the use of {sup 13}C, {sup 27}Al and {sup 29}Si MAS NMR in studies of Portland cement including limestone additions

{sup 13}C isotropic chemical shifts and chemical shift anisotropy parameters have been determined for a number of inorganic carbonates relevant in cement chemistry from slow-speed {sup 13}C MAS or {sup 13}C({sup 1}H) CP/MAS NMR spectra (9.4 T or 14.1 T) for {sup 13}C in natural abundance. The variation in the {sup 13}C chemical shift parameters is relatively small, raising some doubts that different carbonate species in Portland cement-based materials may not be sufficiently resolved in {sup 13}C MAS NMR spectra. However, it is shown that by combining {sup 13}C MAS and {sup 13}C({sup 1}H) CP/MAS NMR carbonate anions in anhydrous and hydrated phases can be distinguished, thereby providing valuable information about the reactivity of limestone in cement blends. This is illustrated for three cement pastes prepared from an ordinary Portland cement, including 0, 16, and 25 wt.% limestone, and following the hydration for up to one year. For these blends {sup 29}Si MAS NMR reveals that the limestone filler accelerates the hydration for alite and also results in a smaller fraction of tetrahedrally coordinated Al incorporated in the C-S-H phase. The latter result is more clearly observed in {sup 27}Al MAS NMR spectra of the cement–limestone blends and suggests that dissolved aluminate species in the cement–limestone blends readily react with carbonate ions from the limestone filler, forming calcium monocarboaluminate hydrate. -- Highlights: •{sup 13}C chemical shift anisotropies for inorganic carbonates from {sup 13}C MAS NMR. •Narrow {sup 13}C NMR chemical shift range (163–171 ppm) for inorganic carbonates. •Anhydrous and hydrated carbonate species by {sup 13}C MAS and {sup 13}C({sup 1}H) CP/MAS NMR. •Limestone accelerates the hydration for alite in Portland – limestone cements. •Limestone reduces the amount of aluminium incorporated in the C-S-H phase.

36 MATERIALS SCIENCE↗

Relationship between operational variables, fundamental physics and foamed cement properties in lab and field generated foamed cement slurries

Foamed cement is a critical component for wellbore stability. The mechanical performance of a foamed cement depends on its microstructure, which in turn depends on the preparation method and attendant operational variables. Determination of cement stability for field use is based on laboratory testing protocols governed by API Recommended Practice 10B-4 (API RP 10B-4, 2015). However, laboratory and field operational variables contrast considerably in terms of scale, as well as slurry mixing and foaming processes. Here in this paper, laboratory and field operational processes are characterized within a physics-based framework. It is shown that the “atomization energy” imparted by the high pressure injection of nitrogen gas into the field mixed foamed cement slurry is – by a significant margin – the highest energy process, and has a major impact on the void system in the cement slurry. There is no analog for this high energy exchange in current laboratory cement preparation and testing protocols. Quantifying the energy exchanges across the laboratory and field processes provides a basis for understanding relative impacts of these variables on cement structure, and can ultimately lead to the development of practices to improve cement testing and performance.

02 PETROLEUM↗