Atomistic modeling of interface strengthening in Al-Si eutectic alloys

Al-Si cast alloys are usually composed of α-Al and Al-Si eutectic. Si flakes and Al matrix generally hold cube-on-cube orientation relationship with the primary interface (111) Al ∥(111) Si . Extensive experimental studies demonstrated that Si flakes cannot significantly improve mechanical properties of Al-Si cast alloys. We hypothesize that the weak strengthening effect associated with Si flakes might be attributed to thermomechanical properties of Al-Si interfaces besides their morphologies. To characterize Al-Si interfaces with a large lattice mismatch (> 30%), we proposed the quasi-coincident site lattice (Q-CSL) as reference lattice, and demonstrated that the Q-CSL Al-Si coherent interface has three characteristic coherent structures, one stable and low energy structure and two metastable and high energy structures. The translation vectors for the same type of coherent Q-CSL structures are consistent with three displacement shift complete (DSC) vectors. The two metastable structures can be obtained by shifting the low energy structure with three partial DSC vectors. Semi-coherent interface is composed of the low energy Q-CSL patches and three sets of interface misfit dislocations with Burgers vectors same as the DSC vectors. Atomistic simulations revealed that Al-Si interface exhibits low shear resistance. Ideal shear strength of the Q-CSL coherent interface is 110 MPa and semi-coherent interface is 20 MPa. The low shear resistance is attributed to the glide of interface misfit dislocations. Al-Si interface also exhibits low formation and migration energies of point defects. Owing to low shear strength and low formation and migration energies of point defects, interface sliding or shear readily happen under mechanical loading or during dislocation-interface interactions. Lattice dislocations can cross slip onto or climb along Al-Si interfaces. These reactions decrease the number of accumulated dislocation loops around Si flakes and promote nucleation and emission of lattice dislocations from Al-Si interfaces to matrix, consequently reduce the repulsive force on approaching dislocations and weaken Si flakes strengthening effect. In situ tension and compression tests in a scanning electron microscope reveal relatively weak strengthening effect due to Si flakes, consistent with the computed dislocation interaction with interfaces and shear behavior of interfaces.

36 MATERIALS SCIENCE↗

Three-dimensional morphology of an ultrafine Al-Si eutectic produced via laser rapid solidification

Al-Si alloys processed by laser rapid solidification yield eutectic microstructures with ultrafine and interconnected fibers. Such fibrous structures have long been thought to bear resemblance to those formed in impurity-doped alloys upon conventional casting. Here, we show that any similarity is purely superficial. By harnessing high-throughput characterization and computer vision techniques, we perform a three-dimensional analysis of the branching behavior of the ultrafine eutectic and compare it against an impurity-modified eutectic as well as a random fractal (as a benchmark). Differences in the branching statistics point to different microstructural origins of the impurity- and quench-modified eutectic. Finally, our quantitative approach is not limited to the data presented here but can be used to extract abstract information from other volumetric datasets, without customization.

36 MATERIALS SCIENCE↗

Friction stir processing on a strontium modified, thin-wall, vacuum-assisted high-pressure die-cast Aural-5 alloy to improve tensile and fatigue performance

Here, this study explores the application of friction stir processing (FSP) to enhance the material properties of Sr-modified Aural-5 alloy, with a focus on improved tensile and fatigue properties. Aural-5 is a well-known vacuum-assisted high-pressure die-cast (HPDC) Al-Si7-Mg alloy used in the automotive industry to reduce vehicle weight, enhance fuel efficiency, and lower carbon emissions. This alloy modifies its material chemistry with Sr for fine fibrous networks of eutectic silicon and manganese (Mn) to reduce die soldering. It has significantly less iron (Fe) content resulting in the elimination of detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. The initial microstructure of as-received HPDC Aural-5 exhibits shrinkage porosity in the middle section, a dendritic microstructure with fibrous Al-Si eutectic colonies, a shear-band structure beneath the die-wall, large dendritic externally solidified crystals (ESCs), needle-shaped Mg 2 Si phase and significant second-phase particulates. Some of those microstructural features, such as porosity, ESCs, needle-shaped Mg 2 Si phase, and large second-phase particles, serve as initiation sites for cracks under mechanical loading, resulting in adverse effects on tensile properties, particularly ductility. FSP effectively transforms the microstructure into a wrought configuration with uniform particle distribution by eliminating porosity and disintegrating dendrites, eutectic colonies, ESCs, second-phase particles, and shear-band structures. FSP-driven microstructure modification enhances yield strength and tensile ductility by ~30% and ~35%, respectively. The fatigue life of the material in a bending mode configuration (stress ratio R = 0.1) after FSP exhibits enhancements ranging from 2.0 to 3.9 times that of the original HPDC Aural-5 alloy, depending on the applied stress level.

36 MATERIALS SCIENCE↗

Enhanced Tensile and Tear Toughness Properties of Thin-Wall Vacuum-Assisted High-Pressure Die-Cast Aural-5 Alloy by Friction Stir Processing

Steadily rising demand for glider weight reduction has driven the development of vacuum-assisted high-pressure die-cast (HPDC) Al-alloys for automotive structural components. Aural-5 is a strontium-modified HPDC alloy utilizing manganese (Mn) to reduce die soldering, eliminating detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. HPDC Aural-5 contains shrinkage porosity, dendrites with Al-Si eutectic colonies, externally solidified crystals (ESCs), shear-band structure, and large second-phase particulates. Porosity, ESCs and large second-phase particles work as crack initiation sites, negatively impacting tensile properties. In this study, friction stir processing (FSP) is employed for microstructural modification of a thin-walled HPDC Aural-5 by eliminating porosity and breaking down dendrites, second-phase particles, eutectic colonies, ESCs and shear-band structures to create wrought microstructure with homogenized particle distribution. Mechanical property characterization indicates ~30% and ~35% enhancement in yield strength and ductility and associated marked effects on ~69% improvement in tear toughness according to the ASTM B871 test.

Friction stir processing, Aural-5, Strength, Tear ↗

Effect of Zr and Sc additions on coarsening- and creep resistance of AlSi10Mg fabricated by laser powder bed fusion

Microstructure and creep properties are studied in a eutectic AlSi10Mg alloy modified with Zr and Sc additions (Al-9.8Si-0.32Mg-0.70Zr-0.23Sc, wt%) manufactured through laser powder-bed fusion (L-PBF). Three types of Zr/Sc-bearing powders - elemental, master-alloy, and pre-alloyed - are employed in the fabrication process, with the pre-alloyed powders providing the highest incorporation of Zr and Sc in the Al matrix. Here, the as-printed alloy exhibits a fine cellular Al-Si eutectic structure which fragments and coarsens into micron-sized Si particles during aging at 300 ºC, leading to a steady drop in alloy microhardness between 0.1 and 1000 h. Coarsening of the eutectic Si phase during aging is not measurably affected by Zr and Sc in solid solution, which precipitate during aging and increases strength, compensating weakening from Si coarsening between 1 and 200 h at 300 ºC. Atom-probe analysis in the peak-aged condition (96 h/300 °C) confirms the presence of Al 3 (Sc,Zr) secondary nano-precipitates with an average radius of 1.0 nm and some Si solubility. Micron-sized grains are present throughout the alloy, with ultra-fine-grained regions at the melt pool boundaries, neither of which coarsen during long-term aging at 300 ºC. Under creep conditions at 300 °C, the Zr/Sc-bearing alloy with Al 3 (Sc,Zr) nano-precipitates exhibits power-law behavior, with a high apparent stress exponent (n a = 9) and a high threshold stress (σ th = 43 MPa), exhibiting nearly double the strength of a Zr/Sc-free AlSi10Mg control alloy (σ th = 22 MPa).

36 MATERIALS SCIENCE↗

Combustion in the ZrF 4 -Mg-Si and ZrF 4 -Al-Si systems for preparation of zirconium silicides

The exothermic reactions in the ZrF 4 –Mg-Si and ZrF 4 -Al-Si systems are investigated by a fast temperature recording (thermocouple) technique, differential scanning calorimetry (DSC), and thermogravimetric analysis (TGA). A quenching method is used to arrest the combustion process and conduct a layer-by-layer analysis of the products by x-ray diffraction (XRD) and electron microscopy. Two seemingly similar reactive systems exhibited considerably different combustion characteristics, composition, and morphology. Based on these investigations, we propose and discuss phase formation mechanisms at the early stages for each system. Three different pathways involving the reaction of ZrF 4 with other reagents and the Mg 2 Si intermediate are identified to occur in the ZrF 4 –Mg-Si system. Contrary to the complex mechanism in the ZrF 4 –Mg-Si system, the early stage of the combustion process for the ZrF 4 -Al-Si system involves the interaction of ZrF 4 with Al-Si eutectic melt. The exothermic reaction between reduced solid Zr and Si melt is the primary heat-generating step for both systems in spite of substantial differences in the early stages of the reactions. The silicon content in the reactive mixtures governs the phase composition of products. The ZrSi 2 phase, with a high growth rate, forms first on the Zr particle surfaces and then grows by a reactive diffusion mechanism. The ZrSi 2+ Zr reaction produces silicon-lean phases (e.g., ZrSi) when the silicon supply is limited. The combustion temperature also has a considerable influence on the phase compositions of the products. High combustion temperature in the ZrF 4 +2Mg+Si mixture enables the formation of multiphase products (α-ZrSi and β-ZrSi), whereas the relatively lower temperatures in the 3ZrF 4 +4Al+3Si mixture yields a single-phase α-ZrSi. As a result, lower combustion temperatures also make the ZrF 4 -Al-Si system more advantageous for the preparation of zirconium silicides.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Corrosion evaluation of Al-Cu-Mn-Zr cast alloys in 3.5% NaCl solution

Corrosion behavior of cast Al-Cu-Mn-Zr (ACMZ) and RR350 alloys was compared to a cast 319 alloy in 3.5 wt.% NaCl. After 168 h immersion, ACMZ and RR350 alloys suffered from preferential attack adjacent to intermetallic particles decorated at grain boundaries while the attack in 319 occurred in eutectic Al-Si dendritic boundaries. Electrochemical data allowed semiquantitative comparison of alloy resistance to corrosion initiation, and ACMZ type alloys, including RR350 and three alloys with higher Cu, were considered more resistant than 319 due to the absence of deleterious Si particles. In case of 319, such Si particles presumably drove higher micro-galvanic influence to initiate and sustain Al corrosion. With lower susceptibility to corrosion initiation, ACMZ alloys should exhibit higher or at minimum similar resistance compared to cast 319.

36 MATERIALS SCIENCE↗

Microstructure and properties of additively manufactured Al–Ce–Mg alloys

Additive manufacturing of aluminum alloys is largely dominated by a near-eutectic Al-Si compositions, which are highly weldable, but have mechanical properties that are not competitive with conventional wrought Al alloys. In addition, there is a need for new Al alloys with improved high temperature properties and thermal stability for applications in the automotive and aerospace fields. In this work, we considered laser powder bed fusion additive manufacturing of two alloys in the Al–Ce–Mg system, designed as near-eutectic (Al–11Ce–7Mg) and hyper-eutectic (Al–15Ce–9Mg) compositions with respect to the binary L → Al + Al 11 Ce eutectic reaction. The addition of magnesium is used to promote solid solution strengthening. A custom laser scan pattern was used to reduce the formation of keyhole porosity, which was caused by excessive vaporization due to the high vapor pressure of magnesium. The microstructure and tensile mechanical properties of the alloys were characterized in the as-fabricated condition and following hot isostatic pressing. The two alloys exhibit significant variations in solidification structure morphology. These variations in non-equilibrium solidification structure were rationalized using a combination of thermodynamic and thermal modeling. Both alloys showed higher yield strength than AM Al-10Si-Mg for temperatures up to 350 °C and better strength retention at elevated temperatures than additively manufactured Scalmaloy.

36 MATERIALS SCIENCE↗

Microstructural refinement in ultrasonically modified A356 aluminum castings

Two A356 aluminum alloys (Al-Si-Mg), one with 0.09 wt.% Fe and one with 0.91 wt.% Fe, were cast in a graphite mold with the simultaneous application of local ultrasonic intensification to refine the as-cast microstructure. Ultrasonication during casting transformed the morphology of primary Al grains from dendritic (~140-290 microns in size) to globular (~33-36 microns in size). The alloy with high Fe exhibited globular grains at distances up to 45 mm away from the ultrasound probe, while the alloy with low Fe exhibited globular grains at distances only up to 6 mm away from the ultrasound probe. Near the location of the ultrasound probe (< 2 mm away), a second non-dendritic microstructural morphology was observed with fine aluminum grains (~9-25 microns in size). This unique fine-grained morphology has not been previously reported, contains a greater concentration of Si relative to the globular microstructure, and may be a large, fully eutectic region. Ultrasonication during casting also transformed the morphology of the ß-Al 5 FeSi phase particles (which are deleterious to the strength and ductility of the alloy) in the high Fe alloy from needle-like to rectangular, which could enable the greater use of secondary Al alloys. Thermodynamic simulations conducted to calculate the solidification paths of the two alloys studied predict that the ß-Al 5 FeSi phase begins to form earlier in the alloy with high Fe. Finally, data suggest that the ß-Al 5 FeSi phase (which is more abundant in alloys with high Fe content) may enhance ultrasonically-induced grain refinement.

36 MATERIALS SCIENCE↗

Plastic homogeneity in nanoscale heterostructured binary and multicomponent metallic eutectics: An overview

Heterostructured materials comprised of relatively soft/hard disparate phases typically exhibit composite strengthening but lack plastic deformability at ambient temperatures. However, heterostructured systems comprised of nanoscale phases can simultaneously enhance yield strength and strain hardening, thereby promoting uniform distribution of plastic flow. In this review, the atomic-scale deformation mechanisms in model systems of eutectic alloys, Al-Al 2 Cu and Al-Si, refined to nanoscales via laser rapid solidification are discussed, and compared with literature on multi-component (high entropy) eutectics such as Ni-Al-Fe-based with Cr and/or Co additions. The nano-lamellar Al-Al 2 Cu structures exhibit unit defect mechanisms not reported in monolithic Al 2 Cu intermetallic: localized shear on {0 1 1} and shear-induced faults on {1 2 1} planes, constrained by closely-spaced dislocation arrays in Al confined by Al/Al 2 Cu interfaces. The unexpected plasticity mechanisms are enabled by slip continuity in nanoscale Al-Al 2 Cu eutectics associated with the orientation relationship and interface habit planes. In nano-fibrous Al-Si eutectic, tensile ductility at strength approaching 600 MPa is observed resulting from dislocation plasticity in the nano-Al channels and cracking in Si nanofibers. Molecular dynamics simulations show that Al dislocations easily cross-slip (screw) or climb (edge) along Al-Si interfaces, making slip transmission difficult. The propagation of nano-cracks is suppressed by surrounding strain hardening Al, retaining good ductility of the sample, in spite of lack of direct slip transmission. Finally, the critical unit mechanisms of slip transmission and interface-enabled plasticity observed in nanoscale eutectic binary systems can also explain the strength-ductility relationship in multi-component eutectics and homogeneously distributed plastic flow with increasing microstructural heterogeneity.

36 MATERIALS SCIENCE↗

In Situ Prediction of Microstructure and Mechanical Properties in Laser-Remelted Al-Si Alloys: Towards Enhanced Additive Manufacturing

Laser surface remelting of aluminum alloys has emerged as a promising technique to enhance mechanical properties through refined microstructures. This process involves rapid cooling rates ranging from 10 3 to 10 8 °C/s, which increase solid solubility within aluminum alloys, shifting their eutectic composition to a larger value of silicon content. Consequently, the resulting microstructure combines a strengthened aluminum matrix with silicon fibers. This study focuses on the laser scanning of Al-Si aluminum alloy to reduce the size of aluminum matrix spacings and transform fibrous silicon particles from micrometer to nanometer dimensions. Analysis revealed that the eutectic structure contained 17.55% silicon by weight, surpassing the equilibrium eutectic composition of 12.6% silicon. Microstructure dimensions within the molten zones, termed ‘melt pools’, were extensively examined using Scanning Electron Microscopy (SEM) at intervals of approximately 20 μm from the surface. A notable increase in hardness, exceeding 50% compared to the base plate, was observed in the melt pool regions. Thus, it is exemplified that laser surface remelting introduces a novel strengthening mechanism in the alloy. Moreover, this study develops an in situ method for predicting melt pool properties and dimensions. A predictive model is proposed, correlating energy density and spectral signals emitted during laser remelting with mechanical properties and melt pool dimensions. This method significantly reduces characterization time from days to seconds, offering a streamlined approach for future studies in additive manufacturing.

36 MATERIALS SCIENCE↗

Phase transformations, microstructural refinement and defect evolution mechanisms in Al-Si alloys under non-hydrostatic diamond anvil cell compression

Non-hydrostatic compression of materials using a diamond anvil cell (DAC) can transform equilibrium microstructure of an alloy to novel, potentially metastable states. In this study, in situ synchrotron X-ray diffraction (XRD) during compression up to 24 GPa and subsequent ex situ, high resolution analytical electron microscopy (AEM) after decompression of an Al-Si alloy provided insight into the crystallographic changes during the compression as well as microstructural refinement, and defect structures caused by such a high pressure compression-decompression process. Pressure resolved in-situ synchrotron XRD was used to detail the phase transformation pathway of the eutectic Si phase in Al-Si alloy, from Si-I → Si-XI → Si-V during compression, and a final transformation predominantly to Si-III after decompression. Using scanning and transmission electron microscopy (S/TEM), site specific analysis of the alloy immediately underneath the anvil contact surface demonstrated a highly complex microstructure. A narrow region of thick amorphous Al oxide interspersed with nanocrystalline grains was found at the top surface. Underneath this Al oxide, while the majority the eutectic Si was transformed into highly-deformed, polycrystalline (PC) Si-III, a complex intermediate layer was discovered at the interface between Al and Si, comprised of a small fraction of Al nanocrystals and a majority of nanocrystalline Si-I. This combination of pressure resolved in-situ synchrotron XRD coupled with subsequent high resolution, electron microscopy resolved the phase transformation as well as non-equilibrium microstructures in a metallic alloy induced by a non-hydrostatic high pressure compression followed by decompression.

36 MATERIALS SCIENCE↗

Strontium Effects on the Formation of Iron-Intermetallic Phases in Secondary Al–9Si–0.6Fe Alloys

The presence and morphology of Fe-containing intermetallic phases affect the mechanical properties of aluminum alloys, especially in secondary Al–Si-based cast alloys. Although strontium (Sr) addition of 50 to 500 ppm is known to refine the needle-type eutectic silicon structure, the influence of Sr on the formation of Fe-intermetallic phases remains unclear. The present work investigates the combined additions of Sr and Mn to Al–9Si–0.6Fe–0.35Mg (All compositions are in wt pct except otherwise stated.) alloys on the formation of Fe-intermetallic phases at different solidification rates from ~ 1.5 to ~ 60 °C/s. Long and branched-type AlFeSi phase with size ranging from 50 to 120 µm are more common when solidified at the rate of 1.5 °C/s regardless of Sr and Mn additions. However, at the fast solidification rate of 60 °C/s, a 60 ppm Sr addition significantly reduced the average length of needle-shaped AlFeSi phase to less than 3 to 5 µm. Thermodynamic simulations have been performed using CALculation of PHAse Diagrams (CALPHAD) models to predict the formation of various phases and their possible interactions during solidification. The results indicated that the combination of a high solidification rate and about 60 ppm of Sr is beneficial to refining the δ-Al 3 FeSi 2 phase in Al–Si–Mg alloys containing 0.6 pctFe. As a result, this unexpected finding of Fe-intermetallic refinement by low Sr addition (~60 ppm) provides an important guide in designing secondary alloys for sustainable casting applications.

36 MATERIALS SCIENCE↗

The Beneficial Effect of Iron in Aluminum-Cerium-Based Cast Alloys

Iron (Fe) has been considered a major impurity since it is detrimental to the mechanical properties of many cast aluminum alloys due to the formation of Fe-containing brittle intermetallic phases. Fe is found naturally as an impurity in bauxite ore, resulting in Fe contamination of aluminum alloys with increasing contamination from current recycling practices. The Al–Ce–Fe system was investigated using CALPHAD (CALculation of PHAse Diagrams) modeling and experimental casting techniques. It was found that additions of Fe to the Al–Ce system are beneficial to the strength (slightly) and ductility (significantly) of the ternary alloys, which is attributed to the formation of fine metastable Al 8 CeFe 2 phase with aggregate morphology and equilibrium Al 10 CeFe 2 phase, suppressing coarse proeutectic Al 11 Ce 3 phase in near-eutectic Al–Ce alloys. Heat treatment study showed that the metastable Al 8 CeFe 2 phase transforms to predicted equilibrium Al 10 CeFe 2 phase at 500 °C, with essentially no intermetallic or grain coarsening; thus, the alloy displayed excellent property retention. The Al–Ce–Fe alloy system offers opportunities for sustainable, recyclable alloy development using low-cost Fe and low-cost cerium (a byproduct of rare-earth extraction).

42 ENGINEERING↗

Effect of Cooling Rate on Nano-Eutectic Formation in Laser Surface Remelted and Rare Earth Modified Hypereutectic Al-20Si Alloys

Laser Surface Remelting (LSR) was applied to arc-melted Al-20Si-0.2Sr, Al-20Si-0.2Ce, and Al-20Si hypereutectic alloys to refine microstructures. Experiments revealed that microstructures in the melt pool varied from fully eutectic to a mixture of Al dendrites and inter-dendritic eutectic. We calculated cooling rates using the Eagar-Tsai model and correlated cooling rates with characteristic microstructures, revealing that a cooling rate on the order of 104 K/s could lead to maximized fully eutectic microstructure morphology. Due to rapid solidification, the Si composition in the LSR eutectic was measured at 18.2 wt.%, higher than the equilibrium eutectic composition of 12.6 wt.%Si. Compared to Al-20Si, Ce addition had no significant effect on the volume fraction of the fully eutectic structure but refined Si fibers to approximately 30 nm in diameter. Sr addition did not further refine the diameter of eutectic Si fibers compared to Al-20Si but increased the volume fraction of the fully eutectic microstructure morphology. The refinement ratio (φ) of the Si fiber diameter from the bottom of the melt pool to the surface for the three alloys was similar, at around 28%. The established correlation between the cooling rate and the size and morphology of the microstructure within the melt pool will enable tailoring of the microstructure in laser-processed as well as deposited alloys for high strength and plasticity.

36 MATERIALS SCIENCE↗