Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FRACTURE PROPERTIES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,675 records · Page 93

Fracture Analysis of ARB-Processed CP-Ti Sheets Under Unidirectional Tensile Loading

The fracture behavior of commercially pure titanium (CP-Ti) processed by accumulative roll bonding (ARB) was investigated in this study. Monolithic and Ti-SiC composite samples were first produced by ARB process and then subjected to uniaxial tensile testing at room temperature. Two different ductile fracture mechanisms including shear dimple rupture and equiaxed dimple rupture were observed in the initial and final ARB cycles, respectively. The difference in the rupture mechanism was attributed to different stress states at the crack tip and different densities of metallurgical defects. A non-uniform distribution of dimple size was obtained for fracture surfaces of the samples processed by a low number of ARB cycles. This was attributed to the heterogeneity of microstructure in the primary ARB cycles. The fracture surface of the samples processed by high ARB cycles represented more uniform dimples. This was attributed to more homogenous microstructure in the final cycles. Moreover, SiC particles showed a major role in fracture of samples, so that they affected the size and depth of the dimples, as well as the number of ARB cycles in which the transmission of the fracture mechanism occurred.

36 MATERIALS SCIENCE↗

Effects of Laser Fluence on Microstructure and Bonding Characteristics of Wideband Laser-Deposited Nickel Composite Coatings

The wideband laser has shown great potential in metal–ceramic coatings deposition due to the high efficiency and low dilution rate. However, the effects of wideband laser process on microstructure evolution and bonding mechanism at the coatings/substrate interface are still a critical problem and need further investigation. In this work, nickel composite coatings are fabricated on the surface high-strength low-alloy steel. The effects of laser fluence on microstructure evolution, shear strength and fracture mechanism are studied. Results indicated the added WC particles were partly dissolved due to the high-power laser irradiation. Many block precipitates and dense eutectic were synthesized in composite coatings. Reinforced phases mainly consist of Cr{sub 5}B{sub 3}, Cr{sub 23}C{sub 6}, W{sub 2}C and Cr{sub 3}Ni{sub 2}. The dilution of Q550 steel contributed to the formation of nickel dendrites and facilitated a dense metallurgical bonding at coating/substrate interface when laser fluence was high. Shear strength tests indicated the laser fluence and shear strength had a positive correlation. For Ni60/WC composite coatings designed in these experiments, the recommend laser fluence should be higher than 55 J/mm{sup 2}, above which the shear strength could be greater than 200 MPa. Fracture surfaces indicated the failure mechanism of composite coatings was quasi-cleavage fracture.

36 MATERIALS SCIENCE↗

Shape retention and infiltration height in complex WC-Co parts made via binder jet of WC with subsequent Co melt infiltration

Additive manufacturing (AM) of complex tungsten carbide-cobalt (WC-Co) parts was achieved using binder jet additive manufacturing (BJAM) of WC powders followed by Co infiltration. The intent of the study is to explore the shape retention, infiltration height, and properties of parts made with this method. Using BJAM with infiltration of the metal phase can limit shrinkage and grain growth in ceramic-metal (cermet) composites compared to other additive manufacturing (AM) methods. Knowledge of previous infiltration studies was used to help process parts to imitate production of parts. The properties such as density, microstructure, grain size, and hardness of the parts are characterized along the infiltration height. Fracture toughness is measured where applicable. Furthermore, this approach has the potential to achieve highly dense WC-Co parts that are net-shaped with some ternary phase and z-direction distortion.

36 MATERIALS SCIENCE↗

Effect of printing parameters on 3D-printed carbon fiber-reinforced polymer composites under magnetic field control

Magnetic field controlled (MFC) 3D printing is a promising method for realizing the intelligent control of the structural performance of carbon fiber-reinforced plastic (CFRP) composites by adjusting the fiber orientation during the printing process. However, few studies have focused on the influence of the printing parameters on the magnetic control of the fiber direction. Therefore, in this study, the mechanical properties and internal fiber distributions of MFC 3D-printed samples of CFRP composites with 10 wt% fiber content, which were printed at different speeds and layer thicknesses, were investigated. Subsequently, the effects of the fiber content on the mechanical properties and fiber distribution of the MFC 3D-printed samples were studied. Furthermore, the origin of fiber fracture was evaluated through observation and analysis of the fracture section using scanning electron microscopy. The fiber orientation could be well adjusted under the action of a magnetic field and adjustment of printing parameters, thereby improving the tensile strength, young's modulus significantly with slightly decrease of fracture elongation. The recommended parameter combinations (printing speed and layer thickness) were 40 mm/s and 0.2 mm for 10 wt% fiber content CFRP composites.

36 MATERIALS SCIENCE↗

Influence of acid leaching surface treatment on indentation cracking of soda lime silicate glass

Past work has shown that water or acid soaking treatments can increase the mechanical strength of soda lime silicate (SLS) glasses. In this work, we show that acid leaching treatments result in an increase in the apparent crack resistance of the acid-leached surface of SLS glass during indentation. Vickers indentation tests in controlled environments show a humidity dependence of radial cracking, suggesting that the transport of water through the leached layer plays a critical role in the propagation of cracks to the glass surface. Here, molecular dynamics simulations with reactive force fields indicate that the leached surface layer can undergo pressure-induced mechanochemical reactions during indentation, which increases the bridging oxygen connectivity in the silica network of the leached layer. Such structural changes can hinder transport of water molecules from the environment to the subsurface crack tip. Based on experimental observations and simulation results, a new hypothesis is proposed that mechanochemical restructuring in the leached layer in response to the applied load may lower the transport kinetics of molecular water to critical flaws, resulting in an apparent enhancement in the crack resistance of the acid-leached surface of SLS glass.

36 MATERIALS SCIENCE↗

Strengthening of σ phase in a Fe20Cr9Ni cast austenite stainless steel

The strengthening mechanism of σ phase in a Fe20Cr9Ni cast austenite stainless steel used for primary coolant pipes of nuclear power plants has been investigated. The yield and ultimate tensile strengths of aged specimens increased comparing with those of the unaged ones. It was found that the increase of strengths is due to the hard and brittle (σ + γ{sub 2}) structure which decomposed from α phase in the steel. Fracture surfaces of specimens after in situ tensile test showed that the inhibition of (σ + γ{sub 2}) structure on the dislocation movements was more significant than ferrite although cracks started predominately at σ/γ{sub 2} interfaces. The (σ + γ{sub 2}) structure behaves like a fiber reinforced composite material. - Highlights: • The strengthening mechanism of σ phase in a Fe20Cr9Ni CASS is investigated. • The yield and ultimate tensile strengths increase with increasing of σ phase. • The increase of strengths is due to hard and brittle (σ + γ{sub 2}) structure. • The (σ + γ{sub 2}) structure in CASS behaves like a fibre reinforced composite material. • The σ/γ{sub 2} and α/σ/γ{sub 2} boundaries hinder the movement of dislocation.

36 MATERIALS SCIENCE↗

Long Fibre Composite Modelling Using Cohesive User's Element

The development glass matrix composites reinforced by unidirectional long ceramic fibre has resulted in a family of very perspective structural materials. The only disadvantage of such materials is relatively high brittleness at room temperature. The main micromechanisms acting as toughening mechanism are the pull out, crack bridging, matrix cracking. There are other mechanisms as crack deflection etc. but the primer mechanism is mentioned pull out which is governed by interface between fibre and matrix. The contribution shows a way how to predict and/or optimise mechanical behaviour of composite by application of cohesive zone method and write user's cohesive element into the FEM numerical package Abaqus. The presented results from numerical calculations are compared with experimental data. Crack extension is simulated by means of element extinction algorithms. The principal effort is concentrated on the application of the cohesive zone model with the special traction separation (bridging) law and on the cohesive zone modelling. Determination of micro-mechanical parameters is based on the combination of static tests, microscopic observations and numerical calibration procedures.

36 MATERIALS SCIENCE↗

The Impact of Ceramic Shell Strength on Hot Tearing during Investment Casting

The effect of ceramic shell strength on hot tearing susceptibility during solidification was inspected practicing investment casting of the cobalt-base superalloy samples with the same casting conditions, but different ceramic shell systems. Results showed that the lower the ceramic shell strength upon using polymer additives, the lower the hindered contraction rate, and the lower the hindered contraction rate, the smaller the hot tearing tendency. Optical microscopy and electron microscopy scanning revealed that the hot tear propagated along the last solidified interdendritic phase, and that the hot tear surface had two major modes: (1) the ductile region in the outer layer; and (2) the inner region of liquid embrittlement.

36 MATERIALS SCIENCE↗

Effect of Grain Refinement on the Mechanical Behaviour of an Al6061 Alloy at Cryogenic Temperatures

A solution treated coarse grained (CG) Al6061 was subjected to high pressure torsion (HPT) at room temperature resulting in the formation of a homogeneous ultra-fine grained (UFG) microstructure with an average grain size of 170 nm. Tensile tests were performed at room temperature (RT) and liquid nitrogen temperature (LNT). The as-HPT UFG Al6061 alloy shows an increased strength at both RT and LNT. The decrease of testing temperature results in increased flow stress and in enhanced elongation to failure in both CG and UFG samples. The ratio {sigma}{sub y}{sup LNT}/{sigma}{sub y}{sup RT} was found to be larger for the CG Al6061 than for the UFG Al6061. Both surface relief and fracture surface observations were performed. The effect of the grain size and of the testing temperature on the mechanical behaviour of the Al6061 alloy is analyzed in detail. It is suggested that the solute atoms play an important role in the plastic deformation of the UFG Al6061 alloy.

36 MATERIALS SCIENCE↗

In situ X-ray imaging of heterogeneity in dynamic compaction of granular media

Dynamic compaction of granular materials is a complex process wherein the material response at the continuum scale arises from fracture, comminution, and fragment ow at the grain scale. Granular materials have heterogeneity due to variation in grain properties, as well as variation in local packing density and structure. These heterogeneities may affect the dynamic compaction response, producing a structured and time-varying compaction front. Methodology used to characterize the shock behavior in solid materials may be inappropriate for granular materials, because of this unsteady behavior and interactions between the granular material and measurement surfaces. To observe the compaction front heterogeneity, in-situ x-ray imaging of granular compaction is conducted at a scale between the grain- and continuum scales. To allow for sufficient x-ray transmission, a thin sample geometry is used, for which boundary affects may result in a significantly different load path than would occur in a 1-D compaction configuration. Numerical simulations of the experimental geometry support analysis of the results so that the feature of the compaction front can be distinguished from artifacts of the experimental configuration. The results suggest compaction front heterogeneity may have structure with a length scale of tens of particle diameters, and demonstrate that finite grain size can inhibit the formation shear-induced features that would arise in a homogenized representation of the same material.

36 MATERIALS SCIENCE↗

Opening-mode fracturing and cementation during hydrocarbon generation in shale: An example from the Barnett Shale, Delaware Basin, West Texas

Relative timing of fracturing is a key input for predictive fracture models, but timing information for fractures is commonly difficult to obtain. In this study, we used crosscutting relations and fluid inclusion assemblage temperatures from fracture cements from a few well-documented sampled fractures, combined with a one-dimensional burial history model, to establish timing for three generations of opening-mode fractures in a Barnett Shale core from the southern part of the Delaware Basin, Pecos County, West Texas. A burial history model is presented for the cored well and matched to measured vitrinite reflectance in samples from the core, and bottomhole temperature in the well. Here, the earliest fractures (group 1) likely formed due to early fluid-expulsion events (ca. 300 Ma) and were folded during host-rock compaction. Later group 2 fractures are sealed with fibrous barite containing primary, liquid hydrocarbon inclusions (mean homogenization temperature [T h ] = –9°C) and aqueous fluid inclusions (mean T h = 108.1°C). Group 2 fractures likely formed in response to fluid overpressure associated with cracking of type II kerogen to oil. Group 3 vertical fractures are up to 2 m in height with kinematic apertures ranging from less than 0.05 to 1.4 mm, partly open, and strike dominantly 010°–020°. Sequentially trapped aqueous fluid inclusions in fracture-spanning quartz cement bridges (mean T h = 110°C in crack-seal texture and 128°C in post-crack-seal fracture cement) record fracture opening under increasing temperature, inferred to reflect increasing burial, with continued overpressuring during the Triassic to Late Cretaceous. Some group 3 fractures may have continued to fill during Cenozoic uplift.

02 PETROLEUM↗

Status report on HFIR irradiation of optimized alumina forming alloys

Properties of FeCrAl alloys under neutron irradiation are of interest because of these materials’ potential application as accident-tolerant fuel cladding in nuclear systems. In parallel, alumina-forming austenitic (AFA) alloys are of interest for use as structural materials in advanced nuclear systems for their potential higher resistance to embrittlement and high-temperature steam oxidation resistance. An irradiation campaign for fiscal year 2024 has been developed under the Advanced Fuels Campaign to perform irradiation testing of various FeCrAl and AFA alloys in Oak Ridge National Laboratory’s High Flux Isotope Reactor (HFIR). The goals of this irradiation campaign are to (1) study the impact of minor alloying elements on the neutron-irradiated mechanical properties of FeCrAl alloys and (2) collect neutron-irradiated mechanical properties on AFA alloys for comparison with those of FeCrAl alloys. This campaign will include both tensile and fracture toughness specimens tested following HFIR irradiation at temperatures representative of normal operating conditions in light-water reactors. The pre-irradiation characterization to date, the irradiation plan for the FeCrAl and AFA specimens, and the subsequent post-irradiation experimental test plan are presented in this report, along with the status of HFIR builds and scheduled insertion dates.

36 MATERIALS SCIENCE↗

Progress in Developing Finite Element Models Replicating Flexural Graphite Testing

This report documents the status of flexural strength evaluations from current ASTM procedures and of developing finite element models predicting the probability of failure. This work is covered under QLD REC-00030. Flexural testing procedures of the American Society for Testing and Materials (ASTM) assume a linear elastic material that has the same moduli for tension and compression. Contrary to this assumption, graphite is known to have different moduli for tension and compression. A finite element model was developed and demonstrated that accounts for the difference in moduli tension and compression. Brittle materials such as graphite exhibit significant scatter in tensile strength, so probabilistic design approaches must be used when designing components fabricated from brittle materials. ASTM procedures predicting probability of failure in ceramics were compared to methods from the current version of the ASME graphite core components rules predicting probability of failure. Using the ASTM procedures yields failure curves at lower applied forces than the ASME rules. A journal paper was published in the Journal of Nuclear Engineering and Design exploring the statistical models of fracture in graphite.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Flaw growth behavior in thick welded plates of 2219-T87 aluminum at room and cryogenic temperatures

Axial load fatigue and fracture tests were conducted on thick welded plates of 2219-T87 aluminum alloy to determine the tensile strength properties and the flaw growth behavior in electron beam, gas metal arc, and pulse current gas tungsten arc welds for plates 6.35 centimeters (2.5 in.) thick. The tests were conducted in room temperature air and in liquid nitrogen environments. Specimens were tested in both the as-welded and the aged after welding conditions. The experimental crack growth rate were correlated with theoretical crack growth rate predictions for semielliptical surface flaws.

Forman, R. G.↗

Rayleigh wave studies in lunar rocks.

An ultrasonic surface wave technique described by the author (1971) is used to verify a hypothesis that links the seismic wave propagation velocities in lunar crust, much too low as compared to those on earth, to the extensive fracturing of lunar rock in the absence of liquids and gases which changed drastically the elastic and inelastic properties of lunar rock. Measurements on lunar rock samples and synthetic analogs suggest that the presence of microfractures have influence on both the wave velocity and Q factor in lunar rocks.

Tittmann, B. R.↗

Microcrack closure in rocks under stress - Direct observation

Direct observations of the closure of microcracks in rocks under increasing stress are reported. Uniaxial stresses up to 300 bars were applied to untreated and previously heated samples of Westerly granite and Frederick diabase by a small hydraulic press which fit entirely within a scanning electron microscope. Crack closure characteristics are found to depend on crack orientation, with cracks perpendicular to the applied stress closing and those parallel tending to open, as well as crack aspect ratio, crack intersection properties, stress concentrations and surface roughness. Uniaxial and hydrostatic stress measurements are found to be strongly dependent on fracture content as observed by SEM, and the observed hysteresis in strain measurements in the first stress cycles is also related to microscopic processes

Batzle, M. L.↗

Work of fracture in aluminum metal-matrix composites

Mechanical tests were conducted on B/Al composites and, for comparison, FP-Al2O3/Al composites in the as-fabricated condition and following high-temperature isothermal exposure or thermal cycling. In B/Al (1100), isothermal exposure at 773 K for 125 hr reduced toughness, measured by the work of fracture, from 76 to 10 kJ/sq m, and a similar reduction was observed after equivalent thermal cycling. In B/Al (6061), the same isothermal exposure reduced toughness from 44.5 to 8 kJ/sq m, but the effect of thermal cycling was less detrimental. In FP-Al2O3/Al, the work of fracture was insensitive to either type of treatment. Experimental results are interpreted in terms of matrix softening, interface properties, and fiber notch sensitivity.

Skinner, A.↗