Solution combustion synthesis of calcium zirconate, CaZrO{sub 3}, powders
Single-phase CaZrO{sub 3} powder was prepared by heating at 300 deg. C an aqueous solution of Ca(NO{sub 3}){sub 2}, ZrO(NO{sub 3}){sub 2} and beta-C{sub 3}H{sub 7}NO{sub 2} (molar ratio=3:3:4). TG-DTA analysis indicated that an intense exothermic reaction occurred at 255 deg. C, which lead to the formation of a voluminous white powder. No additional annealing was required, as pure crystalline CaZrO{sub 3} resulted directly from the combustion reaction. Although no advanced milling was performed, the specific surface area of the powder was 21.5 m{sup 2}/g. The average crystallite size of CaZrO{sub 3} was 23.9 nm. After sintering in air at 1400 deg. C for 2 h, the pellets - shaped by uniaxial pressing at 200 MPa - reached 95% of the theoretical density, had no open pores and were slightly translucent. - Graphical abstract: Single-phase CaZrO{sub 3} powder was prepared by low-temperature combustion synthesis. The resulting powder had a BET area of 21.5 m{sup 2}/g. After sintering at 1400 deg. C for 2 h 95% of the theoretical density was reached.