Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ionic transport”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,747 records · Page 97

Phase diagram of infinite layer praseodymium nickelate Pr 1– x Sr x NiO 2 thin films

In this paper, we report the phase diagram of infinite layer Pr 1-x Sr x NiO 2 thin films synthesized via topotactic reduction from the perovskite precursor phase using CaH 2 . Based on the electrical transport properties, we find a doping-dependent superconducting dome extending between x = 0.12 and 0.28, with a maximum superconducting transition temperature T c of 14 K at x = 0.18, bounded by weakly insulating behavior on both sides. In contrast to the narrower dome observed in Nd 1–x Sr x NiO 2 , a local T c suppression near x = 0.2 was not observed for the Pr 1-x Sr x NiO 2 system. Normal state Hall effect measurements indicate mixed carrier contributions of both electrons and holes, and show a sign change in the Hall coefficient as functions of temperature and x, quite similar to that in Nd 1-x Sr x NiO 2 . Also similar is the observation of a minimum in the normal state resistivity associated with the superconducting compositions. These findings indicate an infinite layer nickelate phase diagram that is relatively insensitive to the rare-earth element, but suggest that disorder arising from the variations of the ionic radii on the rare-earth site affects the superconducting dome.

36 MATERIALS SCIENCE↗

Role of nanoparticle size and surface chemistry on ion transport and nanostructure of perfluorosulfonic acid ionomer nanocomposites

In this work, we present a systematic investigation of the impact of silica nanoparticle (SiNP) size and surface chemistry on the nanoparticle dispersion state and the resulting morphology and vanadium ion permeability of the composite ionomer membranes. Specifically, Nafion containing a mass fraction of 5% silica particles, ranging in nominal diameters from 10 nm to >1 μm and with both sulfonic acid- and amine-functionalized surfaces, was fabricated. Most notably, an 80% reduction in vanadium ion permeability was observed for ionomer membranes containing amine-functionalized SiNPs at a nominal diameter of 200 nm. Further, these membranes exhibited an almost 400% increase in proton selectivity when compared to pristine Nafion. Trends in vanadium ion permeability within a particular nominal diameter were seen to be a function of the surface chemistry, where, for example, vanadyl ion permeability was observed to increase with increasing particle size for membranes containing unfunctionalized SiNPs, while it was seen to remain relatively constant for membranes containing amine-functionalized SiNPs. In general, the silica particles tended to exhibit a higher extent of aggregation as the size of the particles was increased. From small-angle neutron scattering experiments, an increase in the spacing of the hydrophobic domains was observed for all composite membranes, though particle size and surface chemistry were seen to have varying impacts on the spacing of the ionic domains of the ionomer.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Influence of Local Distortions on Proton Mobility in Acceptor Doped Perovskites

Optimizing proton conduction in solids remains the most promising solution for achieving intermediate temperature (~750–1000 K) solid oxide fuel cell devices, and enabling selective membranes for H 2 separation. Proton conduction, a thermally activated process, exhibits its highest rates in yttrium (Y) acceptor doped BaZrO 3 at an optimal doping level of 20% Y. The presence of extended defects such as grain boundaries has typically generated a wide variability in reported conductivity values. This has hindered a fundamental mechanistic understanding of how (acceptor) doping levels correlate with the activation energy of protons to produce an optimal doping level for fast proton transport. While isolated dopants have been suggested as the primary source of proton trapping, our results indicate that it is the local dopant-density that matters. Here in this work, we show that increasing the local dopant density promotes localized lattice distortions in the presence of point defects such as oxygen-vacancies or proton interstitials. An increasing distortion amplitude traps the point defects more strongly in the form of polarons, forming defect-clusters at higher concentrations. This leads to a monotonic increase in the activation energy (and hence a decrease in proton mobility) as observed in our measurements. The optimum doping level can now be explained as a competition between increasing proton concentration with doping levels and increasing activation energy due to defect-clusters formed by defect-polarons. Based on our findings, we demonstrate how to improve proton conductivity in doped BaZrO 3 , by inhibiting this dopant-lattice polaronic interaction. Finally, this approach should be generally applicable for ionic conduction in perovskite oxides such as oxygen-ion conduction in solid-oxide fuel cells and alkali-ion conduction in solid-state batteries where carriers might get trapped as defect-polarons.

36 MATERIALS SCIENCE↗

Simulation of ion transport in layered cuprate La{sub 2}SrCu{sub 2}O{sub 6}

Oxygen diffusion in layered cuprate La{sub 2}SrCu{sub 2}O{sub 6} has been simulated by the molecular dynamics method in the temperature range of 300-2500 K. The lattice is found to transform at temperatures above 1550 K; this transformation is accompanied by a change in the pair correlation functions. The abrupt change in the oxygen diffusion coefficient in the range of 1500-1550 K may indicate the presence of a phase transition to the superionic state. The motion of oxygen anions could be traced at the microscopic level. It has been proven for the first time that the La{sub 2}SrCu{sub 2}O{sub 6} crystal lattice allows, along with displacements of O1 ions within the CuO{sub 2} layer, their migration from the crystallographic positions to the intermediate unoccupied O3 positions. The motion of O2 anions is also fairly complicated: they move not only in their layer over the O2 positions but they also jump to the neighboring layer to occupy the O1 positions. The oxygen diffusion coefficient in layered cuprate La{sub 2}SrCu{sub 2}O{sub 6} exceeds that in cuprates with perovskite structure and structure of the K{sub 2}NiF{sub 4} type (at the same temperatures), which indicates that this material has good prospects for electrodes with mixed ionic-electronic conductivity.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Regenerable Liquid Desiccants for High Efficiency Humidity Control in Microgravity

The NASA X-Hab project aims to design, manufacture, test, and prove functionality of an air humidity control subsystem to dehumidify and re-humidify air from a space cabin. The method of regulating cabin air humidity utilizes vortex phase separation, which uses an ionic liquid (IL) desiccant for air-water phase separation. This subsystem is intended to be integrated with a CO 2 removal system requiring de-humidified air to operate efficiently. The air humidity control subsystem is composed of a cold-desiccant or cold-side Vortex Phase Separator (VPS) that dehumidifies the cabin air. The dehumidified air exits the cold-side (CS) VPS chamber to flow into the CO 2 removal module, and the cold, water-laden liquid desiccant flows to a regenerative heat exchanger. From the heat exchanger the liquid desiccant continues to the heater. After heating, the desiccant flows into a hot-desiccant or hot-side (HS) VPS as the dehumidified air from CO 2 removal module enters through the HS VPS air inlet. The rehumidified air exits the HS VPS into the space cabin. One pump installed at the liquid exit of the CS VPS and one pump installed at the liquid exit of the HS VPS transport the fluid through the system. To evaluate the system’s efficiency and effectiveness, the temperature, pressure, flow rate and relative humidity are read, recorded, and analyzed at critical points along the module.

Gerardo Castro↗

The Origins of the Rate Enhancement in LiNi0.4Co0.2-yAlyMn0.4O2 (0<y<_0.2) Cathode Materials

Recently, much research has been directed towards finding a replacement cathode material for LiCoO{sub 2} combining high performance with lower cost and toxicity. One promising candidate material is the mixed transition metal oxide LiNi{sub 0.4}Co{sub 0.2}Mn{sub 0.4}O{sub 2}, which delivers 180 mAh/g below 4.4 V versus Li/Li{sup +}. However, in this material, there is 4% anti-site cation mixing, which hinders the mobility of lithium within the lattice, adversely affecting its rate performance in lithium batteries. Ongoing work in our lab has shown that partial or full substitution of cobalt with aluminum, LiNi{sub 0.4}Co{sub 0.2-y}Al{sub y}Mn{sub 0.4}O{sub 2} (0 < y {le} 0.2), can lead to significant improvements in rate performance. In particular, LiNi{sub 0.4}Co{sub 0.15}Al{sub 0.05}Mn{sub 0.4}O{sub 2} shows greatly improved rate capability with almost no sacrifice in the overall capacity delivered at low rates between 2.0 and 4.3V (Figure 1). The smaller ionic radius of Al{sup 3+} in octahedral coordination (0.535 {angstrom}) compared to Li{sup +} (0.76 {angstrom}) creates a strong driving force for the formation of a more lamellar structure in the aluminum containing materials. XRD experiments and subsequent Rietveld refinement (Figure 2) reveal a significant decrease in anti-site defect concentration upon aluminum substitution, dropping from {approx}4% at y=0 to {approx}2.5% at y=0.2. Concurrently, there is an increase in the lithium slab dimension from 2.6 {angstrom} to 2.63 {angstrom}. This expansion allows for a reduced activation energy and improved lithium diffusivity through the crystal lattice. Interestingly, the pressed pellet conductivities of Al-substituted compounds are lower than that of the parent as determined by AC impedance measurements. This lends further credence to the hypothesis that structural effects resulting in improved lithium diffusivity are responsible for the rate enhancement, rather than changes in the electronic structure. Further experiments to understand the effect of structural changes induced by Al substitution on the transport properties are underway in this laboratory. The changes in electronic conductivity and the chemical diffusion coefficient of lithium as determined by pressed pellet conductivities and GITT experiments will be discussed. Further refinement of cation ordering and crystal structure parameters as determined from neutron diffraction and XANES experiments will also be presented.

25 ENERGY STORAGE↗

Interfacial water on crystalline silica: a comparative molecular dynamics simulation study

All-atom molecular dynamics simulations were conducted to study the dynamics of aqueous electrolyte solutions confined in slit-shaped silica nanopores of various degrees of protonation. Five degrees of protonation were prepared by randomly removing surface hydrogen atoms from fully protonated crystalline silica surfaces. Aqueous electrolyte solutions containing NaCl or CsCl salt were simulated at ambient conditions. In all cases, the ionic concentration was 1 M. The results were quantified in terms of atomic density distributions within the pores, and the self-diffusion coefficient along the direction parallel to the pore surface. We found evidence for ion-specific properties that depend on ion surface, water ion, and only in some cases ion ion correlations. The degree of protonation strongly affects the structure, distribution, and the dynamic behavior of confined water and electrolytes. Cl ions adsorb on the surface at large degrees of protonation, and their behavior does not depend significantly on the cation type (either Na+ or Cs+ ions are present in the systems considered). The cations show significant ion-specific behavior. Na+ ions occupy different positions within the pore as the degree of protonation changes, while Cs+ ions mainly remain near the pore center at all conditions considered. For a given degree of protonation, the planar self-diffusion coefficient of Cs+ is always greater than that of Na+ ions. The results are useful for better understanding transport under confinement, including brine behavior in the subsurface, with important applications such as environmental remediation.

74 ATOMIC AND MOLECULAR PHYSICS↗

The Origins of the Rate Enhancement in LiNi0.4Co0.2-yAlyMn0.4O2 (0<y<_0.2) Cathode Materials

Recently, much research has been directed towards finding a replacement cathode material for LiCoO{sub 2} combining high performance with lower cost and toxicity. One promising candidate material is the mixed transition metal oxide LiNi{sub 0.4}Co{sub 0.2}Mn{sub 0.4}O{sub 2}, which delivers 180 mAh/g below 4.4 V versus Li/Li{sup +} (1, 2). However, in this material, there is 4% anti-site cation mixing, which hinders the mobility of lithium within the lattice, adversely affecting its rate performance in lithium batteries. Ongoing work in our lab has shown that partial or full substitution of cobalt with aluminum, LiNi{sub 0.4}Co{sub 0.2}Mn{sub 0.4}O{sub 2} (0 < y {le} 0.2), can lead to significant improvements in rate performance (3). In particular, LiNi{sub 0.4}Co{sub 0.2}Mn{sub 0.4}O{sub 2} shows greatly improved rate capability with almost no sacrifice in the overall capacity delivered at low rates between 2.0 and 4.3V (Figure 1). The smaller ionic radius of Al{sup 3+} in octahedral coordination (0.535 {angstrom}) compared to Li{sup +} (0.76 {angstrom}) creates a strong driving force for the formation of a more lamellar structure in the aluminum containing materials (4, 5). XRD experiments and subsequent Rietveld refinement (Figure 2) reveal a significant decrease in anti-site defect concentration upon aluminum substitution, dropping from {approx}4% at y=0 to {approx}2.5% at y=0.2. Concurrently, there is an increase in the lithium slab dimension from 2.6 {angstrom} to 2.63 {angstrom}. This expansion allows for a reduced activation energy and improved lithium diffusivity through the crystal lattice (6). Interestingly, the pressed pellet conductivities of Al-substituted compounds are lower than that of the parent as determined by AC impedance measurements. This lends further credence to the hypothesis that structural effects resulting in improved lithium diffusivity are responsible for the rate enhancement, rather than changes in the electronic structure. Further experiments to understand the effect of structural changes induced by Al substitution on the transport properties are underway in this laboratory. The changes in electronic conductivity and the chemical diffusion coefficient of lithium as determined by pressed pellet conductivities and GITT experiments will be discussed. Further refinement of cation ordering and crystal structure parameters as determined from neutron diffraction and XANES experiments will also be presented.

25 ENERGY STORAGE↗

Transport properties of lithium- lead-vanadium-telluride glass and glass ceramics

Glasses with the chemical composition 35Li{sub 2}O-(45-x)V{sub 2}O{sub 5−}20PbO-xTeO{sub 2} (where x = 2.5, 5, 7.5, 10, 15 mol %) have prepared by conventional melt quenching method. The electrical conductivity of Li{sup +} ion conducting lead vanadium telluride glass samples has been carried out both as a function of temperature and frequency in the temperature range 503K-563K and over frequencies 40 Hz to 10 MHz. The electronic conduction has been observed in the present systems. When these samples annealed around 400°C for 2hour become the glass ceramic, which also shows increase tendency of conductivity. SEM confines glass and glass ceramic nature of the prepared samples.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Fast and Scalable Synthesis of LiNi 0.5 Mn 1.5 O 4 Cathode by Sol–Gel-Assisted Microwave Sintering

High-voltage spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) is a promising cathode material for high-energy-density and high-power-density lithium-ion batteries (LIBs). The high cost of the currently available LIBs needs to be addressed urgently for wide application in the transport sector (electric vehicles, buses) and large-scale energy storage systems (ESS). Of significance, herein, novel fast and scalable microwave-assisted synthesis of LNMO is reported, which leads to a production cost cut. X-ray diffraction (XRD) analysis confirms the formation of the desired phase with high crystallinity. Field emission scanning (FE-SEM) and transmission electron microscopy (TEM) analyses indicate that the synthesized phase is of nanometric size (50–150 nm) due to an extremely short sintering time (20 min). The material synthesized at 750 °C shows a higher initial discharge capacity (130 mA h g -1 ) than that synthesized at 650 °C (115 mA h g -1 ). The materials heat treated at higher temperatures show better electrochemical performance in terms of initial capacity, rate capability, and improved cycling. The improved electrochemical performance of LNMO at 750 °C is attributed to the formation of a stable crystal structure, low charge transfer resistance at the electrode/electrolyte interface, high electrical conductivity due to the presence of a disorder structure, and improved ionic diffusivity.

25 ENERGY STORAGE↗

Aqueous NaCl and CsCl Solutions Confined in Crystalline Slit-Shaped Silica Nanopores of Varying Degree of Protonation

All-atom molecular dynamics simulations were conducted to study the dynamics of aqueous electrolyte solutions confined in slit-shaped silica nanopores of various degrees of protonation. Five degrees of protonation were prepared by randomly removing surface hydrogen atoms from fully protonated crystalline silica surfaces. Aqueous electrolyte solutions containing NaCl or CsCl salt were simulated at ambient conditions. In all cases, the ionic concentration was 1 M. The results were quantified in terms of atomic density distributions within the pores, and the self-diffusion coefficient along the direction parallel to the pore surface. We found evidence for ion-specific properties that depend on ion-surface, water-ion, and only in some cases ion-ion correlations. The degree of protonation strongly affects the structure, distribution, and the dynamic behavior of confined water and electrolytes. Cl - ions adsorb on the surface at large degrees of protonation, and their behavior does not depend significantly on the cation type (either Na + or Cs + ions are present in the systems considered). The cations show significant ion-specific behavior. Na + ions occupy different positions within the pore as the degree of protonation changes, while Cs + ions mainly remain near the pore center at all conditions considered. For a given degree of protonation, the planar self-diffusion coefficient of Cs + is always greater than that of Na + ions. The results are useful for better understanding transport under confinement, including brine behavior in the subsurface, with important applications such as environmental remediation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Technetium (VII) Co-precipitation with Framework Aluminosilicates

Technetium-99 (99Tc), a long-lived radionuclide, is one of the most widespread contaminants within the Hanford subsurface. At some depths, it is only extractable with strong acids, suggesting incorporation into a solid phase. We hypothesized that Tc may have coprecipitated with feldspathoid aluminosilicates under waste tanks that had leaked caustic solutions into the vadose zone. Our objectives were to determine if Tc could be incorporated into the feldspathoids cancrinite and sodalite and under what conditions coprecipitation could occur. Our hypothesis was that sodalite was more likely to incorporate and retain Tc. Our approach was to use known methods of feldspathoid formation in solutions resembling those in Hanford waste tanks contacting sediments in terms of major ion (Na, NO3, OH, Al(OH)4, and Si(OH)4 concentrations. In some cases, Al and Si were supplied from zeolite. We used perrhenate (ReO4) as a surrogate for pertechnetate (TcO4) to avoid the radioactivity. The major findings of this study were 1) ReO4 could be incorporated into either sodalite or cancrinite but the concentration in the solid was < 1% of the competing ion Cl, NO3, or NO2. 2) The small amount of ReO4 incorporated was not exchangeable with NO3 or NO2. 3) In sodalite, NO3 was highly preferred over ReO4 but significant Re-sodalite was formed when the mole fraction in solution (Re/Re+N) exceeded 0.8. 4) A nonlinear relation between the unit cell parameter and amount of Re incorporated suggested that a separate Re-sodalite phase was formed rather than a solid solution. 5) We determined that sodalite preference for sodalite in the presence of different anions increased with the ionic size of the competing anion: Cl < CO3 < NO3 < SO4 < MnO4 < WO4 and significant incorporation did not occur unless the difference in anion radii was less than 12%. 6) Re(VII) was not significantly reduced to Re(IV) under the conditions of this experiment and Re appeared to be a good surrogate for Tc under oxidizing conditions as both oxyanions have the same size. In conclusion, incorporation of TcO4 is unlikely in the close proximity to the tanks where sodalite is likely to form in the presence of high NO3 and other anions much smaller than TcO4.

58 GEOSCIENCES↗

Electronic Structure and Band Alignment at the NiO and SrTiO 3 p–n Heterojunctions

Understanding the energetics at the interface including the alignment of valence and conduction bands, built-in potentials, and ionic and electronic reconstructions, is an important challenge in designing oxide interfaces that have controllable multi-functionalities for novel (opto-)electronic devices. In this work, we report detailed investigations on the hetero-interface of wide bandgap p-type NiO and n-type SrTiO3 (STO). We show that despite a large lattice mismatch (~7%) and dissimilar crystal structure, high-quality NiO and Li doped NiO (LNO) thin films can be epitaxially grown on STO(001) substrates through a domain matching epitaxy (DME) mechanism. X-ray photoelectron spectroscopy (XPS) studies indicate that NiO/STO heterojunctions form a type II “staggered” band alignment. In addition, a large built-in potential of up to 0.97 eV was observed at the interface of LNO and Nb doped STO (NbSTO). The LNO/NbSTO p-n heterojunctions exhibit a large rectification ratio of 2×103, but also a large ideality factor of 4.3. The NiO/STO p-n heterojunctions have important implication for applications in photocatalysis and photodetector as the interface provides favourable energetics for facile separation and transport of photogenerated electrons and holes.

36 MATERIALS SCIENCE↗

Advancing ionomer design to boost interfacial and thin-film proton conductivity via styrene-calix[4]arene-based ionomers

Sub-micrometer-thick ion-conducting polymer (ionomer) layers often suffer from poor ionic conductivity at the substrate/catalyst interface. The weak proton conductivity makes the electrochemical reaction at the cathode of proton-exchange-membrane fuel cells sluggish. To address this, here we report on a class of polystyrene-based ionomers having sub-nanometer-sized, sulfonated macrocyclic calix[4]arene-based pendants (PS-calix). In films with thickness comparable to that of ionomer-based binder layers, the conductivity of PS-calix film (~41 mS/cm) is ~13 times higher than that of the current state-of-the-art ionomer, Nafion. We observe a similar improvement in proton conductivity when PS-calix interfaces with Pt nanoparticles, demonstrating the potential of PS-calix in catalyst ink. Leveraging a favorable interfacial chemical composition, PS-calix enhances proton conduction at the film-substrate interface, a shortcoming of Nafion. Moreover, the water in PS-calix films diffuses faster than bulk water and the water confined in Nafion films, suggesting an important role played by sub-nanometer-sized calix[4]arene cavities in creating unique water/ion transport pathways.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Nanoscale Protection Layers To Mitigate Degradation in High-Energy Electrochemical Energy Storage Systems

In the pursuit of energy storage devices with higher energy and power, new ion storage materials and high-voltage battery chemistries are of paramount importance. Yet, they invite—and often enhance—degradation mechanisms, which are reflected in capacity loss with charge/discharge cycling and sometimes in safety problems. Degradation mechanisms are often driven by fundamentals such as chemical and electrochemical reactions at electrode–electrolyte interfaces, volume expansion and stress associated with ion insertion and extraction, and profound inhomogeneity of electrochemical behavior. Although it is important to identify and understand these mechanisms at some reasonable level, it is even more critical to design strategies to mitigate these degradation pathways and to develop means to implement and validate the strategies. A growing set of research highlights the mitigation benefits achievable by forming thin protection layers (PLs) intentionally created as artificial interphase regions at the electrode–electrolyte interface. These advances highlight a promising—perhaps even generic—pathway for enabling higher-energy and higher-voltage battery configurations. In this Account, we summarize examples of such PLs that serve as mitigation strategies to avoid degradation in lithium metal anodes, conversion-type electrode materials, and alloy-type electrodes. Examples are chosen from a larger body of electrochemical degradation research carried out in Nanostructures for Electrical Energy Storage (NEES), our DOE Energy Frontier Research Center. Overall, we argue on the basis of experimental and theoretical evidence that PLs effectively stabilize the electrochemical interfaces to prevent parasitic chemical and electrochemical reactions and mitigate the structural, mechanical, and compositional degradation of the electrode materials at the electrode–electrolyte interfaces. The evidenced improvement in performance metrics is accomplished by (1) establishing a homogeneous interface for ion insertion and extraction, (2) providing mechanical constraints to maintain structural integrity and robust electronic and ionic conduction pathways, and (3) introducing spatial confinements on the electrode material matrix to alter the phase transformation (delaying the occurrence of the conversion reaction) upon Li insertion, which results in superior electrode performance, excellent capacity retention, and improved reversibility. Taken together, these examples portray a valuable role for thin protection layers synthesized over electrode surfaces, both for their benefit to cycle stability and for revealing insights into degradation and mitigation mechanisms. Furthermore, they underscore the impact of complex electrochemical behavior at nanoscale materials and nanostructure interfaces in modulating the behavior of energy storage devices at the mesoscale and macroscale.

25 ENERGY STORAGE↗

Precipitation chemistry in central Amazonia

Rain samples from three sites in central Amazonia were collected over a period of 6 weeks during the 1987 wet season and analyzed for ionic species and dissolved organic carbon. A continuous record of precipitation chemistry and amount was obtained at two of these sites, which were free from local or regional pollution, for a time period of over 1 month. The volume-weighted mean concentrations of most species were found to be about a factor of 5 lower during the wet season compared with previous results from the dry season. Only sodium, potassium, and chloride showed similar concentrations in both seasons. When the seasonal difference in rainfall amount is taken into consideration, the deposition fluxes are only slightly lower for most species during the wet season than during the dry season, again with the exception of chloride, potassium, and sodium. Sodium and chloride are present in the same ratio as in sea salt; rapid advection of air masses of marine origin to the central Amazon Basin during the wet season may be responsible for the observed higher deposition flux of these species. Statistical analysis suggests that sulfate is, to a large extent, of marine (sea salt and biogenic) origin, but that long-range transport of combustion-derived aerosols also makes a significant contribution to sulfate and nitrate levels in Amazonian rain. Organic acid concentrations in rain were responsible for a large fraction of the observed precipitation acidity; their concentration was strongly influenced by gas/liquid interactions.

Andreae, M. O.↗

Electric Field Effects on Water and Ion Structure and Diffusion at the Orthoclase (001)–Water Interface

Understanding the electrochemical properties of mineral–water interfaces tends to rely upon electrical double layer (EDL) models, but these models are based on the assumption that electrostatic equilibrium is constantly maintained. In reality, interfacial reactions, ion diffusion, and their electrochemical signatures are based in nonequilibrium conditions of locally or globally imbalanced electrical fields where current EDL models have limited purview. In this work, we performed molecular dynamics (MD) simulations of the orthoclase (001) surface in contact with a 1 M NaCl aqueous solution under various electric fields, to explore the interplay between EDL structure and dynamics when perturbed by electric fields of different direction and strength, by confinement, and by different distributions of structural surface charge. The simulations showed that confinement between two opposing (001) surfaces led to the development of an induced field when the applied field was perpendicular to the surfaces and, as a result, to ionic diffusion coefficients that were independent of electric field strength. In contrast, when the applied field was parallel to the surfaces, confinement resulted in ionic diffusion coefficients that were more strongly dependent on the magnitude of the electric field than in bulk water. Differences in the density and distribution of aluminol groups on the two surfaces had a significant impact on how the interfacial structure and dynamics varied in the presence of an electric field. Notably, these differences resulted in an electro-osmotic flow with opposite directions at the two surfaces under parallel applied electric field. Overall, the MD simulations highlighted the importance of considering atomic-level structure and heterogeneities when developing models of the electrochemical properties of mineral–water interfaces.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗