Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “BRITTLENESS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,747 records · Page 97

Fracture and crack growth in orthotropic laminates

Solutions are developed for the two dimensional region containing unidirectional fibers with initial damage in the form of a notch, a rectangular cut out, and a circular hole. An ultimate stress failure criterion is used for both the fibers and the matrix, simple tension for the fibers, and shear failure for the matrix. Models which account for longitudinal matrix yielding and splitting as well as transverse matrix yielding and fiber breakage as a function of initial damage, material properties, and applied stress are presented. For ductile matrix composites the results indicate that longitudinal matrix yielding and transverse notch extension are the most significant forms of damage. The extent of the stable transverse damage is shown to be approximately constant, independent of initial notch length. In the case of brittle matrix composites (graphite/epoxy) longitudinal splitting is shown to be the dominant form of damage.

Goree, J. G.↗

A review of high-temperature adhesives

The development of high temperature adhesives and polyphenylquinoxalines (PPQ) is reported. Thermoplastic polyimides and linear PPQ adhesive are shown to have potential for bonding both metals and composite structures. A nadic terminated addition polyimide adhesive, LARC-13, and an acetylene terminated phenylquinoxaline (ATPQ) were developed. Both of the addition type adhesives are shown to be more readily processable than linear materials but less thermooxidatively stable and more brittle. It is found that the addition type adhesives are able to perform, at elevated temperatures up to 595 C where linear systems fail thermoplastically.

St.clair, A. K.↗

A review and assessment of the stress-intensity factors for surface cracks

The stress-intensity factor solutions proposed for a surface crack in a finite plate subjected to uniform tension are reviewed. Fourteen different solutions obtained over the past 16 years using approximate analytical methods, experimental methods, and engineering estimates are compared. The accuracy of the various solutions is assessed by correlating fracture data on surface-cracked tension specimens made of a brittle epoxy material. Fracture of the epoxy material was characterized by a constant value of stress-intensity factor as failure. Thus, the correctness of various solutions is judged by the variations in the stress-intensity factors at failure. The solutions were ranked in order of minimum standard deviation. The highest ranking solutions correlated 95% of data analyzed within + or - 10% whereas the lowest ranking solutions correlated 95% of data analyzed within + or - 20%. Some solutions could be applied to all data considered, whereas others were limited with respect to crack shapes and crack sizes that could be analyzed.

Newman, J. C., Jr.↗

Influence of fluids on the abrasion of silicon by diamond

Silicon wafers ((100)-p-type) were abraded at room temperature in acetone, absolute ethanol and water by a pyramid diamond and the resulting groove depth was measured as a function of normal force on the diamond and the absorbed fluids, while all other experimental conditions were held constant. The groove depth rates are in the ratio of 1:2:3 for water, absolute ethanol, and acetone, respectively, for a constant normal force. The groove depth rate is lower when the normal force is decreased. The silicon abraded in the presence of water was chipped as expected for a classical brittle material while the surfaces abraded in the other two fluids showed ductile ploughing as the main mechanism for silicon removal.

Danyluk, S.↗

Fundamental studies of the solid-particle erosion of silicon

The predictions of the theories of solid-particle erosion of brittle materials are compared to experimental results of studies in which angular Al2O3 particles with mean diameters D of 23 to 270 microns are used to erode (111) surfaces of silicon single crystals at impact angles alpha from 20 to 90 deg and velocities v from 30 to 150 m/s. The description of the steady state erosion rate by a power law, delta W varies directly as (v sin alpha)(n)D(m) must be modified to include threshold and plasticity effects. Furthermore the velocity exponent n depends on D. Results using abrasives of different sizes mixed together can be explained using a logarithmic-normal distribution. The results of transient experiments can be used to explain the synergistic effects which are observed using a biomodal distribution of abrasives.

Routbort, J. L.↗

Separator for alkaline batteries and method of making same

The preparation of membranes suitable for use as separators in concentrated alkaline battery cells by selective solvolysis of copolymers of methacrylate esters with acrylate esters followed by addition of a base and to the resultant products is described. The method of making copolymers by first copolymerizing a methacrylate ester (or esters) with a more readily hydrolyzable ester, followed by a selective saponification whereby the methacrylate ester moieties remain essentially intact and the readily hydrolyzable ester moiety is suponified and to the partial or complete neutralization of the relatively brittle copolymer acid with a base to make membranes which are sufficiently flexible in the dry state so that they may be wrapped around electrodes without damage by handling is described.

Hoyt, H. E.↗

The relative stress-corrosion-cracking susceptibility of candidate aluminum-lithium alloys for aerospace structural applications

The microstructure and tensile properties of two powder metallurgy processed aluminum-lithium alloys were determined. Strength properties of 480 MPa yield and 550 MPa ultimate tensile strength with 5% strain to fracture were attained. Very little reduction in area was observed and fracture characteristics were brittle. The magnesium bearing alloy exhibited the highest strength and ductility, but fracture was intergranular. Recrystallization and grain growth, as well as coarse grain boundary precipitation, occurred in Alloy 2. The fracture morphology of the two alloys differed. Alloy 1 fractured along a plane of maximum shear stress, while Alloy 2 fractured along a plane of maximum tensile stress. It is found that a fixed orientation relationship exists between the shear fracture plane and the rolling direction which suggests that the PM alloys are strongly textured.

Pizzo, P. P.↗

Hot tensile tests of Inconel 718

The physical metallurgy of near-solidus integranular cracking in Inconel 718 welds was investigated. The data, although inconclusive, suggest at least two mechanisms which might explain intergranular cracking (microfissuring) in the heat-affected zone of several high temperature alloys. One theory is based on the separation of intergranular liquid while the other involves mechanical failure of solid ligaments surrounded by intergranular liquid. Both mechanisms concentrate strain in the grain boundaries resulting in low strain (1%) intergranular brittleness. The mechanisms reported might also pertain to the physical metallurgy of casting, powder metallurgy sintering and hot isostatic pressing.

Source record↗

An empirical stress-intensity factor equation for the surface crack

This paper presents an empirical stress-intensity factor equation for a surface crack as a function of parametric angle, crack depth, crack length, plate thickness and plate width for tension and bending loads. The stress-intensity factors used to develop the equation were obtained from a previous three-dimensional, finite-element analysis of semielliptical surface cracks in finite elastic plates subjected to tension or bending loads. A wide range of configuration parameters was included in the equation. The ratios of crack length to plate thickness and the ratios of crack depth to crack length ranged from 0 to 1.0. The effects of plate width on stress-intensity variations along the crack front were also included. The equation was used to predict patterns of surface-crack growth under tension or bending fatigue loads. The equation was also used to correlate surface-crack fracture data for a brittle epoxy material within + or - 10 percent for a wide range of crack shapes and crack sizes.

Newman, J. C., Jr.↗

Hard permanent magnet development trends and their application to A.C. machines

The physical and magnetic properties of Mn-Al-C, Fe-Cr-Co, and RE-TM (rare earth-transition metal intermetallics) in polymer and soft metal bonded or sintered form are considered for ac circuit machine usage. The manufacturing processes for the magnetic materials are reviewed, and the mechanical and electrical properties of the magnetic materials are compared, with consideration given to the reference Alnico magnet. The Mn-Al-C magnets have the same magnetic properties and costs as Alnico units, operate well at low temperatures, but have poor high temperature performance. Fe-Cr-Co magnets also have comparable cost to Alnico magnets, and operate at high or low temperature, but are brittle, expensive, and contain Co. RE-Co magnets possess a high energy density, operate well in a wide temperature range, and are expensive. Recommendation for exploring the rare-earth alternatives are offered.

Mildrum, H. F.↗

The contribution of activated processes to Q

The possible role of activated processes in seismic attenuation is investigated. In this study, a solid is modeled by a parallel and series configuration of dashpots and springs. The contribution of stress and temperature activated processes to the long term dissipative behavior of this system is analyzed. Data from brittle rock deformation experiments suggest that one such process, stress corrosion cracking, may make a significant contribution to the attenuation factor, Q, especially for long period oscillations under significant tectonic stress.

Spetzler, H. A.↗

Fracture behavior of low-density fibrous ceramics

A study has been carried out to characterize the fracture behavior of a particular class of silica tiles used in the thermal protection system of the Space Shuttle with emphasis on the strength distribution and time dependence of strength. The approach adopted is based on fracture mechanics concepts developed in recent years for the design of brittle materials. The study confirms that proof-testing and tile densification should lead to improved reliability of the thermal protection system. The research also suggests that the subcritical crack growth behavior of the fibrous tiles is similar to that observed in bulk glass of similar composition and that failure occurs by the tensile fracture and fragmentation of individual fibers.

Green, D. J.↗

The application of fracture mechanics to failure analysis of photovoltaic solar modules

Cracking of silicon solar cells and solar module transparent cover panels such as glass or polymethylmethacrylate (PMMA) is a major cause of photovoltaic solar module failure in field service. Silicon and cover materials are brittle, and cracking of these materials is expected to result from the extension of preexisting flaws under stress. Study of the cracking mechanisms is therefore an appropriate area for the application of fracture mechanics principles. In this study, fracture mechanics techniques were employed to identify the mode of crack propagation, to examine the fracture-initiating flaw, to estimate the nature and magnitude of fracture stress in the field, and to predict analytically the service lifetime. Recommendations for corrective actions are also made.

Chen, C. P.↗

Positioning Vise for Crystal Cleavage

Vise manipulates brittle crystals, such as lithium fluoride, so they are in proper position for cleaving. Vise allows crystals as thin as 2 millimeters or less positioned so that cleaved without breakage. Vise holds workpiece firmly but gently. Bushings, shafts and adjusting screw designed to move jaws smoothly and uniformly with great tactile sensitivity.

Hallberg, F. C.↗

Fracture and crack growth in orthotropic laminates. Part 2: Experimental determination of internal damage growth in unidirectional boron/aluminum composite laminates

The fracture behavior of unidirectional boron/aluminum composite laminates is investigated in order to verify the results of mathematical models. These models predict the stresses and displacements of fibers and the amount of damage growth in a center-notched lamina as a function of the applied remote stress and the matrix and fiber material properties. The damage may take the form of longitudinal yielding and splitting in the matrix as well as stable transverse damage consisting of broken fibers and matrix yielding ahead of the notch. A brittle lacquer coating is used to detect the yielding in the matrix while X-ray techniques are used to detemine the number of broken fibers in the laminate. The notched strengths and the amounts of damage found in the experimental specimens agree well with those predicted by the mathematical model.

Goree, J. G.↗

The strength and ductility of polycrystalline NiAl in tension

Experiments at temperatures from 20 C to 400 C at two strain rates (.0001/s and .000005/s) establish that: (1) at room temperatures, binary and microalloyed ( 1000 ppm La, Y, Mo, Ti) NiAl shows negligible ductility, independent of grain size over the range 5 to 140 micrometers; (2) at 295 C the tensile elongation of binary 51 Ni/49 Al increases from 1% to about 5% upon decreasing the grain size to below approximately 10 micrometers; (3) similarly, at 400 C the ductility increases from about 2% to 15% upon decreasing the grain size to below 15 micrometers; (4) the ductility of fine grained (7 micrometer) binary aggregates deformed at 295 C increases from approximately 5% to 12% upon decreasing the strain rate from .0001/s to .000005/s; (5) partial recrystallization (10% to 20%) of warm extruded binary and microalloyed material imparts 1% to 2% ductility at room temperature where fully recrystallized material is brittle; (6) the yield strength obeys a Hall-Petch relationship; and (7) when ductility is not observed, fracture coincides with yielding. The mechanisms underlying the flow and fracture of NiAl are discussed in terms of the nucleation and growth of microcracks. The concept of a critical grain size is considered in the light of the results.

Schulson, E. M.↗

A commentary on solid lubricants and wear resistant solids for use in extreme environments

The need for high temperature tribological coatings and self-lubricating materials in advanced technology is discussed. A qualitative model for the mechanism of solid lubrication is proposed. The model is based upon microscopic observations of the dynamics of third-body solids in lubricated contacts. In this model, the rheology of plastic flow is suggested as a more general criterion for predicting the lubricating potential of a solid material than, for example, a specific crystal structure. Some examples of layer-lattice and nonlayer-lattice solids that lubricate by virtue of their extreme plasticity, film coherence, and adhesion to the lubricated metal are described. Circumstantial evidence for the model is presented for low shear-strength solids at room temperature and for solids such as calcium fluoride that become lubricative only when their brittle-to-ductile transition temperature is exceeded. Some materials considerations in the selection of hard-coat materials for wear control are also presented.

Sliney, H. E.↗

Mixed-mode strain-energy-release rate effects on edge delamination of composites

Unnotched graphite/epoxy laminates, designed to delaminate at the edges under static and cyclic tensile loads, were tested and analyzed. The specimen stacking sequences were chosen so that the total strain-energy-release rate, G, for edge delamination was identical for all three layups. However, each layup had different percentages of crack-opening and shear-mode strain-energy-release rates, G sub 1 and G sub 2, respectively. Results with composites made from T300 graphite fibers and 5208 epoxy, a brittle resin, indicated that only G sub 1 contributed to delamination onset under static loading. However, results with composites made from C6000 fibers and H205 epoxy, a tougher resin, indicated that the total F governed the onset of edge delaminations under cyclic loads. In addition, for both materials, the threshold level of G for delamination onset in fatigue was significantly less than the critical G sub c measured in static tests. Futhermore, although the C6000/H205 material had a much higher static G sub c than T300/5208, its fatigue resistance was only slightly better. A series of mixed-mode tests, like the ones in this study, may be needed to evaluate toughened-resin composites developed for highly strained composite structures subjected to cyclic loads.

Obrien, T. K.↗