Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “nitridation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,675 records · Page 93

Demonstration of a silicon nitride attrition mill for production of fine pure Si and Si3N4 powders

To avoid metallic impurities normally introduced by milling ceramic powders in conventional steel hardware, an attrition mill (high-energy stirred ball mill) was constructed with the wearing parts (mill body, stirring arms, and media) made from silicon nitride. Commercial silicon and Si3N4 powders were milled to fine uniform particles with only minimal contamination - primarily from wear of the sintered Si3N4 media.

Herbell, T. P.↗

Thermogravimetric analysis of silicon carbide-silicon nitride polycarbosilazane precursor during pyrolysis from ambient to 1000 C

Thermogravimetric analysis data are presented on the unmeltable polycarbosilazane precursor of silicon carbide-silicon nitride fibers, over the room temperature-1000 C range in a nitrogen atmosphere, in order to establish the weight loss at various temperatures during the precursor's pyrolysis to the fiber material. The fibers obtained by this method are excellent candidates for use in applications where the oxidation of carbon fibers (above 400 C) renders them unsuitable.

Ledbetter, F. E., III↗

Effect of hot isostatic pressing on reaction-bonded silicon nitride

Specimens of nearly theoretical density have been obtained through the isostatic hot pressing of reaction-bonded silicon nitride under 138 MPa of pressure for two hours at 1850, 1950, and 2050 C. An amorphous phase that is introduced by the hot isostatic pressing partly accounts for the fact that while room temperature flexural strength more than doubles, the 1200 C flexural strength increases significantly only after pressing at 2050 C.

Watson, G. K.↗

Fracture of yttria-doped, sintered reaction-bonded silicon nitride

Flexural strength of an yttria-doped, slip-cast, sintered reaction-bonded silicon nitride was evaluated as a function of temperature (20 to 1400 C in air), applied stress, and time. Static oxidation at 700 to 1400 C was investigated in detail; in tests at 1000 C in air, the material showed anomalous weight gain. Flexural stress-rupture testing at 800 to 1200 C in air indicated that the material is susceptible to stress-enhanced oxidation and early failure. Fractographic evidence for time-dependent and -independent failures is presented.

Govila, R. K.↗

Producing Silicon Carbide/Silicon Nitride Fibers

Manufacturing process makes CxSiyNz fibers. Precursor fibers spun from extruding machine charged with polycarbosilazane resin. When pyrolyzed, resin converted to cross-linked mixture of silicon carbide and silicon nitride, still in fiber form. CxSiyNz fibers promising substitutes for carbon fibers in high-strength, low-weight composites where high electrical conductivity unwanted.

Source record↗

Development of a continuous spinning process for producing silicon carbide - silicon nitride precursor fibers

An apparatus was designed for the continuous production of silicon carbide - silicon nitride precursor fibers. The precursor polymer can be fiberized, crosslined and pyrolyzed. The product is a metallic black fiber with the composition of the type C sub x Si sub y n sub z. Little, other than the tensile strength and modulus of elasticity, is known of the physical properties.

Source record↗

Effect of loading rate on dynamic fracture of reaction bonded silicon nitride

Wedge-loaded, modified tapered double cantilever beam (WL-MTDCB) specimens under impact loading were used to determine the room temperature dynamic fracture response of reaction bonded silicon nitride (RBSN). The crack extension history, with the exception of the terminal phase, was similar to that obtained under static loading. Like its static counterpart, a distinct crack acceleration phase, which was not observed in dynamic fracture of steel and brittle polymers, was noted. Unlike its static counterpart, the crack continued to propagate at nearly its terminal velocity under a low dynamic stress intensity factor during the terminal phase of crack propagation. These and previously obtained results for glass and RBSN show that dynamic crack arrest under a positive dynamic stress intensity factor is unlikely in static and impact loaded structural ceramics.

Liaw, B. M.↗

Making a Silicon-Nitride/Silicon-Carbide Composite

Hot pressing and nitriding produce strong fiber/matrix material. Fabrication method developed for processing strong and tough silicon-based ceramic composite material, SiC/RBSN, which consists of reaction-bonded Si3N4 (RBSN) reinforced by continuous-length, high-modulus, high strength silicon carbide (SiC) fibers prepared by chemical-vapor deposition method. Increased toughness and ultimate strength of SiC/RBSN composite makes it potential structural material for advanced heat engines.

Bhatt, R. T.↗

Adhesion, friction, and deformation of ion-beam-deposited boron nitride films

The tribological properties and mechanical strength of boron nitride films were investigated. The BN films were predominantly amorphous and nonstoichiometric and contained small amounts of oxides and carbides. It was found that the yield pressure at full plasticity, the critical load to fracture, and the shear strength of interfacial adhesive bonds (considered as adhesion) depended on the type of metallic substrate on which the BN was deposited. The harder the substrate, the greater the critical load and the adhesion. The yield pressures of the BN film were 12 GPa for the 440C stainless steel substrate, 4.1 GPa for the 304 stainless steel substrate, and 3.3 GPa for the titanium substrate.

Miyoshi, Kazuhisa↗

Mechanical strength and tribological behavior of ion-beam deposited boron nitride films on non-metallic substrates

An investigation was conducted to examine the mechanical strength and tribological properties of boron nitride (BN) films ion-beam deposited on silicon (Si), fused silica (SiO2), gallium arsenide (GaAs), and indium phosphide (InP) substrates in sliding contact with a diamond pin under a load. The results of the investigation indicate that BN films on nonmetallic substrates, like metal films on metallic substrates, deform elastically and plastically in the interfacial region when in contact with a diamond pin. However, unlike metal films and substrates, BN films on nonmetallic substrates can fracture when they are critically loaded. Not only does the yield pressure (hardness) of Si and SiO2 substrates increase by a factor of 2 in the presence of a BN film, but the critical load needed to fracture increases as well. The presence of films on the brittle substrates can arrest crack formation. The BN film reduces adhesion and friction in the sliding contact. BN adheres to Si and SiO2 and forms a good quality film, while it adheres poorly to GaAs and InP. The interfacial adhesive strengths were 1 GPa for a BN film on Si and appreciably higher than 1 GPa for a BN film on SiO2.

Miyoshi, Kazuhisa↗

Preparation of silicon carbide-silicon nitride fibers by the pyrolysis of polycarbosilazane precursors - A review

The development of silicon carbide-silicon nitride fibers (SiC-Si3N4) by the pyrolysis of polycarbosilazane precursors is reviewed. Precursor resin, which was prepared by heating tris(N-methylamino)methylsilane or tris(N-methylamino)phenylsilane to about 520 C, was drawn into fibers from the melt and then made unmeltable by humidity conditioning at 100 C and 95 percent relative humidity. The humidity treated precursor fibers were pyrolyzed to ceramic fibers with good mechanical properties and electrical resistivity. For example, SiC-Si3N4 fibers derived from tris(N-methylamino)methylsilane had a tensile rupture modulus of 29 million psi and electrical resistivity of 6.9 x ten to the 8th power omega-cm, which is ten to the twelfth power times greater than that obtained for graphite fibers.

Penn, B. G.↗

Fracture of flash oxidized, yttria-doped sintered reaction-bonded silicon nitride

The oxidation behavior of a slip cast, yttria-doped, sintered reaction-bonded silicon nitride after 'flash oxidation' was investigated. It was found that both the static oxidation resistance and flexural stress rupture life (creep deformation) were improved at 1000 C in air compared to those of the same material without flash oxidation. Stress rupture data at high temperatures (1000 to 1200 C) are presented to indicate applied stress levels for oxidation-dependent and independent failures.

Govila, R. K.↗

Slow crack growth in sintered silicon nitride

The strength and crack growth characteristics of a sintered silicon nitride were studied at 1000 C. Fractographic analysis of material failing in dynamic fatigue revealed the presence of slow crack growth (SCG) at stressing rates below 6 ksi/min. This material can sustain a 40-ksi flexural stress at 1000 C for 400 h or more but is susceptible to both SCG and creep deformation at higher stress levels. The crack velocity exponent (N) determined both from dynamic and static fatigue experiments lies in a range from 13 to 22. The subcritical crack growth and creep behavior at 1000 C is primarily controlled by the deformation of an intergranular glassy phase.

Khandelwal, P. K.↗

Adhesion, friction and deformation of ion-beam-deposited boron nitride films

The tribological properties and mechanical strength of boron nitride films were investigated. The BN films were predominantly amorphous and nonstoichiometric and contained small amounts of oxides and carbides. It was found that the yield pressure at full plasticity, the critical load to fracture, and the shear strength of interfacial adhesive bonds (considered as adhesion) depended on the type of metallic substrate on which the BN was deposited. The harder the substrate, the greater the critical load and the adhesion. The yield pressures of the BN film were 12 GPa for the 440C stainless steel substrate, 4.1 GPa for the 304 stainless steel substrate, and 3.3 GPa for the titanium substrate.

Miyoshi, K.↗

Improved "Green" Forming Of Silicon Nitride

Advanced processing techniques reduce incidence of critical flaws. Critical flaws reduced by processing of powders to avoid organic and metallic contamination and combination of colloidal techniques with innovative slurry-pressing technique avoiding agglomeration. Silicon nitride considered for many applications ranging from components of turbine engines to industrial heat exchangers.

Freedman, Marc R.↗

Improved silicon nitride for advanced heat engines

The AiResearch Casting Company baseline silicon nitride (92 percent GTE SN-502 Si sub 3 N sub 4 plus 6 percent Y sub 2 O sub 3 plus 2 percent Al sub 2 O sub 3) was characterized with methods that included chemical analysis, oxygen content determination, electrophoresis, particle size distribution analysis, surface area determination, and analysis of the degree of agglomeration and maximum particle size of elutriated powder. Test bars were injection molded and processed through sintering at 0.68 MPa (100 psi) of nitrogen. The as-sintered test bars were evaluated by X-ray phase analysis, room and elevated temperature modulus of rupture strength, Weibull modulus, stress rupture, strength after oxidation, fracture origins, microstructure, and density from quantities of samples sufficiently large to generate statistically valid results. A series of small test matrices were conducted to study the effects and interactions of processing parameters which included raw materials, binder systems, binder removal cycles, injection molding temperatures, particle size distribution, sintering additives, and sintering cycle parameters.

Yeh, H. C.↗

Improved silicon nitride for advanced heat engines

Silicon nitride is a high temperature material currently under consideration for heat engine and other applications. The objective is to improve the net shape fabrication technology of Si3N4 by injection molding. This is to be accomplished by optimizing the process through a series of statistically designed matrix experiments. To provide input to the matrix experiments, a wide range of alternate materials and processing parameters was investigated throughout the whole program. The improvement in the processing is to be demonstrated by a 20 percent increase in strength and a 100 percent increase in the Weibull modulus over that of the baseline material. A full characterization of the baseline process was completed. Material properties were found to be highly dependent on each step of the process. Several important parameters identified thus far are the starting raw materials, sinter/hot isostatic pressing cycle, powder bed, mixing methods, and sintering aid levels.

Yeh, H. C.↗

Dynamic and static fatigue behavior of sintered silicon nitrides

The dynamic and static fatigue behavior of Kyocera SN220M sintered silicon nitride at 1000 C was studied. Fractographic analysis of the material failing in dynamic fatigue revealed the presence of slow crack growth (SCG) at stressing rates below 41 MPa/min. Under conditions of static fatigue this material also displayed SCG at stresses below 345 MPa. SCG appears to be controlled by microcracking of the grain boundaries. The crack velocity exponent (n) determined from both dynamic and static fatigue tests ranged from 11 to 16.

Chang, J.↗