Precipitation processes in the Beta-Titanium alloy Ti–5Al–5Mo–5V–3Cr
Not Available
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
Abstract not provided
Thermomechanical processing has been used to control the grain size/shape of the equiatomic CrCoNi medium-entropy alloy (MEA) and obtain excellent strength and ductility. However, in the cast state, the alloy has coarse columnar grains with average widths and lengths of approximately 120 and 1000 μm, respectively, resulting in inferior mechanical properties. To overcome this deficiency, we microalloyed with Ti and C and successfully changed the grain shape (from columnar to equiaxed) and refined the grain size. The degree to which the microstructure changes depends on the amount of Ti and C added, with the best results obtained at 0.4 at.% each. In the optimal alloy [(CrCoNi) 99.2 Ti 0.4 C 0.4 ], the as-cast grains were nearly equiaxed with a uniform size of ~75 μm. Associated with this change in grain shape/size was a significant improvement of yield strength, ultimate tensile strength and elongation to fracture at both 293 and 77 K. Finally, the columnar to equiaxed transition is attributed to the strong mutual affinity of C and Ti, which leads to their build-up ahead of the solid-liquid interface and, in turn, to enhanced constitutional undercooling.
Not Available
Not Available
Not Available
Here, this work reports the first mechanical properties of Ti 3 AlC 2 -Ti 5 Al 2 C 3 materials neutron irradiated at ~400, 630 and 700 °C at a fluence of 2 × 10 25 n m -2 (E > 0.1 MeV) or a displacement dose of ~2 dpa. After irradiation at ~400 °C, anisotropic swelling and loss of 90% flexural strength was observed. After irradiation at ~630–700 °C, properties were unchanged. Microcracking and kinking-delamination had occurred during irradiation at ~630–700 °C. Further examination showed no cavities in Ti 3 AlC 2 after irradiation at ~630 °C, and MX and A lamellae were preserved. However, disturbance of (0004) reflections corresponding to M-A layers was observed, and the number density of line/planar defects was ~10 23 m -3 of size 5–10 nm. HAADF identified these defects as antisite Ti Al atoms. Finally, Ti 3 AlC 2 -Ti 5 Al 2 C 3 shows abrupt dynamic recovery of A-layers from ~630 °C, but a higher temperature appears necessary for full recovery.
In this work, the effect of Ti content on phase transformations, microstructures, and mechanical properties of U-Ti alloys are described for alloys containing 0.3 wt.% to 2.0 wt.%Ti. Rapid cooling is required to overcome diffusional decomposition of γ-phase and facilitate diffusionless transformation to supersaturated variants of α-phase. Critical cooling rate increases with increasing Ti content, opposite to the trend observed in U-Mo and U-Nb alloys. This difference occurs because the martensite transformation temperatures in these relatively dilute U-Ti alloys are above the knee of the C-curve for diffusional decomposition, unlike those in the more concentrated U-Mo and U-Nb alloys. In these U-Ti alloys critical cooling rate depends on the amount of undercooling required to reach M s , which increases with increasing Ti content, and the time for diffusional decomposition to occur just above M s , which decreases with increasing Ti content. The net result is that higher cooling rates are required as Ti content increases. Full quenching results in diffusionless transformation of γ-phase to supersaturated variants of α-phase. Very dilute alloys transform via a γ → β → α m sequence of massive transformations. Martensitic γ → α' a transformation begins at ~0.4%Ti, and 100% α' a microstructures are obtained from ~0.65% to ~1.4% Ti. A transition to banded α'b martensite occurs at ~1.5%Ti. Evidence suggests that the α' a to α' b transition may occur when the cubic γ-phase first transforms to tetragonal γ°, which in turn transforms to orthorhombic α' b via the sequence γ → γ° → α' b . Fully quenched alloys exhibit moderate strengths and ductilities, and their supersaturation with Ti makes them amenable to subsequent age hardening. Subcritical quenching typically results in two-phase microstructures with lower ductilities and near-zero Ti-supersaturation, eliminating the possibility of subsequent age hardening.
Here, the effect of Ti content on age hardening and the resulting mechanical properties are described for -quenched U-Ti alloys containing 0.3 wt.% to 2.0 wt.%Ti. Age hardening occurs between ~250°C and ~450°C. Overaging occurs at higher temperatures by cellular decomposition. Age hardening kinetics suggest that different mechanisms occur depending on Ti content and initial microstructure. Strengthening in 'a acicular martensites begins by the formation of Ti clusters which evolve into thin U 2 Ti disc shaped precipitates and later mature into continuous U 2 Ti rods beginning at peak hardness. The mechanism of hardening in 'b banded martensite is more elusive, as significant hardening occurs where atomic mobility is lower than that required for precipitate formation, similar to that reported for age hardening in ''b banded martensite in U-6%Nb. The activation energy for aging varies with Ti content and microstructure. In fully martensitic alloys containing 0.75% to 2.0%Ti it is in the vicinity of ~44 kcal/mole (184 kJ/mole). But it is lower in alloys containing less than 0.6%Ti where quenched microstructures are less than fully martensitic. Tensile ductility is high prior to aging, decreases with age hardening, is effectively zero at peak hardness, and remains low in overaged conditions. Attractive combinations of strength and ductility are best obtained in alloys containing 0.6% to 1.0%Ti which have been partially aged to fractional hardening levels no greater than ~0.6. This corresponds to the very early stages of aging, associated with clustering and the earliest stages of U 2 Ti disc formation. Alloys containing 0.45%Ti or less are not as responsive to age hardening. Alloys containing 1.5% and 2.0%Ti can be aged to higher strengths, but extreme quench rate sensitivity prevents them from being effectively heat treated in realistic section thicknesses.
Radiation damage in beam window materials limits the use of high power proton beams in high energy physics research. The alloy Ti-6Al-4V is presently used as a beam window material but a prospective alternative, Ti-15V-3Cr-3Sn-3Al has been proposed. Since both these alloys contain dual phases at room temperature, we compare the radiation damage in the α and ß-phases of these two materials via primary knock-on atom (PKA) cascade simulations in the 10-40keV energy range. At PKA energies 30 and 40keV, the number of Frenkel pairs in the ballistic stage is higher in the ß-phase of Ti-6Al-4V than that in the ß-phase of Ti-15V-3Cr-3Sn-3Al almost by a factor of 2. The α-phase, of both these alloys, by far outperforms the ß-phases of the two alloys, both in terms of damage during the ballistic stage and in terms of the surviving defects. The average displacement threshold energy (E d ) in the α-phase of both alloys was found to be 66eV while that in the ß-phase of Ti-15-3 was 55 eV and in the ß-phase of Ti-6-4 was 46. Further, while the number of surviving defects is almost equal in both alloys, the vacancy and interstitial clustering mechanisms differ notably, which can impact the degree of radiation hardening and loss of ductility. Our simulations show larger vacancy and interstitial clusters form in Ti-6Al-4V as compared to that in Ti-15-3-3-3 alloy. These results indicate that Ti-15-3-3-3 alloys may be a promising candidate for next generation beam window material with a higher radiation tolerance than the existing Ti-6-4 alloy.
As part of an effort to develop cost-effective ferritic stainless steel-based interconnects for solid oxide fuel cell (SOFC) stacks, AL 441 HPTM was studied in terms of its metallurgical characteristics, oxidation behavior, and electrical performance. Minor alloying elements (Nb and Ti) captured interstitials such as C by forming carbides, stabilizing the ferritic structure and mitigating the risks of sensitization and inter-granular corrosion. Laves phases rich in Nb and Si precipitated along grain boundaries during high temperature exposure, improving the steel’s high temperature mechanical strength. The capture of Si in the Laves phase minimized the Si activity in the steel substrate and prevented formation of an insulating silica layer at the scale/metal interface. However, the relatively high oxidation rate, and thus increasing ASR over time, necessitates the application of a conductive protection layer on the steel. In particular, Mn1.5Co1.5O4 spinel protection layers drastically improved the electrical performance of the ferritic stainless steel 441, acting as barriers to chromium outward and oxygen inward diffusion.
Not Available