Mode I Cohesive Law Characterization of Through-Crack Propagation in a Multidirectional Laminate

A method is proposed and assessed for the experimental characterization of through-the-thickness crack propagation in multidirectional composite laminates with a cohesive law. The fracture toughness and crack opening displacement are measured and used to determine a cohesive law. Two methods of computing fracture toughness are assessed and compared. While previously proposed cohesive characterizations based on the R-curve exhibit size effects, the proposed approach results in a cohesive law that is a material property. The compact tension specimen configuration is used to propagate damage while load and full-field displacements are recorded. These measurements are used to compute the fracture toughness and crack opening displacement from which the cohesive law is characterized. The experimental results show that a steady-state fracture toughness is not reached. However, the proposed method extrapolates to steady-state and is demonstrated capable of predicting the structural behavior of geometrically-scaled specimens.

Bergan, Andrew C.↗

Spontaneous Cracking in Unfired Magnesia Compacts Upon Standing in Air

Analytical-grade magnesium oxide powder without binder was compressed hydrostatically to 50,000 lb. per sq. in. to form compacts. When exposed to moist air immediately after pressing, these compacts developed irregularly shaped cracks. Controlled tests, in which these compacts were exposed for various lengths of time to various atmospheres, indicated that in general water vapor, carbon dioxide, and residual stresses had to be present if cracking was to occur. The probable cause of the cracking was the formation of a less dense and mechanically weak basic carbonate of magnesium at crystallite surface points of high stress concentration which developed during the compacting. The adsorption of dry CO2 at such sites prevented subsequent delayed fracture.

Davies, Myron O.↗

Estimating Orion Heat Shield Failure Due To Ablator Cracking During The EFT-1 Mission

The Orion EFT-1 heatshield suffered from two major certification challenges: First, the mechanical properties used in design were not evident in the flight hardware and second, the flight article itself cracked during fabrication. The combination of these events motivated the Orion Program to pursue an engineering-level Probabilistic Risk Assessment (PRA) as part of heatshield certification rationale. The PRA provided loss of Mission (LOM) likelihoods considering the probability of a crack occurring during the mission and the likelihood of subsequent structure over-temperature. The methods and input data for the PRA are presented along with a discussion of the test data used to anchor the results. The Orion program accepted an EFT-1 Loss of Vehicle (LOV) risk of 1-in-160,000 due to in-mission Avcoat cracking based on the results of this analysis. Conservatisms in the result, along with future considerations for Exploration Missions (EM) are also addressed.

Avcoat↗

The Effects of Salt Water on the Slow Crack Growth of Soda Lime Silicate Glass

The slow crack growth parameters of soda-lime silicate were measured in distilled and salt water of various concentrations in order to determine if stress corrosion susceptibility is affected by the presence of salt and the contaminate formation of a weak sodium film. Past research indicates that solvents effect the rate of crack growth, however, the effects of salt have not been studied. The results indicate a small but statistically significant effect on the slow crack growth parameters A and n. However, for typical engineering purposes, the effect can be ignored.

Toughness↗

Combining Progressive Nodal Release with the Virtual Crack Closure Technique to Model Fatigue Delamination Growth Without Re-Meshing

The present work summarizes an approach to model mixed-mode 3D fatigue crack growth using the Virtual Crack Closure Technique (VCCT) without requiring re-meshing. It is demonstrated that the proposed approach can be used to simulate crack shapes that do not conform to the underlying mesh. The proposed approach relies solely on Paris Law characterization data to model delamination growth. Growth is determined as a post-processing step at the end of each increment, and hence no convergence issues associated with the progressive nodal release are encountered. This approach can be readily applied using standard solid element formulations and is implemented via an interface user element in Abaqus/Standard.

Carvalho, N. V. De↗

An Abrupt Transition to an Intergranular Failure Mode in the Near-Threshold Fatigue Crack Growth Regime in Ni-Based Superalloys

Cyclic near-threshold fatigue crack growth (FCG) behavior of two disk superalloys was evaluated and was shown to exhibit an unexpected sudden failure mode transition from a mostly transgranular failure mode at higher stress intensity factor ranges to an almost completely intergranular failure mode in the threshold regime. The change in failure modes was associated with a crossover of FCG resistance curves in which the conditions that produced higher FCG rates in the Paris regime resulted in lower FCG rates and increased Kth values in the threshold region. High-resolution scanning and transmission electron microscopy were used to carefully characterize the crack tips at these near-threshold conditions. Formation of stable Al-oxide followed by Cr-oxide and Ti-oxides was found to occur at the crack tip prior to formation of unstable oxides. To contrast with the threshold failure mode regime, a quantitative assessment of the role that the intergranular failure mode has on cyclic FCG behavior in the Paris regime was also performed. It was demonstrated that even a very limited intergranular failure content dominates the FCG response under mixed mode failure conditions.

Telesman, J.↗

Stress Corrosion Cracking of Metals in Propellants

Stress corrosion cracking (SCC) of a fracture critical metallic material can cause a premature failure if the material is susceptible in the unique service environment. Material fluid compatibility is an area of interest for the current NASA programs leading the human exploration path to Mars. White Sands Test Facility, the agency's lead on hypergolic propellant testing, identifies a lack in stress corrosion cracking susceptibility data for metallic materials in hypergolic propellants. The development of a stress corrosion cracking screening method is necessary to bridge the knowledge gap and enable the community to more confidently select materials for the use in systems containing corrosive fluids.

Alcantara, Ilse↗

Optical Measurement System for Strain Field Ahead of a Crack Tip for Lattice Structures

The aim of the ARAMADAS project is to automate the construction of cuboctahedral lattice structures. Lattice materials are appealing for aerospace applications due to their strength and stiffness at ultra-light densities. However, in order for any material to be realistically considered for such environments, it must also be damage tolerant. The ability of a material to absorb damage is characterized by its fracture toughness, which remains poorly characterized for lattice materials. Consequently, the objective of this research is to develop an optical measurement system to experimentally validate the strain field ahead of a crack tip in architecture lattice materials. Although the ability to predict the strain field ahead of a crack tip has been investigated for continuum materials, such behaviour of three-dimensional architectures is under-investigated. As such, we will use a custom optical measurement system to track deformation of the voxels in a side-cracked plate fracture specimen. The system shall use 3D pose estimation, stereo imaging, and possibly color tracking, in combination with optical flow algorithms, to compute information regarding the three-dimensional movement movement of the lattice nodes during mechanical testing. Bench top experiments will validate the optical measurement system and characterize precision. Additionally, the effect of multiple cameras on precision, as well as system scalability will be investigated. Final results will compare measured lattice deformation with finite element predictions.

Lennig, Miriam↗

Experimental Study on Mitigation of Lifetime-Limiting Dielectric Cracking in Extreme Temperature 4H-SiC JFET Integrated Circuits

While NASA Glenn Research Center's "Generation 10" 4H-SiC Junction Field Effect Transistor (JFET) integrated circuits (ICs) have uniquely demonstrated 500 °C electrical operation for durations of over a year, this experimental work has also revealed that physical cracking of chip dielectric passivation layers ultimately limits extreme-environment operating lifetime [1-3]. The prevention of such dielectric passivation cracks should therefore improve IC high temperature durability and yield, leading to more beneficial technology adoption into aerospace, automotive, and energy systems. This report describes Generation 10.2, 11.1, and 11.2 die tested under unbiased and unpackaged accelerated age testing at 500 °C, 600 °C, 720 °C, and 800 °C in air-atmosphere ovens for 100- and 200-hour duration. Additional samples were separately subjected to 10 thermal cycles between the same high temperatures (with 10-hour high-temperature soak each cycle) and 50 °C. It is shown that having two stoichiometric Si3N4 layers in the interconnect dielectric stack substantially decreases the amount of dielectric cracking observed following these oven tests.

Spry, D. J.↗

Weldability Investigation of Crack Resistant Aluminum Filler Metals Developed for Large Scale Additive Manufacturing and Industrial Welding Applications

In this study the NASA MSFC welding and manufacturing team investigated a new-age aluminum filler wire designed for welding and additive manufacturing (AM) of high strength aluminum alloys. High strength aluminum alloys are known to exhibit hot cracking and hot tearing issues during fusion welding operations. The goal of this investigation was to determine whether this new-age family of alloys can suppress the hot cracking and hot tearing issues exhibited during welding of high strength aluminum alloys and to do an initial characterization of the mechanical performance of welds created using these filler wires. This study focuses on fusion welding of aluminum alloy 6061 and compares the weldability characteristics of five aluminum filler metals and two forms of 6061 base material. The MSFC team utilized manual gas tungsten arc welding (GTAW) to conduct all welding operations and carried out metallographic analysis accompanied with mechanical testing to evaluate the performance of the welds created during this study. During the study it was observed that the new-age filler wires facilitated grain refinement in the weld fusion zone and were capable of creating crack free welds in aluminum alloy 6061 while exhibiting properties that met or exceeded conventional off the shelf aluminum filler metals.

Welding↗

Stress Corrosion Cracking Behavior of Cast Stainless Steels

Casting of austenitic stainless steels offers the possibility of directly producing large and/or relatively complex structures, such as the first wall shield modules or the diverter cassette for the ITER fusion reactor. Casting offers major cost savings when compared to fabrication via welding of quarter modules machined from large forgings. However, the strength properties of such cast components are typically considered inferior to those of conventionally forged and annealed components. To improve and validate cast stainless steel as a substitute for wrought stainless steel, a development and testing program was initiated, utilizing nitrogen and manganese additions to promote improved performance. This paper focuses on the response of the first set of developmental alloys to neutron-irradiation and susceptibility to stress corrosion cracking. These cast materials may also have applications for different components in light water reactors. Results showed that all steels exhibited irradiation-induced hardening and a corresponding drop in ductility, as expected, although there is still considerable ductility in the irradiated samples. The cast steels all exhibited reduced hardening in comparison to a wrought reference steels, which may be related to a larger grain size. Higher nitrogen contents did not negatively influence irradiation performance. Regarding stress corrosion cracking susceptibility, the large difference in grain size limits the comparison between wrought and cast materials, and inclusions in a reference and archive cast alloy tests complicate analysis of these samples. Results suggest that the irradiated archive heat was more susceptible to cracking than the modified alloys, which may be related to the more complex microstructure. Further, the results suggest that the modified cast steel is at least as SCC resistant as wrought 316LN. The beneficial effect of nitrogen on the mechanical properties of the alloys remains after irradiation and is not detrimental to SCC resistance.

36 MATERIALS SCIENCE↗

Method for fabrication of crack-free ceramic dielectric films

The invention provides a process for forming crack-free dielectric films on a substrate. The process comprise the application of a dielectric precursor layer of a thickness from about 0.3 .mu.m to about 1.0 .mu.m to a substrate. The deposition is followed by low temperature heat pretreatment, prepyrolysis, pyrolysis and crystallization step for each layer. The deposition, heat pretreatment, prepyrolysis, pyrolysis and crystallization are repeated until the dielectric film forms an overall thickness of from about 1.5 .mu.m to about 20.0 .mu.m and providing a final crystallization treatment to form a thick dielectric film. Also provided was a thick crack-free dielectric film on a substrate, the dielectric forming a dense thick crack-free dielectric having an overall dielectric thickness of from about 1.5 .mu.m to about 20.0 .mu.m.

36 MATERIALS SCIENCE↗

A Qualitative Comparison of the C-Ring Test and the Jones Test as Standard Practice Test Methods for Studying Stress Corrosion Cracking in Ferritic Steels

Creep-strength-enhanced-ferritic (CSEF) steels have been widely implemented as water wall alloy materials in the coal-fired power industry for many years. The stress corrosion cracking (SCC) behavior of this class of materials is currently of significant interest to the industry due to recent failures. To better understand the test methods used to characterize SCC behavior in the laboratory, three representative CSEF alloys (T23, T24, and T92) were subjected to two SCC test protocols: the Jones Test set forth in DIN 50915, and the C-ring SCC test set forth in ASTM G38-01. Samples were tested in either the as-received (normalized + tempered) condition or in the normalized condition (quenched from 1065 C). Samples were exposed to aerated water in one test case and de-aerated water in a second test case for a period of 7 days at 200 C. It was found that for both test protocols, the normalized condition with aerated water led to severe cracking for all three alloys, whereas no evidence of cracking was found for the other conditions.

Thomson, Jeffery K↗

Method for fabrication of crack-free ceramic dielectric films

The invention provides a process for forming crack-free dielectric films on a substrate. The process comprises the application of a dielectric precursor layer of a thickness from about 0.3 .mu.m to about 1.0 .mu.m to a substrate. The deposition is followed by low temperature heat pretreatment, prepyrolysis, pyrolysis and crystallization step for each layer. The deposition, heat pretreatment, prepyrolysis, pyrolysis and crystallization are repeated until the dielectric film forms an overall thickness of from about 1.5 .mu.m to about 20.0 .mu.m and providing a final crystallization treatment to form a thick dielectric film. The process provides a thick crack-free dielectric film on a substrate, the dielectric forming a dense thick crack-free dielectric having an overall dielectric thickness of from about 1.5 .mu.m to about 20.0 .mu.m.

36 MATERIALS SCIENCE↗

Method for fabrication of crack-free ceramic dielectric films

The invention provides a process for forming crack-free dielectric films on a substrate. The process comprises the application of a dielectric precursor layer of a thickness from about 0.3 .mu.m to about 1.0 .mu.m to a substrate. The deposition is followed by low temperature heat pretreatment, prepyrolysis, pyrolysis and crystallization step for each layer. The deposition, heat pretreatment, prepyrolysis, pyrolysis and crystallization are repeated until the dielectric film forms an overall thickness of from about 1.5 .mu.m to about 20.0 .mu.m and providing a final crystallization treatment to form a thick dielectric film. The process provides a thick crack-free dielectric film on a substrate, the dielectric forming a dense thick crack-free dielectric having an overall dielectric thickness of from about 1.5 .mu.m to about 20.0 .mu.m.

36 MATERIALS SCIENCE↗

Role of Material Condition in Precursor Corrosion Damage and Stress Corrosion Crack Initiation Behavior of Alloy 600 in PWR Primary Water

Stress corrosion crack (SCC) initiation testing has been performed on a 15% cold-worked UNS N06600 (Alloy 600) heat in the mill-annealed (MA), solution annealed (SA), and thermally treated (TT) conditions to assess the role of grain boundary (GB) carbides on stress-assisted intergranular attack (IGA) and short crack nucleation and growth. The SCC initiation tests were conducted at constant load equivalent to materials yield stress in 360oC simulated PWR primary water with dissolved hydrogen at the Ni/NiO stability line. Results revealed the highest SCC initiation susceptibility in the Alloy 600 MA material followed by the TT and SA materials, suggesting the GB carbide distribution did not have a controlling effect on SCC initiation resistance. Quantitative assessments were conducted on IGA and short cracks to help understand this phenomenon and the role of GB carbides on precursor damage development that lead to differences in macroscopic SCC initiation behavior are discussed.

Zhai, Ziqing↗

LOW-FREQUENCY PHASED-ARRAY METHODS FOR CRACK DETECTION IN CAST AUSTENITIC PIPING COMPONENTS

Studies at the Pacific Northwest National Laboratory (PNNL) in Richland, Washington, are being conducted to evaluate nondestructive examination (NDE) approaches for inspecting coarse-grained, austenitic stainless steel reactor components. The work provides information to the United States Nuclear Regulatory Commission (NRC) on the utility, effectiveness, limitations, and reliability of advanced inspection techniques for application on safety-related components in commercial nuclear power plants. This paper describes results from recent assessments using a low-frequency phased-array methodology for detecting cracks in cast austenitic piping welds. Piping specimens that contain thermal and mechanical fatigue cracks located adjacent to welds were examined. The specimens have surface geometrical conditions and weld features that simulate portions of primary piping systems in many U.S. pressurized water reactors (PWRs). In addition, segments of vintage centrifugally cast piping were examined to assess inherent acoustic noise and scattering due to grain structures and determine consistency of ultrasonic (UT) responses from varied circumferential locations. The phased-array UT methods were applied from the outside surface of the specimens using automated scanning devices and water coupling, and employed a modified instrument operating between 500 kHz and 1.0 MHz. Composite volumetric images of the specimens were generated. Results from laboratory studies for assessing crack detection and sizing effectiveness are discussed, including acoustic parameters observed in centrifugally cast piping base materials.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Sensitivity to temperature and material properties of hydrogen concentration at a crack tip in austenitic stainless steel

It is well known that dissolved hydrogen interacts with the stress field at a crack tip, with one result being an intensification of the hydrogen concentration in the region of maximum crack tip stress. The current paper presents recent calculations in ongoing efforts to use coupled stress-diffusion finite element analyses to aid in the structural integrity assessment of pressure vessels containing tritium. The focus of the current work is quantification of the effect of material properties (structural and diffusion) and temperature on the values of maximum stress and hydrogen concentration at the tip of a crack. A one-way-coupled finite element model of a compact tension specimen is used in which the effect of stress and trapping on the hydrogen diffusion is accounted for. Results show that, within the ranges of inputs considered, maximum stress varies approximately linearly with a material's room temperature yield stress but nonlinearly with temperature. Also, peak lattice hydrogen is shown to be a strong function of solubility parameters, a moderate function of yield stress, but only a weak function of trap binding energy and density when trap density is relatively low.

36 MATERIALS SCIENCE↗