Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “As-S”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Biogenic formation of As-S nanotubes by diverse Shewanella strains

Shewanella sp. strain HN-41 was previously shown to produce novel, photoactive, As-S nanotubes via the reduction of As(V) and S2O3 2* under anaerobic conditions. To determine if this ability was unique to this bacterium, 10 different Shewanella strains, including Shewanella sp. strain HN-41, Shewanella sp. strain PV-4, Shewanella alga BrY, Shewanella amazonensis SB2B, Shewanella denitrificans OS217, Shewanella oneidensis MR-1, Shewanella putrefaciens CN-32, S. putrefaciens IR-1, S. putrefaciens SP200, and S. putrefaciens W3-6-1, were examined for production of As-S nanotubes under standardized conditions. Of the 10 strains examined, three formed As-S nanotubes like those of strain HN-41. While Shewanella sp. strain HN-41 and S.putrefaciens CN-32 rapidly formed As-S precipitates in 7 days, strains S. alga BrY and S. oneidensis MR-1 reduced As(V) at a much lower rate and formed yellow As-S after 30 days. Electron microscopy, energy-dispersive X-ray spectroscopy, and extended X-ray absorption fine-structure spectroscopy analyses showed that the morphological and chemical properties of As-S formed by strains S. putrefaciens CN-32, S. alga BrY, and S. oneidensis MR-1 were similar to those previously determined for Shewanella sp. strain HN-41 As-S nanotubes. These studies indicated that the formation of As-S nanotubes is widespread among Shewanella strains and is closely related to bacterial growth and the reduction rate of As(V) and thiosulfate.

DESULFOTOMACULUM AURIPIGMENTUM↗

Compositional trends of γ-induced optical changes observed in chalcogenide glasses of binary As-S system

Compositional trends of γ-induced optical changes in chalcogenide glasses are studied with the binary As-S system. Effects of γ-irradiation and annealing are compared using the changes measured in the fundamental optical absorption edge region. It is shown that annealing near the glass transition temperature leads to bleaching of As-S glasses, while γ-irradiation leads to darkening; both depend on the glass composition and thermal history of the specimens. These results are explained in terms of competitive destruction–polymerization transformations and physical aging occurring in As-S chalcogenide glasses under the influence of γ-irradiation.

Chalcogenide glasses↗

Thermal and Gamma-ray induced relaxation in As-S glasses: modeling and experiment

Enthalpy relaxation is measured in a series of As-S glasses irradiated with gamma rays and these samples are compared with a set of identical control samples kept in the dark. It is shown that gamma irradiation lifts the kinetic barrier for relaxation at room temperature and speeds up the enthalpy release. The measured values of thermal relaxation in the dark agree closely with modeling results obtained by fitting differential scanning calorimetry curves with the TNM equations. The measured values of activation energy for enthalpy relaxation are also in close agreement with that predicted by the TNM model therefore lending credence to the fitting results. These measurements permit extraction of the effect of gamma irradiation on the glass structure for a series of As-S glasses with increasing structural coordination, and gamma irradiation is shown to reduce the structural relaxation time. It is also shown that lower coordination glasses exhibit greater radiation sensitivity but also greater thermal relaxation due to their lower Tg. On the other end, over-coordinated glasses show lower relaxation and almost no radiation sensitivity. This behavior is similar to the glass response under sub-bandgap light irradiation.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Gamma Radiation Effects on Physical, Optical, and Structural Properties of Binary As-S glasses

Gamma radiation induces changes in physical, optical, and structural properties in chalcogenide glasses., Previous research has focused on As{sub 2}S{sub 3} and families of glasses containing Ge. For the first time, we present composition and dose dependent data on the As-S binary glass series. Binary As{sub x}S{sub 100-x} (x = 30, 33, 36, 40, and 42) glasses were irradiated with gamma radiation using a {sup 60}Co source at 2.8 Gy/s to accumulated doses of 1, 2, 3, and 4 MGy. The irradiated samples were characterized at each dose level for density, refractive index, x-ray diffraction, and Raman spectrum. These results are compared to those of as-made and 1 year aged samples. We report an initial increase in density followed by a decrease as a function of dose that contradicts the expected compositional dependence of molar volume of these glasses. This unusual behavior is explained based on microvoid formation and nanoscale phase-separation induced by the irradiation in these glasses. XRD, Raman, and EPR data provide supporting evidence, underscoring the importance of optimally- or overly-constrained structures for stability under aging or irradiation.

36 MATERIALS SCIENCE↗

Photostructural reconstructions of As-S and As-Se semiconductor glasses

The results of experimental investigation of photoinduced changes in optical properties of semiconductor glasses of the As-Se and As-S systems are presented. With using the data of the Moessbauer emission spectroscopy on the {sup 129}Te({sup 129}I) isotope, the observed changes in optical properties can be attributed to the reconstruction of the glass matrix under the effect of radiation.

36 MATERIALS SCIENCE↗

RADIATION EFFECTS IN PHYSICAL AGING OF BINARY As-S AND As-Se GLASSES

Radiation-induced physical aging effects are studied in binary AsxS100-x and AsxSe100-x (30 ≤ x ≤ 42) glasses by conventional differential scanning calorimetry (DSC) method. It is shown that γ-irradiation (Co60 source, ~ 3 MGy dose) of glassy AsxS100-x caused a measurable increase in glass transition temperature and endothermic peak area in the vicinity of glass transition region, which was associated with acceleration of structural relaxation processes in these materials. In contrast to sulfide glasses, the samples of As-Se family did not exhibit any significant changes in DSC curves after γ-irradiation. The observed difference in radiation-induced physical aging between sulfides and selenides was explained by more effective destruction-polymerization transformations and possible metastable defects formation in S-based glassy network.

36 MATERIALS SCIENCE↗

Biogenic formation of photoactive arsenic-sulfide nanotubes by Shewanella sp. strain HN-41

Microorganisms facilitate the formation of a wide range of minerals that have unique physical and chemical properties as well as morphologies that are not produced by abiotic processes. Here, we report the production of an extensive extracellular network of filamentous, arsenic-sulfide (As-S) nanotubes (20–100 nm in diameter by 30 µm in length) by the dissimilatory metal-reducing bacterium Shewanella sp. HN-41. The As-S nanotubes, formed via the reduction of As(V) and S2O, were initially amorphous As2S3 but evolved with increasing incubation time toward polycrystalline phases of the chalcogenide minerals realgar (AsS) and duranusite (As4S). Upon maturation, the As-S nanotubes behaved as metals and semiconductors in terms of their electrical and photoconductive properties, respectively. The As-S nanotubes produced by Shewanella may provide useful materials for novel nano- and opto-electronic devices.

36 MATERIALS SCIENCE↗

Bonded Paths and van der Waals Interactions in Orpiment, As2S3

Bond critical properties and bond paths have been calculated for the thioarsenide molecular crystal orpiment, As2S3. In addition to the intramolecular As-S bond paths and van der Waals As-S and S-S bond paths within the layers, intermolecular S-S, As-S and As-As van der Waals paths exist between the layers. The S-S bond paths between the layers are identified with the main interlayer restoring forces responsible for the vibrational internal-mode splitting and the low frequency rigid layer modes previously documented in infrared and Raman studies of orpiment. These S-S bond paths are comparable with those calculated for orthorhombic native sulfur and the As4Sn (n = 3,4,5) molecules for several arsenide molecular crystals. The As-S bond paths show that the two nonequivalent arsenic atoms are each coordinated by a highly distorted octahedral array of sulfur atoms. The octahedra consist of three As-S intramolecular bonded interactions and three longer van der Waals interactions (two intramolecular and one intermolecular). One of the arsenic atoms is also coordinated by an arsenic atom in an interlayer As-As bonded interaction. Laplacian isosurface envelopes calculated for the arsenic and sulfur atoms are comparable with those calculated for native arsenic and orthorhombic sulfur. The intermolecular As-S bond paths connect Lewis acid domains on arsenic and an Lewis base domains on sulfur. Van der Waals interactions are traditionally defined as attractive interactions other than those ascribed to bond formation. However, theoretical evidence and arguments, as well as the connection between the bond paths and the vibrational spectra, indicate that the van der Waals interactions in orpiment are directed bonded interactions in the Slater sense. The experimental bond lengths for the As-S and S-S bonded interactions decrease nonlinearly with the increasing value of the electron density at the bond critical point, concomitant with a decrease in the bonded radii of arsenic and sulfur. On the basis of the local energy density, the intramolecular As-S bonded interactions classify as shared interactions and the intramolecular and intermolecular As-S and S-S bonded interactions and the intermolecular As-As van der Waals interactions classify as closed-shell interactions. The so called planar lone electron pair micelle picture for orpiment is spanned by bond paths, substantiating the claim that the layers in the orpiment structure are linked by weak van der Waals bonded interactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thioarsenides: A case for long-range Lewis acid-base-directed van der Waals interactions

Electron density distributions, bond paths, Laplacian and local energy density properties have been calculated for a number of As4Sn (n = 3,4,5) thioarsenide molecular crystals. On the basis of the distributions, the intramolecular As-S and As-As interactions classify as shared bonded interactions and the intermolecular As-S, As-As and S-S interactions classify as closed-shell van der Waals bonded interactions. The bulk of the intermolecular As-S bond paths link regions of locally concentrated electron density (Lewis base regions) with aligned regions of locally depleted electron density (Lewis acid regions) on adjacent molecules. The paths are comparable with intermolecular paths reported for several other molecular crystals that link aligned Lewis base and acid regions in a key-lock fashion, interactions that classified as long range Lewis acid-base directed van der Waals interactions. As the bulk of the intermolecular As-S bond paths (~70%) link Lewis acid-base regions on adjacent molecules, it appears that molecules adopt an arrangement that maximizes the number of As-S Lewis acid-base intermolecular bonded interactions. The maximization of the number of Lewis acid-base interactions appears to be connected with the close-packed array adopted by molecules: distorted cubic close-packed arrays are adopted for alacránite, pararealgar, uzonite, realgar and β-AsS and the distorted hexagonal close-packed arrays adopted by α- and β-dimorphite. A growth mechanism is proposed for thioarsenide molecular crystals from aqueous species that maximizes the number of long range Lewis acid-base vdW As-S bonded interactions with the resulting directed bond paths structuralizing the molecules as a molecular crystal.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A comparative study of the atomic structures of Ge-doped As 4 S 3 and P 4 Se 3 molecular glasses

The structures of pseudo-binary P-Se and As-S glasses with compositions close to the P 4 Se 3 and As 4 S 3 stoichiometry with a few atom %Ge doping were determined using Monte Carlo simulations constrained by density and x-ray scattering measurements. We find that these glasses consist predominantly of P 4 Se 3 and As 4 S 3 molecules. The Ge doping results in some important differences between the two glasses. The P-Se glass displays significantly higher intermolecular connectivity via P-Se-Ge linkages, consistent with the significantly higher glass transition temperature and lower fragility of this liquid compared to its As-S counterpart. We also speculate that a consequence of this difference in the intermolecular connectivity would be to delay any pressure induced conversion from a molecular to a network structure for the Ge doped P-Se glass compared to the Ge-doped As-S glass.

36 MATERIALS SCIENCE↗

SAR optimization studies on modified salicylamides as a potential treatment for acute myeloid leukemia through inhibition of the CREB pathway

Disruption of cyclic adenosine monophosphate response element binding protein (CREB) provides a potential new strategy to address acute leukemia, a disease associated with poor prognosis, and for which conventional treatment options often carry a significant risk of morbidity and mortality. In this paper, we describe the structure-activity relationships (SAR) for a series of XX-650-23 derived from naphthol AS-E phosphate that disrupts binding and activation of CREB by the CREB-binding protein (CBP). Through the development of this series, we identified several salicylamides that are potent inhibitors of acute leukemia cell viability through inhibition of CREB-CBP interaction. Among them, a biphenyl salicylamide, compound 71, was identified as a potent inhibitor of CREB-CBP interaction with improved physicochemical properties relative to previously described derivatives of naphthol AS-E phosphate.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Exploring the in vitro formation of trimethylarsine sulfide from dimethylthioarsinic acid in anaerobic microflora of mouse cecum using HPLC-ICP-MS and HPLC-ESI-MS

Although metabolism of arsenicals to form methylated oxoarsenical species has been extensively studied, less is known about the formation of thiolated arsenical species that have recently been detected as urinary metabolites. Indeed, their presence suggests that the metabolism of ingested arsenic is more complex than previously thought. Recent reports have shown that thiolated arsenicals can be produced by the anaerobic microflora of the mouse cecum, suggesting that metabolism prior to systemic absorption may be a significant determinant of the pattern and extent of exposure to various arsenic-containing species. Here, we examined the metabolism of {sup 34}S labeled dimethylthioarsinic acid ({sup 34}S-DMTA{sup V}) by the anaerobic microflora of the mouse cecum using HPLC-ICP-MS and HPLC-ESI-MS/MS to monitor for the presence of various oxo- and thioarsenicals. The use of isotopically enriched {sup 34}S-DMTA{sup V} made it possible to differentiate among potential metabolic pathways for production of the trimethylarsine sulfide (TMAS{sup V}). Upon in vitro incubation in an assay containing anaerobic microflora of mouse cecum, {sup 34}S-DMTA{sup V} underwent several transformations. Labile {sup 34}S was exchanged with more abundant {sup 32}S to produce {sup 32}S-DMTA{sup V}, a thiol group was added to yield DMDTA{sup V}, and a methyl group was added to yield {sup 34}S-TMAS{sup V}. Because incubation of {sup 34}S-DMTA{sup V} resulted in the formation of {sup 34}S-TMAS{sup V}, the pathway for its formation must preserve the arsenic-sulfur bond. The alternative metabolic pathway postulated for formation of TMAS{sup V} from dimethylarsinic acid (DMA{sup V}) would proceed via a dimethylarsinous acid (DMA{sup III}) intermediate and would necessitate the loss of {sup 34}S label. Structural confirmation of the metabolic product was achieved using HPLC-ESI-MS/MS. The data presented support the direct methylation of DMTA{sup V} to TMAS{sup V}. Additionally, the detection of isotopically pure {sup 34}S-TMAS{sup V} raises questions about the sulfur exchange properties of TMAS{sup V} in the cecum material. Therefore, {sup 34}S-TMAS{sup V} was incubated and the exchange was monitored with respect to time. The data suggest that the As-S bond associated with TMAS{sup V} is less labile than the As-S bond associated with DMTA{sup V}.

60 APPLIED LIFE SCIENCES↗

Spectroscopic Investigation of the Uptake of Arsenite From Solution By Synthetic Mackinawite

As(III) uptake from solution by synthetic mackinawite is examined as a function of pH and initial As(III) concentration using X-ray absorption spectroscopy (XAS) and X-ray diffraction (XRD). XAS data indicate that when mackinawite is reacted at pH 5, 7, and 9 with 5 x 10{sup -4} M As(III), arsenic is reduced from its original +3 valence state and is primarily coordinated as As-S ({approx}2.26 {angstrom}) and As-As ({approx}2.54 {angstrom}), which is consistent with the formation of a realgar-like phase in agreement with XRD data. At 5 x 10{sup -5} M As(III), samples are markedly different from those collected at an order of magnitude higher concentration and differ at each pH value. The XAS analysis of mackinawite samples reacted with 5 x 10{sup -5} M As(III) shows a transition from As-O coordination to As-S coordination as pH decreases, with the sample reacted at pH 5 resembling realgar. Under alkaline conditions, arsenic retains its original valence state of +3 and is primarily coordinated to oxygen at a distance of 1.75 {angstrom}. This may be attributed to uptake by adsorption as an As(III) oxyanion. These results provide the basis for selecting the reactions needed for modeling and are beneficial in understanding the mechanisms of arsenite uptake by mackinawite under anoxic sulfidic conditions.

54 ENVIRONMENTAL SCIENCES↗

High pressure transition in amorphous As{sub 2}S{sub 3} studied by EXAFS

We report an in situ high pressure investigation of the structural change in vitreous As{sub 2}S{sub 3} up to 60 GPa using the diamond anvil cell and energy dispersive x-ray absorption spectroscopy. The main finding of the present study is a gradual elongation of the average As-S bond length, which takes place in the pressure range of 15-50 GPa. This change is interpreted as a signature of the coordination number increase around As atoms. The negative shift of the As K absorption edge position confirms the progressive metallization of the glass at high pressure. The observed changes are reversible after pressure release.

36 MATERIALS SCIENCE↗

Methods for Prediction of Refractive Index in Glasses for the Infrared

It is often useful to obtain custom glasses that meet particular requirements of refractive index and dispersion for high-end optical design and applications. In the case of infrared glasses, limited experimental data are available due to difficulties in processing of these glasses and also measuring refractive indices accurately. This paper proposes methods to estimate refractive index and dispersion as a function of composition for selected infrared-transmitting glasses. Methods for refractive index determination are reviewed and evaluated, including Gladstone-Dale, Wemple-DiDomenico single oscillator, Optical basicity, and Lorentz-Lorenz total polarizability. Various estimates for a set of PbO-Bi2O3-Ga2O3 (heavy metal oxide) and As-S (chalcogenide) glasses will be compared with measured values of index and dispersion.

36 MATERIALS SCIENCE↗

Theoretical Studies on Heavy Metal Sulfides in Solution

'Calculating the stabilities, Raman and UV spectra and acidities of As sulfides in aqueous solution', J. A. Tossell, M. D. Zimmermann and G. R. Helz. Some of the Raman spectra obtained by reacting aqueous As(OH)3 with aqueous bisulfide are shown, taken from Wood, et al. (2002). To interpret these spectra we have carried out an extensive series of calculations, detailed for the case of AsS(SH){sub 2}{sup -} in Table 1 below. By employing state of the art quantum chemical techniques to determine gas-phase harmonic and anharmonic frequencies and solution phase corrections we can accurately match features in the experimental spectrum shown in the top figure. The AsS(SH){sub 2}{sup -}...22 H{sub 2}O nanocluster employed is shown in the lower figure. For this species we have calculated the equilibrium structure and the harmonic vibrational spectrum at the CBSB7 B3LYP level. For the free solute species AsS(SH){sub 2}{sup -} we have carried out a whole series of calculations, evaluating harmonic and anharmonic vibrational frequencies at a number of different quantum mechanical levels. In the spectra below, Fig. 3 and Fig. 5 from Wood, et al. (2002), the features around 700-800 cm{sup -1} are attributed to As-O stretches and those around 350-450 cm{sup -1} to As-S stretches. In the nanocluster an isolated vibrational feature is observed at 425 cm{sup -1}, an As=S stretch, close to the value (415 cm{sup -1}) determined by Wood, et al. (2002). Analysis of the calculated frequencies for AsS(SH){sub 2}{sup -} within a polarizable continuum model yields a similar result. Taking the highest level harmonic results, obtained from a CCSD calculation, and adding anharmonic and PCM corrections at the B3LYP level (designated (3) + (5) - (1) in Table 1) gives a frequency for the intense high frequency As=S stretch within 15 cm{sup -1} of experiment. Although there is still interesting work to be done on the stabilities and the Raman and UV spectra of As sulfides, most of the basic concepts have been worked out and we are therefore proposing to move to a new area, that of humic acids (while continuing our studies complexes formed by As oxides and sulfides, now applied to functional groups present in humic acids).

08 HYDROGEN↗

Molecular Processes Underlying the Structure and Assembly of Thin Films and Nanoparticles at Complex interfaces

Since 1995 we have pursued a number of different studies that are quite diverse in nature but with the common theme of using novel laser based methods to study important processes at buried interfaces. Studies of Corrosion, Passivation on n-GaAs(100)Methanol Photoelectrochemical Cell In these studies we have used picosecond photoluminescence and electrochemical studies to understand the GaAs/methanol interface. In our most extensive set of studies we conducted photo-illumination and XPS experiments to understand the chemistry occurring in the GaAs/methanol photoelectrochemical during photoexcitation. An important distinction between photocorrosion and photoetching of GaAs is elucidated by these studies. The dependence of GaAs photocorrosion on light intensity has been explored to better understand intrinsic differences between the lamplight studies and the picosecond photoluminescence studies. The effect of coating the GaAs with a sulfide layer prior to immersion in the cell has also been explored. This last result has led us to examine n-GaAs as a function of crystallographic orientation after exposure to aqueous Na 2 S containing solutions has been studied as a function of crystallographic orientation of the GaAs surface. The (100) and (110) surfaces are relatively similar, with significant amounts of As-S species present at the interface. The (111)B surface lacks this constituent, but shows significant amounts of metallic As. The XPS results have been correlated with the results of previous photocorrosion and passivation studies conducted in a photoelectrochemical cell. The studies indicate that the metallic As present at (111)B surface contributes strongly to the large surface recombination velocity found there, and to the inability of Na 2 S to passivate the (111)B surface. SAMS Under Water: Water Molecular Structure and Bonding at Hydrophobic Surfaces In these DOE sponsored studies we have been interested in learning the similarities and differences in how water behaves at hydrophobic self-assembled monolayer (SAMS)/water interfaces relative to the organic liquid/water interfaces. Several monolayer films have been examined in these studies using a combination of vibrational sum frequency spectroscopy (VSFS), contact angle measurements and AFM. At the hydrocarbon monolayer/water interface we find that water has a weak bonding interaction with the monolayer film that results in an orientation of water at the terminus of these hydrocarbon chains. The water-film interaction is still present for fluorinated films but it is found to be considerably weaker. Hydration and Surfactant Adsorption at Salt/Water Interfaces This set of studies has examined the molecular characteristics of the CaF 2 /water interface using VSFS. Our first studies detailed the structure and orientation of water molecules adsorbed at this mineral surfaces including studies of the surface in the presence of aqueous solutions of salts. These studies have been followed by a series of static and time-resolved studies of the adsorption of carboxylic acid containing organics at this surface, specifically carboxylic acid surfactants and acetic acid. In the latter we have developed a new method for time resolved studies that involve sequential wavelength tuning and automated control of spatial beam overlap at the target can probe amplitude changes of sum-frequency resonances in widely spaced infrared regions. This offers great advantages for the study of the synchronism of molecular processes at interfaces. This approach is particularly suitable to investigate the synchronization of interfacial processes such as surfactant adsorption at charged mineral surfaces. Macromolecular Assembly at Liquid/Liquid Interfaces Macromolecular assembly at the interface between water and a hydrophobic surface underlies some of the most important biological and environmental processes on the planet. Our work has examined polymer adsorption and assembly of carboxylic acid-containing polyelectrolytes at the carbon tetrachloride–water interface, a model system for an oil–water interface. Using VSFS and interfacial tension techniques, these unique set of studies identify the factors that dictate whether or not polyelectrolytes will adsorb to the oil–water interface and also describe the specifics of the adsorption process that depend upon factors such as polymer size, charge density, hydrophobicity, conformation, and the effect of metal ion electrostatics and bonding. The systems studied include polyelectrolytes polyacrylic acid (PAA) and polymethylacrylic acid (PMA) of different polymer sizes and under different aqueous solution conditions. The studies are the first to show the highly ordered nature of the adsorption of the first monolayer with subsequent monolayers disordered. The second set of studies have examined how peptoid nanosheets assemble at the oil/water interface. Peptoid nanosheets are a recently discovered class of two-dimensional (2D) nanomaterial, which form from the self-assembly of a sequence-specific peptoid polymer at an air-water interface. Nanosheet formation occurs first through the assembly of a peptoid monolayer and subsequent compression into a bilayer structure. In these highly successful studies we have shown that the oil-water interface provides another opportunity for growth of these unique and highly ordered peptoid sheets. The monolayer formed at this interface are found through surface spectroscopic measurements to be highly ordered and electrostatic interactions between the charged moieties, namely carboxylate and ammonium residues, of the peptoid are essential in the ability of these peptoids to form ordered nanosheets at the oil-water interface.

36 MATERIALS SCIENCE↗

Materials Data on As4S3 by Materials Project

As4S3 is beta Np structured and crystallizes in the orthorhombic Pnma space group. The structure is zero-dimensional and consists of four tetraarsenic trisulfide molecules. there are three inequivalent As+1.50+ sites. In the first As+1.50+ site, As+1.50+ is bonded in a single-bond geometry to one S2- atom. The As–S bond length is 2.24 Å. In the second As+1.50+ site, As+1.50+ is bonded in a single-bond geometry to one S2- atom. The As–S bond length is 2.23 Å. In the third As+1.50+ site, As+1.50+ is bonded in a distorted trigonal non-coplanar geometry to three S2- atoms. All As–S bond lengths are 2.27 Å. There are two inequivalent S2- sites. In the first S2- site, S2- is bonded in a water-like geometry to two As+1.50+ atoms. In the second S2- site, S2- is bonded in a water-like geometry to two As+1.50+ atoms.

36 MATERIALS SCIENCE↗