At least 1,765 records · Page 98

Structure, conductivity, and transparency of Ga-doped ZnO thin films arising from thickness contributions

Ga-doped ZnO (GZO) films were deposited on amorphous glass substrates at room temperature by radio frequency magnetron sputtering. It is revealed that the influence of deposition parameters, such as target-substrate distance and deposition time, on the structure and properties of the films arises primarily from the variations in film thickness. For the GZO films with smaller thicknesses ({<=}385 nm), crystallinity is greatly improved with an increase in thickness, which leads to an increase in Hall mobility and a decrease in electrical resistivity. The carrier concentration is, however, found to exhibit only a slight change with the thickness variations. The relationship of electrical property and microstructure suggests that the resistivity of the films arises mainly from ionic impurity scattering rather than from grain boundary scattering. All the films exhibit a transmittance of over 90% in the visible wavelength range. The band gap of the GZO films is widened with increasing film thickness. In combination with the result that the carrier concentration exhibited a slight dependence on thicknesses, the broadening of the band gap with thicknesses is attributed more to the improved crystallinity than to the Moss-Burstein shift.

36 MATERIALS SCIENCE↗

Effect of bombardment with different ions (H, He, Ar) on ordering transformation of Fe{sub 48}Pt{sub 52} films

Fe{sub 48}Pt{sub 52} thin films with a thickness of 50 nm were deposited at room temperature before undergoing glow-discharge-induced ion bombardment at 300 deg. C for 1 h. The energy of the incident ions was adjusted by applying a radio-frequency bias (V{sub b}) from 200 to 600 V. H{sub 2}, He, and Ar were used as the working gases. Significant ordering enhancement was only found in the H-ion bombarded films. The coercivity of such films is greatly increased from 0.5 kOe, for the sample without any bias, to around 8 kOe at V{sub b}=200-600 V, which result is similar to that for a film annealed at 400 deg. C in a vacuum. This result suggests that H-ion bombardment has the effect of a 100 deg. C increase in annealing temperature. Microstructural studies reveal that the average grain size of the H-ion bombarded films is about 30 nm, which is much smaller than that of 400 deg. C-annealed films. The film thickness of He-ion bombarded samples decreases linearly as V{sub b} increases because of the intensive sputtering effect. Under Ar-ion bombardment, most of the film is removed even at V{sub b}=200 V.

36 MATERIALS SCIENCE↗

Synthesis of 8YSZ-LSGM Composite Thick Film Ceramics for Solid Electrolyte From Nanopowder Utilizing Local Zircon Prepared Using Sol Gel Process

Thick film ceramics of 8% mol Y{sub 2}O{sub 3} doped-ZrO{sub 2}(8YSZ)-La{sub 0.8}Sr{sub 0.2}Ga{sub 0.2}Mg{sub 0.8}O{sub 3}(LSGM) composite for solid electrolyte have been synthesized from nanopowder. Concentration of LSGM was 0 and 10% weight. A paste for the thick films was made from 8YSZ nanopowder prepared using sol gel method and LSGM powder prepared by solid state reaction. Precursors for the 8YSZ nanopowder preparation were ZrOCl{sub 2{center_dot}}8H{sub 2}O derived from local zircon as byproduct of Tin processing at Bangka Island using caustic fusion method, and Y(NO{sub 3}){sub 3}. The thick films were produced by screen printing technique on alumina substrates. The films were sintered at 1500 deg. C for 2 hours in air. X-ray diffraction (XRD) data showed that the nanopowder of 8YSZ was well produced with broad peaks. The particle size of the 8YSZ powder was about 12 nm as calculated using Debye Scherrer method. The thick films of 8YSZ and 8YSZ-LSGM (90:10 in weight %) composite could be produced, however, the films still contain voids. The ionic conductance of the YSZ-10LSGM films was smaller than that of the YSZ films.

36 MATERIALS SCIENCE↗

Bias in bonding behavior among boron, carbon, and nitrogen atoms in ion implanted a-BN, a-BC, and diamond like carbon films

In this study, we implanted N{sup +} and N{sub 2}{sup +} ions into sputter deposited amorphous boron carbide (a-BC) and diamond like carbon (DLC) thin films in an effort to understand the chemical bonding involved and investigate possible phase separation routes in boron carbon nitride (BCN) films. In addition, we investigated the effect of implanted C{sup +} ions in sputter deposited amorphous boron nitride (a-BN) films. Implanted ion energies for all ion species were set at 40 KeV. Implanted films were then analyzed using x-ray photoelectron spectroscopy (XPS). The changes in the chemical composition and bonding chemistry due to ion-implantation were examined at different depths of the films using sequential ion-beam etching and high resolution XPS analysis cycles. A comparative analysis has been made with the results from sputter deposited BCN films suggesting that implanted nitrogen and carbon atoms behaved very similar to nitrogen and carbon atoms in sputter deposited BCN films. We found that implanted nitrogen atoms would prefer bonding to carbon atoms in the films only if there is no boron atom in the vicinity or after all available boron atoms have been saturated with nitrogen. Implanted carbon atoms also preferred to either bond with available boron atoms or, more likely bonded with other implanted carbon atoms. These results were also supported by ab-initio density functional theory calculations which indicated that carbon-carbon bonds were energetically preferable to carbon-boron and carbon-nitrogen bonds.

36 MATERIALS SCIENCE↗

High-RRR thin-films of NB produced using energetic condensation from a coaxial, rotating vacuum ARC plasma (CEDTM)

We have recently demonstrated unprecedentedly high values of RRR (up to 542) in thin-films of pure Nb deposited on a-plane sapphire and MgO crystal substrates. The Nb films were grown using a vacuum arc discharge struck between a reactor grade Nb cathode rod (RRR {approx} 30) and a coaxial, semi-transparent Mo mesh anode, with a heated substrate placed just outside it. The substrates were pre-heated for several hours prior to deposition at different temperatures. Low pre-heat temperatures (<300 C) and deposition temperatures (<300 C) give low RRR (<50) films, whereas higher pre-heat (700 C) and coating temperatures (500 C) give RRR=214 on a-sapphire and RRR=542 on MgO. XRD (Bragg-Brentano scans and Pole Figures), EBSD and SIMS data reveal several features: (1) on asapphire, higher temperatures show better 3D registry for epitaxial growth of Nb; the crystal structure evolves from textured, polycrystalline (with twins) to single-crystal; (2) on MgO, there is a transition from {l_brace}110{r_brace} planes to {l_brace}100{r_brace} as the temperature is increased beyond 500 C. The dramatic increase in RRR (from {approx}10 at <300 C to {approx}500 at >600 C) is correlated with better epitaxial crystal structure in both a-sapphire and MgO substrate grown films. However, the SIMS data reveal that the most important requirement for high-RRR Nb films on either substrate is the reduction of impurities in the film, especially hydrogen. The hydrogen content in the MgO grown films is 1000 times lower than in bulk Nb tested as a reference from SRF cavity grade Nb. This result has potential implications for SRF accelerators. Coating bulk Nb cavities with an MgO layer followed by our CEDTM deposited Nb films, might create superior SRF cavities that would avoid Q-slope and operate at higher peak fields.

08 HYDROGEN↗

Growth of (111) oriented NiFe{sub 2}O{sub 4} polycrystalline thin films on Pt (111) via sol-gel processing

Polycrystalline NiFe{sub 2}O{sub 4} (NFO) thin films are grown on (111) platinized Si substrates via chemical solution processing. {theta}-2{theta} x-ray diffraction, x-ray pole figures and electron diffraction indicate that the NFO has a high degree of <111> uniaxial texture normal to the film plane. The texturing is initiated by nucleation of (111) planes at the Pt interface and is enhanced with decreasing film thickness. As the NFO magnetic easy-axis is <111>, the out-of-plane magnetization exhibits improved M{sub r}/M{sub s} and coercivity with respect to randomly oriented films on silicon substrates. The out-of-plane M{sub r}/M{sub s} ratio for (111) textured NFO thin film is improved from 30% in 150 nm-thick films to above 70% in 50 nm-thick films. The improved out-of-plane magnetic anisotropy is comparable to epitaxial NFO films of comparable thickness deposited by pulsed laser deposition and sputtering.

36 MATERIALS SCIENCE↗

Epitaxial (111) films of Cu, Ni, and Cu{sub x}Ni{sub y} on {alpha}-Al{sub 2}O{sub 3} (0001) for graphene growth by chemical vapor deposition

Films of (111)-textured Cu, Ni, and Cu{sub x}Ni{sub y} were evaluated as substrates for chemical vapor deposition of graphene. A metal thickness of 400 nm to 700 nm was sputtered onto a substrate of {alpha}-Al{sub 2}O{sub 3}(0001) at temperatures of 250 Degree-Sign C to 650 Degree-Sign C. The films were then annealed at 1000 Degree-Sign C in a tube furnace. X-ray and electron backscatter diffraction measurements showed all films have (111) texture but have grains with in-plane orientations differing by 60 Degree-Sign . The in-plane epitaxial relationship for all films was [110]{sub metal}||[1010]{sub Al{sub 2O{sub 3}}}. Reactive sputtering of Al in O{sub 2} before metal deposition resulted in a single in-plane orientation over 97% of the Ni film but had no significant effect on the Cu grain structure. Transmission electron microscopy showed a clean Ni/Al{sub 2}O{sub 3} interface, confirmed the epitaxial relationship, and showed that formation of the 60 Degree-Sign twin grains was associated with features on the Al{sub 2}O{sub 3} surface. Increasing total pressure and Cu vapor pressure during annealing decreased the roughness of Cu and Cu{sub x}Ni{sub y} films. Graphene grown on the Ni(111) films was more uniform than that grown on polycrystalline Ni/SiO{sub 2} films, but still showed thickness variations on a much smaller length scale than the distance between grains.

36 MATERIALS SCIENCE↗

Effect of silver incorporation in phase formation and band gap tuning of tungsten oxide thin films

Silver incorporated tungsten oxide thin films are prepared by RF magnetron sputtering technique. The effect of silver incorporation in micro structure evolution, phase enhancement, band gap tuning and other optical properties are investigated using techniques such as x-ray diffraction, micro-Raman spectroscopy, atomic force microscopy, scanning electron microscopy, energy dispersive x-ray spectroscopy, and UV-Visible spectroscopy. Effect of silver addition in phase formation and band gap tuning of tungsten oxide thin films are investigated. It is found that the texturing and phase formation improves with enhancement in silver content. It is also found that as the silver incorporation enhances the thickness of the films increases at the same time the strain in the film decreases. Even without annealing the desired phase can be achieved by doping with silver. A broad band centered at the wavelength 437 nm is observed in the absorption spectra of tungsten oxide films of higher silver incorporation and this can be attributed to surface plasmon resonance of silver atoms present in the tungsten oxide matrix. The transmittance of the films is decreased with increase in silver content which can be due to increase in film thickness, enhancement of scattering, and absorption of light caused by the increase of grain size, surface roughness and porosity of films and enhanced absorption due to surface plasmon resonance of silver. It is found that silver can act as the seed for the growth of tungsten oxide grains and found that the grain size increases with silver content which in turn decreases the band gap of tungsten oxide from 3.14 eV to 2.70 eV.

36 MATERIALS SCIENCE↗

Metal-insulator transition induced in CaVO{sub 3} thin films

Stoichiometric CaVO{sub 3} (CVO) thin films of various thicknesses were grown on single crystal SrTiO{sub 3} (STO) (001) substrates using a pulsed electron-beam deposition technique. The CVO films were capped with a 2.5 nm STO layer. We observed a temperature driven metal-insulator transition (MIT) in CVO films with thicknesses below 4 nm that was not observed in either thick CVO films or STO films. The emergence of this MIT can be attributed to the reduction in effective bandwidth due to a crossover from a three-dimensional metal to a two-dimensional insulator. The insulating phase was only induced with a drive current below 0.1 {mu}A. X-ray absorption measurements indicated different electronic structures for thick and very thin films of CVO. Compared with the thick film ({approx}60 nm), thin films of CVO (2-4 nm) were more two-dimensional with the V charge state closer to V{sup 4+}.

36 MATERIALS SCIENCE↗

Electron beam physical vapor deposition of thin ruby films for remote temperature sensing

Thermographic phosphors (TGPs) possessing temperature-dependent photoluminescence properties have a wide range of uses in thermometry due to their remote access and large temperature sensitivity range. However, in most cases, phosphors are synthesized in powder form, which prevents their use in high resolution micro and nanoscale thermal microscopy. In the present study, we investigate the use of electron beam physical vapor deposition to fabricate thin films of chromium-doped aluminum oxide (Cr-Al{sub 2}O{sub 3}, ruby) thermographic phosphors. Although as-deposited films were amorphous and exhibited weak photoluminescence, the films regained the stoichiometry and {alpha}-Al{sub 2}O{sub 3} crystal structure of the combustion synthesized source powder after thermal annealing. As a consequence, the annealed films exhibit both strong photoluminescence and a temperature-dependent lifetime that decreases from 2.9 ms at 298 K to 2.1 ms at 370 K. Ruby films were also deposited on multiple substrates. To ensure a continuous film with smooth surface morphology and strong photoluminescence, we use a sapphire substrate, which is thermal expansion coefficient and lattice matched to the film. These thin ruby films can potentially be used as remote temperature sensors for probing the local temperatures of micro and nanoscale structures.

36 MATERIALS SCIENCE↗

Fabricating functionally graded films with designed gradient profiles using pulsed laser deposition

A novel picosecond-laser pulsed laser deposition method has been developed for fabricating functionally graded films with pre-designed gradient profiles. Theoretically, the developed method is capable of precisely fabricating films with any thicknesses and any gradient profiles by controlling the laser beam powers for the two different targets based on the film composition profiles. As an implementation example, we have successfully constructed functionally graded diamond-like carbon films with six different gradient profiles: linear, quadratic, cubic, square root, cubic root, and sinusoidal. Energy dispersive X-ray spectroscopy is employed for investigating the chemical composition along the thickness of the film, and the deposition profile and thickness errors are found to be less than 3% and 1.04%, respectively. To the best of the authors' knowledge, this is the first method for fabricating films with designed gradient profiles and has huge potential in many areas of coatings and films, including multifunctional optical films. We believe that this method is not only limited to the example considered in this study, but also can be applied to all material combinations as long as they can be deposited using the pulsed laser deposition technique.

36 MATERIALS SCIENCE↗

Multi-jump magnetic switching in ion-beam sputtered amorphous Co{sub 20}Fe{sub 60}B{sub 20} thin films

Unconventional multi-jump magnetization reversal and significant in-plane uniaxial magnetic anisotropy (UMA) in the ion-beam sputtered amorphous Co{sub 20}Fe{sub 60}B{sub 20}(5–75 nm) thin films grown on Si/amorphous SiO{sub 2} are reported. While such multi-jump behavior is observed in CoFeB(10 nm) film when the magnetic field is applied at 10°–20° away from the easy-axis, the same is observed in CoFeB(12.5 nm) film when the magnetic field is 45°–55° away from easy-axis. Unlike the previous reports of multi-jump switching in epitaxial films, their observance in the present case of amorphous CoFeB is remarkable. This multi-jump switching is found to disappear when the films are crystallized by annealing at 420 °C. The deposition geometry and the energy of the sputtered species appear to intrinsically induce a kind of bond orientation anisotropy in the films, which leads to the UMA in the as-grown amorphous CoFeB films. Exploitation of such multi-jump switching in amorphous CoFeB thin films could be of technological significance because of their applications in spintronic devices.

36 MATERIALS SCIENCE↗

Overcoming challenges to the formation of high-quality polycrystalline TiO{sub 2}:Ta transparent conducting films by magnetron sputtering

The work is focused on understanding the physical processes responsible for the modification of the structure, electrical and optical properties of polycrystalline TiO{sub 2}:Ta films formed by annealing of initially amorphous films grown by direct current magnetron sputtering of electrically conductive ceramic targets. It is shown that fine tuning of the oxygen content during deposition of amorphous TiO{sub 2}:Ta films is critical to achieving low resistivity and high optical transmittance after annealing. Increasing the total pressure during magnetron sputter deposition is shown to decrease the sensitivity of the annealed films to the oxygen flow variation during deposition of the initially amorphous layers. Polycrystalline anatase TiO{sub 2}:Ta films of low electrical resistivity (ρ{sub H} = 1.5 × 10{sup −3}Ω cm), high free electron mobility (μ{sub H} = 8 cm{sup 2}/Vs), and low extinction (k{sub 550nm} = 0.006) are obtained in this way at a total pressure of 2 Pa. The dependence of the polycrystalline film electrical properties on the oxygen content is discussed in terms of Ta dopant electrical activation/deactivation taking into account the formation of compensating defects at different oxygen pressures. The temperature-dependent transport of the polycrystalline anatase TiO{sub 2}:Ta films is investigated showing the dominant role of the optical phonon scattering in the case of films with an optimum Ti/O ratio.

36 MATERIALS SCIENCE↗

Electrical properties of scandium nitride epitaxial films grown on (100) magnesium oxide substrates by molecular beam epitaxy

Scandium nitride (ScN) films were grown on (100) MgO single crystals by a molecular beam epitaxy method. The effects of growth conditions, including [Sc]/[N] ratio, growth temperature, and nitrogen radical state, on the electrical properties of the ScN films were studied. The ScN films comprised many small columnar grains. Hall coefficient measurements confirmed that the ScN films were highly degenerate n-type semiconductors and that the carrier concentration of the ScN films was sensitive to the growth temperature and the nitrogen radical states during the film growth. The carrier concentrations of the ScN films ranged from 10{sup 19}–10{sup 21} cm{sup −3} while the Hall mobilities ranged from 50–130 cm{sup 2}·V{sup −1}·s{sup −1} for undoped films. The temperature-dependent Hall coefficient measurements showed that the carrier concentration is nearly independent of temperature, indicating that the change in resistivity with temperature is explained by a change in the Hall mobility. The temperature-dependence of the Hall mobility was strongly affected by the growth conditions.

36 MATERIALS SCIENCE↗

Effects of substrate temperature, substrate orientation, and energetic atomic collisions on the structure of GaN films grown by reactive sputtering

The combined effects of substrate temperature, substrate orientation, and energetic particle impingement on the structure of GaN films grown by reactive radio-frequency magnetron sputtering are investigated. Monte-Carlo based simulations are employed to analyze the energies of the species generated in the plasma and colliding with the growing surface. Polycrystalline films grown at temperatures ranging from 500 to 1000 °C clearly showed a dependence of orientation texture and surface morphology on substrate orientation (c- and a-plane sapphire) in which the (0001) GaN planes were parallel to the substrate surface. A large increase in interplanar spacing associated with the increase in both a- and c-parameters of the hexagonal lattice and a redshift of the optical bandgap were observed at substrate temperatures higher than 600 °C. The results showed that the tensile stresses produced during the film's growth in high-temperature deposition ranges were much larger than the expected compressive stresses caused by the difference in the thermal expansion coefficients of the film and substrate in the cool-down process after the film growth. The best films were deposited at 500 °C, 30 W and 600 °C, 45 W, which corresponds to conditions where the out diffusion from the film is low. Under these conditions the benefits of the temperature increase because of the decrease in defect density are greater than the problems caused by the strongly strained lattice that occurr at higher temperatures. The results are useful to the analysis of the growth conditions of GaN films by reactive sputtering.

36 MATERIALS SCIENCE↗

Microstructure factor and mechanical and electronic properties of hydrogenated amorphous and nanocrystalline silicon thin-films for microelectromechanical systems applications

Thin-film silicon allows the fabrication of MEMS devices at low processing temperatures, compatible with monolithic integration in advanced electronic circuits, on large-area, low-cost, and flexible substrates. The most relevant thin-film properties for applications as MEMS structural layers are the deposition rate, electrical conductivity, and mechanical stress. In this work, n{sup +}-type doped hydrogenated amorphous and nanocrystalline silicon thin-films were deposited by RF-PECVD, and the influence of the hydrogen dilution in the reactive mixture, the RF-power coupled to the plasma, the substrate temperature, and the deposition pressure on the structural, electrical, and mechanical properties of the films was studied. Three different types of silicon films were identified, corresponding to three internal structures: (i) porous amorphous silicon, deposited at high rates and presenting tensile mechanical stress and low electrical conductivity, (ii) dense amorphous silicon, deposited at intermediate rates and presenting compressive mechanical stress and higher values of electrical conductivity, and (iii) nanocrystalline silicon, deposited at very low rates and presenting the highest compressive mechanical stress and electrical conductivity. These results show the combinations of electromechanical material properties available in silicon thin-films and thus allow the optimized selection of a thin silicon film for a given MEMS application. Four representative silicon thin-films were chosen to be used as structural material of electrostatically actuated MEMS microresonators fabricated by surface micromachining. The effect of the mechanical stress of the structural layer was observed to have a great impact on the device resonance frequency, quality factor, and actuation force.

36 MATERIALS SCIENCE↗

Tuning cationic composition of La:EuTiO{sub 3−δ} films

Eu{sub 1−x}La{sub x}TiO{sub 3−δ} (x = 0, 0.3, 0.5) films were deposited in a p(Ar(96%)/H{sub 2}(4%)) = 4 × 10{sup −4} mbar atmosphere on (LaAlO{sub 3}){sub 0.3}-(Sr{sub 2}AlTaO{sub 6}){sub 0.7} vicinal substrates (0.1°). Reflection high-energy electron diffraction oscillation characteristics of a layer-by-layer growth mode were observed for stoichiometric and Ti-rich films and the laser fluence suited to deposit stoichiometric films was identified to be 1.25 J/cm{sup 2} independent of the La content. The variety of resulting film compositions follows the general trend of Eu-enrichment for low laser and Ti-enrichment for high laser fluence. X-ray diffraction confirms that all the films are compressively strained with a general trend of an increase of c-axis elongation for non-stoichiometric films. The surfaces of non-stoichiometric films have an increased roughness, the highest sheet resistances, exhibit the presence of islands, and are Eu{sup 3+} rich for films deposited at low laser fluence.

36 MATERIALS SCIENCE↗

Phonon and thermal properties of exfoliated TaSe{sub 2} thin films

We report on the phonon and thermal properties of thin films of tantalum diselenide (2H-TaSe{sub 2}) obtained via the “graphene-like” mechanical exfoliation of crystals grown by chemical vapor transport. The ratio of the intensities of the Raman peak from the Si substrate and the E{sub 2g} peak of TaSe{sub 2} presents a convenient metric for quantifying film thickness. The temperature coefficients for two main Raman peaks, A{sub 1g} and E{sub 2g}, are −0.013 and −0.0097 cm{sup −1}/{sup o}C, respectively. The Raman optothermal measurements indicate that the room temperature thermal conductivity in these films decreases from its bulk value of ∼16 W/mK to ∼9 W/mK in 45-nm thick films. The measurement of electrical resistivity of the field-effect devices with TaSe{sub 2} channels shows that heat conduction is dominated by acoustic phonons in these van der Waals films. The scaling of thermal conductivity with the film thickness suggests that the phonon scattering from the film boundaries is substantial despite the sharp interfaces of the mechanically cleaved samples. These results are important for understanding the thermal properties of thin films exfoliated from TaSe{sub 2} and other metal dichalcogenides, as well as for evaluating self-heating effects in devices made from such materials.

36 MATERIALS SCIENCE↗