Vertically oriented ZrO 2 –TiO 2 –Nb 2 O 5 –Al 2 O 3 mixed nanopatterned bioceramics on Ti6Al7Nb implant assessed by laser spallation technique
Recently, reports on the fabrication of nonstructural configuration have generated scientific interest due to increased awareness of the oxide nanotubes in the biomedical implant field and other industrial approaches. In this paper, highly ordered ZrO 2 –TiO 2 –Nb 2 O 5 –Al 2 O 3 nanotube arrays were grown by physical vapor deposition (PVD) of a zirconium layer on titanium-niobium alloy implant (IMPTi67) and succeeding anodic oxidation at a constant voltage (60 V) with exposure times ranging from 30 to 300 min. To crystallize the resulting mixed oxide nanotubes, heat treatment was also applied. The nanotubes were placed in an atmospheric furnace at temperatures ranging from 450 to 800 °C for 2 h. This treatment provided a morphological evolution was strongly influenced by the anodization time, where highly aligned bamboo-shaped oxide nanotubes (161 ± 44 nm in inside diameter and ~1 μm in length) were formed after 300 min of anodization. After annealing at temperature below 500 °C, the nano-array configuration remained stable and the average inner diameter decreased to around 40 nm. The effects of anodically fabrication time on the adhesion strength of four-phase multilayered mixed oxide nanotubes on anodized Zr/IMPTi67 surfaces assed by microscratch analysis. From the results, increasing the annealing temperature further to 800 °C fully destroyed the nanotubes and consequently the tubular arrangement was converted to a coarse grain structure. It was revealed that annealing at 450 °C for 2 h was the optimum conditions for stable nanotubular array generation, where the highest adhesion strength (shifted from 2595.59 to 2640.12 mN), microhardness (372 HV) and hydrophilicity (15 ± 1°) were recorded. It is notify that the adhesion strength of highly ordered mixed nanotubes was remarkably decreased after thermal treatment at 800 °C (1817.51 mN). Through the laser spallation analysis, the intrinsic adhesion strength of the Zr/IMPTi67 interface was found to be at 63 MPa, while the first stages of failure occurred at a stress state of 35 MPa. The adhesion of the film with the tubular structure proved to have a significantly larger adhesion strength of 246 MPa for the complete failure and 203 MPa for incipient stages of spallation. Finally, the considered surface modification can be an effective step in determining the interface strength between biomedical implants and the nanostructured coatings.
Effect of differently oriented interlayer phases on the radiation damage of Inconel-$\mathrm{Ni}$ multimetallic layered composite
Multimetallic layered composites (MMLCs) have shown an excellent potential for application under extreme environments, e.g., accident-tolerant fuel cladding, because of their low oxidation tendency and high corrosion resistance. Interfacial phases or complexions in nanocrystalline materials accelerate the annihilation of defects and enhance the radiation resistance of materials, making MMLCs with engineered interlayer phases compelling to deploy in extreme conditions. However, implementation of MMLCs in full capacity remained a challenge due to a lack of fundamental understanding of the underlying mechanisms governing the characteristics of the interface between the metallic layers. The precise role of interlayer phases in MMLCs and their interaction with defects, specifically under extreme conditions, is still unexplored. Pursuing atomistic simulations for various Inconel-Ni MMLCs model materials, we revealed accelerated defect mobility in interlayers with larger crystalline misorientation and the inverse relationship between the interface sink strength to the misorientation angle. Furthermore, we found a linear relation between interlayer misorientation angle with the density of radiation-induced defects and radiation enhanced displacements. So, our results indicate that radiation-induced material degradation is accelerated by the higher defect formation tendency of MMLCs with a high-angle interlayer interface.
A factorial environment-oriented input-output model for diagnosing urban air pollution
Not Available
Stochastic goal-oriented error estimation with memory
We propose a stochastic dual-weighted error estimator for the viscous shallow-water equation with boundaries. For this purpose, previous work on memory-less stochastic dual-weighted error estimation is extended by incorporating memory effects. The memory is introduced by describing the local truncation error as a sum of time-correlated random variables. The random variables itself represent the temporal fluctuations in local truncation errors and are estimated from high-resolution information at near-initial times. The resulting error estimator is evaluated experimentally in two classical ocean-type experiments, the Munk gyre and the flow around an island. In these experiments, the stochastic process is adapted locally to the respective dynamical flow regime. Our stochastic dual-weighted error estimator is shown to provide meaningful error bounds for a range of physically relevant goals. We prove, as well as show numerically, that our approach can be interpreted as a linearized stochastic-physics ensemble.
Effects of substrate orientation on aluminum grown on MgAl2O4 spinel using molecular beam epitaxy
Explore the source record for details and available documents.
Growing AlN crystals on SiC seeds: Effects of growth temperature and seed orientation
Not Available
Oriented TiO2 nanotubes as a lithium metal storage medium
A new strategy for suppressing dendritic lithium growth in rechargeable lithium metal batteries is introduced, in which TiO2 nanotube (NT) array electrodes prepared by anodization are used as a metallic lithium storage medium. During the first charge process, lithium ions are inserted into the crystal structure of the TiO2 NT arrays, and then, lithium metal is deposited on the surfaces of the NT arrays, i.e., in the NT pores and between NT walls. From the second cycle onward, the TiO2 material is used as lithium ion pathways, which results in the effective current distribution for lithium deposition and prevents disintegration of the deposited metallic lithium. Compared to a Li(Cu foil)-LiCoO2 cell, the Li(TiO2 NT)-LiCoO2 cell exhibits enhanced cycling efficiency. This new concept will enable other 3D structured negative active materials to be used as lithium metal storage media for lithium metal batteries.
Small angle scattering reveals the orientation of cytochrome P450 19A1 in lipoprotein nanodiscs
Not Available
Investigating the orientation dependence of local fields around spherical defects using crystal plasticity simulations
Not Available
Fiber orientation in the frontal region of a center-gated disk: Experiments and simulation
Not Available
Testing orientational closure approximations in dilute and non-dilute suspensions with Rheo-SANS
Not Available
Laser-induced growth of oriented Sb2S3 single crystal dots on the surface of 82SbSI–18Sb2S3 glasses
Not Available
Orientation relationship formed during irradiation induced precipitation of W in Cu
Not Available