Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRONS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,693 records · Page 94

Dual phase transformation and resultant magnetic properties in Fe{sub 3}Pt thin films

Fifty-nm-thick Fe{sub 75}Pt{sub 25} thin films have been made on glass substrates by rf magnetron sputtering at room temperature, and subsequently annealed at 300 -700 deg. C (T{sub a}) for 1 h. The as-deposited Fe{sub 3}Pt film exhibits high magnetization of 1530 emu/cm{sup 3} and a disordered bcc structure, confirmed by high-resolution synchrotron radiation x-ray diffractometry. First-phase transformation from the bcc to disorder fcc structure occurs for samples annealed at 300 deg. C. With increasing of T{sub a} up to 375 deg. C, the film displays a nearly disordered fcc phase with low magnetization of 1083 emu/cm{sup 3}. The fcc phase changes to ordered L1{sub 2} structure for samples with T{sub a} {>=} 400 deg. C. The highly ordered L1{sub 2} phase with magnetization of 1270 emu/cm{sup 3} and coercivity of 66 Oe was obtained in Fe{sub 3}Pt film at 700 deg. C-annealing.

36 MATERIALS SCIENCE↗

Effect of the number of interfaces on the magnetic properties of [SnO{sub 2}/Cu-Zn ferrite] multilayer

The [SnO{sub 2}/Cu-Zn ferrite (CZF)]{sub n} (n = 5, 10, 15, and 20) multilayer (ML) were deposited by rf-magnetron sputtering to study their magnetic properties. The magnetization and ferromagnetic resonance (FMR) measurements were undertaken to understand the effect of interfaces on the magnetic properties of these ML. FMR signal line shape changes from asymmetric to symmetric as n increases. The FMR signal peak to peak intensity, FMR linewidth, effective and saturation magnetization and coercivity exhibit oscillations as a function of n. In the parallel configuration the resonance field increases with increase in n, presumably due to the decrease in the active layer to dead layer thickness ratio. The interlayer coupling is strong in the ML with n = 5 leading to the formation of spin waves. The ML interlayer coupling and anisotropy decreases with increasing n. The oscillatory behavior of the magnetic properties can be ascribed to the nonmonotonic variations in the structure and the geometry of the interfaces.

36 MATERIALS SCIENCE↗

Control of magnetic properties of MnBi and MnBiCu thin films by Kr{sup +} ion irradiation

Mn{sub 52}Bi{sub 48} (15 nm) and Mn{sub 54}Bi{sub 24}Cu{sub 21} (15 nm) thin films were prepared by the magnetron sputtering and vacuum annealing at 350 deg. C, and the variations of their structures and magnetic properties with 30 keV Kr{sup +} ion irradiation were studied. The MnBi and MnBiCu films exhibited saturation magnetizations M{sub s} of 180 emu/cc and 210 emu/cc, the coercivities H{sub c} of 10 kOe and 3.4 kOe, respectively. The M{sub s} and H{sub c} of the MnBi abruptly vanished by the irradiation of ion dose at 3 x 10{sup 14} ions/cm{sup 2}, while those of the MnBiCu film gradually decreased with increasing the ion dose and became zero at 5 x 10{sup 13} ions/cm{sup 2}. The different trend on the ion irradiation between MnBi and MnBiCu films is understood by the surface structure of the film, i.e., the MnBi has convex islands on its surface, which protect the underneath NiAs-type MnBi from the irradiation, while the MnBiCu has rather flat surface, and its crystal structure was uniformly modified by the irradiation. From the surface flatness and the uniformity of the MnBiCu film, as well as the low annealing temperature of 350 deg. C, it was concluded that the MnBiCu film is one of the attractive materials for high-density ion irradiation bit patterned media.

36 MATERIALS SCIENCE↗

One-step fabrication of L1{sub 0} FePt nanocubes and rods by cluster beam deposition

In this work, single crystal L1{sub 0} FePt nanocubes have been successfully produced by a cluster beam deposition technique without the need of post annealing. Particles have been deposited by dc magnetron sputtering using high Ar pressures on both single crystal Si substrates and Au grids for the measurement of magnetic and structural properties, respectively. The nanocubes have a uniform size distribution with an average size of 5 nm. At 1 Torr, the particles have the L1{sub 0} structure with an order parameter of 0.5 and a RT coercivity of 2 kOe with high switching fields observed in the hysteresis loop. Further annealing increased the particle size to 20 nm and the RT coercivity to 10.2 kOe with perfect chemical ordering. In addition to these nanocubes, micron size rods with the L1{sub 0} structure have been observed near the cluster gun. SEM analysis showed that these rods consist of nanoparticles with 20 nm average size. Surfactant assisted high-energy ball milling has been used to separate the nanoparticles from the rods. After one hour of milling, these 20 nm particles showed a room temperature coercivity of 9 kOe with an order parameter of 0.85. These FePt nanocubes have a potential for use in the development of future high-density magnetic recording media because of their high coercivity, good shape and very narrow size distribution.

36 MATERIALS SCIENCE↗

Polycrystalline magnetic garnet films comprising weakly coupled crystallites for piezoelectrically-driven magneto-optic spatial light modulators

We have investigated the magnetization process of the polycrystalline magnetic garnet films in order to determine the most suitable composition of garnet films for piezoelectrically-driven magneto-optic spatial light modulators (MOSLMs). For experiment, the bismuth-dysprosium-aluminum-substituted yttrium iron (Bi{sub 1.3}Dy{sub 0.7}Y{sub 1.0}Fe{sub 3.1}Al{sub 1.9}O{sub 12}) garnet films were deposited by an RF magnetron sputter and annealed at 700 deg. C in air. The annealing time was varied in a range of several minutes to control the grain size. The saturation magnetization, the remanent magnetization and the composition of the fabricated garnet films slightly changed versus the annealing time. Experiments showed that the coercivity and the grain size increased at longer annealing; the coercivity was larger for films with bigger grains. This work shows that garnet films with smaller coercivity are most suitable for controlling the magnetization of garnet and, correspondingly, the magneto-optical rotation of MOSLM pixels driven by piezoelectrics.

36 MATERIALS SCIENCE↗

Breakdown by magnetic field in a La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/MgO/Fe spin valve

A La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/MgO/Fe spin valve with inverse tunneling magnetoresistance (TMR) was fabricated on a (100) SrTiO{sub 3} substrate by radio frequency magnetron sputtering. Giant TMR ratios up to 540% were obtained. The breakdown of the spin valve was observed at high magnetic field, which was attributed to the joint action of the invalidation of MgO barrier and the shift of Fermi energy in La{sub 0.7}Sr{sub 0.3}MnO{sub 3} at high magnetic field.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electrical and optical properties of sputtered amorphous vanadium oxide thin films

Amorphous vanadium oxide (VO{sub x}) is a component found in composite nanocrystalline VO{sub x} thin films. These types of composite films are used as thermistors in pulsed biased uncooled infrared imaging devices when containing face centered cubic vanadium monoxide phase crystallites, and substantial fractions of amorphous material in the composite are necessary to optimize device electrical properties. Similarly, optoelectronic devices exploiting the metal-to-semiconductor transition contain the room-temperature monoclinic or high-temperature (>68 deg. C) rutile vanadium dioxide phase. Thin films of VO{sub x} exhibiting the metal-to-semiconductor transition are typically polycrystalline or nanocrystalline, implying that significant amounts of disordered, amorphous material is present at grain boundaries or surrounding the crystallites and can impact the overall optical or electronic properties of the film. The performance of thin film material for either application depends on both the nature of the crystalline and amorphous components, and in this work we seek to isolate and study amorphous VO{sub x}. VO{sub x} thin films were deposited by pulsed dc reactive magnetron sputtering to produce amorphous materials with oxygen contents {>=}2, which were characterized electrically by temperature dependent current-voltage measurements and optically characterized by spectroscopic ellipsometry. Film resistivity, thermal activation energy, and complex dielectric function spectra from 0.75 to 6.0 eV were used to identify the impact of microstructural variations including composition and density.

36 MATERIALS SCIENCE↗

Designing interlayers to improve the mechanical reliability of transparent conductive oxide coatings on flexible substrates

In this study, we investigate the effect of interlayers on the mechanical properties of transparent conductive oxide (TCO) on flexible polymer substrates. Indium tin oxide (ITO), which is the most widely used TCO film, and Ti, which is the most widely used adhesive interlayer, are selected as the coating and the interlayer, respectively. These films are deposited on the polymer substrates using dc-magnetron sputtering to achieve varying thicknesses. The changes in the following critical factors for film cracking and delamination are analyzed: the internal stress ({sigma}{sup i}) induced in the coatings during deposition using a white light interferometer, the crystallinity using a transmission electron microscope, and the surface roughness of ITO caused by the interlayer using an atomic force microscope. The resistances to the cracking and delamination of ITO are evaluated using a fragmentation test. Our tests and analyses reveal the important role of the interlayers, which significantly reduce the compressive {sigma}{sup i} that is induced in the ITO and increase the resistance to the buckling delamination of the ITO. However, the relaxation of {sigma}{sup i} is not beneficial to cracking because there is less compensation for the external tension as {sigma}{sup i} further decreases. Based on these results, the microstructural control is revealed as a more influential factor than {sigma}{sup i} for improving crack resistance.

36 MATERIALS SCIENCE↗

Preparation and characterization of RF sputtered Ce-V mixed oxide thin films

Cerium-Vanadium mixed oxide thin films were deposited at room temperature by varying RF power in RF magnetron sputtering. The morphology and structural features were studied by taking FESEM and XRD and optical properties were analyzed by taking transmittance and absorption spectra. The crystalline film shows orthorhombic CeVO{sub 3} phase and the observed grain size varies from 89.4nm to 208.7nm. The transmission increases and the absorption edge at 330nm is blue shifted with increase in RF power. The optical band gap is found to increase from 1.59 to 1.94eV. The PL spectra shows blue shift in the emission peak centered at a wavelength of 495nm with increase in RF power.

36 MATERIALS SCIENCE↗

Optical and electronic properties of Ti{sub 1-x}Nb{sub x}N thin films

Ti{sub 1-x}Nb{sub x}N thin films with x=0, 0.26, 0.41, 0.58 and 1 were deposited on silicon (311) substrate by RF magnetron sputtering. The dielectric functions of these films were calculated by fitting measured reflectance spectra to the Drude-Lorentz model. The measured reflectance spectra exhibits a minimum in the visible region and this feature shifts to higher energy (shorter wavelength) with increase in x. The observed behavior can be modeled as the response of four Lorentz oscillators. The real part of the dielectric function is characterized by a screened plasma energy of 2.26 eV for x=0 which increased to 2.80 eV for x=0.58 in the Ti{sub 1-x}Nb{sub x}N film.

36 MATERIALS SCIENCE↗

Optimization of Ti addition in Fe for Fe-Ti-N thin films

In this work we studied the magnetic and structural properties of Fe{sub 1-x}Ti{sub x}(x=0, 0.02, 0.05, 0.07) thin films prepared with dc-magnetron sputtering. It was found that the inter-atomic spacing increases as the amount of Ti is increased indicating that Ti is getting dissolved substitutionally in Fe lattice. We found that the addition of 5% Ti is best suited for its usage in Fe-Ti-N alloys.

36 MATERIALS SCIENCE↗

Morphology of size-selected copper nanocluster film

We report a preliminary study of the morphology of size-selected Copper nanocluster film grown on Si substrate using a state of the art nanocluster deposition system. The clusters are produced in a dc magnetron and gasaggregation type cluster source at room temperature. The size or mass of the nanoclusters are analysed by a quadrupole mass filter. The morphology of cluster assembled surface has been investigated by Scanning electron microscopy (SEM) and atomic force microscopy (AFM).

36 MATERIALS SCIENCE↗

Realization of low resistive p-ZnO thin film by Al-As codoping

Al-As codoping into ZnO has been proposed to realize low resistive and stable p-ZnO thin film by RF magnetron sputtering. Al-As codoping has been achieved by As back diffusion from GaAs substrate and sputtering Al doped ZnO target. Hall measurements showed that the hole concentration increases with the increase of Al concentration from 10{sup 15} to 10{sup 20} cm{sup -3}. Among the grown films, 1 at% Al doped ZnO: As showed low resistivity (3.5x10{sup -2}{Omega}cm) with high hole concentration. X-ray diffraction shows that all the films are crystallized in wurtzite structure with (002) preferential orientation. The diffusion of As atoms from the substrate and the presence of dopants in the film have been confirmed by Rutherford ford back scattering and energy dispersive spectroscopy analysis, respectively.

36 MATERIALS SCIENCE↗

Structural, electrical and optical properties of GaP codoped ZnO thin films

The GaP codoped ZnO (GPZO) thin films of different concentrations (0, 1, 2 and 4 mol%) have been grown by RF magnetron sputtering to realize p-ZnO. The grown films on sapphire substrates have been characterized by X-ray diffraction (XRD), Hall measurement, photoluminescence (PL), and Energy dispersive spectroscopy (EDS). XRD studies reveal that all the films are preferentially oriented along (002) plane. Hall measurement shows that 2% GPZO film shows low resistivity (2.17 {Omega} cm) and high hole concentration (1.8 x 10{sup 18} cm{sup -3} due to optimum amount of P incorporation. EDS spectra confirms the presence of Ga and P in 2 mol% GPZO film.

36 MATERIALS SCIENCE↗

Intrinsic stress in ZrN thin films: Evaluation of grain boundary contribution from in situ wafer curvature and ex situ x-ray diffraction techniques

Low-mobility materials, like transition metal nitrides, usually undergo large residual stress when sputter-deposited as thin films. While the origin of stress development has been an active area of research for high-mobility materials, atomistic processes are less understood for low-mobility systems. In the present work, the contribution of grain boundary to intrinsic stress in reactively magnetron-sputtered ZrN films is evaluated by combining in situ wafer curvature measurements, providing information on the overall biaxial stress, and ex situ x-ray diffraction, giving information on elastic strain (and related stress) inside crystallites. The thermal stress contribution was also determined from the in situ stress evolution during cooling down, after deposition was stopped. The stress data are correlated with variations in film microstructure and growth energetics, in the 0.13-0.42 Pa working pressure range investigated, and discussed based on existing stress models. At low pressure (high energetic bombardment conditions), a large compressive stress is observed due to atomic peening, which induces defects inside crystallites but also promotes incorporation of excess atoms in the grain boundary. Above 0.3-0.4 Pa, the adatom surface mobility is reduced, leading to the build-up of tensile stress resulting from attractive forces between under-dense neighbouring column boundary and possible void formation, while crystallites can still remain under compressive stress.

36 MATERIALS SCIENCE↗

Optical phonon lifetimes in sputtered AlN thin films

We study the vibrational properties of AlN thin films deposited on silicon (100) substrates by the reactive DC-pulsed magnetron sputtering. The frequencies and lifetimes of the E{sub 1}(TO) and A{sub 1}(LO) optical phonons are calculated from Fourier transform infrared spectra using the factorized model of a damped oscillator. We analyze the structural properties by the x-ray diffraction technique to correlate the elongation of phonon lifetimes with increasing film thickness. The lifetimes of the phonon modes in AlN thin films are compared to the values in a single crystal.

36 MATERIALS SCIENCE↗

A comparative study of ultraviolet photoconductivity relaxation in zinc oxide (ZnO) thin films deposited by different techniques

Photoresponse characteristics of ZnO thin films deposited by three different techniques namely rf diode sputtering, rf magnetron sputtering, and electrophoretic deposition has been investigated in the metal-semiconductor-metal (MSM) configuration. A significant variation in the crystallinity, surface morphology, and photoresponse characteristics of ZnO thin film with change in growth kinetics suggest that the presence of defect centers and their density govern the photodetector relaxation properties. A relatively low density of traps compared to the true quantum yield is found very crucial for the realization of practical ZnO thin film based ultraviolet (UV) photodetector.

36 MATERIALS SCIENCE↗

Atomic scale observation of phase separation and formation of silicon clusters in Hf higk-{kappa} silicates

Hafnium silicate films were fabricated by RF reactive magnetron sputtering technique. Fine microstructural analyses of the films were performed by means of high-resolution transmission electron microscopy and atom probe tomography. A thermal treatment of as-grown homogeneous films leads to a phase separation process. The formation of SiO{sub 2} and HfO{sub 2} phases as well as pure Si one was revealed. This latter was found to be amorphous Si nanoclusters, distributed uniformly in the film volume. Their mean diameter and density were estimated to be about 2.8 nm and (2.9 {+-} 0.4) x 10{sup 17} Si-ncs/cm{sup 3}, respectively. The mechanism of the decomposition process was proposed. The obtained results pave the way for future microelectronic and photonic applications of Hf-based high-{kappa} dielectrics with embedded Si nanoclusters.

36 MATERIALS SCIENCE↗