Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “point defects”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,729 records · Page 96

Synthesis and spectral characteristics of Sr{sub 2}Y{sub 8}(SiO{sub 4}){sub 6}O{sub 2}: Eu polycrystals

Spectral-luminescent characteristics of Sr{sub 2}Y{sub 8}(SiO{sub 4}){sub 6}O{sub 2}: Eu powder crystal phosphor with the apatite structure and high-intensity luminescence of Eu{sup 3+} ions have been studied. The charge state of europium in the samples has been characterized by means of X-ray L{sub 3}-adsorption spectroscopy. It was established that Eu{sup 3+} forms two types of optical centers. Besides, luminescence of Eu{sup 2+}ions was found. Reduction Eu{sup 3+}{yields}Eu{sup 2+} was considered, which may be due to V{sub Sr}{sup ||} vacancy formation in the 4f crystal lattice position and to negative charge transfer by this vacancy to two Eu{sub Y}{sup 3+} ions. Thus, in the silicate lattice there exist inhomogeneously distributed oxygen-deficient centers, which are responsible for nonradiative transfer of excitation energy to Eu{sup 3+} and Eu{sup 2+} ions. To study electron-vibrational interactions in the crystal phosphor samples, their IR and Raman spectra were examined. In the luminescence spectrum of Eu{sup 2+}, a series of low-intensity bands caused by interaction of the 4f{sup 6}5d state of Eu{sup 2+} with silicate lattice vibrations was observed. - Graphical abstract: The scheme of nonradiative transfer over of energy of excitation from oxygen vacancies to ions Eu{sup 2+} and Eu{sup 3+} in Sr{sub 2}Y{sub 8}(SiO{sub 4}){sub 6}O{sub 2}: Eu phosphors. Research Highlights: {yields}In Sr{sub 2}Y{sub 8}(SiO{sub 4}){sub 6}O{sub 2}:Eu phosphors optical centers Eu{sup 2+} and Eu{sup 3+} (two types) are formed. {yields}The 4f{sup 6}5d state of Eu{sup 2+} interacts with the lattice vibrations of Sr{sub 2}Y{sub 8}(SiO{sub 4}){sub 6}O{sub 2}:Eu. {yields}In crystal lattice Sr{sub 2}Y{sub 8} (SiO{sub 4})6O{sub 2}:Eu oxygen vacancies are formed. {yields}Oxygen vacancies nonradiatively transfer the energy of excitation to Eu{sup 2+} and Eu{sup 3+} ions. {yields}Oxygen vacancies are non-uniformly distributed in a phosphorus lattice.

36 MATERIALS SCIENCE↗

Microstructure and magnetic properties of electrospun one-dimensional Al{sup 3+}-substituted SrFe{sub 12}O{sub 19} nanofibers

SrAl{sub x}Fe{sub 12-x}O{sub 19} (x=0-3.0) nanofibers with diameters about 100 nm have been prepared by electrospinning and subsequent heat treatment. With Al{sup 3+} ion content ranging from 0 to 3.0, the lattice parameters decrease due to Fe{sup 3+} ions substituted by smaller Al{sup 3+} ions and the average grain size calculated by the Scherrer's equation reduces from 65 to 37 nm. The magnetization shows a continuous reduction with the Al content and its value measured at 77 K is higher than at room temperature, which can be explained by Bloch's law. For the coercivity, its value initially increases, reaching a maximum value of 617 (298 K) and 547 kA m{sup -1} (77 K) at x=2.0, and then reduces with the Al content further increase largely arising from the substituted Al{sup 3+} ion arrangement in different interstitial sites of the strontium ferrite unit cell. -- Graphical abstract: Al{sup 3+} ions substituted strontium ferrite nanofibers have been prepared by the electrospinning with a diameter of about 100 nm and the Al{sup 3+} ion substitution has a great effect on the microstructure and magnetic property of SrAl{sub x}Fe{sub 12-x}O{sub 19} nanofibers. Display Omitted Research highlights: {yields} SrAl{sub x}Fe{sub 12-x}O{sub 19} nanofibers have been fabricated by the electrospinning. {yields} There is a relation between the Al{sup 3+} ions substitution and microstructure. {yields} The magnetic property can be tuned effectively by Al{sup 3+} ion substitution. {yields} The magnetic property is influenced by measurement temperature.

36 MATERIALS SCIENCE↗

Determining the structure of tetragonal Y{sub 2}WO{sub 6} and the site occupation of Eu{sup 3+} dopant

The compound Y{sub 2}WO{sub 6} is prepared by solid state reaction at 750 {sup o}C using sodium chloride as mineralizer. Its structure is solved by ab-initio methods from X-ray powder diffraction data. This low temperature phase of yttrium tungstate crystallizes in tetragonal space group P4/nmm (No. 129), Z=2, a=5.2596(2) A, c=8.4158(4) A. The tungsten atoms in the structure adopt an unusual [WO{sub 6}] distorted cubes coordination, connecting [YO{sub 6}] distorted cubes with oxygen vacancies at the O{sub 2} layers while other yttrium ions Y{sub 2} form [YO{sub 8}] cube coordination. Y{sup 3+} ions occupy two crystallographic sites of 2c (C{sub 4v} symmetry) and 2a (D{sub 2d} symmetry) in the Y{sub 2}WO{sub 6} host lattice. With Eu{sup 3+} ions doped, the high resolution emission spectrum of Y{sub 2}WO{sub 6}:Eu{sup 3+} suggests that Eu{sup 3+} partly substituted for Y{sup 3+} in these two sites. The result of the Rietveld structure refinement shows that the Eu{sup 3+} dopants preferentially enter the 2a site. The uniform cube coordination environment of Eu{sup 3+} ions with the identical eight Eu-O bond lengths is proposed to be responsible for the intense excitation of long wavelength ultraviolet at 466-535 nm. -- Graphical abstract: The excitation and emission spectra of Y{sub 2}WO{sub 6}:Eu{sup 3+} indicates the effect of long wavelength-excited property, which is ascribed to the cube coordination environment of Eu{sup 3+} ions with the uniform Eu-O bond length. Display Omitted Research highlights: Y{sub 2}WO{sub 6} is prepared using sodium chloride as mineralizer. The structure of the compound Y{sub 2}WO{sub 6} is solved by ab-initio methods. The site occupation of Eu{sup 3+} is determined. The cube coordination of Eu{sup 3+} ions is responsible for the long wavelength excitation.

36 MATERIALS SCIENCE↗

First-principles study of the electronic and magnetic properties of oxygen-deficient rutile TiO{sub 2}(1 1 0) surface

Based on first-principles electronic structure calculations we find that the bridging oxygen vacancies on the (1 1 0) surface is more favorable and may be responsible for the unexpected ferromagnetism in undoped rutile TiO{sub 2}. Our results show that the ferromagnetism largely originates from the d orbitals of low-charge-state Ti ions converted from Ti{sup 4+} ions induced by the surface oxygen vacancies. The second-nearest neighbors of these ions (fivefold coordinated Ti) also contribute to the total magnetic moments. The spins induced by the local oxygen vacancies form a ferromagnetic arrangement. -- Graphical Abstract: The study investigates the magnetic properties of the oxygen-deficient rutile TiO{sub 2}(1 1 0) surface from first principle calculations. The adjacent oxygen vacancies form a ferromagnetic arrangement due to the double exchange interaction. Display Omitted Highlights: {yields} There should be more V{sub O}'s than V{sub Ti}'s on the (1 1 0) surface layer of TiO{sub 2}. {yields} Magnetic moments induced by the isolated V{sub O} form a paramagnetic arrangement. {yields} Magnetic moments induced by the concentrated V{sub O}'s form a ferromagnetic arrangement. {yields} Double exchange is the dominant coupling mechanism of the ferromagnetism.

36 MATERIALS SCIENCE↗

Benefits of Damage Engineering for PMOS Junction Stability

As CMOS devices continue to shrink, the formation of ultra shallow junction (USJ) in the source/drain extension remains to be a key challenge requiring high dopant activation, shallow dopant profile and abrupt junctions. The next generations of sub nano-CMOS devices impose a new set of challenges such as elimination of residual defects resulting in higher leakage, difficulty to control lateral diffusion, junction stability post anneal and junction formation in new materials. To address these challenges for advanced technological nodes beyond 32 nm, it is imperative to explore novel species and techniques. Molecular species such as Carborane (C{sub 2}B{sub 10}H{sub 12}), a novel doping species and a promising alternative to monomer Boron is of considerable interest due to the performance boost for 22 nm low power and high performance devices. Also, to reduce residual defects, damage engineering methodologies have generated a lot of attention as it has demonstrated significant benefits in device performance. Varian proprietary techniques to perform implants at cold temperatures (PTC II) have demonstrated lower junction leakage, enhanced activation, reduced dopant diffusion and less dopant deactivation due to the reduction of self-interstitial atoms present at the end-of-range (EOR) with low implant temperatures. In this paper, for the first time, there is a comprehensive study of the effect of implant temperature on defect engineering affecting deactivation/reactivation, and it is well established in this paper that colder the implant temperature the better it is for damage engineering with reduced EOR defects and better amorphization. The effect has been studied over a wide range of implant temperature. To understand any difference in deactivation between molecular and monomer Boron and to provide direct comparison equivalent Boron implants, co-implanted with Carbon were also studied. Implants with wide range of temperatures are implemented using PTC II. This paper will also show how damage reduction correlates with optimum junction formation and stability.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic and transport properties of transparent SrSn{sub 0.9}Sb{sub 0.05}Fe{sub 0.05}O{sub 3} semiconductor films

The effect of antimony doping on the structural, magnetic, and electrical properties of transparent SrSn{sub 0.9}Sb{sub 0.05}Fe{sub 0.05}O{sub 3} films synthesized by RF sputtering on oxidized Si and quartz substrates has been investigated. A reduction in electrical resistivity by two orders of magnitude compared to 5% Fe doped SrSnO{sub 3} film was observed. The electrical conductivity behavior has been analyzed using the Mott's Variable range hopping model. The nature of magnetic ordering were investigated by field cooled (FC) and zero field cooled (ZFC) magnetization measurements. The applicability of models based on oxygen vacancies to explain the magnetic ordering present in the sample has been discussed.

36 MATERIALS SCIENCE↗

Low-temperature irradiation-induced defects in p-type germanium

Besides two well-known dominant peaks, which have been earlier correlated with the single monovacancy and gallium interstitial defect, a number of small lines appear in deep level transient spectroscopy (DLTS) spectra measured in situ after particle irradiation at low temperatures in p-type germanium. Three of the most pronounced have been studied to some detail in the present investigation by combining DLTS and high-resolution Laplace DLTS. These three lines are called H70, H280 and H290, where the H refers to their hole-trap nature, and the numbers to their apparent enthalpy for hole emission relative to the valence-band edge. The H70 trap is most probably a primary defect, and its observed energy level is found to be an acceptor level. Possible defects related to these DLTS lines are discussed with special emphasis on the divacancy defect in germanium.

36 MATERIALS SCIENCE↗

EPR and ab initio calculation study on the EI4 center in 4H- and 6H-SiC

We present results from electron paramagnetic resonance (EPR) studies of the EI4 EPR center in 4H- and 6H-SiC. The EPR signal of the EI4 center was found to be drastically enhanced in electron-irradiated high-purity semi-insulating materials after annealing at 700-750 deg. C. Strong EPR signals of the EI4 center with minimal interferences from other radiation-induced defects in irradiated high-purity semi-insulating materials allowed our more detailed study of the hyperfine (hf) structures. An additional large-splitting {sup 29}Si hf structure and {sup 13}C hf lines of the EI4 defect were observed. Comparing the data on the hf interactions and the annealing behavior obtained from EPR experiments and from ab initio supercell calculations of different carbon-vacancy-related complexes, we suggest a complex between a carbon vacancy-carbon antisite and a carbon vacancy at the third-neighbor site of the antisite in the neutral charge state, (V{sub C}-C{sub Si}V{sub C}){sup 0}, as a new defect model for the EI4 center.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Excitons and photoluminescence in ZnO and Zn{sub 0.99}Mn{sub 0.01}O nanocrystals

The photoluminescence and photoluminescence excitation spectra for Zn{sub 1-x}Mn{sub x}O nanocrystals are presented. After annealing of powders in air, the intensity of the bands attributable to manganese decreases noticeably. This suggests that the oxygen vacancies affect the Zhang-Rice-like states appearing due to strong d-p-hybridization, which is confirmed by an increase in the band gap of Zn{sub 1-x}Mn{sub x}O for low x. The origin of the 2.9-eV peak and the shape of its excitation spectrum are discussed qualitatively. For Zn{sub 1-x}Mn{sub x}O nanocrystals, the shape of the excitation spectrum is as unusual as the intense absorption in the range (2.2-3.0) eV.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Features of subthreshold defect formation in CdS and CdS:Cu single crystals subjected to irradiation with X-ray photons

Experimental results of the study of the effect of irradiation with 230-keV electrons and with X-ray photons with energies of 8.06 and 17.5 keV and the effect of quenching on the formation and reconstruction of the centers of slow recombination of nonequilibrium charge carriers (the so-called r centers) in nominally undoped and Cu doped (N{sub Cu} {approx} 10{sup 18} cm{sup -3}) CdS single crystals are reported. It is shown that defects in cadmium sublattice in the crystal (specifically, the V{sub Cd} vacancies and the Cu{sub Cd} defects with parameters close to those of the above vacancies) are responsible for the r centers. In the case of the X-ray irradiation of both undoped and Cu-doped CdS single crystals, subthreshold defect formation of cadmium vacancies and Cu{sub Cd} defects takes place; this occurs at sites with distorted and weakened interatomic bonds, i.e., at 'weak sites' near large structural imperfections of the lattice, of technological or other origin. Starting with a quenching temperature 170 deg. C, the spectrum of slow-recombination centers is appreciably affected by thermally formed vacancies V{sub Cd} and secondary defects Cu{sub Cd}. At quenching temperatures higher than 250 deg. C, a significant contribution to the spectrum of optical quenching of photoconductivity is made by thermally introduced free (away from structural imperfections) r centers, i.e., the V{sub Cd} and Cu{sub Cd} defects.

36 MATERIALS SCIENCE↗

Mechanism of compensation of the donor impurity in the near-surface layer of gap during heat treatment in phosphorus vapors

The secondary ion mass spectrometry and capacitance-voltage measurements have been used to study the mechanism of formation of the near-surface layer with a low concentration of uncompensated donors in n-GaP grown by vapor-phase epitaxy and subjected to heat treatment at different pressures of phosphorus vapors. The dependence of the thickness of the mentioned layer on the pressure of phosphorus vapors has a minimum at a pressure of (1.5 {+-} 0.5) x 10{sup 3} Pa. It is shown that at vapor pressures above the mentioned value, the interstitial P, which forms a deep electron trap, is a suitable candidate for the role of compensating acceptor. At low pressures, the probable compensating center is the P vacancy giving rise to a deep level with the energy Ec-(0.21 {+-} 0.01) eV. At 700 deg. C, the effective diffusivity of interstitial P is {approx}(3 {+-} 1) s- 10{sup -15} cm{sup 2}/s, while that of the P vacancy is {approx}(3 {+-} 1) x 10{sup -14} cm{sup 2}/s.

36 MATERIALS SCIENCE↗

High-pressure crystal growth and magnetic and electrical properties of the quasi-one dimensional osmium oxide Na{sub 2}OsO{sub 4}

Na{sub 2}OsO{sub 4} crystals were grown by a NaCl flux method under high pressure. It crystallizes in the Ca{sub 2}IrO{sub 4}-type structure without having additional elements or metal vacancies, which are usually accommodated. It appears that Na{sub 2}OsO{sub 4} is a metal-stoichiometric Ca{sub 2}IrO{sub 4}-type compound never been synthesized to date. Na{sub 2}OsO{sub 4} has the octahedral environment of Os{sup 6+}O{sub 6} so that the electronic configuration is 5d{sup 2}, suggesting the magnetic S=1 ground state. However, magnetization, electrical resistivity, and specific heat measurements indicated that the non-magnetic S=0 state is much likely for Na{sub 2}OsO{sub 4} than the S=1 state. Band structure calculations and the structure analysis found that the disagreement is probably due to the statically uniaxial compression of the OsO{sub 6} octahedra, resulting in splitting of the t{sub 2{sub g}} band. - Graphical abstract: Na{sub 2}OsO{sub 4} crystals were grown by a NaCl flux method under high pressure. It crystallizes in the Ca{sub 2}IrO{sub 4}-type structure comprising infinite Os{sup 6+}O{sub 6} octahedra (5d{sup 2}) chains. The crystal growth, the crystal structure, and the magnetic and electrical properties are reported.

36 MATERIALS SCIENCE↗

Local structure in solid solutions of stabilised zirconia with actinide dioxides (UO{sub 2}, NpO{sub 2})

The local structure of (Zr,Lu,U)O{sub 2-x} and (Zr,Y,Np)O{sub 2-x} solid solutions has been investigated by extended X-ray absorption fine structure (EXAFS). Samples were prepared by mixing reactive (Zr,Lu)O{sub 2-x} and (Zr,Y)O{sub 2-x} precursor materials with the actinide oxide powders, respectively. Sintering at 1600 {sup o}C in Ar/H{sub 2} yields a fluorite structure with U(IV) and Np(IV). As typical for stabilised zirconia the metal-oxygen and metal-metal distances are characteristic for the different metal ions. The bond lengths increase with actinide concentration, whereas highest adaptation to the bulk stabilised zirconia structure was observed for U---O and Np---O bonds. The Zr---O bond shows only a slight increase from 2.14 A at 6 mol% actinide to 2.18 A at infinite dilution in UO{sub 2} and NpO{sub 2}. The short interatomic distance between Zr and the surrounding oxygen and metal atoms indicate a low relaxation of Zr with respect to the bulk structure, i.e. a strong Pauling behaviour. -- Graphical abstract: Metal-oxygen bond distances in (Zr,Lu,U)O{sub 2-x} solid solutions with different oxygen vacancy concentrations (Lu/Zr=1 and Lu/Zr=0.5). Display Omitted Research Highlights: {yields} EXAFS indicates high U and Np adaption to the bulk structure of stabilised zirconia. {yields} Zr---O bond length is 2.18 A at infinite Zr dilution in UO{sub 2} and NpO{sub 2}. {yields} Low relaxation (strong Pauling behaviour) of Zr explains its low solubility in UO{sub 2}.

36 MATERIALS SCIENCE↗

Enhancement of conductivity and transmittance of ZnO films by post hydrogen plasma treatment

We studied the effects of hydrogen plasma treatment on the electrical and optical properties of ZnO films deposited by radio frequency magnetron sputtering. It is found that the ZnO:H film is highly transparent with the average transmittance of 92% in the visible range. Both carrier concentration and mobility are increased after hydrogen plasma treatment, correspondingly, the resistivity of the ZnO:H films achieves the order of 10{sup -3} OMEGA cm. We suggest that the incorporated hydrogen not only passivates most of the defects and/or acceptors present, but also introduces shallow donor states such as the V{sub O}-H complex and the interstitial hydrogen H{sub i}. Moreover, the annealing data indicate that H{sub i} is unstable in ZnO, while the V{sub O}-H complex remains stable on the whole at 400 deg. C, and the latter diffuses out when the annealing temperature increases to 500 deg. C. These results make ZnO:H more attractive for future applications as transparent conducting electrodes.

36 MATERIALS SCIENCE↗

Phase transitions and electrical behavior of lead-free (K{sub 0.50}Na{sub 0.50})NbO{sub 3} thin film

Lead-free (K{sub 0.50}Na{sub 0.50})NbO{sub 3} (KNN) thin films with a high degree of (100) preferred orientation were deposited on the SrRuO{sub 3}-buffered SrTiO{sub 3}(100) substrate by off-axis radio frequency magnetron sputtering. They possess lower phase transition temperatures (T{sub o-t}approx120 deg. C and T{sub c}approx310 deg. C), as compared to those of KNN bulk ceramic (T{sub o-t}approx190 deg. C and T{sub c}approx400 deg. C). They also demonstrate enhanced ferroelectric behavior (e.g., 2P{sub r}=24.1 muc/cm{sup 2}) and fatigue endurance, together with a lower dielectric loss (tan deltaapprox0.017) and a lower leakage current, as compared to the bulk ceramic counterpart. Oxygen vacancies are shown to be involved in the conduction of the KNN thin film.

36 MATERIALS SCIENCE↗

Major deep levels with the same microstructures observed in n-type 4H-SiC and 6H-SiC

Major deep levels observed in as-grown and irradiated n-type 4H-SiC and 6H-SiC epilayers have been investigated. After low-energy electron irradiation, by which only carbon atoms are displaced, five traps, EH1 (E{sub C}-0.36 eV), Z{sub 1}/Z{sub 2} (E{sub C}-0.65 eV), EH3 (E{sub C}-0.79 eV), EH5 (E{sub C}-1.0 eV), and EH6/7 (E{sub C}-1.48 eV), were detected in 4H-SiC and four traps, E{sub 1}/E{sub 2} (E{sub C}-0.45 eV), RD{sub 5} (E{sub C}-0.57 eV), ES (E{sub C}-0.80 eV), and R (E{sub C}-1.25 eV), were detected in 6H-SiC. The Z{sub 1}/Z{sub 2}, EH6/7 centers in 4H-SiC and the E{sub 1}/E{sub 2}, R centers in 6H-SiC exhibit common features as follows: their generation rates by the e{sup -}-irradiation were almost the same each other, their concentrations were not changed by heat treatments up to 1500 deg. C, and they showed very similar annealing behaviors at elevated temperatures. Furthermore, these defect centers were almost eliminated by thermal oxidation. Taking account of the observed results and the energy positions, the authors suggest that the Z{sub 1}/Z{sub 2} center in 4H-SiC corresponds to the E{sub 1}/E{sub 2} center in 6H-SiC, and the EH6/7 center in 4H-SiC to the R center in 6H-SiC, respectively. Since the concentrations of these four centers are almost the same for as-grown, electron-irradiated, annealed, and oxidized samples, these centers will contain a common intrinsic defect, most likely carbon vacancy. The authors also observed similar correspondence for other thermally unstable traps in 4H-SiC and 6H-SiC.

36 MATERIALS SCIENCE↗

Analysis of Interstitial Elements in Niobium with Secondary Ion Mass Spectrometry (SIMS)

Superconducting Radio Frequency (SRF) cavities provide enhanced efficiency and reduced energy utilization in present day particle accelerators. Niobium (Nb) is the material of choice for these cavities due to its high critical temperature and critical magnetic field. In order to understand why certain treatments, especially a low temperature bake, improve performance, it is important to study Nb surface characteristics and identify elemental contamination that can affect the performance of the cavity. H, C, O, and N are of interest because they are interstitial impurities in Nb. In earlier work, SIMS analysis using a CAMECA IMS-6F with Cs{sup +} primary beam showed that C and N were probably not significant factors impacting performance but there was a very high level of H in the Nb. Ion implants of C, N, O, and D into Nb provided quantification of C, N, O and indicated that D is very mobile in the Nb. Further analyses showed that heat treated Nb has lower levels of surface H than non heat treated Nb and subsequent removal of surface oxide by etching causes intake of H in a heat treated Nb sample. This result helps confirm the role of surface oxide as a hydrogen barrier. To further understand the oxide, Nb samples were anodized to obtain a thicker surface oxide and H and D were implanted into this oxide to check for the appearance of implant peaks. SIMS depth profile analyses were carried out and confirmed the presence of the implant shape for these elements in the oxide. Relative Sensitivity Factor (RSFs) could then be calculated for quantification of H in the oxide. Since the Nb matrix signal showed little change from the oxide to the substrate, the same RSF was used to estimate the H concentration in the Nb at 2x10{sup 22} atoms/cm{sup 3}(approximately 40% mole fraction H).

36 MATERIALS SCIENCE↗