Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Band gap”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

High band gap 2-6 and 3-5 tunneling junctions for silicon multijunction solar cells

A multijunction silicon solar cell of high efficiency is provided by providing a tunnel junction between the solar cell junctions to connect them in series. The tunnel junction is comprised of p+ and n+ layers of high band gap 3-5 or 2-6 semiconductor materials that match the lattice structure of silicon, such as GaP (band gap 2.24 eV) or ZnS (band gap 3.6 eV). Each of which has a perfect lattice match with silicon to avoid defects normally associated with lattice mismatch.

Daud, Taher↗

A theoretical study of heterojunction and graded band gap type solar cells

Heterojunction and graded band gap type solar cells are theoretically investigated. A computer program is developed to account for energy band gap variations and the resulting built-in electric fields which result from heterojunctions and graded energy band gaps. This program is used in studying solar cell operation under various optical irradiation conditions. Results are summarized.

Hauser, J. R.↗

Small band gap superlattices as intrinsic long wavelength infrared detector materials

Intrinsic long wavelength (lambda greater than or equal to 10 microns) infrared (IR) detectors are currently made from the alloy (Hg, Cd)Te. There is one parameter, the alloy composition, which can be varied to control the properties of this material. The parameter is chosen to set the band gap (cut-off wavelength). The (Hg, Cd)Te alloy has the zincblend crystal structure. Consequently, the electron and light-hole effective masses are essentially inversely proportional to the band gap. As a result, the electron and light-hole effective masses are very small (M sub(exp asterisk)/M sub o approx. M sub Ih/M sub o approx. less than 0.01) whereas the heavy-hole effective mass is ordinary size (M sub hh(exp asterisk)/M sub o approx. 0.4) for the alloy compositions required for intrinsic long wavelength IR detection. This combination of effective masses leads to rather easy tunneling and relatively large Auger transition rates. These are undesirable characteristics, which must be designed around, of an IR detector material. They follow directly from the fact that (Hg, Cd)Te has the zincblend crystal structure and a small band gap. In small band gap superlattices, such as HgTe/CdTe, In(As, Sb)/InSb and InAs/(Ga,In)Sb, the band gap is determined by the superlattice layer thicknesses as well as by the alloy composition (for superlattices containing an alloy). The effective masses are not directly related to the band gap and can be separately varied. In addition, both strain and quantum confinement can be used to split the light-hole band away from the valence band maximum. These band structure engineering options can be used to reduce tunneling probabilities and Auger transition rates compared with a small band gap zincblend structure material. Researchers discuss the different band structure engineering options for the various classes of small band gap superlattices.

Smith, Darryl L.↗

Theoretical optimization and parametric study of n-on-p Al/x/Ga/1-x/As-GaAs graded band-gap solar cell

A comprehensive theoretical model of the graded band-gap Al(x)Ga(1-x)As-GaAs solar cell is used to optimize the n-on-p cell. The model includes power losses due to surface, bulk, and junction minority-carrier recombination, series resistance, and photon reflection from an SiO antireflection coating of optimum thickness. The optimized cell has a junction depth/graded band-gap layer thickness of 1.0 micron, respective donor and acceptor concentrations of 4 x 10 to the 17th power and 2 x 10 to the 17th power per cu cm, and a surface AlAs mode fraction of x = 0.35. The optimized graded band-gap cell has an air-mass-zero efficiency of 17.7% (not corrected for a 13% front surface contact area) and is shown to be less sensitive than a similar n-on-p GaAs cell to material degradation in the form of decreased minority-carrier diffusion lengths and increased surface-recombination velocity

Hutchby, J. A.↗

Growth of Wide Band Gap II-VI Compound Semiconductors by Physical Vapor Transport

The studies on the crystal growth and characterization of II-VI wide band gap compound semiconductors, such as ZnTe, CdS, ZnSe and ZnS, have been conducted over the past three decades. The research was not quite as extensive as that on Si, III-V, or even narrow band gap II-VI semiconductors because of the high melting temperatures as well as the specialized applications associated with these wide band gap semiconductors. In the past several years, major advances in the thin film technology such as Molecular Beam Epitaxy (MBE) and Metal Organic Chemical Vapor Deposition (MOCVD) have demonstrated the applications of these materials for the important devices such as light-emitting diode, laser and ultraviolet detectors and the tunability of energy band gap by employing ternary or even quaternary systems of these compounds. At the same time, the development in the crystal growth of bulk materials has not advanced far enough to provide low price, high quality substrates needed for the thin film growth technology.

Su, Ching-Hua↗

Wind tunnel tests of modified cross, hemisflo, and disk-gap-band parachutes with emphasis in the transonic range

Transonic wind-tunnel studies were conducted with modified cross, hemisflo, and disk-gap-band parachute models in the wake of a cone-cylinder shape forebody. The basic cross design was modified with the addition of a circumferential constraining band at the lower edge of the canopy panels. The tests covered a Mach number range of 0.3 to 1.2 and a dynamic pressure range from 479 Newtons per square meter to 5746 Newtons per square meter. The parachute models were flexible textile-type structures and were tethered to a rigid forebody with a single flexible riser. Different size models of the modified cross and disk-gap-band canopies were tested to evaluate scale effects. Model reference diameters were 0.30, 0.61, and 1.07 meters (1.0, 2.0, and 3.5 ft) for the modified cross; and nominal diameters of 0.25 and 0.52 meter (0.83 and 1.7 ft) for the disk-gap-band; and 0.55 meter (1.8 ft) for the hemisflo. Reefing information is presented for the 0.61-meter-diameter cross and the 0.52-meter-diameter disk-gap-band. Results are presented in the form of the variation of steady-state average drag coefficient with Mach number. General stability characteristics of each parachute are discussed. Included are comments on canopy coning, spinning, and fluttering motions.

Foughner, J. T., Jr.↗

Method and apparatus for measuring minority carrier lifetime in a direct band-gap semiconductor

A direct band-gap semiconductor is exposed to intensity-modulated photon radiation having a characteristic energy at least as great as the energy gap of the semiconductor. This produces a time dependent concentration of excess charge carriers through the material, producing a luminescence signal modulated at the same frequency as the incident radiation but shifted in phase by an amount related to the lifetime of minority carriers. In a preferred embodiment, the phase shift of the luminescence signal is determined by transforming it to a modulated electrical signal and mixing the electrical signal with a reference signal modulated at the same frequency and having a phase which is known relative to the incident radiation. Minority carrier lifetime is calculated by integrating a direct current component of the mixed signal (F sub dc) over a 2 pi range in phase of the reference signal.

Vonroos, Oldwig↗

Wind Tunnel Testing of Various Disk-Gap-Band Parachutes

Two Disk-Gap-Band model parachute designs were tested in the NASA Langley Transonic Dynamics Tunnel. The purposes of these tests were to determine the drag and static stability coefficients of these two model parachutes at various subsonic Mach numbers in support of the Mars Exploration Rover mission. The two model parachute designs were designated 1.6 Viking and MPF. These model parachute designs were chosen to investigate the tradeoff between drag and static stability. Each of the parachute designs was tested with models fabricated from MIL-C-7020 Type III or F-111 fabric. The reason for testing model parachutes fabricated with different fabrics was to evaluate the effect of fabric permeability on the drag and static stability coefficients. Several improvements over the Viking-era wind tunnel tests were implemented in the testing procedures and data analyses. Among these improvements were corrections for test fixture drag interference and blockage effects, and use of an improved test fixture for measuring static stability coefficients. The 1.6 Viking model parachutes had drag coefficients from 0.440 to 0.539, while the MPF model parachutes had drag coefficients from 0.363 to 0.428. The 1.6 Viking model parachutes had drag coefficients 18 to 22 percent higher than the MPF model parachute for equivalent fabric materials and test conditions. Model parachutes of the same design tested at the same conditions had drag coefficients approximately 11 to 15 percent higher when manufactured from F-111 fabric as compared to those fabricated from MIL-C-7020 Type III fabric. The lower fabric permeability of the F-111 fabric was the source of this difference. The MPF model parachutes had smaller absolute statically stable trim angles of attack as compared to the 1.6 Viking model parachutes for equivalent fabric materials and test conditions. This was attributed to the MPF model parachutes larger band height to nominal diameter ratio. For both designs, model parachutes fabricated from F-111 fabric had significantly greater statically stable absolute trim angles of attack at equivalent test conditions as compared to those fabricated from MILC-7020 Type III fabric. This reduction in static stability exhibited by model parachutes fabricated from F-111 fabric was attributed to the lower permeability of the F-111 fabric. The drag and static stability coefficient results were interpolated to obtain their values at Mars flight conditions using total porosity as the interpolating parameter.

Cruz, Juan R.↗

Multi Band Gap High Efficiency Converter (RAINBOW)

The RAINBOW multi band gap system represents a unique combination of solar cells, concentrators and beam splitters. RAINBOW is a flexible system which can readily expand as new high efficiency components are developed.

RAINBOW multi band gap system solar cells concentr↗

Band-gap Engineering in Sputter Deposited Amorphous/Microcrystalline Sc(x)Ga(1-x)N

Reactive sputtering was used to grow thin films of Sc(x)Ga(1-x)N with scandium concentrations of 20%-70% on quartz substrates at temperatures of 300-675 K. X-ray diffraction (XRD) of the films showed either weak or no structure, suggesting the films are amorphous or microcrystalline. Optical absorption spectra were taken of each sample and the optical band gap was determined. The band gap varied linearly with increasing Ga concentration between 2.0 and 3.5 eV. Ellipsometry was used to confirm the band gap measurements and provide optical constants in the range 250-1200 nm. ScN and GaN have different crystal structures (rocksalt and wurzite, respectively), and thus may form a heterogeneous mixture as opposed to an alloy. Since the XRD data were inconclusive, bilayers of ScN/GaN were grown and optical absorption spectra taken. A fundamental difference in the spectra between the bilayer films and alloy films was seen, suggesting the films are alloys, not heterogeneous mixtures.

Little, Mark E.↗

InAsSbBi, a direct band-gap, III-V, LWIR material

In the last several years Dr. Stringfellow's group at the University of Utah has reported success in incorporating over 3 percent Bi in InAs and 1.5 percent in InAsSb using Organometallic Vapor Phase Epitaxy (OMVPE) growth techniques. For InAs the lattice constant increase is linear with a=6.058+0.966x (InAs(1-x)Bi(x)), and a decrease in band gap energy of dEg / dx = -55meV / at a percentage Bi. Extrapolating this to the ternary minimum band gap at InAs(0.35)Sb(0.65), an addition of 1 to 2 percent Bi should drop the band gap to the 0.1 to 0.05eV range (10 to 20 microns). These alloys are direct band gap semiconductors making them candidates for far IR detectors. The current status of the InAsSbBi alloys is that good crystal morphology and x ray diffraction data has been obtained for up to 3.4 percent Bi. The Bi is metastable at these concentrations but the OMVPE grown material has been able to withstand the 400 C growth temperature for several hours without phase separation.

Stringfellow, G. B.↗

High efficiency graded band-gap Al/x/Ga/1-x/As-GaAs p-on-n solar cell

A theoretical analysis of p-on-n (p/n) graded band-gap Al/x/Ga/1-x/As-GaAs solar cells including all practical energy loss mechanisms predicts air mass zero efficiencies of 17.3%. The energy losses include those due to spectral reflection, surface, bulk and junction recombination currents, and series resistance. The device consists of a layer of p-type Al/x/Ga/1-x/As 3.5-micron thick on top of an n-type GaAs substrate. The graded band-gap is achieved by decreasing x from 0.35 at the surface to zero at the junction. The same structure without the graded Al concentration, no longer an optimum device, has an efficiency of 10.4%. The primary function of the graded band-gap material is the reduction of surface and bulk recombination losses in the surface layer by a built-in electric field. A comparison of the p/n structure with an optimized n/p structure indicates that the latter has a slightly higher efficiency (17.7%) for assumed minority carrier diffusion lengths and surface recombination velocity.

Hutchby, J. A.↗

The determination of minority carrier lifetimes in direct band-gap semiconductors by monitoring intensity-modulated luminescence radiation

When an extrinsic, direct band-gap semiconductor sample is irradiated by photons of an energy higher than the energy of the band gap between valence and conduction bands, excess electron-hole pairs are generated which, while diffusing through the sample, produce luminescence via radiative recombination. If, furthermore, the intensity of the impinging beam of photons is modulated sinusoidally, the luminescence radiation escaping from the sample will be phase shifted with respect to the original photon beam in a characteristic way. It will be shown that by measuring the phase shift at different modulation frequencies, the Shockley-Read-Hall lifetime of minority carriers may be ascertained. The method is nondestructive inasmuch as there is no need to fabricate p-n junctions or Ohmic contacts, nor is it necessary to remove already existing Ohmic contacts of angle lap the surface, etc., procedures often needed when determining lifetimes with the scanning electron microscope (in which case a p-n junction must be present).

Von Roos, O.↗

High-Power Fiber Lasers Using Photonic Band Gap Materials

High-power fiber lasers (HPFLs) would be made from photonic band gap (PBG) materials, according to the proposal. Such lasers would be scalable in the sense that a large number of fiber lasers could be arranged in an array or bundle and then operated in phase-locked condition to generate a superposition and highly directed high-power laser beam. It has been estimated that an average power level as high as 1,000 W per fiber could be achieved in such an array. Examples of potential applications for the proposed single-fiber lasers include welding and laser surgery. Additionally, the bundled fibers have applications in beaming power through free space for autonomous vehicles, laser weapons, free-space communications, and inducing photochemical reactions in large-scale industrial processes. The proposal has been inspired in part by recent improvements in the capabilities of single-mode fiber amplifiers and lasers to produce continuous high-power radiation. In particular, it has been found that the average output power of a single strand of a fiber laser can be increased by suitably changing the doping profile of active ions in its gain medium to optimize the spatial overlap of the electromagnetic field with the distribution of active ions. Such optimization minimizes pump power losses and increases the gain in the fiber laser system. The proposal would expand the basic concept of this type of optimization to incorporate exploitation of the properties (including, in some cases, nonlinearities) of PBG materials to obtain power levels and efficiencies higher than are now possible. Another element of the proposal is to enable pumping by concentrated sunlight. Somewhat more specifically, the proposal calls for exploitation of the properties of PBG materials to overcome a number of stubborn adverse phenomena that have impeded prior efforts to perfect HPFLs. The most relevant of those phenomena is amplified spontaneous emission (ASE), which causes saturation of gain and power at undesirably low levels, and scattering of light from dopants. In designing a given fiber laser for reduced ASE, care must be taken to maintain a correct fiber structure for eventual scaling to an array of many such lasers such that the interactions among all the members of the array would cause them to operate in phase lock. Hence, the problems associated with improving a single-fiber laser are not entirely separate from the bundling problem, and some designs for individual fiber lasers may be better than others if the fibers are to be incorporated into bundles. Extensive calculations, expected to take about a year, must be performed in order to determine design parameters before construction of prototype individual and fiber lasers can begin. The design effort can be expected to include calculations to optimize overlaps between the electromagnetic modes and the gain media and calculations of responses of PBG materials to electromagnetic fields. Design alternatives and physical responses that may be considered include simple PBG fibers with no intensity-dependent responses, PBG fibers with intensity- dependent band-gap shifting (see figure), and broad-band pumping made possible by use of candidate broad-band pumping media in place of the air or vacuum gaps used in prior PBG fibers.

DiDomenico, Leo↗

The growth of low band-gap InAs on (111)B GaAs substrates

The use of low band-gap materials is of interest for a number of photovoltaic and optoelectronic applications, such as bottom cells of optimized multijunction solar cell designs, long wavelength light sources, detectors, and thermophotovoltaics. However, low band-gap materials are generally mismatched with respect to lattice constant, thermal expansion coefficient, and chemical bonding to the most appropriate commercially available substrates (Si, Ge, and GaAs). For the specific case of III-V semiconductor heteroepitaxy, one must contend with the strain induced by both lattice constant mismatch at the growth temperature and differences in the rates of mechanical deformation during the cool down cycle. Several experimental techniques have been developed to minimize the impact of these phenomena (i.e., compositional grading, strained layer superlattices, and high-temperature annealing). However, in highly strained systems such as InAs-on-GaAs, three-dimensional island formation and large defect densities (greater than or equal to 10(exp 8)/ cm(exp -2)) tend to limit their applicability. In these particular cases, the surface morphology and defect density must be controlled during the initial stages of nucleation and growth. At the last SPRAT conference, we reported on a study of the evolution of InAs islands on (100) and (111)B GaAs substrates. Growth on the (111)B orientation exhibits a number of advantageous properties as compared to the (100) during these early stages of strained-layer epitaxy. In accordance with a developing model of nucleation and growth, we have deposited thin (60 A - 2500 A), fully relaxed InAs films on (111)B GaAs substrates. Although thicker InAs films are subject to the formation of twin defects common to epitaxy on the (111)B orientation, appropriate control of the growth parameters can greatly minimize their density. Using this knowledge base, InAs films up to 2 microns in thickness with improved morphology and structural quality have been grown on (111)B GaAs substrates, thereby enabling the measurement of electronic and optical properties.

Welser, R. E.↗

Theoretical analysis of Al/x/Ga/1-x/As-GaAs graded band-gap solar cell

A practical theoretical analysis of an n/p graded band-gap Al(x)Ga(1-x)As-GaAs solar cell indicates that the presence of a built-in electric field acting on holes in the surface layer increases the hole collection efficiency of a nearly optimum cell to a maximum of 97.8%. The electric field is created by the band-gap gradient and serves to reduce the surface hole recombination by 97% and reduce the bulk hole recombination by 80%, compared to a similar GaAs cell. These reduced losses increase cell response substantially for wavelengths less than 0.59 micron and yield a maximum air-mass-zero efficiency of 17.7% (not corrected for a 13% front-surface contact). The model includes an optimized antireflection coating, series resistance, and junction-recombination current.

Hutchby, J. A.↗

Energy Band Gap, Intrinsic Carrier Concentration and Fermi Level of CdTe Bulk Crystal between 304 K and 1067 K

Optical transmission measurements were performed on CdTe bulk single crystal. It was found that when a sliced and polished CdTe wafer was used, a white film started to develop when the sample was heated above 530 K and the sample became opaque. Therefore, a bulk crystal of CdTe was first grown in the window area by physical vapor transport; the optical transmission was then measured and from which the energy band gap was derived between 304 and 1067 K. The band gaps of CdTe can be fit well as a function of temperature using the Varshini expression: Eg (e V) = 1.5860 - 5.9117xl0(exp -4) T(sup 2)/(T + 160). Using the band gap data, the high temperature electron-hole equilibrium was calculated numerically by assuming the Kane's conduction band structure and a heavy-hole parabolic valance band. The calculated intrinsic carrier concentrations agree well with the experimental data reported previously. The calculated intrinsic Fermi levels between 270 and 1200 K were also presented.

Su, Ching-Hua↗