Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solid electrolytes”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,657 records · Page 92

In situ SEM Study of Lithium Intercalation in individual V 2 O 5 Nanowires

Progress in rational engineering of Li-ion batteries requires better understanding of the electrochemical processes and accompanying transformations in the electrode materials on multiple length scales. In spite of recent progress in utilizing transmission electron microscopy (TEM) to analyze these materials, in situ scanning electron microscopy (SEM) was mostly overlooked as a powerful tool that allows probing these phenomena on the nano and mesoscale. In this paper, we report on in situ SEM study of lithiation in a V 2 O 5 -based single-nanobelt battery with ionic liquid electrolyte. Coupled with cyclic voltammetry measurements, in situ SEM revealed the peculiarities of subsurface intercalation, formation of solid-electrolyte interface (SEI) and electromigration of liquid. We observed that single-crystalline vanadia nanobelts do not undergo large-scale amorphization or fracture during electrochemical cycling, but rather transform topochemically with only a slight shape distortion. Lastly, the SEI layer seems to have significant influence on the lithium ion diffusion and overall capacity of the single-nanobelt battery.

25 ENERGY STORAGE↗

Effect of epoxidation level on thermal properties and ionic conductivity of epoxidized natural rubber solid polymer nanocomposite electrolytes

Effect of epoxide content on the thermal and conductivity properties of epoxidized natural rubber (ENR) solid polymer nanocomposite electrolytes was investigated. Commercial available epoxidized natural rubber having 25 (ENR25) and 50 mole% (ENR50) epoxide, respectively were incorporated with lithium perchlorate (LiClO{sub 4}) salt and titanium dioxide (TiO{sub 2}) nanofiller via solution casting method. The solid polymer nanocomposite electrolytes were characterized by differential scanning calorimetry (DSC) and impedance spectroscopy (IS) for their thermal properties and conductivity, respectively. It was evident that introduction of LiClO{sub 4} causes a greater increase in glass transition temperature (T{sub g}) and ionic conductivity of ENR50 as compared to ENR25. Upon addition of TiO{sub 2} in ENR/LiClO{sub 4} system, a remarkable T{sub g} elevation was observed for both ENRs where ENR50 reveals a more pronounced changes. It is interesting to note that they exhibit different phenomenon in ionic conductivity with TiO{sub 2} loading where ENR25 shows enhancement of conductivity while ENR50 shows declination.

36 MATERIALS SCIENCE↗

Electrolyte Role in SEI Evolution at Si in the Pre-lithiation Stage vs the Post-lithiation Stage

The formation and evolution of the dynamic solid electrolyte interphase (SEI) at the Si anode/electrolyte interface are yet to be completely understood to solve irreversible capacity loss and increase battery cycle life. Herein, the evolution of SEI and its dynamic properties at the Si anode/electrolyte interface are investigated in two electrolyte systems, a 1.2 M LiPF6 in EC: EMC 3:7 (wt%) electrolyte (referred to as Gen2) and a 1.2 M LiTFSI in EC: EMC 3:7 (wt%) electrolyte (referred to as LiTFSI). Two lithiation stages are studied: the pre-lithiation (pre-Li) SEI stage and the post-lithiation (post-Li) stage. Findings reveal at the pre-Li, SEI formation starts at an early potential and contributes to the greater mass gain in the Si/Gen2, and it is dominated by the formation of a non-uniform F- and P-rich layer in Si/Gen2, in contrast to a homogeneous F- and C-containing layer at the Si/LiTFSI interphase. The initially formed SEI in LiTFSI further benefits the charge transfer kinetics. At the post-Li stage, a more substantial SEI evolution is observed at Si/LiTFSI. This paper offers a foundational understanding of the SEI dynamic evolution with electrolyte dependence. Findings from this report offer important insights into solving the complex SEI stability issues on Si.

25 ENERGY STORAGE↗

A High-Rate Aqueous Proton Battery Delivering Power Below -78 °C via an Unfrozen Phosphoric Acid

Lithium-sulfur batteries are attractive for automobile and grid applications due to their high theoretical energy density and the abundance of sulfur. Despite the significant progress in cathode development, lithium metal degradation and the polysulfide shuttle remain two critical challenges in the practical application of Li-S batteries. Development of advanced electrolytes has become a promising strategy to simultaneously suppress lithium dendrite formation and prevent polysulfide dissolution. Here, a new class of concentrated siloxane-based electrolytes, demonstrating significantly improved performance over the widely investigated ether-based electrolytes are reported in terms of stabilizing the sulfur cathode and Li metal anode as well as minimizing flammability. Through a combination of experimental and computational investigation, it is found that siloxane solvents can effectively regulate a hidden solvation-ion-exchange process in the concentrated electrolytes that results from the interactions between cations/anions and solvents. As a result, it could invoke a quasi-solid-solid lithiation and enable reversible Li plating/stripping and robust solid-electrolyte interphase chemistries. The solvation-ion-exchange process in the concentrated electrolytes is a key factor in understanding and designing electrolytes for other high-energy lithium metal batteries.

25 ENERGY STORAGE↗

An Artificial SEI Enables the Use of A LiNi0.5Mn1.5O4 5 V Cathode with Conventional Electrolytes

LiNi0.5Mn1.5O4 spinel is considered one of the most promising cathodes for advanced lithium ion batteries. However, the operation potential of LiNi0.5Mn1.5O4, ~4.75 V, is beyond the high voltage limit of the state-of-art electrolyte, ~4.3 V. Here, using thin films of LiNi0.5Mn1.5O4 as a model material, we show evidence that an artificial solid electrolyte interphase (SEI) enables the use of this 5 V cathode with conventional carbonate electrolytes. A thin coating of Lipon (lithium phosphorus oxynitride) as an artificial SEI on LiNi0.5Mn1.5O4 could remedy the decomposition of the electrolyte. The thickness of the Lipon artificial SEI is optimized by balancing the protection and additional resistance. The strategy of artificial SEI on cathodes is expected to enable the wide application of other high voltage cathodes for lithium ion batteries.

artificial SEI↗

Electrochemical-mechanical coupling failure mechanism of composite cathode in all-solid-state batteries

Composite cathode composed of active particles and solid electrolytes (SEs) can considerably enlarge the particle-SE contact areas and achieve high areal loadings in all-solid-state batteries (ASSBs). However, the challenging interfacial instability and particle damage problems remain unsolved. Herein, we establish a 3D electrochemical-mechanical coupled model to investigate the underlying failure mechanism by considering the governing electrochemical and physics processes. Micro-scale heterogeneous primary particles with random crystallographic orientation and size inside the LiNi 1/3 Co 1/3 Mn 1/3 O 2 (NCM111) secondary particle of the model result in the anisotropic Li diffusion and volume variation within the secondary particle, leading to significant nonuniformity of the Li concentration, and GPa-level stress distributions at primary particle boundaries, and finally causing the particle internal cracks. The particle volume shrinkage under the constraint of stiff Li 7 La 3 Zr 2 O 12 (LLZO) SE triggers the interface debonding (gap>50 nm) with increased interfacial impedance to degrade cell capacity. Higher C-rates result in larger residual stress (~100 MPa)/strain/debonding gap at dis-charging end, more likely to deteriorate the cell performance. Increasing the interfacial strength between the particle and SE can suppress the interface debonding but induces high stress (up to 10 GPa). In conclusion, results reveal the underlying mechanism of the electrochemical-mechanical coupling failure mechanism for composite cathode and provide promising guidance on the further improvement of a more robust composite cathode for ASSBs.

25 ENERGY STORAGE↗

Enhanced cycling stability of Ni-rich Li-metal cells enabled by dual vinylene carbonate and tris(trimethylsilyl)borate electrolyte additives

NMC811 (LiNi 0.8 Co 0.1 Mn 0.1 O 2 ) and other high-Ni chemistries are promising cathode candidates for high-performance electric vehicles, owing to their high energy density and reduced cobalt content. However, their long-term cycling stability is hindered by surface degradation, particularly when paired with conventional electrolytes and a lithium metal anode. Electrolyte additives represent a practical approach to enhance interfacial stability and improve overall battery performance by promoting the formation of a robust electrolyte–electrode interphase (EEI). In this study, we revisit the effects of vinylene carbonate (VC) and tris(trimethylsilyl)borate (TMSB) additives on single-crystal SC-NMC811||Li cells. While TMSB only increases the open-circuit voltage and initial overpotential, it delivers superior capacity retention at C/3 compared to cells containing only VC or a dual additive system (VC and TMSB). Notably, under fast-charging conditions (1C, 2C, and 5C), the dual-additive system significantly outperforms other formulations, achieving markedly enhanced long-term capacity retention. Comprehensive electrochemical and spectroscopic analyses reveal that the VC/TMSB dual-additive system suppresses surface transition in NMC811, mitigates structural degradation by forming a thin, LiF-deficient cathode-electrolyte interface (CEI) layer. Moreover, they promote smooth and dense Li deposition and generate a LiF-deficient solid-electrolyte interphase (SEI). Consequently, the synergistic stabilization of both the CEI and SEI effectively limits the overall cell impedance growth during extended cycling. These findings provide key insights into co-additive strategies for engineering stable interfaces in high-energy Ni-rich Li-metal batteries.

36 MATERIALS SCIENCE↗

The Science of Battery Degradation

This report documents work that was performed under the Laboratory Directed Research and Development project, Science of Battery Degradation. The focus of this work was on the creation of new experimental and theoretical approaches to understand atomistic mechanisms of degradation in battery electrodes that result in loss of electrical energy storage capacity. Several unique approaches were developed during the course of the project, including the invention of a technique based on ultramicrotoming to cross-section commercial scale battery electrodes, the demonstration of scanning transmission x-ray microscopy (STXM) to probe lithium transport mechanisms within Li-ion battery electrodes, the creation of in-situ liquid cells to observe electrochemical reactions in real-time using both transmission electron microscopy (TEM) and STXM, the creation of an in-situ optical cell utilizing Raman spectroscopy and the application of the cell for analyzing redox flow batteries, the invention of an approach for performing ab initio simulation of electrochemical reactions under potential control and its application for the study of electrolyte degradation, and the development of an electrochemical entropy technique combined with x-ray based structural measurements for understanding origins of battery degradation. These approaches led to a number of scientific discoveries. Using STXM we learned that lithium iron phosphate battery cathodes display unexpected behavior during lithiation wherein lithium transport is controlled by nucleation of a lithiated phase, leading to high heterogeneity in lithium content at each particle and a surprising invariance of local current density with the overall electrode charging current. We discovered using in-situ transmission electron microscopy that there is a size limit to lithiation of silicon anode particles above which particle fracture controls electrode degradation. From electrochemical entropy measurements, we discovered that entropy changes little with degradation but the origin of degradation in cathodes is kinetic in nature, i.e. lower rate cycling recovers lost capacity. Finally, our modeling of electrode-electrolyte interfaces revealed that electrolyte degradation may occur by either a single or double electron transfer process depending on thickness of the solid-electrolyte-interphase layer, and this cross-over can be modeled and predicted.

25 ENERGY STORAGE↗

Lithium-Ion Electrolytes Containing Flame Retardant Additives for Increased Safety Characteristics

The invention discloses various embodiments of Li-ion electrolytes containing flame retardant additives that have delivered good performance over a wide temperature range, good cycle life characteristics, and improved safety characteristics, namely, reduced flammability. In one embodiment of the invention there is provided an electrolyte for use in a lithium-ion electrochemical cell, the electrolyte comprising a mixture of an ethylene carbonate (EC), an ethyl methyl carbonate (EMC), a fluorinated co-solvent, a flame retardant additive, and a lithium salt. In another embodiment of the invention there is provided an electrolyte for use in a lithium-ion electrochemical cell, the electrolyte comprising a mixture of an ethylene carbonate (EC), an ethyl methyl carbonate (EMC), a flame retardant additive, a solid electrolyte interface (SEI) film forming agent, and a lithium salt.

Smart, Marshall C.↗

(Invited) All-Solid-State Batteries Using Li 7 La 3 Zr 2 O 12 Garnet Electrolyte Framework

All-solid-state batteries (ASSB) using LLZO (variants of Li 7 La 3 Zr 2 O 12 ) garnet solid electrolyte with lithium metal anode potentially offer higher energy density and improved safety. Rational design of cell architecture as well as manufacturing scalability are key aspects to consider as the technology readiness level advances. A thick composite cathode layer attached to a thin solid electrolyte layer is desirable to obtain superior energy densities. Furthermore, the architecture within the composite cathode may be engineered to contain directional conduction paths of lithium ions or electrons for enhanced rate capabilities. Here, we demonstrate a functioning bulk-type LLZO based all-solid-state battery with a practical form factor incorporating the above described design concepts. Freeze-tape-casting (FTC), a scalable and environmentally friendly ceramic processing method, is used to construct 3D porous LLZO scaffolds composed of vertical arrays of LLZO walls. The thin solid-electrolyte layer is fabricated by tape-casting (TC). By sintering the stacks of FTC and TC green tapes, porous/dense bilayers and porous/dense/porous trilayers of LLZO frameworks are obtained. An ASSB was constructed using a porous/dense bilayer by infiltrating LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathode powder and carbon black into the porous layer and adhering lithium metal foil to the dense side. We find it crucial to introduce a plastic crystal based soft solid electrolyte to the porous layer to electrochemically connect all cathode components, obviating the need for co-sintering to establish contact. The soft nature of the plastic crystal based solid-electrolyte may be able to accommodate the volume change of the cathode material as it cycles. In this device, which contained no liquid component, the initial discharge capacities were similar to those observed in a lithium ion battery configuration using the same cathode powder at C/10 rates.

25 ENERGY STORAGE↗

Direct regeneration of degraded LiFePO4 cathodes via a separator-enabled prelithiation strategy

A persistent challenge in lithium-ion batteries is the loss of active lithium due to the solid electrolyte interphase (SEI) formation and associated side reactions. While prelithiation employing lithium replenishment separator (LRS) has been proven effective in compensating for lithium loss, previous studies have largely been accompanied by gas evolution or solid residue formation during the prelithiation process. To surmount this challenge, we present a LRS based on 4-fluoro-1,2-dihydroxybenzene lithium salt (LiDF), capable of mitigating lithium loss while producing decomposition products that integrate directly into the electrolyte as functional additives which can assist with the stability of the SEI, free from gas or solid formation, thus establishing a sustainable and environmentally benign strategy for lithium compensation. Incorporation of the LRS enables the pristine LiFePO4||graphite (Gr) full cell to achieve 10.8% higher capacity than the cell with a polypropylene separator (PPS) after 200 cycles at 0.5C. Remarkably, the degraded LiFePO4 (D-LFP)||Gr full cell with the LRS exhibits a 135.8% capacity improvement over the PPS-based cell after 500 cycles. These findings establish the LRS as a powerful approach for both boosting high-performance lithium-ion batteries and recovering the capacity of degraded batteries.

Tao, Fujun↗

Growth of Lithium Dendrites and Globules through a Solid Block Copolymer Electrolyte as a Function of Current Density

The uncontrollable nonplanar electrodeposition of lithium is a significant barrier to the widespread adoption of high energy density rechargeable batteries with a lithium metal anode. A promising approach for preventing the growth of lithium dendrites is the use of solid polymer electrolytes with a high shear modulus. Current density is the key variable in the electrodeposition of lithium. The present study is the first attempt at quantifying the effect of current density on the geometry and density of dendrites and other protrusions during electrodeposition through a solid polymer electrolyte. The geometry and density of defects formed on the lithium electrode were determined by X-ray microtomography. The tomograms revealed protrusions on the electrodeposited lithium electrodes that were either globular or dendritic, or void defects. The range of current densities over which stable, planar deposition was observed is quantified. At higher current densities, globular protrusions were observed. At the highest current density, both globular and dendritic protrusions were observed. The areal density of protrusion defects increased sharply with current density, while the overall defect density is a weak function of current density. Finally, our work enables comparisons between the experimentally determined onset of nonplanar electrodeposition and prevailing theoretical predictions with no adjustable parameters.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Fast‐Charging and High‐Temperature All‐Organic Rechargeable Potassium Battery

Abstract Developing fast‐charging, high‐temperature, and sustainable batteries is critical for the large‐scale deployment of energy storage devices in electric vehicles, grid‐scale electrical energy storage, and high temperature regions. Here, a transition metal‐free all‐organic rechargeable potassium battery (RPB) based on abundant and sustainable organic electrode materials (OEMs) and potassium resources for fast‐charging and high‐temperature applications is demonstrated. N‐doped graphene and a 2.8 m potassium hexafluorophosphate (KPF 6 ) in diethylene glycol dimethyl ether (DEGDME) electrolyte are employed to mitigate the dissolution of OEMs, enhance the electrode conductivity, accommodate large volume change, and form stable solid electrolyte interphase in the all‐organic RPB. At room temperature, the RPB delivers a high specific capacity of 188.1 mAh g −1 at 50 mA g −1 and superior cycle life of 6000 and 50000 cycles at 1 and 5 A g −1 , respectively, demonstrating an ultra‐stable and fast‐charging all‐organic battery. The impressive performance at room temperature is extended to high temperatures, where the high‐mass‐loading (6.5 mg cm −2 ) all‐organic RPB exhibits high‐rate capability up to 2 A g −1 and a long lifetime of 500 cycles at 70–100 °C, demonstrating a superb fast‐charging and high‐temperature battery. The cell configuration demonstrated in this work shows great promise for practical applications of sustainable batteries at extreme conditions.

25 ENERGY STORAGE↗

New promising lithium malonatoborate salts for high voltage lithium ion batteries

Here, three new lithium salts, lithium difluoro-2-methyl-2-fluoromalonaoborate (LiDFMFMB), lithium difluoro-2-ethyl-2-fluoromalonaoborate (LiDFEFMB), and lithium difluoro-2-propyl-2-fluoro malonaoborate (LiDFPFMB), have been synthesized and evaluated for application in lithium ion batteries. These new salts are soluble in a mixture of ethylene carbonate (EC) and ethyl methyl carbonate (EMC) (1:2 by wt.) and 1.0 M salt solutions can be easily prepared. The ionic conductivities of these new salts are close to those of LiBF 4 and LiPF 6 . Cyclic voltammograms reveal that these new salt based electrolytes can passivate both natural graphite and high voltage spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) to form effective solid electrolyte interphases (SEIs). In addition, these new salts based electrolytes exhibit good cycling stability with high coulombic efficiencies in both LiNi 0.5 Mn 1.5 O 4 and graphite based half-cells and full cells.

25 ENERGY STORAGE↗

New Engineering Concepts to High Energy Density Li-S Batteries

Li-S batteries (LSBs) with energy densities > 500 Wh/kg @ C/5 and >1000 cycles, cycle life operating over wide temperatures has been identified to be critical for meeting the global energy demands. Progress is however, very much limited due to several major hurdles related to the following: (a) poor Li' reaction kinetics (conductivity/diffusivity) enabling full reversible S conversion to Li2S, (b) inferior electron (e) conductivity, specific capacity and cycle life due to electrolyte soluble species of polysulfides (PSs) formed with the reaction of Li ions with sulfur migrating to anode, (c) unstable solid electrolyte interphase (SEI) formation and finally, (d) dendrites that are formed on the Li metal anode severely limiting the cycle life due to polarization at the solid/liquid interfaces causing safety, inferior capacity, energy density, rate, and cycle life issues. Creation of a fully functional economical ≤$80/kWh, high energy density LSBs is vital for enabling its widespread commercial deployment and use in current and next generation electric vehicles.

25 ENERGY STORAGE↗

Reaction Current Heterogeneity at the Interface between a Lithium Electrode and Polymer/Ceramic Composite Electrolytes

Although lithium metal anodes are expected to increase the energy density of next-generation batteries, dendrite growth during charge remains a major bottleneck preventing widespread implementation. Composite solid electrolytes with ceramic particles embedded in a polymer matrix have the potential to prevent dendrites owing to the higher mechanical stiffness while also possessing the flexibility to maintain contact with the electrode. However, microscopically, the different mechanical and electrochemical properties of the polymer and ceramic domains can cause inhomogeneous charge transfer at the Li/electrolyte interface, which can lead to nonuniform Li deposition and propagation of dendrites. Here, we computationally examine the coupled electrochemical, transport, and mechanical processes at the interface to determine the propensity for dendrite formation and possible approaches to mitigate this issue. Predictions of two possible microstructures at the interface, namely, (i) where both the polymer and ceramic come in contact with Li metal and (ii) when only the polymer comes in contact with Li metal, suggest that the former has a greater tendency for nonuniform plating. In addition, predictions suggest that minimizing the interfacial resistance between polymers and ceramics and incorporating interlayers between the electrode and electrolyte help mitigate current heterogeneity. In conclusion, these predictions provide guidance for experimental approaches to prevent dendrites in composite electrolytes.

25 ENERGY STORAGE↗

Investigation of the Cathode–Catalyst–Electrolyte Interface in Aprotic Li–O 2 Batteries

Enabled by a unique integrated fabrication and characterization platform, X-ray photoelectron spectroscopy (XPS) studies reveal the formation of a thin solid electrolyte interphase (SEI) layer on a Li–O2 cathode after the first cycle. Subsequent cycling indicates that this SEI layer is very stable in terms of both chemistry and morphology, even after extensive cycling, preserving reversibility at the cathode/electrolyte interface. Remarkably, even after cell failure, replacement of the lithium anode resulted in recovery of the cycling behavior with the same cathode. These results demonstrate that chemical stabilization of the cathode/electrolyte interface promotes long-term operation of DMSO-based Li–O2 Ru-catalyzed batteries. Characterization of the Li anode surface reveals electrolyte decomposition, and a partial mechanism is proposed for the observed chemical composition of the cathode SEI. These studies are enabled by conformal deposition of a heterogeneous OER catalyst on a freestanding, binder-free, mesoporous, carbon-based Li–O2 cathode with high capacity and long-term cycling stability.

25 ENERGY STORAGE↗

Probing the Formation of Cathode-Electrolyte Interphase on Lithium Iron Phosphate Cathodes via Operando Mechanical Measurements

Interfacial instabilities in electrodes control the performance and lifetime of Li-ion batteries. While the formation of solid-electrolyte interface (SEI) on anodes has received much attention, there is still lack of understanding about the formation of cathode-electrolyte interface (CEI) on the cathodes. To fill this gap, we report on dynamic deformations on lithium iron phosphate, LiFePO 4 cathodes during charge / discharge by utilizing in-operando digital image correlation, impedance spectroscopy and Cryo X-ray photoelectron spectroscopy. LiFePO4 cathodes were cycled in either LiPF 6 , LiClO 4 or LiTFSI- containing organic liquid electrolytes. Beyond the first cycle, Li-ion intercalation results in a nearly linear correlation between electrochemical strains and the state of (dis)-charge, regardless of the electrolyte chemistry. However, during the first charge in LiPF 6 - containing electrolyte, there is a distinct irreversible positive strain evolution at the onset of anodic current rise as well as current decay at around 4.0V. Impedance studies show the increase in surface resistance in the same potential window, suggesting the formation of CEI layers on the cathode. The chemistry of the CEI layer was characterized by X-ray photoelectron spectroscopy. LiF is detected in CEI layer starting as early as 3.4 V and Li $x$ PO $y$ F $z$ appeared at voltages higher than 4.0 V during the first charge. In conclusion, our approach offers new insights into the formation mechanism of CEI layers on the cathode electrodes, which is crucial for the development of robust cathode and electrolyte chemistries for higher performance batteries.

25 ENERGY STORAGE↗