Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ash Corrosion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Coal Ash Corrosion Resistant Materials Testing

In April 1999, three identical superheater test sections were installed into the Niles Unit No.1 for the purpose of testing and ranking the coal ash corrosion resistance of candidate superheater alloys. The Niles boiler burns high sulfur coal (3% to 3.5%) that has a moderate alkali content (0.2% sodium equivalents), thus the constituents necessary for coal ash corrosion are present in the ash. The test sections were controlled to operate with an average surface metal temperature from approximately 1060 F to 1210 F which was within the temperature range over which coal ash corrosion occurs. Thus, this combination of aggressive environment and high temperature was appropriate for testing the performance of candidate corrosion-resistant tube materials. Analyses of the deposit and scale confirmed that aggressive alkali sulfate constituents were present at the metal surface and active in tube metal wastage. The test sections were constructed so that the response of twelve different candidate tube and/or coating materials could be studied. The plan was to remove and evaluate one of the three test sections at time intervals of 1 year, 3 years, and 5 years. This would permit an assessment of performance of the candidate materials as a function of time. Test Section A was removed in November 2001 after about 24 months of service at the desired steam temperature set point, with about 15.5 months of exposure at full temperature. A progress report, issued in October 2002, was written to document the performance of the candidate alloys in that test section. The evaluation described the condition of each tube sample after exposure. It involved a determination of the rate of wall thickness loss for these samples. In cases where there was more than one sample of a candidate material in the test section, an assessment was made of the performance of the alloy as a function of temperature. Test Sections B and C were examined during the November 2001 outage, and it was decided that, due to excessive wastage, certain tube samples needed to be removed and replaced in order to ensure that Test Sections B and C would have a chance of remaining in the boiler for their intended exposure period. These suspect tube samples were replaced and the two remaining test sections were put back into service. The tube samples that were removed from Test Sections B and C were set aside for later analysis at the end of the planned exposure period. Test Sections B and C were again examined approximately six months later. At that time, measured wall thickness losses raised concerns about additional tube samples. These suspect samples were also removed, set aside for later analysis, and replaced. The test sections then went back into service until the end of the second exposure period, which was concluded in May 2003 when, due to evidence of excessive wastage, the valves were opened increasing cooling steam flow and thereby effectively stopping corrosion. In August 2003, Test Sections B and C were removed for closer examination. Section C had experienced about 42 months of service at the desired team temperature set point with 28.5 months at temperature at full temperature. Additional suspect samples were removed from Test Section B, then, it was re-installed into the boiler (at the location originally occupied by Section C), where it remained in service until the end of the program. Due to this removal history, the samples from Test Section B had a total service duration that varied from a minimum of 15.5 months (for samples that performed poorly) to 37 months for samples the survived for the full intended service exposure for Section B. The figure below shows a schematic of Test Section B and indicates the length of service exposure for different locations. This report provides the results of the evaluation of Test Section B, including the samples that remained in the Test Section for the full exposure period as well as those that were removed early. This report also is intended to compare and summarize the results for all three test sections. The analysis of Test Section B followed much the same protocol that was employed in the assessment of the other two test sections. The focus was on determining and documenting the relative corrosion rates of the candidate materials; however, additional investigations were undertaken to better understand the wastage mechanism, and to characterize how selected candidate materials performed either well, or poorly, in the severe coal ash corrosion environment in the convection pass of Niles Unit No.1. The detailed results of the investigation are included in this report as a series of twelve appendices. Each appendix is devoted to the performance of one of the candidate alloys. The table below summarizes metal loss rate for the worst case sample of each of the candidate materials in all three test sections. The body of this report compares these for all of the samples in the test section.

01 COAL, LIGNITE, AND PEAT↗

Recovery Boiler Superheater Ash Corrosion Field Study

With the trend towards increasing the energy efficiency of black liquor recovery boilers operated in North America, there is a need to utilize superheater tubes with increased corrosion resistance that will permit operation at higher temperatures and pressures. In an effort to identify alloys with improved corrosion resistance under more harsh operating conditions, a field exposure was conducted that involved the insertion of an air-cooled probe, containing six candidate alloys, into the superheater section of an operating recovery boiler. A metallographic examination, complete with corrosion scale characterization using EMPA, was conducted after a 1,000 hour exposure period. Based on the results, a ranking of alloys based on corrosion performance was obtained.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Effects of Chlorine in Ash on the Corrosion Performance of Ni-Based Alloys in a Simulated Oxy-Fuel Environment

Coal ash can severely attack alloy materials at high temperature. To understand coal ash corrosion, a critical study is needed to determine the effect of the elements in ash on corrosion and find an approach to reduce the corrosion rates in an ash environment at high temperature. Chlorine is a harmful element in coal. The role of chlorine in ash corrosion is investigated in simulated oxy-fuel environments. Long time tests up to 3000 hours were performed on various structural alloys at 750°C. Detailed results are presented on weight change, scale thickness, internal penetration, microstructural characteristics of corrosion products, and the cracking of scales for the alloys after exposure at 750°C for 3000h. In addition, we performed synchrotron nanobeam Furthermore X-ray analysis to study the phase and chemical composition of the oxide layers on the alloy surface. Results from these studies are used to address the role of chlorine in ash in the long-term corrosion performance of alloys. Nanobeam X-ray and SEM analyses indicate that chlorine can modify the diffusion mechanism near alloy surface, and increase corrosion rate.

01 COAL, LIGNITE, AND PEAT↗

Effects of calcium in ash on the corrosion performance of Ni-based alloys in simulated oxy-fuel environment

Increasing the efficiency of coal power plants requires raising the operating temperature above 650°C. However, coal ash can severely attack alloy materials at high temperature. For example, the corrosion rates of commercial Fe- and Ni-based alloys are generally greater than 2 mm/year at 750°C in the gas environment of oxy-fuel combustion. Thus, a critical study is needed to determine the effect of the constituents in the ash on corrosion and find an approach to reduce the corrosion rates in an ash-laden environment at high temperature. The role of CaO in the ash (typical of U.S. Western coal ash) has been investigated in laboratory exposure environments with various structural alloys. Detailed results are presented on weight change, scale thickness, internal penetration, microstructural characteristics of corrosion products, and the cracking of scales for the alloys after exposure at 750°C. The thermal stability of K3Al(SO4)3 under the environment of oxy-fuel combustion was determined by thermogravimetric analysis and differential thermal analysis. The reaction of this low melting temperature salt with the CaO-containing ash is discussed. In addition, we performed synchrotron nanobeam X-ray analysis to study the phase and chemical composition of the oxide layers on the alloy surface. Results from these studies are used to address the role of CaO in ash in the long-term corrosion performance of alloys.

36 MATERIALS SCIENCE↗

Fireside Corrosion

Oxy-fuel fireside research goals are: (1) determine the effect of oxyfuel combustion on fireside corrosion - flue gas recycle choice, staged combustion ramifications; and (2) develop methods to use chromia solubility in ash as an ash corrosivity measurement - synthetic ashes at first, then boiler and burner rig ashes.

36 MATERIALS SCIENCE↗

Fireside Corrosion USC Steering

Oxy-Fuel Fireside Research goals are: (1) Determine the effect of oxy-fuel combustion on fireside corrosion - (a) Flue gas recycle choice, Staged combustion ramifications, (c) JCOAL Collaboration; and (2) Develop methods to use chromia solubility in ash as an 'ash corrosivity' measurement - (a) Synthetic ashes at first, then boiler and burner rig ashes, (b) Applicable to SH/RH conditions.

36 MATERIALS SCIENCE↗

Co-firing coal and municipal solid waste

The aim of this study was to experimentally investigate how different the organic fraction of municipal solid waste (OFMSW) or municipal solid waste (MSW) utilizing strategies affects the gas emission in simple fluidized bed combustion (FBC) of biomass. In this study, ground OFMSW and pulverized coal (PC) were used for co-firing tests. The tests were carried out in a bench-scale bubbling FBC. Coal and bio-waste fuels are quite different in composition. Ash composition of the bio-waste fuels is fundamentally different from ash composition of the coal. Chlorine (Cl) in the MSW may affect operation by corrosion. Ash deposits reduce heat transfer and also may result in severe corrosion at high temperatures. Nitrogen (N) and carbon ) assessments can play an important role in a strategy to control carbon dioxide (CO{sub 2}) and nitrogen oxide (NOx) emissions while raising revenue. Regulations such as subsidies for oil, liquid petroleum gas (LPG) for natural gas powered vehicles, and renewables, especially biomass lines, to reduce emissions may be more cost-effective than assessments. Research and development (RD) resources are driven by energy policy goals and can change the competitiveness of renewables, especially solid waste. The future supply of co-firing depends on energy prices and technical progress, both of which are driven by energy policy priorities.

01 COAL, LIGNITE, AND PEAT↗

Development of Creep-Resistant, Alumina-Forming Ferrous Alloys for High-Temperature Structural Use

This paper overviews recent advances in developing novel alloy design concepts of creep-resistant, alumina-forming Fe-base alloys, including both ferritic and austenitic steels, for high-temperature structural applications in fossil-fired power generation systems. Protective, external alumina-scales offer improved oxidation resistance compared to chromia-scales in steam-containing environments at elevated temperatures. Alloy design utilizes computational thermodynamic tools with compositional guidelines based on experimental results accumulated in the last decade, along with design and control of the second-phase precipitates to maximize high-temperature strengths. The alloys developed to date, including ferritic (Fe-Cr-Al-Nb-W base) and austenitic (Fe-Cr-Ni-Al-Nb base) alloys, successfully incorporated the balanced properties of steam/water vapor-oxidation and/or ash-corrosion resistance and improved creep strength. Development of cast alumina-forming austenitic (AFA) stainless steel alloys is also in progress with successful improvement of higher temperature capability targeting up to ~1100°C. Current alloy design approach and developmental efforts with guidance of computational tools were found to be beneficial for further development of the new heat resistant steel alloys for various extreme environments.

Yamamoto, Yukinori↗

Development of Self-Powered Wireless-Ready High Temperature Electrochemical Sensors for In-Situ Corrosion Monitoring for Boiler Tubes in Next Generation Coal-based Power Systems

The key innovation of this project is the synergy of the high temperature sensor technology based on the science of electrochemical measurement and state-of-the-art wireless communication technology. A novel self-powered wireless high temperature electrochemical sensor system has been developed for coal-fired boilers used for power generation. An initial prototype of the in-situ sensor demonstrated the capability of the wireless communication system in the laboratory and in a pilot plant (Industrial USC Boiler Setting) environment to acquire electrochemical potential and current signals during the corrosion process. Uniform and localized under-coal ash deposit corrosion behavior of Inconel 740 superalloy has been studied at different simulated coal ash hot corrosion environments using the developed sensor. Two typical potential noise patterns were found to correlate with the oxidation and sulfidation stages in the hot coal ash corrosion process. Two characteristic current noise patterns indicate the extent of the corrosion. There was a good correlation between the responses of electrochemical test data and the results from corroded surface analysis. Wireless electrochemical potential and current noise signals from a simulated coal ash hot corrosion process were concurrently transmitted and recorded. The results from the performance evaluation of the sensor confirm a high accuracy in the thermodynamic and kinetic response represented by the electrochemical noise and impedance test data.

47 OTHER INSTRUMENTATION↗

Superheater Tube Corrosion in Wood Gasifier Ash Deposits

The upper operating temperature of tubes in heat exchangers/steam generators is strongly influenced by the degradation that can occur because of the reaction of the exchanger/generator tubing with the deposits that accumulate on the surface of the tubes. In fact, severe corrosion has been observed in some biomass fired systems, particularly with elevated potassium and chlorine concentrations in the deposits. Wood gasifiers have recently been and are currently being constructed at several sites in North America. In these systems, the syngas is burned to produce steam and the performance of the heat exchanger tubes under ash deposits is of great concern. As temperatures of the heat exchangers are increased in an effort to increase their operating efficiency, the performance of the tubes is of greater interest. The corrosion behavior of alloy steel tubes as a function of temperature has been investigated by exposing samples of selected alloys to ash collected from the steam generator fired by syngas produced in wood gasifiers. This study compares corrosion rates from laboratory exposures of synthesis gas and ash at 500 C and 600 C. This study investigated the material performance of four ferritic steels and one austenitic steel exposed to conditions expected on the fireside of a wood gasifier. The purpose of this study was to identify an effective method for determining material performance for samples exposed to both the process gas and the fly ash that is typically observed within the steam generator for times up to 1000 hours. Mass changes were measured for all of the samples, but this information can be misleading concerning material performance due to the difficulty in sufficiently cleaning the samples after exposure in the ash. Therefore, small cross sections of the samples were collected and imaged using optical microscopy. Oxide thicknesses were measured along with metal losses. The metal loss information provides a clear indication of material performance. The metal loss rates for the ferritic steels at 500 C were almost half of those observed at 600 C and the rates decreased with increasing exposure time. It was also reported that the metal loss rates generally decrease with increasing chromium concentration.

09 BIOMASS FUELS↗

Corrosion Performance of Fe-Based Alloys in Simulated Oxy-Fuel Environment

The long-term corrosion of Fe-based alloys in simulated oxy-fuel environment at 1023 K (750 A degrees C) was studied. Detailed results are presented on weight change, scale thickness, internal penetration, microstructural characteristics of the corrosion products, and the cracking of scales for the alloys after exposure at 1023 K (750 A degrees C) for up to 3600 hours. An incubation period during which the corrosion rate was low was observed for the alloys. After the incubation period, the corrosion accelerated, and the corrosion process followed linear kinetics. Effects of alloy, CaO-containing ash, and gas composition on the corrosion rate were also studied. In addition, synchrotron nanobeam X-ray analysis was employed to determine the phase and chemical composition of the oxide layers on the alloy surface. Results from these studies are being used to address the long-term corrosion performance of Fe-based alloys in various coal-ash combustion environments and to develop methods to mitigate high-temperature ash corrosion.

36 MATERIALS SCIENCE↗

Role of carbon treating in piperazine oxidation

Bench-scale experiments were performed to test the effects of carbon treating (8 × 30 mesh, lignite-based granular activated carbon from Nowata Filtration) on the oxidation of aqueous piperazine (PZ) at conditions of CO 2 capture. The combined mitigation with carbon treating and N 2 sparging was also tested. When carbon treating is applied, the UV–Vis absorbance at 320 nm, the NH 3 production rate, and the accumulation rate of dissolved Fe concentration and total formate concentration decrease. The effects of carbon treating last even when the carbon is bypassed, which is possibly due to the removal of catalytic degradation products. Therefore, it is better to apply carbon treating in the early stages of oxidation. Combining carbon treating and nitrogen sparging is more effective in oxidation mitigation than applying the methods separately. The amount of Fe removed by the carbon bed is greater than the result calculated from the solvent inventory and concentration difference of Fe in solvent, indicating that Fe colloids or other “soluble” Fe will dissolve into the solvent and replace the dissolved Fe that is adsorbed and removed. Furthermore, the carbon removes the degradation products that can complex with Fe 3+ , even if they are not complexed. Since the source of Fe includes fly ash and corrosion, removing the complexing agents instead of all the available Fe is a more feasible target.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗