Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ZIRCONIUM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,711 records · Page 95

Diffusion Barrier Properties of Nitride-Based Coatings on Fuel Cladding

In this work titanium nitride (TiN) and zirconium nitride (ZrN) coatings are proposed as diffusion barriers between stainless steel nuclear fuel cladding and lanthanide fission products. TiN and ZrN have been coated as barrier materials between pure Fe and Ce, i.e. diffusion couples of Fe/TiN/Ce and Fe/ZrN/Ce, annealed up to a temperature of 600 degrees C, and compared to the diffusion behavior of uncoated Fe/Ce. Backscattered electron images and electron dispersive X-ray spectroscopy measurements confirm that, with a 500 nm TiN or ZrN layer, no obvious diffusion is observed between Fe and Ce. Basic diffusion characteristics of the Fe/Ce couple have also been measured and compared with the TiN and ZrN coated ones. The results strongly advocate that TiN and ZrN coatings provide reliable diffusion barrier characteristics against Ce and possibly other lanthanide fission products.

36 MATERIALS SCIENCE↗

Thermal expansion in the garnet-type solid electrolyte (Li 7 - x Al x /3 )La 3 Zr 2 O 12 as a function of Al content

The thermal expansion (TE) coefficients of the lithium-stable lithium-ion conducting garnet lithium lanthanum zirconium oxide (LLZ) and the effect of aluminum substitution were measured from room temperature up to 700 °C by a synchrotron-based X-ray diffraction. The typical TE value measured for the most reported composition (LLZ doped with 0.3 wt.% or 0.093 mol% aluminum) was 15.498 × 10-6 K-1, which is approximately twice the value reported for other garnet-type structures. As the Al(III) concentration has been observed to strongly affect the structure observed and the ionic conductivity, we also assessed its role on thermal expansion and noted only a small variation with increasing dopant concentration. The materials implications for using LLZ in a solid state battery are discussed.

36 MATERIALS SCIENCE↗

Vertically oriented ZrO 2 –TiO 2 –Nb 2 O 5 –Al 2 O 3 mixed nanopatterned bioceramics on Ti6Al7Nb implant assessed by laser spallation technique

Recently, reports on the fabrication of nonstructural configuration have generated scientific interest due to increased awareness of the oxide nanotubes in the biomedical implant field and other industrial approaches. In this paper, highly ordered ZrO 2 –TiO 2 –Nb 2 O 5 –Al 2 O 3 nanotube arrays were grown by physical vapor deposition (PVD) of a zirconium layer on titanium-niobium alloy implant (IMPTi67) and succeeding anodic oxidation at a constant voltage (60 V) with exposure times ranging from 30 to 300 min. To crystallize the resulting mixed oxide nanotubes, heat treatment was also applied. The nanotubes were placed in an atmospheric furnace at temperatures ranging from 450 to 800 °C for 2 h. This treatment provided a morphological evolution was strongly influenced by the anodization time, where highly aligned bamboo-shaped oxide nanotubes (161 ± 44 nm in inside diameter and ~1 μm in length) were formed after 300 min of anodization. After annealing at temperature below 500 °C, the nano-array configuration remained stable and the average inner diameter decreased to around 40 nm. The effects of anodically fabrication time on the adhesion strength of four-phase multilayered mixed oxide nanotubes on anodized Zr/IMPTi67 surfaces assed by microscratch analysis. From the results, increasing the annealing temperature further to 800 °C fully destroyed the nanotubes and consequently the tubular arrangement was converted to a coarse grain structure. It was revealed that annealing at 450 °C for 2 h was the optimum conditions for stable nanotubular array generation, where the highest adhesion strength (shifted from 2595.59 to 2640.12 mN), microhardness (372 HV) and hydrophilicity (15 ± 1°) were recorded. It is notify that the adhesion strength of highly ordered mixed nanotubes was remarkably decreased after thermal treatment at 800 °C (1817.51 mN). Through the laser spallation analysis, the intrinsic adhesion strength of the Zr/IMPTi67 interface was found to be at 63 MPa, while the first stages of failure occurred at a stress state of 35 MPa. The adhesion of the film with the tubular structure proved to have a significantly larger adhesion strength of 246 MPa for the complete failure and 203 MPa for incipient stages of spallation. Finally, the considered surface modification can be an effective step in determining the interface strength between biomedical implants and the nanostructured coatings.

36 MATERIALS SCIENCE↗

Unveiling the nucleation and growth of Zr oxide precipitates in internally oxidized Nb3Sn superconductors

We report on atomic-scale analyses of nucleation and growth of Zr oxide precipitates and the microstructural evolution of internally oxidized Nb3Sn wires for high-field superconducting magnet applications, utilizing atom probe tomography (APT), transmission electron microscopy (TEM), and first-principles calculations. APT analyses reveal that oxygen and zirconium are already segregated at grain boundaries (GBs) in the unreacted Nb-1Zr-4Ta (at%) alloy prior to forming Nb3Sn through reacting the Nb alloy with Sn and SnO2. After forming Nb3Sn, Zr oxide precipitates nucleate both at the Nb3Sn/Nb heterophase interfaces and in the Nb3Sn grains, driven by the small solubilities of Zr and O in Nb3Sn compared to their value in Nb. A high number density (Nv) of Zr oxide nanoprecipitates is observed in the Nb3Sn layers, ∼10 23 m −3 , with a mean diameter <10 nm for a heat treatment at 625 °C. Quantitative APT and TEM analyses of the Zr oxide precipitates in the reacted Nb3Sn layers elucidate details of the nucleation, growth, and coarsening processes of the Zr oxide precipitates in Nb3Sn. First-principles calculations and classical nucleation theory are employed to study the nucleation of Zr oxide precipitates in Nb3Sn and to estimate the maximum energy barrier and critical radius for nucleation. Our research unveils the kinetic pathways for nucleation and growth of Zr oxide precipitates and the microstructural evolution of Nb3Sn layers, which helps to understand and improve the superconducting properties of internally oxidized Nb3Sn wires for use in high-field superconducting magnets. •We investigated the nucleation and growth of Zr oxide nanoprecipitates in Nb3Sn superconductors for magnet applications.•APT and TEM analyses reveals the nucleation and growth process of Zr oxide precipitates in Nb3Sn layers.•Classical nucleation theory with DFT is employed to describe the nucleation process of Zr oxide precipitates in Nb3Sn.•We find that the interfacial reactions at Nb/Nb3Sn interface play a critical role in the nucleation of Zr oxide precipitates.•Current study provides a pathway to improve the properties of internally oxidized Nb3Sn superconducting wires.

43 PARTICLE ACCELERATORS↗

Tetragonal structure and uniaxial magnetic anisotropy in the arc-melted (Ce,Zr) 2 (Fe,M) 17 (M = Mo, W, Co) alloys

The tetragonal ThMn 12 -type structure is stabilized in (Ce 1-x Zr x ) 2 T 16 M (x = 0.2 – 0.3; T = Fe or Fe/Co, M = Mo or W) arc-melted alloys. Approximately 5 at% of Mo or W admixture is sufficient to transform the hexagonal Th 2 Ni 17 -type structure of (Ce 1-x Zr x ) 2 Fe 17 into the tetragonal ThMn 12 -type structure of nearly single-phase (Ce 1-x Zr x ) 2 Fe 16 M and/or (Ce 1-x Zr x ) 2 Fe 15 CoM bulk alloys. X-ray Rietveld refinements reveal that Zr and Mo (W) substitute different sites in the tetragonal crystal structure. Zirconium preferentially replaces Ce, whereas Mo (W) substitutes Fe. At room temperature, the tetragonal phases exhibit strong ferromagnetism and a uniaxial magneto-crystalline anisotropy with anisotropy fields of 15 – 17 kOe. These materials possess room-temperature saturation magnetizations of 95 – 105 emu/g and Curie temperature of 420 – 505 K. At some concentrations, concurrent Zr and Mo (W) site occupancy facilitates 1:12 structure formation in bulk alloys with minimal presence of non-magnetic element in the Fe sublattice, thus securing the highest known magnetic moment per Fe atom (∼ 1.37 µ B ) in this type of materials. The intrinsic magnetic characteristics, as well as the absence of critical rare earths (RE), make these compounds interesting for development as low-cost permanent magnets. In conclusion, small Co additions improve the Curie temperature, especially if combined with W.

36 MATERIALS SCIENCE↗

Thermodynamic complexity of sulfated zirconia catalysts

Here, a series of sulfated zirconia (SZ) catalysts were synthesized by immersion of amorphous zirconium hydroxide in sulfuric acid of various concentrations (1–5 N). Additionally, these samples were fully characterized by X-ray diffraction (XRD), thermogravimetric analysis and mass spectrometry (TGA-MS), and aqueous sulfuric acid immersion and high temperature oxide melt solution calorimetry. We investigated the enthalpies of the complex interactions between sulfur species and the zirconia surface (ΔH SZ ) for the sulfated zirconia precursor (SZP), ranging from -109.46 ± 7.33 (1 N) to -42.50 ± 0.89 (4 N) kJ/mol S. ΔHSZ appears to be a roughly exponential function of sulfuric acid concentration. On the other hand, the enthalpy of SZ formation (ΔH f ), becomes more exothermic linearly as sulfur surface coverage increases, from -147.90 ± 4.16 (2.14 nm -2 ) to -317.03 ± 4.20 (2.29 nm -2 ) kJ/mol S, indicating formation of energetically more stable polysulfate species.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Controlling kinetic and diffusive length-scales during absorptive hydrogen removal in methane dehydroaromatization on MoC x /H-ZSM-5 catalysts

Addition of Zr metal absorbent to MoC x /H-ZSM-5 in the form of staged-bed, stratified-bed, and interpellet physical mixtures effectively scavenges H 2 from catalyst proximity, enhancing maximum single-pass benzene + naphthalene yield during methane dehydroaromatization (DHA) reactions to 14-16% compared to 8% in formulations without zirconium. The coupling of spatially-distinct catalytic and absorptive functions is achieved by dispersive/diffusive transport which conveys H 2 to staged Zr both co- and counter-current to bulk advection, thereby suppressing axial H 2 partial pressure profiles along the catalyst bed and enhancing net aromatization rates. We evince hitherto unreported significance of dispersive hydrogen transport during methane DHA by measurement of Péclet number, Pe = 1.32, in H 2 tracer studies with step-change or impulse input to inert catalyst proxies. Kinetic limits to methane pyrolysis are quantified by Damköhler number, Da, for synthesis of benzene, Da B = 0.15, and naphthalene, Da N = 0.03, determined from kinetic studies which rigorously account for reversibility of DHA reactions. Here, detailed reaction-transport models synthesize interplay of kinetic, diffusive, and convective length-scales captured by Péclet and Damköhler number to predict influence of catalyst-absorbent proximity and process flow-conditions on aromatization rates. Systematic control of catalyst bed-length, L, or linear flow velocity, u, predictably alters Pe and Da to effect improvements in methane conversion with and without Zr metal, corroborating results from simulation of the reaction-transport model.

03 NATURAL GAS↗

Synthesis and Corrosion Study of Zirconia-Coated Carbonyl Iron Particles

This paper describes the surface modification of micrometer-sized magnetic carbonyl iron particles (CI) with zirconia from zirconium(IV) butoxide using a sol–gel method. Zirconia shells with various thicknesses and different grain sizes and shapes are coated on the surface of CI particles by changing the reaction conditions, such as the amounts of zirconia sol, nitric acid, and CI particles. A silica adhesive layer made from 3-aminopropyl trimethoxysilane (APTMS) can be introduced first onto the surface of CI particles in order to adjust both the size and the shape of zirconia crystals, and thus the roughness of the coating. The microanalyses on these coated particles are studied by field-emission scanning electron microscopy (FE-SEM) and X-ray-diffraction (XRD). Accelerated acid corrosion and air oxidation tests indicate that the coating process dramatically improved oxidation and acid corrosion resistances, which are critical issues in various applications of CI magnetic particles.

carbonyl iron↗

Enhanced catalytic performance of Zr modified CuO/ZnO/Al 2 O 3 catalyst for methanol and DME synthesis via CO 2 hydrogenation

Zirconium (Zr) modified CuO/ZnO/Al 2 O 3 (CZA) catalysts with different aluminum (Al) and Zr contents were synthesized by the co-precipitation method. The synthesized CuO/ZnO/ZrO 2 /Al 2 O 3 (CZZA) catalysts were comprehensively characterized and studied for methanol synthesis via CO 2 hydrogenation. The CZZA catalyst showed the highest methanol yield of 12.4 % at 220 °C and 2.76 MPa with an optimized catalyst composition of Cu/Zn/Zr/Al (atomic ratio) at 4:2:1:0.5. The CZZA catalyst showed better activity than that of the CZA catalyst and a superior stability for methanol synthesis. There was no decrease in the BET surface area and very little coke formation for the spent CZZA catalyst, after 300 h of methanol synthesis. Bifunctional catalysts, composed of CZZA and HZSM-5, were investigated for dimethyl ether (DME) synthesis directly from CO 2 hydrogenation, and a maximum DME yield of 18.3 % was obtained at a reaction temperature of 240 °C and a pressure of 2.76 MPa. The stability of the bifunctional CZZA and HZSM-5 catalyst during the DME synthesis also significantly improved, as compared to that of the CZA and HZSM-5. A significant decrease in the BET surface area and an increase in coking on the spent CZZA catalyst were observed after 100 h of DME synthesis, indicating a detrimental effect on CZZA stability when a HZSM-5 catalyst was present. The changes in structural properties (e.g., BET surface area and crystallinity) and coking for HZSM-5 could be responsible for the deactivation of the bifunctional catalyst.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Onion-Like nanoparticles of the metal–organic framework UiO-66 synthesized by sequential spike crystal growth

Reproducible size and morphology of metal–organic framework (MOF) particles are essential for tuning these materials for applications like heterogeneous catalysis. Particle size measurements from electron micrographs provide information about the impact of changing synthetic parameters on MOF growth, but reported data are usually limited to averages and statistical distributions. Further elucidating synthetic control parameters could facilitate studies of facet-dependent and non-classical growth mechanisms. Here, in this work, phase-pure nanoparticles of the MOF UiO-66 were synthesized using alternating spikes of zirconium and hafnium-based nodes, forming an onion-like structure with alternating layers of Zr-UiO-66 and Hf-UiO-66. In conventional, bright-field transmission electron micrographs, Hf-UiO-66 and Zr-UiO-66 layers appeared darker and lighter, respectively. Alternating layers of Hf-UiO-66 and Zr-UiO-66 were also apparent in elemental maps obtained using scanning transmission electron microscopy with energy-dispersive X-ray spectroscopy. Average particle sizes increased monotonically with each spike, and no Zr-only or Hf-only particles were observed after the first spike, indicating that new material was consistently incorporated onto existing seeds. Surface area of the onion-like particles and their uptake of Ni 2+ from solution were both between the values measured for Zr-UiO-66 and Hf-UiO-66. Results demonstrate the use of sequential spikes of nodes in monitoring crystal growth in MOFs.

36 MATERIALS SCIENCE↗

Separation of metallic residues from the dissolution of a high-burnup BWR fuel using nitrogen trifluoride

Nitrogen trifluoride (NF 3 ) was used to fluorinate the metallic residue from the dissolution of a high burnup, boiling water reactor fuel (~70 MWd/kgU). The metallic residue included the noble metal phase (containing ruthenium, rhodium, palladium, technetium, and molybdenum), and smaller amounts of zirconium, selenium, tellurium, and silver. Exposing the noble metal phase to 10% NF 3 in argon between 400 and 550°C, removed molybdenum and technetium near 400°C as their volatile fluorides, and ruthenium near 500C as its volatile fluoride. The events were thermally and temporally distinct and the conditions specified are a recipe to separate these transition metals from each other and from the noble metal phase nonvolatile residue. Depletion of the volatile fluorides resulted in substantial exothermicity. Thermal excursion behavior was recorded under non-adiabatic, isothermal conditions that typically minimize heat release. Physical characterization of the metallic noble phase and its thermal behavior are consistent with high kinetic velocity reactions encouraged by the nanoparticulate phase or perhaps catalytic influences of the mixed platinum metals with nearly pure phase structure. Post-fluorination, only two phases were present in the residual nonvolatile fraction. These were identified as a nano-crystalline, metallic palladium cubic phase and a hexagonal rhodium trifluoride (RhF 3 ) phase. The two phases were distinct as the sub-µm crystallites of metallic palladium were in contrast to the RhF 3 phase, which grew from the parent nano-crystalline noble-metal phase during fluorination, to acicular crystals exceeding 20-µm in length.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Isotropic nanocrystalline Sm(Fe,Co) 11.3 Ti 0.7 magnets modified with B and Zr

Rare-earth-lean Sm(Fe,Co,Ti) 12 alloys with the ThMn 12 crystal structure and less than one Ti atom per formula unit have the potential of exceptionally powerful permanent magnets, but all prior attempts to develop high coercivity in bulk alloys, especially coercivity combined with crystallographic texture, have fallen short of the expectations. This study was aimed at improvement of the currently best Sm(Fe,Co,Ti) 12 magnets prepared through melt-spinning which are inherently isotropic. Modifications of the alloys with B and Zr, already demonstrated in earlier studies to be effective separately, have been implemented simultaneously. Here, a systematic study of Sm 1.1-x (Fe,Co) 11.3-y Ti 0.7 B y alloys melt-spun at a tangential speed of 50 m/s and annealed at 600–950 °C allowed for monitoring the continuous evolution of the two consecutive crystal structures, those of the TbCu 7 and ThMn 12 types. Zirconium was found to facilitate the formation of the 1:12 structure at the expense of the 1:7, whereas boron has the opposite effect, at certain concentrations completely suppressing the 1:12. When the two alloying elements are introduced simultaneously, they inhibit growth of the 1:12 crystallites at annealing temperatures higher than 800 °C, thus allowing for the development of a higher coercivity. Because of instrumental limitations, bulk magnets were prepared through a two-step process – compaction of the melt-spun ribbons at 650 °C and additional treatment at a higher temperature – and they were characterized by a reduced, 90–93%, density. Nevertheless, an isotropic Sm 0.9 Zr 0.2 (Fe,Co) 10.8 Ti 0.7 B 0.5 magnet exhibited fair values of the remanence (7.4 kG), maximum energy product (8.5 MGOe) and coercivity (5.4 kOe), as well as high Curie temperature of 525 °C and remarkably small temperature coefficient of the coercivity, -0.25%/°C.

36 MATERIALS SCIENCE↗

Effect of alloying with Sc, Nb and Zr on reduction-diffusion synthesis of magnetically hard Sm(Fe,Co,Ti) 12 -based monocrystalline powders

Powders of Sm(Fe,Co) 11.2 Ti 0.8 alloys modified with Sc, Nb and Zr, as well as with additional Ti were prepared by reducing mechanically activated raw oxides with Ca metal in the furnace preheated to 990–1250 °C. Expansion of the crystal lattice upon introduction of Nb or additional Ti implies that atoms of these elements replace the smaller Fe atoms in the tetragonal ThMn 12 -type structure. On the other hand, contraction of the lattice upon introduction of Sc or Zr was smaller than what was expected for replacement of the Sm atoms, which suggests that the Sc and Zr atoms replace both the Sm and Fe atoms. Washing away the reduction byproducts expands the crystal lattice of the 1:12 particles and increases their coercivity. The lattice expansion associated with the washing is believed to be caused by interstitial H atoms; more research, however, is needed to establish the mechanism(s) of the washing effect on the coercivity. The earlier reported development of a high coercivity in zirconium-modified monocrystalline particles achieved by increasing the reduction annealing temperature to ≈1200 °C was similarly characteristic of the particles modified with Sc (the coercivity reaches 11.5 kOe) and Nb (8.1 kOe), but not for the particles prepared with additional Ti where the maximum coercivity of 8.3 kOe develops for a lower annealing temperature. Furthermore, it is concluded that Sc, Nb and Zr modify the high-temperature phase equilibria of the Sm(Fe,Co) 11.2 Ti 0.8 alloys allowing for an effective high-temperature processing, whereas the alloy coercivity increases with the synthesis temperature through a different, still unknown mechanism which may involve suppression of the defects specific to the 1:12 crystals.

36 MATERIALS SCIENCE↗

A multiscale model to understand the interface chemistry, contacts, and dynamics during lithium stripping

A reversible Li-metal electrode, paired with a solid electrolyte, is critical for attaining higher energy density and safer batteries beyond the current lithium-ion cells. A stable stripping process may be even harder to attain as the stripping process will remove Li-atoms from the surface, and naturally reduce surface contact area, if not self-corrected by other mechanisms, such as diffusion and plastic deformation under an applied external stack pressure. Here, we capture these mechanisms occurring at multiple length- and time- scales, i.e., interface interactions, vacancy hopping, and plastic deformation, by integrating density functional theory (DFT) simulations, kinetic Monte Carlo (KMC), and continuum finite element method (FEM). By assuming the self-affine nature of multiscale contacts, we predict the steady-state contact area as a function of stripping current density, interface wettability, and stack pressure. We further estimate the exponential increase of overpotential due to contact area loss to maintain the same stripping current density. We demonstrate that a lithiophilic interface requires less stack pressure to reach the same steady-state contact area fraction than a lithiophobic interface. A “tolerable steady-state” contact area loss for maintaining stable stripping is estimated at 20 %, corresponding to a 10 % increase in overpotential. To constrain contact loss within the tolerance, the required stack pressure is 0.1, 0.5, and 2 times the yield strength of lithium metal for three distinct interfaces, lithiophilic Li/lithium oxide(Li2O), Li/lithium lanthanum zirconium oxide(LLZO), and lithiophoblic Li/lithium fluoride(LiF), respectively. The modeling results agree with experiments on the impact of the stack pressure quantitatively, while the discrepancy in stripping rate sensitivity is attributed to the simplifying interface interaction in our simulations. Overall, this multiscale simulation framework demonstrates the importance of electrochemical-mechanical coupling in understanding the dynamics of the Li/SE interface during stripping.

Feng, Min↗

Multimodal analysis and characterization of the boehmite layer formed on AA6061 before and after alkaline etching

Low-enriched uranium (LEU) alloyed with 10% Mo (U-10Mo) is being considered as a promising alternative to oxide-based dispersion fuel with high-enriched uranium for use in research reactors. The configuration of this proposed LEU monolithic LEU fuel plate consists of a U-10Mo plate-type fuel foil with a 25 µm zirconium interlayer barrier clad with an aluminum alloy (AA6061). In certain research reactors, the clad AA6061 is coated with a boehmite layer to prevent corrosion. The boehmite layer has a high-pH passivation range, which makes it resistant to oxidation. Boehmite is usually formed on the AA6061 surface by autoclave processing. Before the boehmite layer is added, the surface of the AA6061 is cleaned using techniques such as polishing and wet etching. In this study, we use multimodal analysis to examine how pretreatment of AA6061 using polishing followed by alkaline etching affects the chemical composition of the boehmite layer. X-ray photoelectron microscopy (XPS), transmission electron microscopy (TEM), and x-ray diffraction (XRD) were used to study the chemical changes in the boehmite layer caused by alkaline etching pretreatment. XPS provides quantitative analysis for the Al:O ratio as well as oxidation states present on the surface, which suggests slight oxidation of the boehmite surface after alkaline etching of the AA6061 surface. We further explored this suggested oxidation of the boehmite surface using high-resolution transmission electron microscopy with selected area electron diffraction (SAED) and grazing incidence x-ray diffraction (GI-XRD), which suggested only a small amount of aluminum oxide at the surface. The multimodal analysis and imaging yielded new insights for optimizing boehmite growth on AA6061 for research reactors.

36 MATERIALS SCIENCE↗

Weldable ductile molybdenum alloy development

Molybdenum and its alloys are attractive structural materials for high-temperature applications. However, various practical issues have limited its use. One concern relates to the loss of ductility occurring in the heat-affected weld zone caused by segregation of oxygen to grain boundaries. In this study, a series of arc melted molybdenum alloys have been produced containing controlled additions of B, C, Zr, and Al. These alloys were characterized with respect to their tensile properties, smooth bend properties, and impact energy for both the base metal and welds. These alloys were compared with a very high purity low carbon arc cast molybdenum reference. For discussion purposes the alloys produced are separated into two categories: Mo Al B alloys, and Mo Zr B alloys. The properties of Mo Zr B alloy welds containing higher carbon levels exhibited slight improvement over unalloyed molybdenum, though the base-metal properties for all Mo Zr B alloys were somewhat inconsistent with properties better, or worse, than unalloyed molybdenum. A Mo Al B alloy exhibited the best DBTT values for welds, and the base metal properties were comparable to or slightly better than unalloyed molybdenum. The Mo Al B alloy contained a low volume fraction of second-phase particles, with segregation of boron and carbon to grain boundaries believed to displace oxygen resulting in improved weld properties. The volume fractions of second-phase particles are higher for the Mo Zr B alloys, and these alloys were prone to brittle fracture. It is also noted that these Mo Zr B alloys exhibited segregation of zirconium, boron and carbon to the grain boundaries.

Cockeram, B. V.↗

Uncertainty Studies of Real Anode Surface Area in Computational Analysis for Molten Salt Electrorefining

This study examines how much cell potential changes with five differently assumed real anode surface area cases. Determining real anode surface area is a significant issue to be resolved for precisely modeling molten salt electrorefining. Based on a three-dimensional electrorefining model, calculated cell potentials compare with an experimental cell potential variation over 80 hours of operation of the Mark-IV electrorefiner with driver fuel from the Experimental Breeder Reactor II. We succeeded to achieve a good agreement with an overall trend of the experimental data with appropriate selection of a mode for real anode surface area, but there are still local inconsistencies between theoretical calculation and experimental observation. In addition, the results were validated and compared with two-dimensional results to identify possible uncertainty factors that had to be further considered in a computational electrorefining analysis. These uncertainty factors include material properties, heterogeneous material distribution, surface roughness, and current efficiency. Zirconium's abundance and complex behavior have more impact on uncertainty towards the latter period of electrorefining at given batch of fuel. The benchmark results found that anode materials would be dissolved from both axial and radial directions at least for low burn-up metallic fuels after active liquid sodium bonding was dissolved.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗