Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ROLLING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,711 records · Page 95

Tensile Behavior of Electron Beam-Welded and Post-Weld Vacuum-Annealed Nb-10% Hf-1% Ti Refractory Alloy Weldments

Nb-10% Hf-1% Ti refractory alloy is a high performance material extensively used for high temperature applications. Electron beam welding is one of the most widely used techniques to join refractory and reactive alloys. Bigger sizes of nozzles for rocket propulsion applications can be either made through deep drawing and flow turning route or by roll bending and welding route both using sheets/plates as input material for fabrication. The latter is a more economical option for mass production of the hardware using such exotic and expensive alloys. In view of this, both as-welded (AW) coupon and weld plus post-weld vacuum-annealed (AW + VA) coupon have been prepared to study their mechanical behavior. It has been observed that tensile strength and ductility have not been reduced in both these conditions vis-à-vis the base metal, confirming weld efficiency of the alloy to be ~ 100%. Microhardness is found to be 150-160 VHN in the base metal and 200-225 VHN in the weld fusion zone in AW condition, which became uniform (145-155 VHN) throughout the weldment in AW + VA condition. Microstructure of the weldment in AW condition is found to be consisting of grains solidified by epitaxial mode from base metal toward the weld centre. In AW + VA condition, improvement in tensile elongation is observed, which is found to be due to the presence of homogenized grains/more uniform microstructure near the heat-affected zone as compared to the steep gradient in grain size in different zones in the weld in AW condition.

36 MATERIALS SCIENCE↗

Controlled High Filler Loading of Functionalized Al{sub 2}O{sub 3}-Filled Epoxy Composites for LED Thermal Management

Thermal management in light-emitting diode (LED) has been extensively researched recently. This study is intended to develop an effective thermally conductive epoxy composite as thermal interface material (TIM) for headlamp LEDs. Silane-functionalized aluminum oxide (Al{sub 2}O{sub 3}) powder of different average particle sizes (44 and 10 µm) was studied for its feasibility as filler at its maximum loading. A detailed comparison of three different methods of particle dispersions, hand-mix, speed-mix and calendaring process (3-roll mill), has been reported. The dispersion of Al{sub 2}O{sub 3} particles, the thermal conductivity and thermal degradation characteristics of the composites were investigated and explained in detail. At 75 wt.% filler loading, 10 and 44 µm Al{sub 2}O{sub 3} achieved composite thermal conductivities of 1.13 and 2.08 W/mK, respectively, which is approximately 528 and 1055% of enhancement with respect to neat epoxy. The package-level thermal performance of the LED employing the Al{sub 2}O{sub 3}-filled TIMs was carried out using thermal transient analysis. The experimental junction-to-ambient thermal resistances (R{sub thJ-A}) achieved were 6.65, 7.24, and 8.63 K/W for Al{sub 2}O{sub 3-44µm}, Al{sub 2}O{sub 3-10µm} and neat epoxy, respectively. The results revealed that the Al{sub 2}O{sub 3-44µm} fillers-filled composite performed better in both material-level and package-level thermal characteristics.

36 MATERIALS SCIENCE↗

Exploring the Short-Channel Characteristics of Asymmetric Junctionless Double-Gate Silicon-on-Nothing MOSFET

This paper presents an analytical model of an asymmetric junctionless double-gate (asymmetric DGJL) silicon-on-nothing metal-oxide-semiconductor field-effect transistor (MOSFET). Solving the 2-D Poisson’s equation, the expressions for center potential and threshold voltage are calculated. In addition, the response of the device toward the various short-channel effects like hot carrier effect, drain-induced barrier lowering and threshold voltage roll-off has also been examined along with subthreshold swing and drain current characteristics. Performance analysis of the present model is also demonstrated by comparing its short-channel behavior with conventional DGJL MOSFET. The effect of variation of the device features due to the variation of device parameters is also studied. The simulated results obtained using 2D device simulator, namely ATLAS, are in good agreement with the analytical results, hence validating our derived model.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Effect of Prestrain Temperature on Kinetics of Static Recrystallization, Microstructure Evolution, and Mechanical Properties of Low Carbon Steel

In this research, the samples of a low carbon steel sheet were rolled up to a thickness prestrain of 67% at three different temperatures consisted of room, blue brittleness, and subzero temperature. Microhardness, SEM, and tensile tests were carried out to evaluate the static recrystallization kinetics defined by the Avrami equation, microstructural evolution, and mechanical properties. It was found that the Avrami exponent is altered with change in prestrain temperature and it achieves the value of 1 to 1. 5. Moreover, it was indicated that prestraining at subzero temperature followed by annealing at 600 °C leads to considerable enhancement in tensile properties and kinetics of static recrystallization compared to room and blue brittleness temperatures. The prestraining at blue brittleness temperature followed by annealing treatment caused, however, a higher strength and faster kinetics compared with that at room temperature. It was concluded that although from the steel ductility point of view, the blue brittleness temperature is called an unsuitable temperature, but it can be used as prestraining temperature to develop noticeable combination of strength and ductility in low carbon steel.

36 MATERIALS SCIENCE↗

Computational Design of a Novel Medium-Carbon, Low-Alloy Steel Microalloyed with Niobium

The design of a new steel with specific properties is always challenging owing to the complex interactions of many variables. In this work, this challenge is dealt with by combining metallurgical principles with computational thermodynamics and kinetics to design a novel steel composition suitable for thermomechanical processing and induction heat treatment to achieve a hardness level in excess of 600 HV with the potential for good fracture toughness. CALPHAD-based packages for the thermodynamics and kinetics of phase transformations and diffusion, namely Thermo-Calc{sup ®} and JMatPro{sup ®}, have been combined with an interdendritic segregation tool (IDS) to optimize the contents of chromium, molybdenum and niobium in a proposed medium-carbon low-manganese steel composition. Important factors taken into account in the modeling and optimization were hardenability and as-quenched hardness, grain refinement and alloying cost. For further investigations and verification, the designed composition, i.e., in wt.% 0.40C, 0.20Si, 0.25Mn, 0.90Cr, 0.50Mo, was cast with two nominal levels of Nb: 0 and 0.012 wt.%. The results showed that an addition of Nb decreases the austenite grain size during casting and after slab reheating prior to hot rolling. Validation experiments showed that the predicted properties, i.e., hardness, hardenability and level of segregation, for the designed composition were realistic. It is also demonstrated that the applied procedure could be useful in reducing the number of experiments required for developing compositions for other new steels.

36 MATERIALS SCIENCE↗

Rapid Strengthening Without Loss of Ductility via Electropulsing Treatment in Ti-6Al-4V Alloy

The commercial (hot-rolled and annealed) Ti-6Al-4V alloy subjected to electropulsing was investigated in this study. The results show that the electropulsing-treated sample with optimized parameter exhibits greatly refined microstructure and notable strength improvement without loss of ductility. The main strengthening mechanism is recognized as phase transformation and rapid grain refinement induced by recrystallization under EPT.

36 MATERIALS SCIENCE↗

Cryorolling-Induced Texture, Mechanical Properties and Fracture Behavior of Al-Mg-Si Alloys During Cold Deformation

This study investigated the texture, mechanical properties, and fracture behavior during cold working of cryorolled (CR) Al-Mg-Si alloys. An x-ray texture goniometer was used to examine the crystallographic texture, and tensile tests were performed to understand the deformation behavior in more detail. SEM/EBSD/TEM was used to observe the microstructures and fracture morphology of the alloy during cryorolling. The microstructures indicated that a large number of ultrafine grains and dislocations formed after cryorolled. The recrystallization was prohibited due to low temperature during deformation. The ultrafine grains and dislocation strength improved the tensile strength from 279.38 MPa for the room-rolled alloy to 313.98 MPa for the cryorolled alloy; better plasticity (4.6%) was observed in the CR sheet. Ductile and intergranular fractures were observed in the CR sheet deformation from 20 to 90%.

36 MATERIALS SCIENCE↗

Effect of Plane Strain Compression and Subsequent Recrystallization Annealing on Microstructures and Phase Transformation of NiTiFe Shape Memory Alloy

The effect of plane strain compression and subsequent recrystallization annealing on microstructures and phase transformation of NiTiFe shape memory alloy (SMA) is investigated. Inhomogeneous plastic deformation at various deformation degrees occurs in NiTiFe SMA during plane strain compression. Nanocrystalline phase and amorphous phase increase as the deformation degree increases. B2 austenite, B19′ martensite, nanocrystalline and amorphous phases coexist in the NiTiFe samples subjected to large plastic strain. The static recrystallization mechanisms depend on the microstructures of the deformed NiTiFe samples. The static recrystallization mechanisms deal with nucleation and growth of the recrystallized grains, growth of nanocrystalline phase and crystallization of amorphous phase. Grain size, subgrain boundaries, geometrically necessary dislocation density and Schmid factor are captured on the basis of electron backscattered diffraction data. The process of recrystallization annealing cannot eliminate the deformation texture completely. The slip direction [110] is the most favorable slip direction in the recrystallized NiTiFe sample. Plane strain compression along with subsequent recrystallization annealing changes the phase transformation path of as-rolled NiTiFe SMA, and it results in the decreasing martensite transformation start temperature. The three annealed NiTiFe samples exhibit the similar phase transformation behavior since complete recrystallization annealing leads to the similar microstructures.

36 MATERIALS SCIENCE↗

Planar Anisotropy, Tension–Compression Asymmetry, and Deep Drawing Behavior of Commercially Pure Titanium at Room Temperature

The planar anisotropy (PA) and tension–compression asymmetry (TCA) of the CP-Ti were investigated via uniaxial tension and compression tests at room temperature. The formability and the earing behavior of the CP-Ti sheet were studied via deep drawing experiment. The deep drawing simulations using the uniaxial tensile and the compressive curves as the hardening rules were compared with each other and with the experimental results. The CP-Ti sheet showed PA and TCA in yielding and strain hardening. The PA was characterized by the plastic strain ratio r{sub 0}, r{sub 45}, and r{sub 90} of 1.47, 2.06, and 2.05. The TCA showed PA, which showed tension–compression yield strength ratios of 1.12, 1.08, and 1.04 in 0°, 45°, and 90° in the rolling direction, and tensile and compressive hardening exponent ratios of 0.86, 0.8, and 0.62. The orientation distribution functions (ODFs) analysis demonstrated that the tensile and the compressive deformation textures were different and showed PA. The simulative results, including the simulated forming force and the earing profiles using the uniaxial tensile and compressive curves as the hardening rules, were not in agreement with each other. The results were not in good agreement with the experimental results, implying that the TCA had an important effect on the formability of the sheet. The TCA tended to reduce the thickness of the deep drawing parts, increase the earing ratio, and affect the drawing force.

36 MATERIALS SCIENCE↗

Fracture Analysis of ARB-Processed CP-Ti Sheets Under Unidirectional Tensile Loading

The fracture behavior of commercially pure titanium (CP-Ti) processed by accumulative roll bonding (ARB) was investigated in this study. Monolithic and Ti-SiC composite samples were first produced by ARB process and then subjected to uniaxial tensile testing at room temperature. Two different ductile fracture mechanisms including shear dimple rupture and equiaxed dimple rupture were observed in the initial and final ARB cycles, respectively. The difference in the rupture mechanism was attributed to different stress states at the crack tip and different densities of metallurgical defects. A non-uniform distribution of dimple size was obtained for fracture surfaces of the samples processed by a low number of ARB cycles. This was attributed to the heterogeneity of microstructure in the primary ARB cycles. The fracture surface of the samples processed by high ARB cycles represented more uniform dimples. This was attributed to more homogenous microstructure in the final cycles. Moreover, SiC particles showed a major role in fracture of samples, so that they affected the size and depth of the dimples, as well as the number of ARB cycles in which the transmission of the fracture mechanism occurred.

36 MATERIALS SCIENCE↗

Study on Texture Evolution and Shear Behavior of an Al/Ni/Cu Composite

The microstructure, texture, and mechanical properties of the Al/Ni/Cu composite during various accumulative roll bonding (ARB) cycles were studied using optical microscopy, scanning electron microscopy, x-ray diffraction, shear punch test, and hardness test. In addition, ImageJ software and Rietveld software were used in order to study microstructure and dislocation density variations, respectively. It was found that Ni and Cu layers were fractured and distributed in the Al matrix due to differences in their mechanical properties. Fracture and distribution of Cu and Ni particles after cycle five led to the alteration of the composite structure from a layered to a particle-reinforced structure. ARB process leads to the formation of strong orientation along the β-fiber and also to pronounced copper and dillamore components in both Al and Cu phases. Furthermore, the shear yield stress and ultimate shear strength of the composite increased as the ARB process advanced; however, shear elongation presented a non-uniform variation. Investigation of the fracture surfaces revealed that the mechanical properties of the composite are affected not only by the strain hardening of the Cu layer, but also by the structural change in the composite during the initial ARB cycles. During the last stages of the process, however, changes in mechanical properties were mostly governed by reinforcement particles serving as strain concentration zones and the strain hardening of the Al matrix.

36 MATERIALS SCIENCE↗

The Effect of Chemical Composition and Processing Technology on the Microstructure, Texture and Earing Behavior of DR Tinplate

The influence of alloying elements and processing technology on the microstructure, crystallographic texture and earing propensity has been investigated in two kinds of DR tinplate differing in Ti content: steel A, no Ti addition, and steel B 0.015% added. The cementite distribution, second-phase particles and the content of dissolved carbon and nitrogen atoms were obtained by SEM, TEM and XPS, respectively. Since the two steels develop both a partial 〈110〉//RD fiber and a {111}//ND fiber, the relative intensities of the several vital texture components seem to differ visibly. There are three types of strengthening mechanisms involved here: strengthening by grain size reduction, solution strengthening and strain hardening. That the tensile strength of steel B is greater than A implies the third mode plays a dominant role in the strength increasing for the DR tinplate. The crystallographic texture of materials not only results in a “preferential orientation” of the mechanical property, but also takes the primary responsibility for ears forming during drawing. Increasing the second cold-rolled reduction is not favorable to reduce the ear height, but this situation seems to be ameliorable. The average ears height of steel B is smaller than that of A, which demonstrated a low level of solute atoms and an ideal texture characteristic before deformation could alleviate the adverse effect caused by an elevated second cold reduction.

36 MATERIALS SCIENCE↗

Importance of Martensite Spatial Distribution at Large Volume Fractions in Imparting Ductility in High-Strength Dual-Phase Steel

Controlled austenite decomposition in a cold-rolled steel was carried out in a hot-dip process simulator with different inter-critical annealing process parameters to produce dual-phase steel consisting of martensite phase fraction above 50%. The evolving microstructure was characterized by using scanning electron microscope and electron backscattered diffraction techniques. Macro- and micro-texture was characterized by using x-ray diffraction and electron backscattered diffraction techniques, respectively. Uniaxial tensile deformation showed a very good combination of ultra-high strength above 900 MPa with uniform elongation of above 7%. An anomalous increase in ductility was observed for steel with high martensite volume fraction of 62.2% compared to that of lower fraction of 52.3%, indicating the influence of size and spatial distribution arrangement of ferrite and martensite phases. The enhancement in the ductility with high strength was attributed to the improved plastic deformability of hard fine martensite phase along with fine ferrite surrounding it. The nature of micro- and macro-texture was also found to affect strain partitioning compatibility between ferrite and martensite in this study.

36 MATERIALS SCIENCE↗

Effects of Nb on Superelasticity and Low Modulus Properties of Metastable β-Type Ti-Nb-Ta-Zr Biomedical Alloys

In this work, a series of Ti-xNb-2Ta-3Zr (x = 25, 30, 35, 40 wt.%) alloys are designed, and the transformation of β-phase to α″ martensitic, β-phase stability, microstructure, mechanical properties and corrosion performance of these alloys are investigated. The phase analysis shows as the Nb content increases, the α″ phase in these alloys decreases, while the intensity of the two main peaks β(110) and β(211) of Ti-40Nb-2Ta-3Zr alloy is reduced. These results can be attributed to the variation of β-phase stability caused by Nb element of alloy and cold rolling process. The mechanical properties test shows that the elastic modulus (52 GPa) of the Ti-35Nb-2Ta-3Zr alloy is the lowest and the elongation (18.8%) is the maximum. In addition, the alloy is susceptible to β-phase elastic deformation and stress-induced martensitic transformation resulting in the highest recovery strain of the alloy (66.87%). The polarization curves show that the Ti-35Nb-2Ta-3Zr alloy has the highest corrosion potential (− 0.34 V) and the lowest corrosion current density (0.21 μA cm{sup −2}) exhibiting the best corrosion resistance.

36 MATERIALS SCIENCE↗

Characterization of Static Performance and Failure of Resistance Spot Welds of High-Strength and Press-Hardened Steels

The static performances and failure characteristics of resistance spot welds (RSW) of steel sheets were studied in this work. Both similar and dissimilar joints of press-hardened steel grade 22MnB5 and as-rolled high-strength steel grade 1000 were examined. From metallographic analyses and micro-hardness measurements, it was shown that the microstructures of base metal (BM), heat affected zone (HAZ) and fusion zone of steel joints were noticeably different. In particular, the HAZ close to BM or subcritical HAZ (SCHAZ) of 22MnB5 steel exhibited greatly decreased hardness due to occurring tempered martensite, in which carbide precipitation was clearly observed. Furthermore, tensile shear test and cross-tension test of the welded steel sheets were carried out. The determined maximum loads, energy absorbability and corresponding failure mechanisms were analyzed and compared. The RSW samples of similar steel grade 1000 provided the highest load-carrying capacity and absorbed energy in both tests. Due to the large hardness difference and soft zone in weldment of dissimilar steel specimen, failure loads and static absorbed energies were deteriorated up to 17 and 68%, respectively. The observed fracture occurrences of all investigated joints were pullout failure mode, in which BM and HAZ were the crack initiation sites of grades 1000 steel and 22MnB5 steel, respectively. The SCHAZ of welded boron steel considerably caused the failure onset in tension shear test, but seemed to have negligible effect on cross-tension test.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Behavior of MnO{sub 2}/Pb Nanocomposite

MnO{sub 2}/Pb nanocomposite was produced by solid-state accumulative roll-bonding (ARB) technique. Composites with different amounts of MnO{sub 2} were synthesized with the highest probable ARB cycles. The mechanical properties of composites were studied by tensile, microhardness and shear punch tests. It was observed that yield stress, tensile stress and elongation were improved by increasing the ARB cycles. On the other hand, increasing the amount of MnO{sub 2} up to 0.5 wt.% improved the mechanical properties of the composites. Tensile tests results revealed that the maximum tensile strength could be achieved in the composite containing 0.5 wt.% MnO{sub 2} after 10 passes (up to 4.35 times higher than control sample, Pb-10 pass). In comparison with Pb-10 pass, the hardness of 0.5 wt.% MnO{sub 2}/Pb nanocomposite was enhanced up to 7.5 times after 10 ARB passes. ARB process led to a proper distribution of MnO{sub 2} particles in Pb matrix with the mean size of less than 30 nm.

36 MATERIALS SCIENCE↗

Strength Variation in Processing Multiport Extrusion Tubes of A1100 and A3102 Alloys

The manufacturing process of multiport extrusion tubes generally includes homogenization, extrusion, roll leveling and heat treatment. In order to investigate the influence of the manufacturing procedures on strength variation of multiport extrusion tubes made of A1100 and A3102 alloys, the tube fabrication experiments and following materials characterization are carried out. The alloys’ stress–strain curves after every processing procedure are measured, and pressure-bearing capacity of the tubes is tested. The tubes’ strength and pressure-bearing capacity reach the peak values after straightening process and drop to the minimum after annealing. The contributions of solid solution hardening, grain boundary hardening and constituent particle strengthening to yield strength are evaluated. It is deduced that cluster hardening is the dominant strengthening mechanism for the as-homogenized and as-extruded samples; the contribution of clusters is second to work hardening after straightening process; slight cold work in conjunction with high-temperature annealing accelerates abnormal grain growth. The loss of strength increment from clusters can be interpreted by the remarkable reduction of high-angle grain boundaries after abnormal grain growth.

36 MATERIALS SCIENCE↗

Deformation Behavior and Microstructure Evolution of Powder Metallurgy Ti6Al4V Alloy During Hot Compression

In order to determine appropriate workability parameters for cross-wedge rolling products of powder metallurgy (PM) Ti6Al4V alloys, thermal compression experiments were carried out within the temperature range of 850-1050 °C, the strain rate range of 0.1-10 s{sup −1}, and with a height decrease of 60%. The compression deformation behavior was investigated. A strain-compensated constitutive model was established based on the flow stress curves corrected by the friction, which can predict the flow behaviors under the entirety of the experimental deformation conditions. Moreover, the processing map was developed, and stable and unstable deformation regimes were established. The microstructure analysis illustrated that globularization and dynamic recrystallization were the main deformation mechanisms. The porosity of the compressed samples was greatly reduced and influenced by the temperature and strain rate. Considering the material flow stress, hot processing map, microstructure and porosity, the appropriate hot deformation parameters for PM Ti6Al4V alloy preforms are suggested.