Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “VAPOR PHASE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,675 records · Page 93

Epitaxial growth and thermal stability of Fe{sub 4}N film on TiN buffered Si(001) substrate

Epitaxial Fe{sub 4}N thin films were grown on TiN buffered Si(001) substrate by dc reactive sputtering deposition at different substrate temperatures. Fe{sub 4}N films epitaxially grew on TiN within the substrate temperature range from 250 to 350 deg. C. Lower than 250 deg. C there will be some other Fe{sub x}N compounds formed and higher than 400 deg. C there will be only Fe left. Fe{sub 4}N is metastable and the postannealing process in vacuum will decompose Fe{sub 4}N film to Fe. However, introducing 30% N{sub 2} in the postannealing atmosphere can stabilize the Fe{sub 4}N up to 350 deg. C in the (Ar,N{sub 2}) gas mixture. The surface roughness of the epitaxial Fe{sub 4}N films decreases with film thickness. There is in-plane biaxial magnetic anisotropy of epitaxial Fe{sub 4}N(001) on Si(001) with the [100] easy direction.

36 MATERIALS SCIENCE↗

Two-domain formation during the epitaxial growth of GaN (0001) on c-plane Al{sub 2}O{sub 3} (0001) by high power impulse magnetron sputtering

We study the effect of high power pulses in reactive magnetron sputter epitaxy on the structural properties of GaN (0001) thin films grown directly on Al{sub 2}O{sub 3} (0001) substrates. The epilayers are grown by sputtering from a liquid Ga target, using a high power impulse magnetron sputtering power supply in a mixed N{sub 2}/Ar discharge. X-ray diffraction, micro-Raman, micro-photoluminescence, and transmission electron microscopy investigations show the formation of two distinct types of domains. One almost fully relaxed domain exhibits superior structural and optical properties as evidenced by rocking curves with a full width at half maximum of 885 arc sec and a low temperature band edge luminescence at 3.47 eV with the full width at half maximum of 10 meV. The other domain exhibits a 14 times higher isotropic strain component, which is due to the higher densities of the point and extended defects, resulting from the ion bombardment during growth. Voids form at the domain boundaries. Mechanisms for the formation of differently strained domains, along with voids during the epitaxial growth of GaN are discussed.

36 MATERIALS SCIENCE↗

Aligned and exchange-coupled L1{sub 0} (Fe,Co)Pt-based magnetic films

Films of aligned L1{sub 0}-structure (Fe,Co)Pt with fcc Fe(Co,Pt) are synthesized by co-sputtering Fe, Co, and Pt on an (001) MgO substrate with in situ heating at 830 deg. C. The nanostructures and magnetic properties of the films are characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), and superconducting quantum interference device (SQUID). The compositions of the samples (Fe,Co){sub x}Pt{sub 1-x} are designed to maintain an atomic Fe: Co ratio of 65: 35 while increasing the Fe,Co content in each successive sample. In samples with low Fe and Co concentration, the XRD patterns exhibit three strong peaks, namely L1{sub 0} (Fe,Co)Pt (001), L1{sub 0} (Fe,Co)Pt (002), and MgO (002). A fourth peak is observed in samples with high Fe and Co concentration and identified as fcc (002). The XRD patterns confirm the formation of L1{sub 0}-ordered (Fe,Co)Pt and its epitaxial growth on MgO. TEM shows that the (Fe,Co)Pt films form isolated magnetic grains of about 100 nm in diameter. Hysteresis-loop measurements show that the increase of the Fe,Co concentration from 57.3 to 68.3 at % enhances the saturation magnetization M{sub s} from 1245 emu/cm{sup 3} to 1416 emu/cm{sup 3}, and the coercivity decreases from 32 kOe to 8.9 kOe. The nominal maximum energy product per grain is 64 MGOe.

36 MATERIALS SCIENCE↗

Epitaxial Ag(001) grown on MgO(001) and TiN(001): Twinning, surface morphology, and electron surface scattering

Epitaxial Ag(001) layers were deposited on MgO(001) in order to study electron surface scattering. X-ray reflection indicates 3D layer nucleation with a high rms surface roughness of 1.0 nm for a layer thickness d = 3.5 nm. X-ray diffraction shows that {l_brace}111{r_brace} twins form at d < 11 nm, followed by 2nd generation twinning for 11 nm < d < 120 nm. Increasing the growth temperature from 25 to 150 deg. C suppresses 2nd generation twinning and reduces the twin density by 2 orders of magnitude. In situ deposition of epitaxial 2.5-nm-thick TiN(001) underlayers prior to Ag deposition results in twin-free single-crystal Ag(001) with 10 x smoother surfaces for d = 3.5 nm. This is attributed to a better wetting on the higher energy TiN(001) than MgO(001) surface, resulting in the absence of 3D nuclei with exposed {l_brace}111{r_brace} facets, which facilitate twin nucleation. The twinned Ag/MgO layers have a higher resistivity {rho} than the single crystal Ag/TiN layers at both 298 and 77 K, due to electron scattering at grain and twin boundaries. The {rho} for single-crystal Ag layers increases with decreasing d, which is well explained with known surface scattering models and provides specularity parameters for the Ag-vacuum and the Ag-air interfaces of p = 0.8 {+-} 0.1 and 0.4 {+-} 0.1, respectively. A comparison with corresponding epitaxial Cu(001) layers shows that {rho}{sub Ag} < {rho}{sub Cu} for d > 50 nm, consistent with known bulk values. However, {rho}{sub Ag} > {rho}{sub Cu} for d < 40 nm. This is attributed to the larger electron mean free path for electron-phonon scattering and a correspondingly higher resistivity contribution from surface scattering in Ag than Cu. In contrast, air exposure causes {rho}{sub Ag} < {rho}{sub Cu} for all d, due to diffuse scattering at the oxidized Cu surface and the correspondingly higher Cu resistivity.

36 MATERIALS SCIENCE↗

Epitaxial two dimensional aluminum films on silicon (111) by ultra-fast thermal deposition

Aluminum thin films are known for their extremely rough surface, which is detrimental for applications such as molecular electronics and photonics, where protrusions cause electrical shorts or strong scattering. We achieved atomically flat Al films using a highly non-equilibrium approach. Ultra-fast thermal deposition (UFTD), at rates >10 nm/s, yields RMS roughness of 0.4 to 0.8 nm for 30-50 nm thick Al films on variety of substrates. For UFTD on Si(111) substrates, the top surface follows closely the substrate topography (etch pits), indicating a 2D, layer-by-layer growth. The Al film is a mixture of (100) and (111) grains, where the latter are commensurate with the in-plane orientation of the underlying Si (epitaxy). We show the use of these ultra-smooth Al films for highly reproducible charge-transport measurements across a monolayer of alkyl phosphonic acid as well as for plasmonics applications by directly patterning them by focused ion beam to form a long-range ordered array of holes. UFTD is a one-step process, with no need for annealing, peeling, or primer layers. It is conceptually opposite to high quality deposition methods, such as MBE or ALD, which are slow and near-equilibrium processes. For Al, though, we find that limited diffusion length (and good wetting) is critical for achieving ultra-smooth thin films.

36 MATERIALS SCIENCE↗

MOVPE and MBE growth of semiconductor thin films

Fundamental aspects of MBE and MOVPE growth techniques are briefly discussed. The capabilities and limitation of the two epitaxial growth techniques are summarized. A few examples of the MOVPE and MBE growth of high crystalline quality semiconductor thin films are also given including the characterization results obtained from spectroscopic and high resolution x-ray diffraction methods.

36 MATERIALS SCIENCE↗

Epitaxial growth of Ti{sub 3}SiC{sub 2} thin films with basal planes parallel or orthogonal to the surface on {alpha}-SiC

The growth of Ti{sub 3}SiC{sub 2} thin films were studied onto {alpha}-SiC substrates differently oriented by thermal annealing of TiAl layers deposited by magnetron sputtering. For any substrate's orientation, transmission electron microscopy coupled with x-ray diffraction showed the coherent epitaxial growth of Ti{sub 3}SiC{sub 2} films along basal planes of SiC. Specifically for the (1120) 4H-SiC, Ti{sub 3}SiC{sub 2} basal planes are found to be orthogonal to the surface. The continuous or textured nature of Ti{sub 3}SiC{sub 2} films does not depend of the SiC stacking sequence and is explained by a step-flow mechanism of growth mode. The ohmic character of the contact was confirmed by current-voltage measurements.

36 MATERIALS SCIENCE↗

Low-temperature formation of epitaxial graphene on 6H-SiC induced by continuous electron beam irradiation

It is observed that epitaxial graphene forms on the surface of a 6H-SiC substrate by irradiating electron beam directly on the sample surface in high vacuum at relatively low temperature ({approx}670 Degree-Sign C). The symmetric shape and full width at half maximum of 2D peak in the Raman spectra indicate that the formed epitaxial graphene is turbostratic. The gradual change of the Raman spectra with electron beam irradiation time increasing suggests that randomly distributed small grains of epitaxial graphene form first and grow laterally to cover the entire irradiated area. The sheet resistance of epitaxial graphene film is measured to be {approx}6.7 k{Omega}/sq.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structure determination of thin CoFe films by anomalous x-ray diffraction

This work reports on the investigation of structure-property relationships in thin CoFe films grown on MgO. Because of the very similar scattering factors of Fe and Co, it is not possible to distinguish the random A2 (W-type) structure from the ordered B2 (CsCl-type) structure with commonly used x-ray sources. Synchrotron radiation based anomalous x-ray diffraction overcomes this problem. It is shown that as grown thin films and 300 K post annealed films exhibit the A2 structure with a random distribution of Co and Fe. In contrast, films annealed at 400 K adopt the ordered B2 structure.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Strain controlled systematic variation of metal-insulator transition in epitaxial NdNiO{sub 3} thin films

We report here the strain dependent structural and electrical transport properties of epitaxial NdNiO{sub 3} thin films. Pulsed laser deposition technique was used to grow the NdNiO{sub 3} thin films on c-axis oriented SrTiO{sub 3} single crystals. Deposited films were irradiated using 200 MeV Ag{sup 15+} ion beam at the varying fluence (1 Multiplication-Sign 10{sup 11}, 5 Multiplication-Sign 10{sup 11}, and 1 Multiplication-Sign 10{sup 12} ions/cm{sup 2}). X-ray diffraction studies confirm the epitaxial growth of the deposited films, which is maintained even up to the highest fluence. Rise in the in-plane compressive strain has been observed after the irradiation. All the films exhibit metal-insulator transition, however, a systematic decrease in the transition temperature (T{sub MI}) has been observed after irradiation, which may be attributed to the increase in the in-plane compression. Raman spectroscopy data reveal that this reduction in T{sub MI}, with the irradiation, is related to the decrease in band gap due to the stress generated by the in-plane compressive strain.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Optical doping of Al{sub x}Ga{sub 1-x}N compounds by ion implantation of Tm ions

Al{sub x}Ga{sub 1-x}N (0 axis for samples with AlN contents of 0.15 and 0.77 suggest a relation between the AlN content and Tm specific sites in the lattice. Rapid thermal annealing treatments under N{sub 2} ambient were performed to remove damage and promote optical activation of rare earth intra-4f{sup n} transitions. After annealing the observed intraionic emissions of Tm{sup 3+} ions were characterized by photoluminescence.

36 MATERIALS SCIENCE↗

X-ray photoelectron diffraction study of dopant effects in La{sub 0.7}X{sub 0.3}MnO{sub 3} (X = La, Sr, Ca, Ce) thin films

We present and discuss element-specific x-ray photoelectron diffraction (XPD) patterns of La, Mn, O and the dopant ions Ca, Sr and Ce of various La{sub 0.7}X{sub 0.3}MnO (LXMO) films grown epitaxially on SrTiO{sub 3}(001) substrates. The recorded XPD polar scans are explained in the framework of multiple-scattering cluster calculations, where in general a very good agreement between experimental and theoretical data has been found. Results for all thin films are compatible with a tetragonally distorted cubic perovskite structure with similar MnO{sub 6} network. Strong evidence for Mn-site termination was found in all thin films. Dopant locations on A-type sites were clearly confirmed for Sr in LSMO and Ca in LCMO films by means of XPD polar scans. The absence of surface-sensitive Ce3d diffraction features for Ce in LCeMO points to non-equivalent Ce sites and related near-surface disorder.

36 MATERIALS SCIENCE↗

Formation of epitaxial Co{sub 1-x}Ni{sub x}Si{sub 2} nanowires on thin-oxide-capped (001)Si

Epitaxial Co{sub 1-x}Ni{sub x}Si{sub 2} alloy nanowires have been grown on (001)Si substrates by a combination of reactive deposition epitaxy and oxide-mediated epitaxy. The thin native oxide layer can serve as a diffusion barrier to diminish the flux of metal atoms from the top of oxide layer to Si surface and promote the growth of nanowires. The elemental distributions of Ni and Co in nanowires were determined by energy dispersive spectroscopy in a transmission electron microscope. The factors that cause the distributions of Ni and Co in nanowires were discussed.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Hydrogen plasma treatments for passivation of amorphous-crystalline silicon-heterojunctions on surfaces promoting epitaxy

The impact of post-deposition hydrogen plasma treatment (HPT) on passivation in amorphous/crystalline silicon (a-Si:H/c-Si) interfaces is investigated. Combining low temperature a-Si:H deposition and successive HPT, a high minority carrier lifetime >8 ms is achieved on c-Si <100>, which is otherwise prone to epitaxial growth and thus inferior passivation. It is shown that the passivation improvement stems from diffusion of hydrogen atoms to the heterointerface and subsequent dangling bond passivation. Concomitantly, the a-Si:H hydrogen density increases, leading to band gap widening and void formation, while the film disorder is not increased. Thus, HPT allows for a-Si:H band gap and a-Si:H/c-Si band offset engineering.

36 MATERIALS SCIENCE↗

Ion irradiation induced enhancement of out-of-plane magnetic anisotropy in ultrathin Co films

Ga{sup +} or He{sup +} irradiated MBE grown ultrathin films of sapphire/Pt/Co(d{sub Co})/Pt(d{sub Pt}) were studied using polar Kerr effect in wide ranges of both cobalt d{sub Co} and platinum d{sub Pt} thicknesses as well as ion fluences F. Two branches of increased magnetic anisotropy and enhanced Kerr rotation angle induced by Ga{sup +} or He{sup +} irradiation are clearly visible in two-dimensional (d{sub Co}, LogF) diagrams. Only Ga{sup +} irradiation induces two branches of out-of-plane magnetization state.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Competition between (001) and (111) MgO thin film growth on Al-doped ZnO by oxygen plasma assisted pulsed laser deposition

We report on the study of epitaxial MgO thin films on (0001) Al-doped ZnO (Al: ZnO) underlayers, grown by oxygen plasma assisted pulsed laser deposition technique. A systematic investigation of the MgO thin films was performed by X-ray diffraction and atomic force microscopy, along with the current-voltage characteristics. A distinguished behavior was observed that the preferred MgO orientation changes from (111) to (001) in the films as the growth temperature increases. Two completely different in-plane epitaxial relationships were also determined from X-ray diffraction as: [110]MgO//[1120]Al: ZnO and [110]MgO//[1100]Al: ZnO for (001) MgO with 60 Degree-Sign rotated triplet domains, and [110]MgO//[1120]Al: ZnO for (111) MgO with 180 Degree-Sign rotated twin. The pronounced temperature dependence indicates a reconciliation of the nucleation driving forces among surface, interfacial, and strain energy for heteroepitaxy of cubic MgO on hexagonal Al: ZnO. The related interfacial atomic registry is considered to be important to the formation of unusual (001) MgO on hexagonal crystals. In addition, the electrical characterization revealed a dramatic reduction of the leakage current in (001) MgO thin films, whereas the small grain size of (111) MgO is identified by atomic force microscopy as a main cause of large leakage current.

36 MATERIALS SCIENCE↗

Accurate determination of optical bandgap and lattice parameters of Zn{sub 1-x}Mg{sub x}O epitaxial films (0{<=}x{<=}0.3) grown by plasma-assisted molecular beam epitaxy on a-plane sapphire

Zn{sub 1-x}Mg{sub x}O epitaxial films with Mg concentrations 0{<=}x{<=}0.3 were grown by plasma-assisted molecular beam epitaxy on a-plane sapphire substrates. Precise determination of the Mg concentration x was performed by elastic recoil detection analysis. The bandgap energy was extracted from absorption measurements with high accuracy taking electron-hole interaction and exciton-phonon complexes into account. From these results a linear relationship between bandgap energy and Mg concentration is established for x{<=}0.3. Due to alloy disorder, the increase of the photoluminescence emission energy with Mg concentration is less pronounced. An analysis of the lattice parameters reveals that the epitaxial films grow biaxially strained on a-plane sapphire.

36 MATERIALS SCIENCE↗

Epitaxial growth of (111)-oriented BaTiO{sub 3}/SrTiO{sub 3} perovskite superlattices on Pt(111)/Ti/Al{sub 2}O{sub 3}(0001) substrates

Symmetric BaTiO{sub 3}/SrTiO{sub 3} (BTO/STO) superlattices (SLs) were epitaxially grown on Pt(111)/Ti/Al{sub 2}O{sub 3}(0001) substrates with various modulation periods (Λ = 4.8 − 48 nm) using double ion beam sputter deposition. The BTO/STO SLs exhibit high (111) orientation with two in-plane orientation variants related by a 180° rotation along the [111]{sub Pt} axis. The BTO layer is under an in-plane compressive state, whereas the STO layer is under an in-plane tensile state due to the effect of lattice mismatch. A remarkable enhancement of dielectric constant is observed for the SL with relatively small modulation period, which is attributed to both the interlayer biaxial strain effect and the Maxwell-Wagner effect.

36 MATERIALS SCIENCE↗