At least 1,711 records · Page 95

Melting curve of silicon to 15 GPa determined by two-dimensional angle-dispersive diffraction using a Kawai-type apparatus with X-ray transparent sintered diamond anvils

The melting curve of silicon has been determined up to 15 GPa using a miniaturized Kawai-type apparatus with second-stage cubic anvils made of X-ray transparent sintered diamond. Our results are in good agreement with the melting curve determined by electrical resistivity measurements [V.V. Brazhkin, A.G. Lyapin, S.V. Popova, R.N. Voloshin, Nonequilibrium phase transitions and amorphization in Si, Si/GaAs, Ge, and Ge/GaSb at the decompression of high-pressure phases, Phys. Rev. B 51 (1995) 7549] up to the phase I (diamond structure)-phase II ({beta}-tin structure)-liquid triple point. The triple point of phase XI (orthorhombic, Imma)-phase V (simple hexagonal)-liquid has been constrained to be at 14.4(4) GPa and 1010(5) K. These results demonstrate that the combination of X-ray transparent anvils and monochromatic diffraction with area detectors offers a reliable technique to detect melting at high pressures in the multianvil press.

36 MATERIALS SCIENCE↗

Electrical characterization and water sensitivity of Sr 2 Fe 1.5 Mo 0.5 O 6-δ as a possible solid oxide fuel cell electrode

Sr 2 Fe 1.5 Mo 0.5 O 6-δ (SFMO) powders were synthesized by combustion synthesis. Porous samples were formed by uniaxial pressing of powder compacts and sintering in air. Electrical conductivity was measured by a four-point DC technique over a temperature range from 200 °C to 800 °C in air and in hydrogen. Crystal structures were investigated by X-ray diffractometry. Stability of powder samples was investigated in H 2 O-containing atmospheres. It was observed that Sr 2 Fe 1.5 Mo 0.5 O 6-δ was stable at 800 °C in water-containing atmospheres. However, it reacts with water at low temperatures. Reaction of Sr 2 Fe 1.5 Mo 0.5 O 6-δ (SFMO) with water at low temperatures is a potential shortcoming of this material for application in solid oxide fuel cells (SOFC) due to concerns regarding degradation of the electrodes at low temperatures during cycling.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterizing the Li–Li 7 La 3 Zr 2 O 12 interface stability and kinetics as a function of temperature and current density

The stability and kinetics of the Li–Li 7 La 3 Zr 2 O 12 (LLZO) interface were characterized as a function of temperature and current density. Polycrystalline LLZO was densified using a rapid hot-pressing technique achieving 97 ± 1% relative density, and <10% grain boundary resistance; effectively consisting of an ensemble of single LLZO crystals. It was determined that by heating to 175 °C, the room temperature Li-LLZO interface resistance decreases dramatically from 5822 (as-assembled) to 514 Ω cm 2 ; a > 10-fold decrease. In characterizing the maximum sustainable current density (or critical current density – CCD) of the Li-LLZO interface, several signs of degradation were observed. In DC cycling tests, significant deviation from Ohmic behavior was observed. In post-cycling tests, regions of metallic Li were observed; propagating parallel to the ionic current. For the cells cycled at 30, 70, 100, 130 and 160 °C, the CCD was determined to be 50, 200, 800, 3500, and 20000 μA cm –2 , respectively. As a result, the relationships and phenomena observed in this work can be used to better understand the Li-LLZO interface stability, enabling the use of batteries employing Li metal anodes.

36 MATERIALS SCIENCE↗

Facile and scalable fabrication of polymer-ceramic composite electrolyte with high ceramic loadings

Solid state electrolytes are a promising alternative to flammable liquid electrolytes for high-energy lithium battery applications. In this work polymer-ceramic composite electrolyte membrane with high ceramic loading (greater than 60 vol%) is fabricated using a model polymer electrolyte poly(ethylene oxide) + lithium trifluoromethane sulfonate and a lithium-conducting ceramic powder. The effects of processing methods, choice of plasticizer and varying composition on ionic conductivity of the composite electrolyte are thoroughly investigated. The physical, structural and thermal properties of the composites are exhaustively characterized. We demonstrate that aqueous spray coating followed by hot pressing is a scalable and inexpensive technique to obtain composite membranes that are amazingly dense and uniform. The ionic conductivity of composites fabricated using this protocol is at least one order of magnitude higher than those made by dry milling and solution casting. The introduction of tetraethylene glycol dimethyl ether further increases the ionic conductivity. The composite electrolyte's interfacial compatibility with metallic lithium and good cyclability is verified by constructing lithium symmetrical cells. As a result, a remarkable Li + transference number of 0.79 is discovered for the composite electrolyte.

36 MATERIALS SCIENCE↗

Mitigating cerium migration for perfluorosulfonic acid membranes using organic ligands

Improving the electrochemical stability of proton exchange membranes is a pressing priority for heavy-duty fuel cell vehicles. The lifetime of the most widely used perfluorosulfonic acid membranes is limited by reactive free radicals generated inside the system. Cerium has been found to reduce the chemical degradation of the membranes. However, cerium migration during fuel cell operation limits the chemical durability enhancement effect expected from the radical scavenging activity of cerium. Here we investigate a wide range of organic immobilizers for cerium, measuring their suitability concerning cerium retention, radical scavenging activity, and fuel cell performance. Further, we report that partially fluorinated phosphonic acids enhance cerium retention up to 45 times and reduce fluoride emission rate by 38% compared to the commercial Nafion™ XL membrane pre-impregnated with cerium. The energetics of cerium-phosphonic acid complex systems by density functional theory calculations rationalizes effective cerium immobilization.

25 ENERGY STORAGE↗

Determination of Ce 3+ , Co 2+ , Mn 2+ and Fe 2+ diffusion coefficients in Nafion® membrane

Concentration gradient diffusion coefficients for Ce 3+ , Co 2+ , Mn 2+ and Fe 2+ cations are determined in Nafion®211 membranes over a wide range of environmental conditions. Measurements are made using finite-width cation-rich bands introduced to NR211 via a hot-pressing procedure. A robust method of accurate diffusion coefficient determination of the finite-width deposits is developed using a Fick's second law of diffusion solution for one-dimensional systems. The transition metal dications are found to have nearly identical NR211 diffusion coefficients under water saturated conditions over the 22–80 °C range. The powerful chemical mitigant, Ce 3+ , is about one-half as diffusive as the dications under identical conditions. Derived diffusion coefficients for Ce 3+ and Co 2+ are found to be independent of initial cation concentration over the range of 12.5–70 mol% exchange level. The diffusion behavior of Ce 3+ in 80 °C liquid water and saturated water vapor is identical. The diffusion coefficients of Ce 3+ are shown to have a strong dependence on membrane hydration level varying by a factor of more than 30 over the range of 95 to 40% RH. Finally, the implications of these new diffusion findings are applied to a discussion of potential guidelines for the development of highly durable fuel cell systems, which employ mobile metal cations as lifetime-extending redox stabilizers.

08 HYDROGEN↗

Structure and high-temperature thermoelectric properties of SrAl{sub 2}Si{sub 2}

Single crystals of SrAl{sub 2}Si{sub 2} were synthesized by reaction of the elements in an aluminum flux at 1000 deg. C. SrAl{sub 2}Si{sub 2} is isostructural to CaAl{sub 2}Si{sub 2} and crystallizes in the hexagonal space group P-3m1 (90 K, a=4.1834 (2), c=7.4104 (2) A, Z=1, R1=0.0156, wR2=0.0308). Thermal analysis shows that the compound melts at {approx}1020 deg. C. Low-temperature resistivity on single crystals along the c-axis shows metallic behavior with room temperature resistivity value of {approx}7.5 m{omega} cm. High-temperature Seebeck, resistivity, and thermal conductivity measurements were made on hot-pressed pellets. The Seebeck coefficient shows negative values in entire temperature range decreasing from {approx}-78 {mu}V K{sup -1} at room temperature to -34 {mu}V K{sup -1} at 1173 K. Seebeck coefficients are negative indicating n-type behavior; however, the temperature dependence is consistent with contribution from minority p-type carriers as well. The lattice contribution to the thermal conductivity is higher than for clathrate structures containing Al and Si, approximately 50 mW cm{sup -1} K, and contributes to the overall low zT for this compound. - Abstract: Single crystals of SrAl{sub 2}Si{sub 2} have been prepared via an Al flux reaction and are of the CaAl{sub 2}Si{sub 2} structure type. The melting point is approximately 1020deg. C. Low temperature resistivity curve is similar to that observed for single crystals of CaAl{sub 2}Si{sub 2} High temperature Seebeck coefficient is negative, indicating n-type carriers. Display Omitted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Solution combustion synthesis of calcium zirconate, CaZrO{sub 3}, powders

Single-phase CaZrO{sub 3} powder was prepared by heating at 300 deg. C an aqueous solution of Ca(NO{sub 3}){sub 2}, ZrO(NO{sub 3}){sub 2} and beta-C{sub 3}H{sub 7}NO{sub 2} (molar ratio=3:3:4). TG-DTA analysis indicated that an intense exothermic reaction occurred at 255 deg. C, which lead to the formation of a voluminous white powder. No additional annealing was required, as pure crystalline CaZrO{sub 3} resulted directly from the combustion reaction. Although no advanced milling was performed, the specific surface area of the powder was 21.5 m{sup 2}/g. The average crystallite size of CaZrO{sub 3} was 23.9 nm. After sintering in air at 1400 deg. C for 2 h, the pellets - shaped by uniaxial pressing at 200 MPa - reached 95% of the theoretical density, had no open pores and were slightly translucent. - Graphical abstract: Single-phase CaZrO{sub 3} powder was prepared by low-temperature combustion synthesis. The resulting powder had a BET area of 21.5 m{sup 2}/g. After sintering at 1400 deg. C for 2 h 95% of the theoretical density was reached.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Formation of scandium carbides and scandium oxycarbide from the elements at high-(P, T) conditions

Synchrotron diffraction experiments with in situ laser heated diamond anvil cells and multi-anvil press synthesis experiments have been performed in order to investigate the reaction of scandium and carbon from the elements at high-(P,T) conditions. It is shown that the reaction is very sensitive to the presence of oxygen. In an oxygen-rich environment the most stable phase is ScO{sub x}C{sub y}, where for these experiments x=0.39 and y=0.50-0.56. If only a small oxygen contamination is present, we have observed the formation of Sc{sub 3}C{sub 4}, Sc{sub 4}C{sub 3} and a new orthorhombic ScC{sub x} phase. All the phases formed at high pressures and temperatures are quenchable. Experimentally determined elastic properties of the scandium carbides are compared to values obtained by density functional theory based calculations. - Graphical Abstract Legend (TOC Figure): Table of Contents Figure Selected images recorded with a MAR345 image plate detector show the reaction of alpha-Sc and graphite at high-(P,T) conditions. Left: mixture of alpha-Sc and graphite. Right: recovered sample after laser heated the diamond anvil cell.

36 MATERIALS SCIENCE↗

Effects of Rh on the thermoelectric performance of the p-type Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} half-Heusler alloys

We show that Rh substitution at the Co site in Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} (0<=x<=1) half-Heusler alloys strongly reduces the thermal conductivity with a simultaneous, significant improvement of the power factor of the materials. Thermoelectric properties of hot-pressed pellets of several compositions with various Rh concentrations were investigated in the temperature range from 300 to 775 K. The Rh 'free' composition shows n-type conduction, while Rh substitution at the Co site drives the system to p-type semiconducting behavior. The lattice thermal conductivity of Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} alloys rapidly decreased with increasing Rh concentration and lattice thermal conductivity as low as 3.7 W/m*K was obtained at 300 K for Zr{sub 0.5}Hf{sub 0.5}RhSb{sub 0.99}Sn{sub 0.01}. The drastic reduction of the lattice thermal conductivity is attributed to mass fluctuation induced by the Rh substitution at the Co site, as well as enhanced phonon scattering at grain boundaries due to the small grain size of the synthesized materials. - Graphical abstract: Significant reduction of the lattice thermal conductivity with increasing Rh concentration in the p-type Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} half-Heusler materials prepared by solid state reaction at 1173 K.

36 MATERIALS SCIENCE↗

Cu{sub 22}Bi{sub 12}S{sub 21}Cl{sub 16}-A mixed conductor with fast one-dimensional copper(I) ion transport

Melting reactions of Cu, CuCl, S, and Bi{sub 2}S{sub 3} yield black, shiny needles of Cu{sub 22(1)}Bi{sub 12}S{sub 21(1)}Cl{sub 16(1)}. The compound decomposes peritectically at 649(5) K. Oxidation state +I of the copper atoms is supported by Cu-K-XANES. The compound crystallizes in the hexagonal space group P6/m with a=2116.7(7) pm and c=395.17(5) pm. Seven anions coordinate each of the two independent bismuth cations in the shape of mono-capped trigonal prisms. These polyhedra share edges and faces to form trigonal and hexagonal tubes running along [0 0 1]. The hexagonal tubes are centered by chloride ions, which are surrounded by disordered copper cations. The majority of copper cations are distributed over numerous sites between the tubes. The Joint Probability Density Function (JPDF) reveals a continuous pathway along [0 0 1]. The high mobility of the copper cations along [0 0 1] was demonstrated by impedance spectroscopy and DC polarization measurements on single crystals. The ionic conductivity at 450 K is about {sigma}{sub ion}=0.06 S cm{sup -1}, and the activation energy for Cu{sup +} ion conduction is E{sub a}=0.44 eV. The chemical diffusion coefficient of copper is in the order of D{sub cu}{sup {delta}=}10{sup 19} cm{sup -3} at 420 K. The electronic band gap (p-type conductor) was determined as E{sub g}=0.06 eV. At room temperature the thermal conductivity of a pressed pellet is about {kappa}=0.3 W K{sup -1} m{sup -1} and the Seebeck coefficient is S=43 {mu}V K{sup -1}. -- Graphical Abstract: Copper cations easily move through the rigid tubular crystal structure of Cu{sub 22}Bi{sub 12}S{sub 21}Cl{sub 16}. Display Omitted

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crystal structure, characterization and thermoelectric properties of the type-I clathrate Ba{sub 8-y}Sr{sub y}Al{sub 14}Si{sub 32} (0.6{<=}y{<=}1.3) prepared by aluminum flux

The title compound was prepared as single crystals using an aluminum flux technique. Single crystal and powder X-ray diffraction indicate that this composition crystallizes in the clathrate type-I structure, space group Pm3-bar n. Electron microprobe characterization indicates the composition to be Ba{sub 8-y}Sr{sub y}Al{sub 14.2(2)}Si{sub 31.8(2)} (0.77<y<1.3). Single-crystal X-ray diffraction data (90 and 12 K) were refined with the Al content fixed at the microprobe value (12 K data: R{sub 1}=0.0233, wR{sub 2}=0.0441) on a crystal of compositions Ba. The Sr atom preferentially occupies the 2a position; mixed Al/Si occupancy was found on all framework sites. These refinements are consistent with a fully occupied framework and nearly fully occupied cation guest sites as found by microprobe analysis. Temperature dependent electrical resistivity and thermal conductivity have been measured from room temperature to 1200 K on a hot-pressed pellet. Electrical resistivity reveals metallic behavior. The negative Seebeck coefficient indicates transport processes dominated by electrons as carriers. Thermal conductivity is between 22 and 25 mW/cm K. The sample shows n-type conductivity with a maximum figure of merit, zT of 0.3 at 1200 K. A single parabolic band model predicts a five-fold increase in zT at 800 K if carrier concentration is lowered. -- Graphical abstract: The inorganic type-I clathrate phase with nominal composition Ba{sub 7}Sr{sub 1}Al{sub 14}Si{sub 32} has been prepared by Al flux. Single crystal diffraction at 90 and 12 K reveal that the framework is fully occupied with the cation sites nearly fully occupied. The lattice thermal conductivity is low thereby suggesting further optimization of the carrier concentration will lead to a high zT. Display Omitted Highlights: {yields} Ba{sub 7}Sr{sub 1}Al{sub 14}Si{sub 32} is a light element phase ideal for thermoelectric power generation. {yields} Ba{sub 7}Sr{sub 1}Al{sub 14}Si{sub 32} is a high melting point cubic structure ideal for efficient power generation. {yields} The framework is fully occupied with the cation sites nearly fully occupied. {yields} Further optimization of the carrier concentration is expected to lead to a high zT.

36 MATERIALS SCIENCE↗

Thermoelectric and microstructural properties of Pb{sub 0.9-x}Sn{sub 0.1}Ge{sub x}Te compounds prepared by spinodal decomposition

Three samples of Pb{sub 0.9-x}Sn{sub 0.1}Ge{sub x}Te with x=0.25, 0.35, 0.6 were prepared by heating the mixtures above the melting point of the constituent elements followed by quenching in water. The x=0.6 sample is close to the center of the immiscibility region, while the x=0.25 and 0.35 samples are in the Pb rich region inside the spinodal miscibility gap. Microstructural investigations using Powder X-ray Diffraction, Scanning Electron Microscopy and Energy Dispersive X-ray Spectroscopy revealed both GeTe-rich and PbTe-rich phases. The samples were uniaxially hot pressed and the thermoelectric properties were characterized in the temperature range 2-400 K using a commercial apparatus and from 300 to 650 K with a custom designed setup. The best sample (x=0.6) reached zT{approx}0.6 at 650 K, while the x=0.25 and 0.35 samples showed thermal instability at elevated temperatures. -- Graphical abstract: Spinodal decomposition in the GeTe-SnTe-PbTe system demonstrated by SEM and EXS images. Display Omitted Highlights: {yields} Investigation of Pb-rich part of the spinodal miscibility gap in PbTe-SnTe-GeTe. {yields} zT=0.6 at 650 K reproduced for Pb{sub 0.3}Sn{sub 0.1}Ge{sub 0.6}Te. {yields} Pb-rich phases shown to be thermally instable. {yields} Thermoelectric property characterization at low and high temperature. {yields} Microstructural investigations using PXRD, SEM, EDX and PSM.

36 MATERIALS SCIENCE↗

High-pressure synthesis and crystal structure of the lithium borate HP-LiB{sub 3}O{sub 5}

The new lithium borate HP-LiB{sub 3}O{sub 5} was synthesized under high-pressure/high-temperature conditions of 6 GPa and 1050 deg. C in a multianvil press with a Walker-type module. The compound crystallizes in the space group Pnma (no. 62) with the lattice parameters a=829.7(2), b=759.6(2), and c=1726.8(4) pm (Z=16). The high-pressure compound HP-LiB{sub 3}O{sub 5} is built up from a three-dimensional network of BO{sub 4} tetrahedra and BO{sub 3} groups, which incorporates Li{sup +} ions in channels along the b-axis. Band assignments of measured IR- and Raman spectra were done via quantum-mechanical calculations. Additionally, the thermal behavior of HP-LiB{sub 3}O{sub 5} was investigated. - Graphical abstract: The new high-pressure compound HP-LiB{sub 3}O{sub 5} is built up from a three-dimensional network of BO4 tetrahedra and BO{sub 3} groups, which incorporates Li{sup +} ions in channels along the b-axis. In this paper, the synthesis, the crystal structure, and the properties of HP-LiB{sub 3}O{sub 5} are described. Highlights: > Synthesis of a new lithium borate with the composition HP-LiB{sub 3}O{sub 5} at high pressure. > In contrast to the non-centrosymmetric phase LiB{sub 3}O{sub 5}, this high-pressure phase is centrosymmetric. > First example of ternary alkali borates exhibiting threefold bridging oxygen atoms.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermoelectric properties and nonstoichiometry of GaGeTe

Polycrystalline samples of composition Ga{sub 1+x}Ge{sub 1-x}Te (x=-0.03 Division-Sign 0.07) and GaGeTe{sub 1-y} (y=-0.02 Division-Sign 0.02) were synthesized from elements of 5 N purity using a solid state reaction. The products of synthesis were identified by X-ray diffraction; phase purity and microstructure were examined by EDX/SEM. Samples for measurement of transport properties were prepared using hot-pressing. They were characterized by measurement of electrical conductivity, the Hall coefficient, and the Seebeck coefficient over a temperature range 80-480 K and of thermal conductivity over a temperature range 300-580 K. All samples show p-type conductivity. We discuss the influence of stoichiometry on the phase purity of the samples and on free carrier concentration. The investigation of thermoelectric properties shows that the power factor of these samples is low compared to state-of-the-art materials at room temperature but increases distinctly with temperature. - Graphical abstract: Structure and preparation of GaGeTe. Electrical conductivity {sigma}, the Hall coefficient R{sub H}, the Seebeck coefficient S and thermal conductivity {kappa} as a function of temperature for the Ga{sub 1.01}Ge{sub 0.99}Te{sub 0.99} sample. Highlights: Black-Right-Pointing-Pointer We explore thermoelectric and transport properties of Ga{sub 1+x}Ge{sub 1-x}Te and GaGeTe{sub 1-y}. Black-Right-Pointing-Pointer GaGeTe is p-type degenerate semiconductor; the hole concentration increase with x and y. Black-Right-Pointing-Pointer Maximum power factor {sigma}S{sup 2}=3.6 Multiplication-Sign 10{sup -4} Wm{sup -1} K{sup -2} at 475 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Influence of nanoinclusions on scattering of holes and phonons and transport coefficients in Bi{sub x}Sb{sub 1-x}Te{sub 3} bulk nanostructures

One of the possible ways to increase the thermoelectric figure of merit is the use of bulk nanostructured materials fabricated by melt spinning with subsequent hot pressing or spark plasma sintering. Among a variety of nanostructure types these materials contain regions of initial solid solution with nanometer sized inclusions of different compositions. In the present work the scattering of holes and phonons on nanoinclusions in such p-Bi{sub x}Sb{sub 1-x}Te{sub 3} based materials is considered. The change of transport coefficients due to this scattering mechanism is theoretically estimated. The estimations showed that the reduction of lattice thermal conductivity (about 12-13%) for nanoinclusions of Bi{sub 2}Te{sub 3}-Sb{sub 2}Te{sub 3} solid solution with different compositions is much greater than the change in power factor. Therefore the corresponding increase of the thermoelectric figure of merit for this case is determined mainly by phonon scattering. Also it is shown that the results of estimations depend on phonon spectrum approximation, e.g. in the case of sine-shaped instead of linear phonon spectrum the estimations give two times higher thermal conductivity reduction. - Graphical abstract: Relative phonon thermal conductivity {kappa}{sub ph} change (black line) due to nanoinclusion scattering versus nanoinclusion radius a, and relative thermoelectric power factor change (red line) due to nanoinclusion scattering versus chemical potential {mu} at nanoinclusion size a=1.5 nm and U{sub 0}=-0.146 eV. Highlights: Black-Right-Pointing-Pointer p-Bi{sub x}Sb{sub 1-x}Te{sub 3} solid solutions with nanosized inclusions were considered. Black-Right-Pointing-Pointer Selective hole scattering can increase power factor at high carrier concentrations. Black-Right-Pointing-Pointer Lattice thermal conductivity estimations depend on phonon spectrum approximation. Black-Right-Pointing-Pointer Phonon scattering can reduce lattice thermal conductivity by about 12-13%. Black-Right-Pointing-Pointer The latter factor mainly determines the increase of thermoelectric efficiency.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Power factor improvement in hydrothermally synthesized Bi{sub 2-x}Sb{sub x}Te{sub 3} (x=1.5) - carbon sphere composites

We report fabrication of compacted Bi{sub 0.5}Sb{sub 1.5}Te{sub 3} composites by adding 1 wt% of carbon spheres in the hydrothermal synthesis. The processing parameter of sintering temperature is investigated in order to optimize the thermoelectric power factor of pressed Bi{sub 0.5}Sb{sub 1.5}Te{sub 3} composites. As a result, we find that the composite sintered at 360 Degree-Sign C shows the best power factor performance among the composites and has a largest power factor of 15.4 {mu}W/cm K{sup 2} at 205 K and 13.5 {mu}W/cm K{sup 2} at 290 K. When compared with the samples without addition of carbon sphere in the hydrothermal synthesis, the composites sintered at 340 Degree-Sign C and 360 Degree-Sign C both surpass the largest power factor of 12.1 {mu}W/cm K{sup 2} at 280 K and 11.9 {mu}W/cm K{sup 2} at 290 K for the 340 Degree-Sign C-sintered counterpart. - Graphical abstract: Compacted Bi{sub 0.5}Sb{sub 1.5}Te{sub 3-{delta}} composites obtained by adding 1 wt% of carbon spheres in the hydrothermal synthesis. The composites sintered at 340 Degree-Sign C and 360 Degree-Sign C both surpass the largest power factor of 12.1 {mu}W/cm K{sup 2} at 280 K and 11.9 {mu}W/cm K{sup 2} at 290 K for the 340 Degree-Sign C-sintered counterpart. Highlights: Black-Right-Pointing-Pointer Fabrication of Bi{sub 0.5}Sb{sub 1.5}Te{sub 3-{delta}} composites. Black-Right-Pointing-Pointer Addition of 1 wt% carbon spheres in the hydrothermal synthesis. Black-Right-Pointing-Pointer Investigation of sintering temperature using encapsulating-and-sintering techniques. Black-Right-Pointing-Pointer 360 Degree-Sign C-sintered composite showing the largest power factor of 15.4 {mu}W/cm K{sup 2} at 205 K. Black-Right-Pointing-Pointer 10-60% improvement over the counterpart without adding carbon spheres.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Solid-state synthesis of Mg{sub 2}Si via short-duration ball-milling and low-temperature annealing

In this work, a short duration ball-milling of elemental Mg and Si followed by a thermal treatment is suggested in order to synthesize magnesium silicide via solid-state reaction. The formation of magnesium silicide was studied in terms of its structure and thermal characteristics by powder X-ray diffraction, scanning electron microscopy, energy dispersive spectroscopy and differential scanning calorimetry. Pure Mg{sub 2}Si was formed after short milling and heating at temperatures as low as 280 Degree-Sign C. Differential scanning calorimetry analysis was performed to study the kinetics of the reaction. The activation energy of the reaction was calculated using the Ozawa-Flynn-Wall and Friedman methods. The thermoelectric properties suggested semiconducting behavior whereas thermal conductivity values of highly dense hot-pressed pellets are consistent with the literature. - Graphical abstract: Thermographs of ball-milled Mg and Si powders (1 and 2) show exothermic areas suggesting Mg{sub 2}Si formation at low temperatures. Unmilled Mg and Si mixture (3) forms Mg{sub 2}Si at higher temperatures. Highlights: Black-Right-Pointing-Pointer Ball-milling process is crucial for the formation of pure Mg{sub 2}Si at low temperatures. Black-Right-Pointing-Pointer Synthesis profiles based on different temperature settings and duration are suggested. Black-Right-Pointing-Pointer Thermal analysis confirms the shift of the Mg{sub 2}Si formation at low temperatures.

36 MATERIALS SCIENCE↗