Process–Property–Performance Mapping of Additively Manufactured 316H Stainless Steel Components

The Advanced Materials and Manufacturing Technologies Program is focused on accelerating the development of advanced materials and components fabricated via additive manufacturing, and is using laser powder bed fusion (LPBF) of 316H stainless steel as an initial case study. In the previous fiscal year, miniature high-throughput specimens were printed on multiple LPBF systems to provide initial processing windows to minimize porosity and limit epitaxial grain growth during prints. This fiscal year, scaled builds were completed on three different LPBF systems at ORNL: a GE Concept Laser M2, a Renishaw AM400, and an EOS M290. Builds on the Concept Laser were conducted on multiple powder lots and processing parameter ranges to provide microstructure effects on time-independent and time-dependent mechanical properties. Builds on the Renishaw were produced using Oak Ridge National Laboratory (ORNL)-optimized printing parameters and Argonne National Laboratory (ANL)-optimized printing parameters to compare outcomes of parallel process optimization efforts at different national laboratories on the same LPBF system. Similarly, the build completed on the EOS M290 replicated the processing parameters of builds completed at Los Alamos National Laboratory (LANL). Optical microscopy and electron backscatter diffraction characterization was completed on all builds. In addition to the general round robin characterization, this work-package generated time-independent data, including tensile and fracture toughness test data on scaled Concept Laser builds as a function of processing parameters and post-build heat treatment. This analysis is complimentary to work in parallel work packages aiming to establish heat treatment and processing effects on time-dependent properties. It was found that although the stress-relief heat treatment provides the highest strength at lower-temperatures, tensile strength begins to converge at higher temperatures regardless of heat treatment condition. In addition, the more rigorous solution annealing and hot-isostatic pressing post-build heat treatments result in higher fracture toughness than the stress-relieved condition. The root-causes of the lower fracture toughness of the stress-relieved LPBF 316H material was informed via a stress-relief optimization study on a scaled concept laser print, where it was found that although dislocation recovery was largely complete after only a couple hours at 650°C, the extended hold of the current 24h heat treatment employed on scaled builds likely caused increased carbide volume fractions along the LPBF 316H grain boundaries, thereby deteriorating crack propagation resistance. This trend was seen to become more deleterious with additional increases of stress-relief temperature to 750°C or 850°C. These results have helped inform a new optimal stress-relief annealing condition for LPBF 316H for future campaign testing (650°C for 2h).

36 MATERIALS SCIENCE↗

Mechanisms of Rhyolitic Glass Hydration Below the Glass Transition

Although a great deal is known about the interaction between water and rhyolitic glasses and melts at temperatures above the glass transition, the nature of this interaction at lower temperatures is much more obscure. Comparisons between high- and low-temperature diffusion studies suggest that several factors play important roles under lower-temperature conditions that are not significant at higher temperatures. Water concentrations in rhyolitic glasses hydrated at low temperatures are significantly greater than in those hydrated at high temperatures and low pressures. Surface concentrations, which equilibrate quickly with the surrounding environment at high temperature, change far more slowly as temperature decreases, and may not equilibrate at room temperature for hundreds or thousands of years. Temperature extrapolations of high- and low-temperature diffusion data are not consistent, suggesting that a change in mechanism occurs. These differences may be due to the inability of "self-stress," caused by the in-diffusing species, to relax at lower temperature. Preliminary calculations suggest that the level of stress caused by glass-water interaction may be greater than the tensile strength of the glass. On a microstuctural scale, extrapolations of high-temperature Fourier transform infrared spectroscopy (FTIR) data to lower temperatures suggests that there should be little or no hydroxyl present in glasses hydrated at low temperature. Comparisons of low-temperature hydration results among SiO2, obsidian, and albite compositions show distinct differences, and features are present in the spectra that do not occur at high temperature. Analysis of H2O and D2O diffusion also suggest that mechanistic differences occur between low- and high-temperature diffusive processes.

58 GEOSCIENCES↗

Micromechanical modeling of non-linear stress-strain behavior of polycrystalline microcracked materials under tension

The stress-strain behavior of microcracked polycrystalline materials (such as ceramics or rocks) under conditions of tensile, displacement-controlled, loading is discussed. Micromechanical explanation and modeling of the basic features, such as non-linearity and hysteresis in stress-strain curves, is developed, with stable microcrack propagation and “roughness” of intergranular cracks playing critical roles. Experiments involving complex loading histories were done on large- and medium grain size β-eucryptite ceramic. As a result, the model is shown to reproduce the basic features of the observed stress-strain curves.

36 MATERIALS SCIENCE↗

Optimization of the Mechanical Properties and Residual Stresses in 2024 Aluminum Alloy Through Heat Treatment

Residual stresses induced during quenching of aluminum alloys cause dimensional instability and distortion. In this study, the effects of different concentrations of polyalkylene glycol (PAG) quenchants on residual stresses and mechanical properties of 2024 aluminum alloy were investigated. Surface residual stresses were measured by using hole-drilling strain-gauge method. Also, mechanical properties and microstructure of the heat-treated samples were analyzed using hardness measurements, tensile tests, and transmission electron microscopy. Results showed that quenching into a 15% polymeric solution and aging at 190 °C for 12 h cause 50% reduction in residual stress as compared with quenching in water at 20 °C and naturally aging. Moreover, tensile strength decreased by 104 MPa (~ 20%) in compared with the T6 sample.

36 MATERIALS SCIENCE↗

In-situ stress analysis with X-Ray diffraction for yield locus characterization of sheet metals

A main problem in the field of sheet metal characterization is the inhomogeneous plastic deformation in the gauge regions of specimens which causes the analytically calculated stresses to differ from the sought state of stress acting in the middle of the gauge region. To overcome this problem, application of X-Ray diffraction is analyzed. For that purpose a mobile X-ray diffractometer and an optical strain measurement system are mounted on a universal tensile testing machine. This enables the recording of the whole strain and stress history of a material point. The method is applied to uniaxial tension tests, plane strain tension tests and shear tests to characterize the interstitial free steel alloy DC06. The applicability of the concepts of stress factors is verified by uniaxial tension tests. The experimentally obtained values are compared with the theoretical values calculated with crystal elasticity models utilizing the orientation distribution functions (ODF). The relaxation problem is addressed which shows itself as drops in the stress values with the strain kept at a constant level. This drop is analyzed with elasto-viscoplastic material models to correct the measured stresses. Results show that the XRD is applicable to measure the stresses in sheet metals with preferred orientation. The obtained yield locus is expressed with the Yld2000–2D material model and an industry oriented workpiece is analyzed numerically. The comparison of the strain distribution on the workpiece verifies the identified material parameters.

36 MATERIALS SCIENCE↗

Shape stabilised phase change materials (SSPCMs): High density polyethylene and hydrocarbon waxes

Shape stabilised phase change materials (SSPCMs) based on high density polyethylene (HDPE) with high (HPW, T{sub m}=56-58 °C) and low (L-PW, T{sub m}=18-23 °C) melting point waxes were prepared by melt-mixing in a twin-screw extruder and their potential in latent heat thermal energy storage (LHTES) applications for housing assessed. The structure and morphology of these blends were investigated by scanning electron microscopy (SEM). Both H-PW and L-PW were uniformly distributed throughout the HDPE matrix. The melting point and latent heat of the SSPCMs were determined by differential scanning calorimetry (DSC). The results demonstrated that both H-PW and L-PW have a plasticisation effect on the HDPE matrix. The tensile and flexural properties of the samples were measured at room temperature (RT, 20±2 °C) and 70 °C, respectively. All mechanical properties of HDPE/H-PW and HDPE/L-PW blends decreased from RT to 70 °C. In all instances at RT, modulus and stress, irrespective of the mode of deformation was greater for the HDPE/H-PW blends. However, at 70 °C, there was no significant difference in mechanical properties between the HDPE/H-PW and HDPE/L-PW blends.

36 MATERIALS SCIENCE↗

Residual Stress Reversal in Highly Strained Shot Peened Structural Elements

The purpose of this research was to further the understanding of a crack initiation problem in a highly strained pressure containment housing. Finite Element Analysis methods were used to model the behavior of shot peened materials undergoing plastic deformation. Analytical results are in agreement with laboratory tensile tests that simulated the actual housing load conditions. These results further validate the original investigation finding that the shot peened residual stress had reversed, changing from compressive to tensile, and demonstrate that analytical finite element methods can be used to predict this behavior.

Mitchell, William S.↗

Some observations on loss of static strength due to fatigue cracks

Static tensile tests were performed on simple notched specimens containing fatigue cracks. Four types of aluminum alloys were investigated: 2024-T3(formerly 24S-T3) and 7075-T6(formerly 75S-T6) in sheet form, and 2024-T4(formerly 24S-T4) and 7075-T6(formerly 75S-T6) in extruded form. The cracked specimens were tested statically under four conditions: unmodified and with reduced eccentricity of loading by three methods. Results of static tests on C-46 wings containing fatigue cracks are also reported.

MATERIALS, PROPERTIES - FATIGUE↗

Wire Cloth as Porous Material for Transpiration-cooled Walls

The permeability characteristics and tensile strength of a porous material developed from stainless-steel corduroy wire cloth for use in transpiration-cooled walls where the primary stresses are in one direction were investigated. The results of this investigation are presented and compared with similar results obtained with porous sintered metal compacts. A much wider range of permeabilities is obtainable with the wire cloth than with the porous metal compacts considered and the ultimate tensile strength in the direction of the primary stresses for porous materials produced from three mesh sizes of wire cloth are from two to three times the ultimate tensile strengths of the porous metal compacts.

MATERIALS - TYPES↗

Refining whisker size of 2024Al/Al18B4O33w composite through extrusion and its effects on the material's micro-structures and mechanical properties

Highlights: • The nonuniform distributions of stress and velocity along whisker lead to whisker breakage. • The microcrack between broken whiskers can propagate into interface or matrix, related to the wedge angle of broken whisker. • The whisker breakage and staggered result in the decreasing distance between neighboring whiskers. • The smaller distance between neighboring whiskers reduces the resistance to the propagation of crack resulting in the lower ultimate tensile strength of extruded composite. - Abstract: Hot extrusion is used to improve the distribution of whiskers and refine the whisker sizes of 2024Al/Al{sub 18}B{sub 4}O{sub 33}w composite. The grain size and the ultimate tensile strength of the extruded 2024Al/Al{sub 18}B{sub 4}O{sub 33}w composite are analyzed. The results show that the average length of whiskers decreases due to the whisker breakage. The nonuniform distributions of stress and velocity along the whisker lead to whisker breakage. The microcrack between the broken whiskers can propagate into the interface or the matrix, related to the wedge angle of the broken whisker. The extrusion is beneficial to the whisker staggered and makes it easy for the microcracks filled with matrix. The whisker breakage and the whisker staggered result in the decreasing distance between the neighboring whiskers. Due to the dislocation motion constrained by matrix and the overlap of the deformation areas, the decreasing distance between the neighboring whiskers promoting the recrystallization results in the smaller grain size. During tensile tests, due to the smaller resistance with the smaller distance between the neighboring whiskers, the cracks between the progressive broken whiskers are easy to coalesce resulting in the lower ultimate tensile strength of the extruded composite.

36 MATERIALS SCIENCE↗

Strain-induced stabilization of Al functionalization in graphene oxide nanosheet for enhanced NH{sub 3} storage

Strain effects on the stabilization of Al ad-atom on graphene oxide (GO) nanosheet as well as its implications for NH{sub 3} storage have been investigated using first-principles calculations. Tensile strain is found to be very effective in stabilizing the Al ad-atom on GO. It strengthens the C-O bonds through an enhanced charge transfer from C to O atoms. Interestingly, Al's stability is governed by the bond strength of C-O rather than that of Al-O. Optimally strained Al-functionalized GO binds up to 6 NH{sub 3} molecules, while it binds no NH{sub 3} molecule in unstrained condition.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Thermomechanical behavior and microstructural evolution of a Ni(Pd)-rich Ni 24.3 Ti 49.7 Pd 26 high temperature shape memory alloy

We investigated the effect of thermomechanical cycling on a slightly Ni(Pd)-rich Ni 24.3 Ti 49.7 Pd 26 (near stochiometric Ni–Ti basis with Pd replacing Ni) high temperature shape memory alloy. Furthermore, aged tensile specimens (400 °C/24 h/furnace cooled) were subjected to constant-stress thermal cycling in conjunction with microstructural assessment via in situ neutron diffraction and transmission electron microscopy (TEM), before and after testing. It was shown that in spite of the slightly Ni(Pd)-rich composition and heat treatment used to precipitation harden the alloy, the material exhibited dimensional instabilities with residual strain accumulation reaching 1.5% over 10 thermomechanical cycles. This was attributed to insufficient strengthening of the material (insufficient volume fraction of precipitate phase) to prevent plasticity from occurring concomitant with the martensitic transformation. In situ neutron diffraction revealed the presence of retained martensite while cycling under 300 MPa stress, which was also confirmed by transmission electron microscopy of post-cycled samples. Neutron diffraction analysis of the post-thermally-cycled samples under no-load revealed residual lattice strains in the martensite and austenite phases, remnant texture in the martensite phase, and peak broadening of the austenite phase. The texture we developed in the martensite phase was composed mainly of those martensitic tensile variants observed during thermomechanical cycling. Presence of a high density of dislocations, deformation twins, and retained martensite was revealed in the austenite state via in-situ TEM in the post-cycled material, providing an explanation for the observed peak broadening in the neutron diffraction spectra. Despite the dimensional instabilities, this alloy exhibited a biased transformation strain on the order of 3% and a two-way shape memory effect (TWSME) strain of ~2%, at relatively high actuation temperatures.

36 MATERIALS SCIENCE↗

Impact of specimen preparation method on photovoltaic backsheet degradation during accelerated aging test

In this study, we highlight some important factors in the specimen preparation methods for evaluating photovoltaic backsheet properties after accelerated aging. Two different sequences are considered: Method (I) cut-then-age: cut into 1-cm wide strips and then expose to stress, and Method (II) age-then-cut: expose a larger sheet to stress and then cut into 1-cm widths for mechanical property measurements. We also compare the effect of three cutting methods, (a) tensile specimen punch, (b) paper cutter, and (c) fresh razor blade. Several commercial backsheets were evaluated, with stress exposures including (a) pressure cooker test (PCT), (b) dry ultraviolet (UV) radiation exposure, and (c) UV combined damp heat tests. Fourier transform infrared spectrometer (FTIR) and intrinsic viscosity (IV) were used to analyze the materials on unstressed materials and samples exposed to PCT. The results show that both the cutting method and the time of cutting have an impact on the backsheet mechanical properties. Additionally, under UV exposure, Method II, age-then-cut, generally resulted in a higher average value, with more variation than Method I; however, if the side strips from Method II were excluded, the variation dropped to the same level. This is because the specimens at the sides of the sheet get additional damage from UV light from the exposed sides of the sample. In contrast to UV exposure, PCT specimens prepared by Method II result in lower average values and higher variability. This is attributed to embrittlement through the bulk of the sample where the cutting of embrittled specimens appears to result in more edge defects which can then initiate a break at smaller strains. The data suggest that for UV exposures, the specimens should be cut after aging and the exposed side specimens discarded, and that for PCT exposures, the specimens should be cut before the exposure.

14 SOLAR ENERGY↗

On the Prediction of Uniaxial Tensile Behavior Beyond the Yield Point of Wrought and Additively Manufactured Ti-6Al-4V

In this paper, phenomenological relationships are presented that permit the prediction of the plastic regime of stress–strain curves using a limited number of parameters. These relationships were obtained from both conventional (wrought + β annealed) and additively manufactured (i.e., “3D printed”) Ti-6Al-4V. Three different methods of additive manufacturing have been exploited to produce the materials, including large-volume electron beam additive manufacturing, large-volume laser hot wire additive manufacturing, and small-volume selective laser melting. The general fundamental expressions are independent not only of the additive manufacturing process, but also of a wide variety of post-deposition heat treatments, however the coefficients are specific to material states. Thus, this work demonstrates that it is possible to predict not only the ultimate tensile strength, but also the full true stress, true strain curves, if certain parameters of the material are known. In general, the prediction of ultimate tensile strength are within 5% of the experimentally measured values across all additive manufacturing variants and subsequent heat treatments. The absolute values of ultimate tensile strength range from ~ 910 MPa to ~ 1170 MPa for the single alloy Ti-6Al-4V. Data representing 113 explicit samples are included in this work.

36 MATERIALS SCIENCE↗

Fatigue Behavior of a Third Generation PM Disk Superalloy

The fatigue behavior of a 3rd generation PM disk alloy, LSHR, was studied at 1300 F. Tensile, creep, and fatigue tests were run on smooth and notched (Kt = 2) bars under a variety of conditions. Analysis of smooth bar fatigue data, run under strain and load control with R ratios of 0 and -1, showed that a stress based Smith-Watson-Topper approach could collapse the data set. While the tensile and creep data showed substantial notch strengthening at 1300 F, the fatigue data showed a life deficit for the notch specimens. A viscoplastic finite element model, which accounted for stress relaxation at the notch tip, provided the best correlation between the notched and smooth bar behavior, although the fatigue data was not fully rationalized based on this simplified viscoplastic model of the stresses at the notch tip.Inclusion of a 90 sec dwell at peak load was found to dramatically decrease notch fatigue life. This result was shown to be consistent with a simple linear creep-fatigue damage rule, where creep damage dominated at low stresses and fatigue damage was more prevalent at higher stresses.

Gayda, John↗

Deformation and fracture behavior of composite structured Ti-Nb-Al-Co(-Ni) alloys

Tensile ductility of the Ti-based composites, which consist of a β-Ti phase surrounded by ultrafine structured intermetallics, is tunable through the control of intermetallics. The two Ti-based alloys studied exhibit similar compressive yield strength (about 1000 MPa) and strain (about 35%–40%) but show a distinct difference in their tensile plasticity. The alloy Ti{sub 71.8}Nb{sub 14.1}Ni{sub 7.4}Al{sub 6.7} fractures at the yield stress while the alloy Ti{sub 71.8}Nb{sub 14.1}Co{sub 7.4}Al{sub 6.7} exhibits about 4.5% of tensile plastic deformation. To clarify the effect of microstructure on the deformation behavior of these alloys, tensile tests were carried out in the scanning electron microscope. It is shown that the distribution as well as the type of intermetallics affects the tensile ductility of the alloys.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Slow Strain Rate Tensile Testing to Assess the Ability of Superalloys to Resist Environment-Assisted Intergranular Cracking

Intergranular fatigue crack initiation and growth due to environmental degradation, especially at notched features, can often limit the fatigue life of disk superalloys at high temperatures. For clear comparisons, the effects of alloy composition on cracking in air needs to be understood and compared separately from variables associated with notches and cracks such as effective stress concentration, plastic flow, stress relaxation, and stress redistribution. The objective of this study was to attempt using simple tensile tests of specimens with uniform gage sections to compare the effects of varied alloy composition on environment-assisted cracking of several powder metal and cast and wrought superalloys including ME3, LSHR, Udimet 720, ATI 718Plus alloy, Haynes 282, and Inconel 740. Slow and fast strain-rate tensile tests were found to be a useful tool to compare propensities for intergranular surface crack initiation and growth. The effects of composition and heat treatment on tensile fracture strain and associated failure modes were compared. Environment interactions were determined to often limit ductility, by promoting intergranular surface cracking. The response of various superalloys and heat treatments to slow strain rate tensile testing varied substantially, showing that composition and microstructure can significantly influence environmental resistance to cracking.

Heat resistant alloys↗

Molecular Based Temperature and Strain Rate Dependent Yield Criterion for Anisotropic Elastomeric Thin Films

A molecular formulation of the onset of plasticity is proposed to assess temperature and strain rate effects in anisotropic semi-crystalline rubbery films. The presented plane stress criterion is based on the strain rate-temperature superposition principle and the cooperative theory of yielding, where some parameters are assumed to be material constants, while others are considered to depend on specific modes of deformation. An orthotropic yield function is developed for a linear low density polyethylene thin film. Uniaxial and biaxial inflation experiments were carried out to determine the yield stress of the membrane via a strain recovery method. It is shown that the 3% offset method predicts the uniaxial elastoplastic transition with good accuracy. Both the tensile yield points along the two principal directions of the film and the biaxial yield stresses are found to obey the superposition principle. The proposed yield criterion is compared against experimental measurements, showing excellent agreement over a wide range of deformation rates and temperatures.

Bosi, F.↗