On the genesis of molybdenum carbide phases during reduction-carburization reactions
Molybdenum carbide has been prepared according to the carbothermal reduction method. Carbon black substrate was used as C-source whereas a H{sub 2}-flow was the reducing agent. Two different H{sub 2} consumption steps were identified during the carburization treatment. The low temperature step is related to the reduction of Mo{sup 6+}-to-Mo{sup 4+}, the higher temperature process accounts for the deep reduction of Mo{sup 4+}-to-metal Mo{sup 0} and its subsequent reaction with C to form the Mo-carbide. The influences of the maximum carburization temperature, carburization time, gas hourly space velocity regarding Mo-loading, heating rate and temperature of Ar pre-treatment were analyzed. All these conditions are interrelated to each other. Thus, the carburization process ends at 700 Degree-Sign C when Mo-loading is 10 wt%, however Mo-loading higher than 10 wt% requires higher temperatures. Carburization temperatures up to 800 Degree-Sign C are needed to fulfill Mo-carbide formation with samples containing 50 wt% Mo. Nevertheless, Ar pre-treatment at 550 Degree-Sign C and slow heating rates favor the carburization, thus requiring lower carburization temperatures to reach the same carburization level. - Graphical Abstract: H{sub 2}-consumption profile (TPR) during the molybdenum carburization process, XRD patterns of the reduced Mo-samples after carburization and TEM-micrographs with two different enlargement of the samples with 5, 20 and 50 wt% Mo. Highlights: Black-Right-Pointing-Pointer Control of carburization variables: tailor the reduced/carbide Mo-phases (single/mixture). Black-Right-Pointing-Pointer Mo carburization in two stages: (1) Mo{sup 6+}-Mo{sup 4+}; (2) Mo{sup 4+}-Mo{sup 0} and, at once, MoC. Black-Right-Pointing-Pointer The carburization process is faster than Mo{sup 4+} reduction. Black-Right-Pointing-Pointer XPS probed: reduced Mo particles show core-shell structure. Black-Right-Pointing-Pointer Core: reduced Mo (Mo{sub 2}C, MoO{sub 2} and/or Mo{sup 0}); Shell: 2-3 nm of MoO{sub 3}.