Effect of Cu2+ Activation on Interfacial Water Structure at the Sphalerite Surface as Studied by Molecular Dynamics Simulation

In the first part of this paper, an experimental contact angle study of the fresh and Cu2+ activated sphalerite-ZnS surface as well as the covellite-CuS (001) surface is reported describing the increased hydrophobic character of the surface during Cu2+ activation. In addition to these experimental results, the fresh sphalerite-ZnS (110), copper-zinc sulfide-CuZnS2 (110), villamaninite- CuS2 (100), and covellite-CuS (001) surfaces were examined using Molecular Dynamics Simulation (MDS). Our MDS results on the behavior of interfacial water at the fresh sphalerite-ZnS (110), copper-zinc sulfide-CuZnS2 (110), villamaninite-CuS2 (100), and covellite-CuS (001) surfaces include simulated contact angles, water number density distribution, water dipole orientation, water residence time, and hydrogen-bonding considerations. The copper content at the Cu2+ activated sphalerite surface seems to account for the increased hydrophobicity as revealed by both experimental and MD simulated contact angle measurements. The relatively greater hydrophobic character developed at the Cu2+ activated sphalerite surface and at the copper-zinc sulfide surface has been described by MDS, based on the structure of interfacial water and its dynamic properties. L.X.D. acknowledges funding from the U.S. Department of Energy, Office of Science, Office of Basic Energy Sciences, Division of Chemical Sciences, Geosciences, and Biosciences.

Jin, Jiaqi↗

Effect of aging temperature on phase decomposition and mechanical properties in cast duplex stainless steels

The microstructure and mechanical properties in unaged and thermally aged (at 280 oC, 320 oC, 360 oC, and 400 oC to 4300 h) CF–3 and CF–8 cast duplex stainless steels (CDSS) are investigated. The unaged CF–8 steel has Cr-rich M23C6 carbides located at the δ–ferrite/γ– austenite heterophase interfaces that were not observed in the CF–3 steel and this corresponds to a difference in mechanical properties. Both unaged steels exhibit incipient spinodal decomposition into Fe-rich α–domains and Cr-rich α’–domains. During aging, spinodal decomposition progresses and the mean wavelength (MW) and mean amplitude (MA) of the compositional fluctuations increase as a function of aging temperature. Additionally, G–phase precipitates form between the spinodal decomposition domains in CF–3 at 360 oC and 400 oC and in CF–8 at 400 oC. The microstructural evolution is correlated to changes in mechanical properties.

atom probe tomography↗

Effect of temperature on the fatigue cracking mechanisms in A356 Al alloy

This work builds on our previous investigation of the room temperature fatigue cracking mechanisms of an A356 Al alloy. Here, we analyze the elevated temperature fatigue cracking mechanisms in cast and friction stir processed (FSP) A356, and contrast them with the room temperature behavior. Two sets of FSP parameters were used to modify the microstructure of the cast alloy. After heat treatment, both the FSPed microstructures exhibited severe abnormal grain growth (AGG) leading to a very wide grain size distribution (from a few microns to a few millimeters). During room temperature fatigue tests, the FSP conditions exhibited significant improvements in fatigue lives, even up to an order of magnitude. However, with increasing temperature, the difference in the performance of the FSPed and Cast microstructures decreased until, at 200 °C, all three microstructural conditions exhibited similar fatigue response. Detailed electron back scattered diffraction (EBSD) imaging of failed fatigue specimens was used to study crack behavior. At room temperature, cracks initiated at defect sites or along persistent slip bands (PSBs) and propagated transgranularly. The grain boundaries acted as barriers to crack growth. At elevated temperatures, there was a complete role reversal of the grain boundaries. Cracks initiated along grain boundaries and propagated intergranularly in all microstructures. Below, we explore this transition of the cracking mechanism in detail.

Nelaturu, Plalgun↗