Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “phase boundary”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,657 records · Page 92

Reversible defect engineering in graphene grain boundaries

Research efforts in large area graphene synthesis have been focused on increasing grain size. Here, it is shown that, beyond 1 μm grain size, grain boundary engineering determines the electronic properties of the monolayer. It is established by chemical vapor deposition experiments and first-principle calculations that there is a thermodynamic correlation between the vapor phase chemistry and carbon potential at grain boundaries and triple junctions. As a result, boundary formation can be controlled, and well-formed boundaries can be intentionally made defective, reversibly. In 100 µm long channels this aspect is demonstrated by reversibly changing room temperature electronic mobilities from 1000 to 20,000 cm2 V-1 s-1 . Water permeation experiments show that changes are localized to grain boundaries. Electron microscopy is further used to correlate the global vapor phase conditions and the boundary defect types. Such thermodynamic control is essential to enable consistent growth and control of two-dimensional layer properties over large areas.

36 MATERIALS SCIENCE↗

Electrodynamics of the Inner Magnetosphere Observed in the Dusk Sector by CRRES and DMSP during the Magnetic Storm of June 4-6, 1991

We compare equatorward/earthward boundaries of convection electric fields and auroral/plasma sheet electrons detected by the DMSP F8 and CRRES satellites during the June 1991 magnetic storm. Measurements come from the dusk magnetic local time sector where the ring current penetrates closest to the Earth. The storm was triggered by a rapid increase in the solar wind dynamic pressure accompanied by a southward turning of the interplanetary magnetic field (IMF). Satellite data show the following: (1) all particle and field boundaries moved equatorward/earthward during the initial phase, probably in response to the strong southward IMF turning; (2) electric field boundaries were either at lower magnetic L shells or close to the inner edge of ring current ions throughout the main and early recovery phases. Penetration earthward of the ring current occurred twice as the polar cap potential increased rapidly; (3) electric potentials at subauroral latitudes were large fractions of the total potentials in the afternoon cell, twice exceeding 60 kV; and (4) the boundaries of auroral electron precipitation were more variable than those of electric fields and mapped to lower L shells than where CRRES encountered plasma sheet electrons. Observations qualitatively agree with predictions of empirical models for auroral electron and electric field boundaries.

Bruke, W. J.↗

Investigations of γ′, γ″ and δ precipitates in heat-treated Inconel 718 alloy fabricated by selective laser melting

Highlights: • The γ austenite matrix shows a fine cellular substructure. • γ′ and three variants of γ″ precipitates around 10–50 nm develop within cellular γ. • Coarser acicular γ″ and plate-like δ occur at grain boundaries and intragranular γ. • The orientation relationships of γ″ with γ, and of δ with γ are observed. - Abstract: Inconel 718 alloy samples were fabricated by selective laser melting (SLM). Microstructure and precipitation in solution-heat-treated- and double-aging-SLM-made Inconel 718 were studied by scanning and transmission electron microscopy. Electron microscope observations showed that disc-shaped and cuboidal γ″, and circular γ′ precipitates with an average size of 10–50 nm developed within cellular γ austenite matrix. The simulated, experimentally observed electron diffraction patterns, and dark-field imaging further revealed that the precipitation of three variants of γ″ in the γ matrix occurred. The coarser acicular γ″, and globular as well as plate-like δ phases precipitated at grain boundaries and also within the interior of austenite matrix. The morphology, distribution and crystallography of these precipitates and their formation mechanisms were analyzed and discussed.

36 MATERIALS SCIENCE↗

Magnetic excitations and anomalous spin-wave broadening in multiferroic FeV2O4

We report on the different roles of two orbital-active Fe2+ at the A site and V3+ at the B site in the magnetic excitations and on the anomalous spin-wave broadening in FeV2O4. FeV2O4 exhibits three structural transitions and successive paramagnetic (PM)–collinear ferrimagnetic (CFI)–noncollinear ferrimagnetic (NCFI)/ferroelectric transitions. The high-temperature tetragonal/PM–orthorhombic/CFI transition is accompanied by the appearance of a large energy gap in the magnetic excitations due to strong spin-orbit-coupling-induced anisotropy at the Fe2+ site. While there is no measurable increase in the energy gap from the orbital ordering of V3+ at the orthorhombic/CFI–tetragonal/NCFI transition, anomalous spin-wave broadening is observed in the orthorhombic/CFI state due to V3+ spin fluctuations at the B site. The spin-wave broadening is also observed at the zone boundary without softening in the NCFI/ferroelectric phase, which is discussed in terms of magnon-phonon coupling. Our study also indicates that the Fe2+ spins without the frustration at the A site may not play an important role in inducing ferroelectricity in the tetragonal/NCFI phase of FeV2O4.

36 MATERIALS SCIENCE↗

Effect of heat treatment on microstructure and interface of SiC particle reinforced 2124 Al matrix composite

The microstructure and interface between metal matrix and ceramic reinforcement of a composite play an important role in improving its properties. In the present investigation, the interface and intermetallic compound present in the samples were characterized to understand structural stability at an elevated temperature. Aluminum based 2124 alloy with 10 wt.% silicon carbide (SiC) particle reinforced composite was prepared through vortex method and the solid ingot was deformed by hot rolling for better particle distribution. Heat treatment of the composite was carried out at 575 °C with varying holding time from 1 to 48 h followed by water quenching. In this study, the microstructure and interface of the SiC particle reinforced Al based composites have been studied using optical microscopy, scanning electron microscopy (SEM) coupled with energy dispersive X-ray spectroscopy (EDS), electron probe micro-analyzer (EPMA) associated with wavelength dispersive spectroscopy (WDS) and transmission electron microscopy (TEM) to identify the precipitate and intermetallic phases that are formed during heat treatment. The SiC particles are uniformly distributed in the aluminum matrix. The microstructure analyses of Al–SiC composite after heat treatment reveal that a wide range of dispersed phases are formed at grain boundary and surrounding the SiC particles. The energy dispersive X-ray spectroscopy and wavelength dispersive spectroscopy analyses confirm that finely dispersed phases are CuAl{sub 2} and CuMgAl{sub 2} intermetallic and large spherical phases are Fe{sub 2}SiAl{sub 8} or Al{sub 15}(Fe,Mn){sub 3}Si. It is also observed that a continuous layer enriched with Cu and Mg of thickness 50–80 nm is formed at the interface in between Al and SiC particles. EDS analysis also confirms that Cu and Mg are segregated at the interface of the composite while no carbide is identified at the interface. - Highlights: • The composite was successfully heat treated at 575°C for 1-48 hrs. • A layer of 50-75 nm is formed at interface after heat treatment. • No Carbide formation and SiC dissolution is observed at this temperature. • MgAl{sub 2}O{sub 4}, CuMgAl{sub 2} phases are segregated at interface of Al-SiC composite. • Mg and Cu are also segregated at near to the grain boundary.

36 MATERIALS SCIENCE↗

The role of pre-existing heterogeneities in materials under shock and spall

There has been a challenge for many decades to understand how heterogeneities influence the behavior of materials under shock loading, eventually leading to spall formation and failure. Experimental, analytical, and computational techniques have matured to the point where systematic studies of materials with complex microstructures under shock loading and the associated failure mechanisms are feasible. This is enabled by more accurate diagnostics as well as characterization methods. As interest in complex materials grows, understanding and predicting the role of heterogeneities in determining the dynamic behavior becomes crucial. Early computational studies, hydrocodes, in particular, historically preclude any irregularities in the form of defects and impurities in the material microstructure for the sake of simplification and to retain the hydrodynamic conservation equations. Contemporary computational methods, notably molecular dynamics simulations, can overcome this limitation by incorporating inhomogeneities albeit at a much lower length and time scale. This review discusses literature that has focused on investigating the role of various imperfections in the shock and spall behavior, emphasizing mainly heterogeneities such as second-phase particles, inclusions, and voids under both shock compression and release. Pre-existing defects are found in most engineering materials, ranging from thermodynamically necessary vacancies, to interstitial and dislocation, to microstructural features such as inclusions, second phase particles, voids, grain boundaries, and triple junctions. This literature review explores the interaction of these heterogeneities under shock loading during compression and release. Systematic characterization of material heterogeneities before and after shock loading, along with direct measurements of Hugoniot elastic limit and spall strength, allows for more generalized theories to be formulated. Further, continuous improvement toward time-resolved, in situ experimental data strengthens the ability to elucidate upon results gathered from simulations and analytical models, thus improving the overall ability to understand and predict how materials behave under dynamic loading.

36 MATERIALS SCIENCE↗

Scalar excursions in large-eddy simulations

Here, the range of values of scalar fields in turbulent flows is bounded by their boundary values, for passive scalars, and by a combination of boundary values, reaction rates, phase changes, etc., for active scalars. The current investigation focuses on the local conservation of passive scalar concentration fields and the ability of the large-eddy simulation (LES) method to observe the boundedness of passive scalar concentrations. In practice, as a result of numerical artifacts, this fundamental constraint is often violated with scalars exhibiting unphysical excursions. The present study characterizes passive-scalar excursions in LES of a shear flow and examines methods for diagnosis and assesment of the problem. The analysis of scalar-excursion statistics provides support of the main hypothesis of the current study that unphysical scalar excursions in LES result from dispersive errors of the convection-term discretization where the subgrid-scale model (SGS) provides insufficient dissipation to produce a sufficiently smooth scalar field. In the LES runs three parameters are varied: the discretization of the convection terms, the SGS model, and grid resolution. Unphysical scalar excursions decrease as the order of accuracy of non-dissipative schemes is increased, but the improvement rate decreases with increasing order of accuracy. Two SGS models are examined, the stretched-vortex and a constant-coefficient Smagorinsky. Scalar excursions strongly depend on the SGS model. The excursions are significantly reduced when the characteristic SGS scale is set to double the grid spacing in runs with the stretched-vortex model. The maximum excursion and volume fraction of excursions outside boundary values show opposite trends with respect to resolution. The maximum unphysical excursions increase as resolution increases, whereas the volume fraction decreases. The reason for the increase in the maximum excursion is statistical and traceable to the number of grid points (sample size) which increases with resolution. In contrast, the volume fraction of unphysical excursions decreases with resolution because the SGS models explored perform better at higher grid resolution.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Investigation of Zr-doped BSCF perovskite membrane for oxygen separation in the intermediate temperature range

The series of (Ba₀.₅Sr₀.₅)(Co₀.₈Fe₀.₂){sub 1–z}Zr{sub z}O{sub 3–δ} (z=0, 0.01, 0.03, 0.05, 0.07, and 0.09) was synthesized by a sol–gel method. The materials with a zirconium content up to 3 mol% were found to be single phase. Further increase results in formation of a mixed (Ba,Sr)ZrO₃ by-phase, which was found along the grain boundaries and in the grains. With increasing zirconium content the oxygen permeation flux decreases considerably. The effect of the zirconium substitution on the long-term phase stability was investigated by long-term oxygen permeation experiments and X-ray diffraction. A slight stabilization of the oxygen flux of (Ba₀.₅Sr{sub 0.5})(Co₀.₈Fe₀.₂)₀.₉₇Zr₀.₀₃O{sub 3–δ} was found after 180 h at 1023 K. However, all compositions show a decrease in permeation flux with time, but the pure BSCF membrane exhibited the strongest drop after 180 h of operation. The decomposition products of the cubic perovskite phase were found to be a hexagonal Ba{sub 0.5±x}Sr{sub 0.5±x}CoO₃ and a rhombohedral Ba{sub 1–x}Sr{sub x}Co{sub 2–y}Fe{sub y}O{sub 5–δ}. - Graphical abstract: Backscattered-electron channeling contrast image of BSCF membrane cross-section after long-term oxygen permeation at 1023 K showing different phases in different colors. Highlights: • Ba₀.₅Sr₀.₅Co₀.₈Fe₀.₂O{sub 3–δ} systematically doped with increasing amount of zirconium. • Cubic single-phase materials up to 3 wt% zirconium. • Mixed (Ba,Sr)ZrO₃ by-phase formed mainly in the grain boundaries. • Jänecke prism was proposed by XRD and EDXS data. • (Ba₀.₅Sr₀.₅)(Co₀.₈Fe₀.₂)₀.₉₇Zr₀.₀₃O{sub 3–δ} showed a slight stabilization of oxygen flux as compared to pure Ba₀.₅Sr₀.₅Co₀.₈Fe₀.₂O{sub 3–δ}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Perovskite Electrolyte That Is Stable in Moist Air for Lithium‐Ion Batteries

Abstract Solid‐oxide Li + electrolytes of a rechargeable cell are generally sensitive to moisture in the air as H + exchanges for the mobile Li + of the electrolyte and forms insulating surface phases at the electrolyte interfaces and in the grain boundaries of a polycrystalline membrane. These surface phases dominate the total interfacial resistance of a conventional rechargeable cell with a solid–electrolyte separator. We report a new perovskite Li + solid electrolyte, Li 0.38 Sr 0.44 Ta 0.7 Hf 0.3 O 2.95 F 0.05 , with a lithium‐ion conductivity of σ Li =4.8×10 −4 S cm −1 at 25 °C that does not react with water having 3≤pH≤14. The solid electrolyte with a thin Li + ‐conducting polymer on its surface to prevent reduction of Ta 5+ is wet by metallic lithium and provides low‐impedance dendrite‐free plating/stripping of a lithium anode. It is also stable upon contact with a composite polymer cathode. With this solid electrolyte, we demonstrate excellent cycling performance of an all‐solid‐state Li/LiFePO 4 cell, a Li‐S cell with a polymer‐gel cathode, and a supercapacitor.

Li, Yutao↗

On the effect of elemental partitioning to secondary phases after solution and aging heat treatments in a Co-Ni-based superalloy

Here, this paper presents the phase stability and elemental partitioning in a Co-40Ni-10Al-7.5W-10Cr-3Nb-0.06B-0.6C (at.%) superalloy (referred to as 3Nb) after a two-step heat treatment. The resulting microstructure consisted of γ, γ', MC carbides and µ-Co 7 W 6 phase decorating the regions near and at the grain boundaries. Nb preferentially partitioned to the γ'-phase and other elements such as Ni, Cr and W were responsible for the μ-phase formation.

36 MATERIALS SCIENCE↗

Computational Examination of Orientation-Dependent Morphological Evolution during the Electrodeposition and Electrodissolution of Magnesium

Here a new model of electrodeposition and electrodissolution is developed and applied to the evolution of Mg deposits during anode cycling. The model captures Butler-Volmer kinetics, facet evolution, the spatially varying potential in the electrolyte, and the time-dependent electrolyte concentration. The model utilizes a diffuse interface approach, employing the phase field and smoothed boundary methods. Scanning electron microscope (SEM) images of magnesium deposited on a gold substrate show the formation of faceted deposits, often in the form of hexagonal prisms. Orientation-dependent reaction rate coefficients were parameterized using the experimental SEM images. Three-dimensional simulations of the growth of magnesium deposits yield deposit morphologies consistent with the experimental results. The simulations predict that the deposits become narrower and taller as the current density increases due to the depletion of the electrolyte concentration near the sides of the deposits. Increasing the distance between the deposits leads to increased depletion of the electrolyte surrounding the deposit. Two models relating the orientation-dependence of the deposition and dissolution reactions are presented. Finally, the morphology of the Mg deposit after one deposition-dissolution cycle is significantly different between the two orientation-dependence models, providing testable predictions that suggest the underlying physical mechanisms governing morphology evolution during deposition and dissolution.

36 MATERIALS SCIENCE↗

AFM CHARACTERIZATION OF RAMAN LASER INDUCED DAMAGE ON CDZNTECRYSTAL SURFACES

High quality CdZnTe (or CZT) crystals have the potential for use in room temperature gamma-ray and X-ray spectrometers. Over the last decade, the methods for growing high quality CZT have improved the quality of the produced crystals however there are material features that can influence the performance of these materials as radiation detectors. The presence of structural heterogeneities within the crystals, such as twinning, pipes, grain boundaries (polycrystallinity), and secondary phases (SPs) can have an impact on the detector performance. There is considerable need for reliable and reproducible characterization methods for the measurement of crystal quality. With improvements in material characterization and synthesis, these crystals may become suitable for widespread use in gamma radiation detection. Characterization techniques currently utilized to test for quality and/or to predict performance of the crystal as a gamma-ray detector include infrared (IR) transmission imaging, synchrotron X-ray topography, photoluminescence spectroscopy, transmission electron microscopy (TEM), atomic force microscopy (AFM) and Raman spectroscopy. In some cases, damage caused by characterization methods can have deleterious effects on the crystal performance. The availability of non-destructive analysis techniques is essential to validate a crystal's quality and its ability to be used for either qualitative or quantitative gamma-ray or X-ray detection. The work presented herein discusses the damage that occurs during characterization of the CZT surface by a laser during Raman spectroscopy, even at minimal laser powers. Previous Raman studies have shown that the localized annealing from tightly focused, low powered lasers results in areas of higher Te concentration on the CZT surface. This type of laser damage on the surface resulted in decreased detector performance which was most likely due to increased leakage current caused by areas of higher Te concentration. In this study, AFM was used to characterize the extent of damage to the CZT crystal surface following exposure to a Raman laser. AFM data reveal localized surface damage and increased conductivity in the areas exposed to the Raman laser beam.

43 PARTICLE ACCELERATORS↗

Direct Observation of Defect‐Aided Structural Evolution in a Nickel‐Rich Layered Cathode

Abstract Ni‐rich LiNi 1− x − y Mn x Co y O 2 (NMC) layered compounds are the dominant cathode for lithium ion batteries. The role of crystallographic defects on structure evolution and performance degradation during electrochemical cycling is not yet fully understood. Here, we investigated the structural evolution of a Ni‐rich NMC cathode in a solid‐state cell by in situ transmission electron microscopy. Antiphase boundary (APB) and twin boundary (TB) separating layered phases played an important role on phase change. Upon Li depletion, the APB extended across the layered structure, while Li/transition metal (TM) ion mixing in the layered phases was detected to induce the rock‐salt phase formation along the coherent TB. According to DFT calculations, Li/TM mixing and phase transition were aided by the low diffusion barriers of TM ions at planar defects. This work reveals the dynamical scenario of secondary phase evolution, helping unveil the origin of performance fading in Ni‐rich NMC.

Li, Shuang↗

Direct observation of defect-aided structural evolution in Ni-rich layered cathode

Ni-rich LiNi 1-x-y Mn x Co y O 2 (NMC) layered compounds have become the dominated cathode for lithium ion batteries. The role of crystallographic defects on their structure evolution and consequent performance degradation during electrochemical cycling is not yet fully understood. In this work, we investigated the structural evolution of Ni-rich NMC cathode in a solid-state cell via in-situ transmission electron microscopy. We identified antiphase boundary (APB) and twin boundary (TB) separating layered phases played an important role on phase change. Upon the lithium depletion, the APB extends across the layered structure, while Li/transition metal (TM) ion mixing in the layered phases is detected to induce the rock-salt phase formation along the coherent TB. According to DFT calculations, Li/TM mixing and phase transition are aided by the low diffusion barriers of TM ions at planar defects. Finally, this work reveals the dynamical scenario of secondary phase evolution, which helps to unveil the origin of performance fading in Ni-rich NMC.

25 ENERGY STORAGE↗

Spontaneous breaking of scale invariance in a D = 3 U(N ) model with Chern-Simons gauge fields

We study spontaneous breaking of scale invariance in the large N limit of three dimensional U(N ) κ Chern-Simons theories coupled to a scalar field in the fundamental representation. When a λ 6 ( Ø † · Ø) 3 self interaction term is added to the action we find a massive phase at a certain critical value for a combination of the λ(6) and ’t Hooft’s λ = N/κ couplings. This model attracted recent attention since at finite κ it contains a singlet sector which is conjectured to be dual to Vasiliev’s higher spin gravity on AdS 4 . Our paper concentrates on the massive phase of the 3d boundary theory. We discuss the advantage of introducing masses in the boundary theory through spontaneous breaking of scale invariance.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

The analytic structure of non-global logarithms: Convergence of the dressed gluon expansion

Non-global logarithms (NGLs) are the leading manifestation of correlations between distinct phase space regions in QCD and gauge theories and have proven a challenge to understand using traditional resummation techniques. Recently, the dressed gluon ex-pansion was introduced that enables an expansion of the NGL series in terms of a “dressed gluon” building block, defined by an all-orders factorization theorem. Here, we clarify the nature of the dressed gluon expansion, and prove that it has an infinite radius of convergence as a solution to the leading logarithmic and large-N c master equation for NGLs, the Banfi-Marchesini-Smye (BMS) equation. The dressed gluon expansion therefore provides an expansion of the NGL series that can be truncated at any order, with reliable uncertainty estimates. In contrast, manifest in the results of the fixed-order expansion of the BMS equation up to 12-loops is a breakdown of convergence at a finite value of α s log. We explain this finite radius of convergence using the dressed gluon expansion, showing how the dynamics of the buffer region, a region of phase space near the boundary of the jet that was identified in early studies of NGLs, leads to large contributions to the fixed order expansion. We also use the dressed gluon expansion to discuss the convergence of the next-to-leading NGL series, and the role of collinear logarithms that appear at this order. Finally, we show how an understanding of the analytic behavior obtained from the dressed gluon expansion allows us to improve the fixed order NGL series using conformal transformations to extend the domain of analyticity. Furthermore, this allows us to calculate the NGL distribution for all values of α s log from the coefficients of the fixed order expansion.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

The Role of Wheel Surface Quality on Structural and Hard Magnetic Properties of Nd–Fe–B Permanent Magnet Powders

Rapidly solidified Nd{sub 15}Fe{sub 77}B{sub 8} magnetic alloy powders have been produced by using melt-spinning method. Different wheel surface structures such as smooth and textured were tested to investigate the effect of wheel surface morphology on powder shape, microstructure, Curie temperature, and magnetic properties. Produced powders were subjected to surfactant-active ball-milling process for powder size reduction and to enhance magnetic and thermal properties. Generally, flaky-shaped powders were obtained with smooth surface wheels and spherical-shaped powders were produced with textured surface wheel. Microstructure of flaky-shaped powders consisted of polygonal fine equiaxed grains with an average grain size of 0.45 µm. Spherical-shaped powders had dendritic microstructure regardless of their sizes. Both flaky and spherical powders involved hard magnetic Nd{sub 2}Fe{sub 14}B phase located in the grain interior and a fine network of Nd-rich phase at the grain boundaries. Surfactant-active ball-milling process significantly contributed to magnetic and thermal properties of powders. The coercivity values of flaky-shaped powders milled for 90, 150, 210, 270, 330, and 390 min milling times were substantially higher than that of spherical-shaped powders milled for the same period of times. The Curie temperatures of Nd{sub 15}Fe{sub 77}B{sub 8} ingot alloy and spherical- and flaky-shaped powders were found as 279, 305, and 321 {sup ∘}C, respectively. On the other hand, the Curie temperatures of flaky- and spherical-shaped powders milled for 390 min were measured as 331 and 311 {sup ∘}C, respectively.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗