FY24 progress report on A709 mechanical properties data development and A709 thermal aging status

The report provides the status of the creep, fatigue, and creep-fatigue testing to date conducted at Idaho National Laboratory to generate the data package. This data package evaluates the material performance from three commercial heats to support the Alloy 709 qualification in American Society of Mechanical Engineers, Boiler and Pressure Vessel Code, Section III, Division 5. First procured heat was manufactured by G.O. Carlson with heat number 58776. Second and third heats were fabricated by ATI Specialty Rolled Products with heat numbers 529900 and 530843, respectively. A series of creep and cyclic specimens were fabricated from these three heats and tests were performed. A list of finished, ongoing, and planned test are presented for creep, fatigue, and creep-fatigue tests. Cyclic properties of three commercial heats are compared.

36 - MATERIALS SCIENCE

Summary report on the mechanical testing performed at INL for creep rupture, fatigue, creep-fatigue, and aging of A709 base material

The report provides the status of the creep, fatigue, and creep-fatigue testing to conducted at Idaho National Laboratory to generate a data package to support Alloy 709 qualification in American Society of Mechanical Engineers, Boiler and Pressure Vessel Code, Section III, Division 5. These tests were performed on three commercial heats of plate material. The first procured heat was manufactured by G.O. Carlson with heat number 58776. Second and third heats were fabricated by ATI Specialty Rolled Products, with heat numbers 529900 and 530843, respectively. A series of creep and cyclic specimens were fabricated from these three heats, and tests were performed. This report presents a master list of all completed and ongoing creep, fatigue, and creep fatigue tests. Cyclic properties of three commercial heats are compared. Thermal aging of three commercial heats for 3000 hours were completed in FY 2025. The thermal aging campaign to age plate material from three commercial heats up to 100,000 hours is ongoing.

36 - MATERIALS SCIENCE

FY25 Status Update on A709 Code Case Testing at ANL

This report provides an update on the status of the creep rupture testing on the precipitation-treated (PT) Alloy 709 samples fabricated from the first, the second and the third commercial heats, in support of the first, 100,000-hour Alloy 709 Code Case development under the American Society of Mechanical Engineers (ASME) Section III, Division 5 for high-temperature reactor construction. In Fiscal Year (FY) 25, no new tests were initiated, while 5 previously loaded tests were completed. This report presents an overview of the creep-rupture data gathered at Argonne National Laboratory (ANL) since FY21 that totaled 52 completed tests. Metallographic images showing crack morphologies in some representative samples ruptured in FY25 are also included. Key conclusions include: 1) the creep behavior of the three heats of Alloy 709 can be well described by the Larson-Miller relationship; 2) higher temperatures and larger stresses lead to shorter creep life and higher minimum creep rate; 3) Alloy 709 is overall very ductile under creep; 4) the crack morphologies near fracture surfaces are dependent on material’s grain size and test conditions.

22 GENERAL STUDIES OF NUCLEAR REACTORS

Sodium Chemistry Assessment and Initiation of Sodium Exposure Experiment on A709 Commercial Heats and LPBF 316H SS

This report documents sodium chemistry characterization and the initiation of forced‑convection sodium exposure experiments for two structural materials for sodium‑cooled fast reactors (SFRs): Alloy 709 (solution‑annealed and with an additional 775 °C/10 h precipitation treatment) and laser powder bed fusion (LPBF) 316H stainless steel tensile specimens printed with an as‑built surface condition. The sodium exposure experiment was conducted in a forced‑convection sodium loop with two vessels operated at 550 °C and 600 °C, and a cold trap maintained at <130 °C. Carbon activity in sodium was quantified using a nickel‑foil equilibration method. Initial post‑exposure evaluation after ~1,000 h indicates negligible thickness change for Alloy 709 and a small but measurable mass decrease. To isolate thermal effects from sodium effects, parallel thermal‑aging experiments were performed on Alloy 709 at 550 °C and 600 °C. Baseline tensile tests at room temperature, 550 °C, and 600 °C show expected reduction in strength with increasing temperature and serration tensile curves at elevated temperatures, consistent with dynamic strain aging. After 3,000 h thermal aging, Alloy 709 exhibits modest strengthening and reduced ductility at 550 °C. Together, these results establish the loop chemistry conditions and provide the initial corrosion and mechanical property results for ongoing long‑duration sodium exposure of Alloy 709 and LPBF 316H stainless steel.

22 GENERAL STUDIES OF NUCLEAR REACTORS

Report on Preliminary Detailed Experimental Plan for Neutron Irradiation of A709 at ATR and HFIR

Advanced nuclear power technologies will use higher temperatures as a means to extract energy at a higher efficiency than current plants and therefore put a larger demand on the structural materials. Improved performance of structural materials could enable greater safety margins, longer plant lifetimes, and reduce maintenance costs. Alloy 709 is championed as the next generation of austenitic alloys for advanced nuclear reactors. In parallel to the ASME code case pursued, the AMMT program is initiating a neutron irradiation campaign to provide first-of-a-kind engineering data to establish operational design parameters and how the mechanical response is modified by environmental factors. This document refines the AMMT neutron irradiation campaign to a 4 year program to support the generation of creep knockdown factors for Alloy 709 and welded Alloy 709. The campaign is divided among two national laboratories, Oak Ridge National Laboratory and Idaho National Laboratory, to use the strengths of each laboratory. Through a cooperative plan, time-independent properties and time-dependent properties will be obtained across a large temperature window, nominally 300°C to 800°C, damage levels up to 10 dpa, and with and without the impacts of transmutation produced helium.

99 GENERAL AND MISCELLANEOUS

Report on Preliminary Detailed Experimental Plan for Neutron Irradiation of A709 at ATR and HFIR

Advanced nuclear power technologies will use higher temperatures as a means to extract energy at a higher efficiency than current plants and therefore put a larger demand on the structural materials. Improved performance of structural materials could enable greater safety margins, longer plant lifetimes, and reduce maintenance costs. Alloy 709 is championed as the next generation of austenitic alloys for advanced nuclear reactors. In parallel to the ASME code case pursued, the AMMT program is initiating a neutron irradiation campaign to provide first-of-a-kind engineering data to establish operational design parameters and how the mechanical response is modified by environmental factors. This document refines the AMMT neutron irradiation campaign to a 4 year program to support the generation of creep knockdown factors for Alloy 709 and welded Alloy 709. The campaign is divided among two national laboratories, Oak Ridge National Laboratory and Idaho National Laboratory, to use the strengths of each laboratory. Through a cooperative plan, time-independent properties and time-dependent properties will be obtained across a large temperature window, nominally 300°C to 800°C, damage levels up to 10 dpa, and with and without the impacts of transmutation produced helium.

22 GENERAL STUDIES OF NUCLEAR REACTORS

Laser Powder Directed Energy Deposition of Steels for Nuclear Applications

This comprehensive investigation examines the structure–property relationships in two nuclear alloy systems—Alloy 709 (A709) austenitic stainless steel and Grade 92 (G-92) ferritic/martensitic (F/M) steel—manufactured via directed energy deposition (DED) for sodium-cooled fast reactor applications. This study establishes the fundamental mechanisms for controlling microstructures for optimizing the mechanical performance of additively manufactured nuclear materials through systematic heat treatment optimization and multiscale characterization. As-deposited A709 steel develops a complex multiscale strengthening architecture consisting of a fine cellular solidification structure with diameter of 2-3 µm within10–50 µm grains, elevated dislocation densities from rapid thermal cycling, and grain boundary precipitates that activate concurrent Hall–Petch, dislocation, and precipitation hardening mechanisms to achieve exceptional properties [yield strength (YS): 603 MPa, ultimate tensile strength (UTS): 844 MPa, Vickers hardness: 220 HV] that achieve a 44% superior strength compared to that of the wrought material. Heat treatments produce different results. Solution annealing (SA) dissolves the cellular structure and reduces the hardness to 190 HV. Precipitation treatment (PT) keeps the cellular structure but adds carbides, allowing the hardness to reach 205 HV. The best approach combines both treatments (SA+PT) and creates uniform precipitate distributions with M 23 C 6 carbides at the grain boundaries and MX carbonitrides in the matrix, achieving a hardness of 195 HV. However, directional differences persist, with a 12%–15% strength variation between orientations due to the inherited layered microstructural architecture that survives aggressive heat treatment. While tensile testing at 550°C demonstrates 40%–50% thermal softening with dynamic strain aging, DED A709 steel still maintains a 71% higher YS than that of the wrought material. Ion irradiation studies (100–400 dpa) of DED A709 steel reveal progressive radiation damage with increasing void density and radiation-induced segregation causing nickel enrichment and chromium depletion, which will ultimately compromise mechanical properties. As-deposited G-92 exhibits exceptional strength (UTS: 1650–1700 MPa, 430 HV) through a complex microstructure containing both ferrite and martensite phases, a high geometrically necessary dislocation (GND) density (17.04×10 14 /m 2 ), and fine carbides. Heat treatments create distinct changes. Normalizing produces fresh martensite with the highest hardness (460 HV) and an increased GND density (20.23×10 14 /m 2 ). Tempering develops dual precipitation systems and reduces the hardness to 290 HV. The optimal approach uses sequential normalizing plus tempering, achieving balanced properties with the lowest hardness (250 HV) and a reduced GND density (11.01×10 14 /m 2 ). A processing-dependent anisotropy is observed: horizontal specimens achieve superior ductile behavior, while vertical specimens exhibit brittle failure. A tempering heat treatment successfully mitigates this anisotropic behavior by transforming the hard martensitic as-deposited structure into tempered martensite enabling both horizontal and vertical specimens to exhibit similar stress–strain characteristics with visible necking behavior. Remarkably, testing at 550°C reveals a reversal in the anisotropy, where as-deposited specimens achieve near isotropy with superior thermal stability (a 15%–20% strength reduction), while tempered specimens develop an orientation dependence with a 25%–30% strength reduction. Both alloy systems demonstrate that DED processing creates specimens with a superior strength through refined microstructural features, though with distinct strengthening mechanisms—austenitic through cellular structures and precipitates versus F/M through phase transformations and precipitates. Heat treatment optimization requires alloy-specific approaches, with A709 benefiting from controlled precipitation while G-92 requires careful phase transformation control. The results show that DED manufacturing can produce nuclear materials with exceptional performance, but directional effects and temperature-dependent behavior must be carefully considered for reactor component design and qualification.

22 GENERAL STUDIES OF NUCLEAR REACTORS

Development of Predictive Model for Accurate Rupture Time from Multi-Axial Creep in Alloy 709 with Physics-Based Simulations

A physics-based model is developed to predict multiaxial creep behavior in Alloy 709 (A709), an advanced austenitic stainless steel intended for high-temperature applications such as Sodium Fast Reactors (SFRs). Compared to conventional stainless steels like 316H, A709 offers superior high-temperature performance; however, comprehensive data on its multiaxial creep response remain limited. To address this gap, a crystal plasticity finite element (CPFE) framework is used to simulate the deformation and failure mechanisms of A709 under multiaxial loading conditions. The model incorporates an extended Hu-Cocks dislocation creep formulation that accounts for precipitation effects, along with the Sham–Needleman model to capture grain boundary cavitation-driven failure. These advanced constitutive models enable a detailed understanding of the interplay between microstructural evolution and macroscopic creep response. Furthermore, the study evaluates the predictive accuracy of various effective stress measures in estimating creep rupture life, leveraging simulated multiaxial creep data. The findings provide critical insights into the applicability of different stress measures for engineering design and life prediction of A709 components operating under complex loading conditions. This work contributes to improving the reliability of high-temperature structural components by advancing predictive modeling capabilities for advanced austenitic steels.

Alloy 709

Influence of post deposition annealing on the microstructural evolution and tensile behavior of austenitic stainless-steel alloy 709 made by laser powder bed fusion

Structural materials used in the next generation nuclear reactors or other advanced energy systems are often required to withstand higher operating temperatures for a longer service life. Alloy 709 (A709), a Nb-containing and N-stabilized Fe-25Ni-20Cr austenitic stainless steel, has been recommended for high-temperature reactor constructions due to the better performance over the baseline Type 316H stainless steel. Here, in the current manuscript, for the first time, the microstructure evolution and tensile behavior of an A709 made by laser powder bed fusion (LPBF) is discussed. The as deposited and heat treated LPBF alloys are compared with a reference wrought alloy. Owing to the chemical segregation and a higher number of dislocations, the LPBF materials show a significantly higher density of precipitates formed during high temperature treatments when compared to the wrought samples. This is reflected when looking at the tensile properties, both at room and elevated temperatures, where LPBF samples show higher strengths compared to wrought materials.

36 MATERIALS SCIENCE

Additive Manufacturing of Fe-based Alloys for Nuclear Reactor Environments

This report is a Milestone 2 deliverable in FY2025, under work package MT-25AN090211 to support research and qualification activities supported by the Advanced Materials and Manufacturing Technologies (AMMT) program. It provides an update on the work done on the laser based additive manufacturing of steels for nuclear applications, conducted collaboratively by Argonne National Laboratory and Pacific Northwestern National Laboratory. Building upon FY23 and FY24 efforts, the focus of FY25 includes continued optimization of process parameters for the alloys: A709 & G92. The work package also includes fabricating test samples to conduct a thorough microstructural analysis and perform preliminary mechanical testing. The major accomplishments of this work package are summarized below, applicable to both Laser Powder Bed Fusion (LPBF) processes conducted at Argonne National Laboratory and Laser Powder Directed Energy Deposition (LP-DED) processes conducted at Pacific Northwest National Laboratory.

22 GENERAL STUDIES OF NUCLEAR REACTORS

Environmental degradation testing of Alloy 709

Alloy 709 is an advanced austenitic stainless steel developed to meet the demanding conditions of sodium fast reactors (SFRs) but may also be of use for lead fast reactors, high temperature gas reactors, and molten salt reactors. Understanding environmental degradation modes and quantifying degradation rates are crucial to ensure the long-term, reliable operation of these reactors. This paper discusses recent neutron irradiation results, future neutron irradiation test plans, and sodium corrosion testing to communicate current best understanding of the performance of Alloy 709 in SFR environments.

A709