Oxide dispersoid coherency of a ferritic-martensitic 12Cr oxide-dispersion-strengthened alloy under self-ion irradiation

Ferritic-martensitic oxide-dispersion-strengthened (ODS) alloy has shown excellent mechanical property and high radiation tolerance. However, the stability of dispersoids during displacive irradiation in the individual ferritic and martensitic phases is unclear. In this work, the correlation among dispersoid coherency, size, density, and matrix phase are studied in dual-phase 12Cr ODS after 100 peak displacements-per-atom (dpa) irradiation at 475°C, using 3.5 MeV Fe 2+ self-ions. The size and density changes of coherent and incoherent dispersoids were analyzed as a function of irradiation depth. The average dispersoid size decreased after irradiation in both phases, and the large incoherent dispersoids in the tempered martensite phase underwent a more dramatic change than those in the ferrite phase. The dispersoid density significantly increased in the ferrite phase within the irradiated region, mostly resulting in an increase in coherent dispersoid density. On the other hand, only a small change in density was observed in the tempered martensite phase for both coherent and incoherent dispersoids. This study shows that dispersoid evolution is dramatically different in ferrite and tempered martensite phases.

36 MATERIALS SCIENCE↗

A microscopic and crystallographic study of proton irradiated alloy 718

Solution annealing and age hardening are important processes for achieving good engineering and chemical properties of alloy 718. The composition of alloy 718 also plays an important role as it can affect both mechanical (γ”- and γ’-phase formation) and irradiation behaviors. Therefore, in this study five different sets of alloy 718 samples with two different chemical compositions were fabricated using different processing conditions and irradiated up to 4 dpa. Based on the effects of irradiation on the microstructural data of γ”- and γ’-phases, irradiation-induced dislocation statistics, and crystallographic data, it can be inferred that the samples processed at high solution annealing temperature (1093°C) behave better under irradiation compared to the samples processed at low solution annealing temperatures (945 and 1065°C).

36 MATERIALS SCIENCE↗

Neutron irradiation induced defects and clustering in NF616 and T91

NF616 is a third-generation ferritic martensitic steel, developed to have better creep resistance than the prior generation T91. Unlike relatively numerous studies of T91, there is a lack of understanding of the irradiation effect on the microstructural evolution and mechanical response of NF616. This work evaluated the microstructures and radiation hardening of NF616 irradiated up to 8.2 displacement per atom (dpa) at 292 °C – 431 °C, compared with T91 from two heats. Dislocation loops were observed in all investigated samples. NF616 exhibited comparable loop size but slightly lower loop density than those in the general T91 heat at 430 °C. Cavities were only observed in NF616 at 431 °C but absent at lower irradiation temperatures (292 °C and 359 °C). Ni-rich clusters were also observed in NF616 at 431 °C, while only weak Ni-clustering were observed at lower irradiation temperatures. Compared to the general T91 heat, NF616 demonstrated better swelling resistance (e.g., one third of swelling in the general T91 heat at 430 °C), a slightly higher number density of Ni-rich clusters, and slightly lower radiation hardening. The low-carbon T91 showed the greatest hardening with the largest swelling and loop sizes, despite its lowest irradiation temperature and intermediate dose. The calculated hardening from loops, cavities and Ni-rich clusters using the classic dispersed barrier-hardening model had reasonable agreement with the experiment-derived results, with the primary hardening contribution attributed to dislocation loops.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Optical transmission and dimensional stability of single-crystal sapphire after high-dose neutron irradiation at various temperatures up to 688 °C

The use of single-crystal sapphire optical fibers has been considered to extend fiber-optic sensing to the extreme temperature (>1000 °C) environments encountered in nuclear applications. However, before these sapphire fiber–based sensors can be deployed, their optical transmission and dimensional stability (which impacts drift of some sensors) must be characterized under representative testing conditions. Data regarding the optical transmission of sapphire following high-dose neutron irradiation at temperatures >100 °C is extremely limited. This work provides measurements of optical density (i.e., attenuation) and directional dimensional changes in bulk single-crystal sapphire materials irradiated to a fast neutron fluence of 2.4 × 10 21 n/cm 2 (3.5 displacements per atom) at temperatures ranging from 95 to 688 °C. Optical density measured after irradiation at 95 and 298 °C showed ultraviolet and visible absorption bands corresponding to known defect centers and temperature trends that were generally consistent with previous ex situ and in situ measurements made at much lower neutron fluence. However, optical density measured after irradiation at 688 °C was as much as two orders of magnitude higher, indicating that the fundamental mechanism for radiation-induced attenuation changes at this irradiation temperature. Additional analysis and comparison with previous works suggest that the attenuation may result from void formation, leading to increased Rayleigh scattering losses in the material and increased swelling that would also result in drift of Bragg grating-based sensors in sapphire fibers. These results pose serious questions regarding the feasibility of sapphire fiber–based sensors for high-temperature nuclear applications.

36 MATERIALS SCIENCE↗

Properties and microstructure evolution of silicon nitride and zirconium nitride following Ni ion irradiation

We report that silicon nitride and zirconium nitride have been proposed as potential materials for multiple nuclear applications (inert matrix fuels, accident tolerant fuels, space nuclear power, fusion reactor design), yet knowledge on their behavior under irradiation remains limited. Ion irradiations were performed using 15 MeV Ni 5+ ions on Si 3 N 4 and ZrN samples, with midrange doses (around 3 µm) from 1 to 50 dpa and temperatures from 300 to 700°C. Volumetric lattice swelling was determined by grazing incidence X-ray diffraction, defect production and evolution were tracked using Transmission Electron Microscopy, and nanoindentation was performed to quantify the ceramics’ mechanical properties evolution. The results from these irradiation studies on nitride ceramics help fill the current gap present in the literature. Behavior consistent with past work on irradiated Si 3 N 4 was observed with respect to mechanical properties and defect formation up to 15 dpa and 500°C. Failure of the grain boundary sintering aid in Si 3 N 4 was observed above these conditions. Different behavior was observed in both nitrides at 50 dpa and 700°C, where lattice swelling increased past potential saturation values. Unreported cavity formation was witnessed in both materials under all irradiation conditions, with stable number density and slight size increase above 15 dpa. The mechanism for the cavity formation remains to be determined.

36 MATERIALS SCIENCE↗

Computational determination of a primary diffusion mode in γ U-10Mo under irradiation

Low enriched uranium (< 20 % 235 U)-molybdenum (U-Mo) monolithic fuel is the primary candidate for high performance research and test reactors, and is in the process of being qualified to replace highly enriched uranium (≥ 20 % 23 5U) fuel. As part of the qualification process, it is critical to understand and predict the behavior of fission gas bubbles under irradiation, which affects fuel swelling and fuel failure. Mechanistic fuel models are being developed that can both reproduce the existing experimental data for fuel swelling, and be further applied to irradiation conditions beyond the experimental scope. Diffusion of species under irradiation conditions is an important parameter in the mechanistic fuel models; however, no temperature-relevant experimental diffusion data exists. In the present work, radiation-enhanced diffusion coefficients of U, Mo, and Xe in λU-10wt.%Mo were calculated in the temperature range between 300 K and 1400 K via rate-theory models and molecular dynamics simulations with an embedded-atom method interatomic potential for the U-Mo-Xe system. Accordingly, total diffusion coefficients under relevant irradiation conditions are determined using previously obtained intrinsic thermal diffusion and radiation-driven diffusion coefficients, as well as the newly calculated radiation-enhanced diffusion coefficients presented herein. Radiation-enhanced diffusion of U and Mo was dominant in the intermediate temperature range, whereas radiation-enhanced diffusion of Xe did not significantly contribute to total diffusion of Xe at the relevant fission rate densities. Radiation-enhanced diffusion of Xe became faster than both intrinsic thermal diffusion and radiation-driven diffusion at a fission rate density of 5 x 10 22 fissions/m 3 /s, which is higher than the typical fission rate density range in research reactors. The temperature regime that radiation-enhanced diffusion of each element dominated was dependent on the fission rate density. Finally, the total diffusion coefficients of U, Mo, and Xe, updated in this work, will be utilized as parameters in the mechanistic fuel models to help predict the behavior of fission gas bubbles under irradiation more accurately.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fracture behavior of irradiation induced nanocrystalline UO 2 studied by in-situ mechanical testing in transmission electron microscopy

Uranium Dioxide (UO 2 ) is widely used as a fuel in current light water reactors (LWRs). Upon accumulation of radiation damage, LWR UO 2 fuel pellets start to develop a different microstructure at the pellet periphery when fuel burnup exceeds 45–50 GWd/tHM. The resulting porous, nanocrystalline microstructure is one of the most prominent microstructural changes occurring in such fuel. Its fracture mechanisms, which causes fuel fine fragmentation, could impact safety limits when the cladding breaches. Direct measurements of these properties are challenging, therefore a surrogate obtained via ion irradiation can be used. In this study, multiple microcantilevers were fabricated by focused ion beam from both fresh UO 2 and UO 2 irradiated with 84 MeV Xe 26+ ions to a peak dose of 1357 displacements per atom (dpa). Further, the irradiation produced a pseudo high burnup structure approximately 2 µm below the surface. In-situ nano-mechanical bending tests were conducted to investigate the fracture behavior and the effect of the surrogate UO 2 high burnup structure on local fracture properties. Fresh UO 2 fuel was observed to fracture in transgranular mode without nucleation or movement of dislocations. However, the Xe-irradiated nanocrystalline microcantilevers fractured along the grain boundaries, with no influence from the pre-existing micro-cracks in the microcantilever. Fracture toughness for this type of surrogate high burnup UO 2 structure is reported for the first time in literature. Both the fracture stress and toughness show degradation for UO 2 as a result of Xe-irradiation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Micro-tensile characteristics of As-fabricated and irradiated AGR-2 TRISO fuel particle buffer, IPyC, and buffer-IPyC interlayer regions

A recently developed micro-tensile sample preparation technique was implemented to evaluate the tensile strengths of the buffer, IPyC, and buffer-IPyC interlayer regions of the unirradiated and irradiated AGR-2 TRISO fuel particles. Understanding the mechanical properties of the buffer-IPyC interlayer is essential for developing thermomechanical models of buffer-IPyC separation, yet there is a lack of experimental data on its micro-tensile properties. TEM analysis was conducted on these regions to determine the microstructural changes relevant to the samples' tensile properties. In the unirradiated TRISO particle samples, the buffer layer demonstrated the weakest tensile strength, while the IPyC layer exhibited the highest. Conversely, in the irradiated TRISO particle samples, the buffer-IPyC interlayer region showed the lowest tensile strength, with the IPyC layer being the strongest. Fractures in the samples from the buffer-IPyC region predominantly occurred either in the buffer layer or at the buffer-IPyC interface. However, some buffer-IPyC interlayer samples displayed stress-strain and fracture behaviors more akin to the IPyC layer than the buffer layer. Analysis of diffraction patterns suggests that irradiation may have increased anisotropy in the three regions tested. Despite this suggested increase in anisotropy, there was no evidence that it affected the measured strengths. The irradiated TRISO particles demonstrated a considerable increase in void space and a decrease in ultimate tensile strength within the buffer-IPyC interlayer region due to the densification and contraction of the buffer layer. Minor variations in diffraction ring patterns were also observed. These changes, coupled with a significant reduction in the Weibull modulus/shape parameter, imply that irradiation-induced densification leads to tearing between the buffer and IPyC layers at locations of elevated porosity in the buffer-IPyC interlayer region.

Tristructural isotropic (TRISO)↗

Plutonium migration and phase evolution in irradiated U-Pu-Zr metallic fuels: An integrated EPMA-SEM-TEM study

Constituent redistribution is a defining feature of irradiated U-Pu-Zr metallic fuels, yet its mechanisms and effects on fuel performance are not sufficiently resolved to guide model development. Although decades of irradiation testing have established broad trends, a true mechanistic understanding of constituent redistribution has not been achieved. Here, in this study, we use electron probe microanalysis (EPMA), scanning electron microscopy (SEM), and transmission electron microscopy-based (TEM) selective area electron diffraction (SAED) on a EBR-II irradiated U-19 wt.% Pu-6 wt.% Zr fuel pin cross-section to correlate the composition, porosity, and crystallographic phases formed after irradiation. Constituent redistribution is thought to consist of three distinct zones, in which uranium and zirconium migrate while plutonium remains relatively unchanged. Our EPMA results resolve eight distinct compositional regions, and more importantly, show that plutonium redistributes alongside zirconium, contrary to historical assumptions. The distribution of fission products was highly asymmetric with a few large lanthanide precipitates observed at isolated sites on the pin periphery instead of a uniform distribution of smaller precipitates around the periphery. Using thermodynamic data from TAF-ID and the measured EPMA compositions, matrix phase fractions were predicted across the fuel radius. Phase predictions based on composition did not match TEM/SAED results, which revealed a much higher fraction of α−U phase than would be expected if phases were retained from reactor temperatures. These findings highlight the need for expanded SAED phase identification to capture post-irradiation and storage effects, as well as rigorous uncertainty quantification in fuel performance and phase diagram modeling to better constrain predictions from compositional data.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Helium co-implantation effects on dislocation loop evolution during in situ ion irradiations of a novel additive-manufactured Fe-9Cr steel alloy

This study examines the impact of helium injection rate on dislocation loop evolution during ion irradiation of a novel, additively manufactured (AM) 9Cr reduced-activation ferritic/martensitic (RAFM) steel. Through in situ transmission electron microscopy ion irradiations and post-irradiation characterization, the effects of simultaneous 1 MeV Kr²⁺ and 12 keV He⁺ ion irradiation at 400°C to 5 dpa with varying helium levels were examined. The findings reveal that helium co-injection significantly increases dislocation loop density, primarily through the formation of small defect features exhibiting contrast and projected morphologies consistent with a⟨100⟩ loops (∼1 nm), while suppressing larger a/2⟨111⟩ loops. The findings underscore the complex interplay among continuously increasing helium content, temperature, and alloy composition in the evolution of dislocation loops under irradiation in RAFM steels. The study highlights the need for further investigation into helium-mediated mechanisms, such as proposed interactions between self-interstitial atoms and helium atoms, to enhance the performance of RAFM steels in advanced nuclear reactors.

ANA2↗

Defect formation and transmutation behaviors in irradiated tungsten under thermal-neutron shielded and mixed spectrum conditions

Here, this study investigates the microstructural evolution of pure tungsten irradiated under thermal-neutron shielded and mixed spectrum conditions in the High Flux Isotope Reactor (HFIR). Four samples were irradiated at temperatures from 570 °C to 1130 °C up to 0.73 dpa. Neutron spectrum significantly influenced the accumulation of transmutation products, with Re+Os content estimated at ∼0.3–0.6% under thermal-neutron shielded conditions and ∼5.2% under the mixed spectrum condition. Irradiation temperature strongly influences tungsten’s microstructure, with dislocation loops and fine voids forming at lower temperatures and only larger voids and Re/Os segregation observed at higher temperature. Under thermal-neutron shielded conditions, dislocation loops and voids were observed at 570 °C and 790 °C. At the highest irradiation temperature (1130 °C), dislocation loops were no longer observed, while larger but less dense voids remained. Re and Os segregation to void surfaces was evident at 790 °C and 1130 °C, though no precipitation was observed. In contrast, under the mixed-spectrum condition, both spherical and needle-like Re/Os-rich precipitates were observed, frequently accompanied by large voids. Dislocation loops were not observed, but loop-like contrast within the precipitates suggests they may have nucleated on pre-existing loops. Irradiation-induced hardening was assessed for the shielded samples at 570 °C and 790 °C. Dispersed barrier hardening (DBH) analysis, based on TEM-resolved defects, revealed that voids were the dominant contributors to hardening, consistent with literature results. A schematic model is proposed to describe defect and precipitate evolution in tungsten under fusion-relevant transmutation-to-dpa conditions.

Dislocation loops↗

The role of Cr concentration and temperature on cavity swelling with co-injected helium in dual-ion irradiated Fe and Fe-Cr alloys

The level of chromium plays an essential role in irradiation tolerance of Fe-Cr ferritic alloys. However, conflicting results have been reported regarding the dependence of cavity swelling under irradiation on Cr level and temperature. Here, we have performed a comprehensive set of simultaneous dual-ion (Ni + He) irradiations to high dose (~30 displacements per atom, dpa) at 400–550 °C on a series of ultra-high purity Fe and Fe-Cr binary alloys (3–14 wt.%Cr). Helium co-implantation rates of 0.1 and 10 appm He/dpa were selected to examine He synergistic effects relevant for fission and fusion reactor conditions, respectively. Cavities were observed in all irradiated samples by transmission electron microscopy. The results show that higher He implantation rate causes a shift in the swelling peak to higher temperatures in both Fe and Fe-Cr alloys. When assuming smaller cavities as biased sinks, the non-monotonic nature of the cavity swelling behavior is related to the ratio of biased to unbiased point defect sink strengths. Cr-enriched precipitates were observed in Fe-14Cr irradiated at 400 °C by atom probe tomography. Our analysis suggests the formation of Cr-enriched precipitates could suppress cavity swelling for Fe-Cr alloys with Cr content above 10 wt%.

36 MATERIALS SCIENCE↗

Synthesis of nanosize BPO{sub 4} under microwave irradiation

Highlights: ► Nanosize BPO{sub 4} are prepared under microwave-irradiation conditions. ► This reaction is only performed at less than 640 W power for 2.5–5 min. ► The particles of sample irradiated at 400 W are 40–90 nm in size and well dispersed. ► A simple, fast and green procedure for synthesis of nanosize BPO{sub 4} is developed. -- Abstract: Nanosize BPO{sub 4} was synthesized using H{sub 3}BO{sub 3} and H{sub 3}PO{sub 4} (85%) as raw materials under microwave irradiation. This reaction was performed at powers lower than 640 W and irradiation time ranging from 2.5 min to 5 min, which were only a fraction of the time required for conventional synthetic procedures. The structure of the as-prepared BPO{sub 4} is analogous to that of a high cristobalite. The particle sizes of the samples irradiated at 640 and 400 W range from 40 nm to 90 nm and 30 nm to 60 nm, respectively. The effects of different conditions on the experimental outcome are also discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of polymeric films subjected to lithium ion beam irradiation

Two different polymeric materials that are candidate materials for use as binders for mixed uranium–plutonium oxide nuclear fuel pellets were subjected to Li ion beam irradiation, in order to simulate intense alpha irradiation. The materials (a polyethylene glycol 8000 and a microcrystalline wax) were then analyzed using a combination of mass spectrometry (MS) approaches and X-ray photoelectron spectroscopy (XPS). Samples of the irradiated PEG materials were dissolved in H2O and then analyzed using electrospray ionization-MS, which showed the formation of a series of small oligomers in addition to intact large PEG oligomers. The small oligomers were likely formed by radiation-induced homolytic scissions of the C–O and C–C bonds, which furnish radical intermediates that react by radical recombination with Hradical dot and OHradical dot. Surface analysis using SIMS revealed a heterogeneous surface that contained not only PEG-derived polymers, but also hydrocarbon-based entities that are likely surface contaminants. XPS of the irradiated PEG samples indicated the emergence of different carbon species, with peak shifts suggesting the presence of sp2 carbon atoms. Analysis of the paraffinic film using XPS showed the emergence of oxygen on the surface of the sample, and also a broadening and shifting of the C1s peak, demonstrating a change in the chemistry on the surface. The paraffinic film did not dissolve in either H2O or a H2O–methanol solution, and hence the bulk of the material could not be analyzed using electrospray. However a series of oligomers was leached from the bulk material that produced ion series in the ESI-MS analyses that were identified octylphenyl ethoxylate oligomers. Upon Li ion bombardment, these shifted to a lower average molecular weight, but more importantly showed the emergence of three new ion series that are being formed as a result of radiation damage. Surface analysis of the paraffinic polymers using SIMS produced spectra that were wholly dominated by hydrocarbon ion series, and no difference was observed between unirradiated and irradiated samples. The studies demonstrate that for the PEG-based polymers, direct evidence for radiolytic scission can be observed using ESI-MS, and suggests that both radiolytic pathways and efficiencies as a function of dose should be measurable by calibrating instrument response to the small oligomeric degradation products.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Swift heavy ion irradiation effects in zirconium and hafnium carbides

The behavior of microcrystalline zirconium carbide (ZrC) and hafnium carbide (HfC) was studied under highly ionizing irradiation conditions at room temperature. The induced structural modifications were characterized via synchrotron-based X-ray diffraction experiments. Unit-cell expansion and buildup of microstrain were determined across a wide fluence range and linked to chemical compositions of the target material. The observed swelling resulting from irradiation with 198 MeV Xe ions in both carbide materials is characterized by two distinct mechanisms that operate within different fluence regimes. Unit-cell expansion initially proceeds by a direct-impact behavior that reaches saturation, followed at higher fluences by a second, linear swelling regime. The overall behavior, particularly the direct-impact regime, is similar for ZrC and HfC, with a more pronounced second defect accumulation process in HfC. Swelling in ZrC shows the same two distinct mechanisms upon irradiation with 198 MeV Xe ions and 946 MeV Au ions, but swelling induced by the lower-energy ions is greater across the entire fluence series. Accounting for the difference in energy deposition density between the two irradiation conditions reveals that the first swelling mechanism (direct-impact behavior) is likely related to the formation of more simple defects. In contrast, the second damaging mechanism at higher fluences (linear increase) cannot be fully explained by the induced energy density, and swelling remains somewhat higher for the low-velocity Xe irradiation. This may suggest that more complex defects and defect clusters are responsible for this swelling regime, with either their size and/or morphology modified at different energy densities.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Design of a separate effects MiniFuel irradiation experiment investigating microstructure evolution in high burnup UO 2

The microstructural evolution of UO 2 fuel pellets during commercial operation in light water reactors (LWRs) is known to vary significantly across the pellet radius due to spatial variations in local temperature and burnup. The primary obstacle to extending LWR refueling cycles to 24-month intervals is the susceptibility of certain high burnup fuel microstructures to fuel fragmentation, relocation, and dispersal (FFRD) during a loss of coolant accident (LOCA). Although FFRD of the high burnup structure in the rim region of a pellet is well studied, the fine fragmentation that has been observed in a second region, near the midradius of the pellet (termed the “dark zone”) following mock LOCA testing of high burnup commercial fuel rods is less understood. This paper describes the design, analysis, and execution of a separate effects MiniFuel irradiation experiment that aims to identify the specific temperature and burnup regimes under which FFRD-susceptible dark zone microstructures form. The small disc specimens (3 mm diameter by ∼0.3 mm thick) enable more precise control of the relatively uniform temperature and burnup conditions. A total of 42 specimens were fabricated with typical LWR fuel densities (∼96%–98% of theoretical density) and grain sizes (∼12 μm) and are being irradiated over a range of temperatures (600°C–1000°C) and discharge burnups (50–72 MWd/kg-U) that bound the midradius region of high burnup LWR fuel. Fuel specimens with identical 235 U enrichments were inserted in two irradiation locations in the High Flux Isotope Reactor and are currently undergoing irradiation to further evaluate the impact of rate effects (fission rate, time at temperature) on the microstructural evolution. The fuel fabrication and the thermal and neutronic simulations used for designing the experiment are detailed in this paper. A secondary objective of the experiment is to observe fission gas release (FGR) under the various irradiation conditions, and this work provides first-order predictions of FGR from all fuel specimens. The insights gained from these experiments will inform future high burnup core designs that could minimize the formation of susceptible microstructures and ultimately enable 24-month refueling cycles while minimizing the fraction of the fuel susceptible to FFRD.

FFRD↗

Plasmonic Ag nanocomposite phosphate glasses produced via γ-ray irradiation as reduction route

This paper reports on the impact of γ-ray irradiation (10, 100 kGy) on melt-quenched Ag + -doped phosphate glass and the effects of subsequent thermal processing leading to the production of plasmonic Ag nanocomposites. The γ-irradiated glasses were characterized alongside the pristine by differential scanning calorimetry (DSC), Raman spectroscopy, electron paramagnetic resonance (EPR) spectroscopy, optical absorption, and photoluminescence (PL) spectroscopy. DSC characterization showed consistent glass transition temperatures (T g ) before and after γ-irradiation whereas the crystallization temperatures tended to decrease with increasing γ-ray dose. However, a lack of alteration of the glass network structure was supported by Raman spectroscopy. Room temperature EPR spectra clearly showed the formation of phosphorus oxygen hole center (POHC) defects in the undoped host, in addition to another doublet likely associated with a P 3 defect. The presence of paramagnetic silver species encompassing Ag 2+ and 107/109 Ag 0 atoms was also indicated in the silver-activated glass together with POHC defects. Optical absorption spectra were also consistent with the presence of various radiation-induced centers. Further analyzing the glass absorption edge via Tauc plots suggested the formation of electron center (EC) defects in γ-irradiated samples wherein the silver-doped glass exhibited decreasing band gap energies with increasing γ-ray dose. The PL characterization showed the silver-related radio-PL effect was induced exhibiting broad band emission with two maxima around 500 and 625 nm stemming from various molecular Ag$^{x+}_{n}$ clusters. Emission decay analyses revealed that the longer wavelength emission exhibited slower decay. The highest radiation dose of 100 kGy however resulted in weaker emission and faster decay kinetics attributed to energy transfer between the luminescent silver species and POHC defects. Finally subjecting the γ-irradiated Ag-doped glasses to heat treatment near the T g at 490 °C led to the development of the surface plasmon resonance of Ag nanoparticles (NPs) and the vanishing of the Ag$^{x+}_{n}$ clusters luminescence. In conclusion, the presence of the matrix-related EC defects was deemed accountable for the thermally induced reduction and consequent precipitation of Ag NPs making the plasmonic glasses attractive for photonic applications such as nonlinear optics.

36 MATERIALS SCIENCE↗

Characteristics and radiolysis behavior of polyvinylchloride under accelerated proton and γ-irradiation

Here the effect of high energy protons and γ-irradiation on the structural properties, surface-energies, and toxicological properties of polyvinyl chloride (PVC) were studied due to the role PVC products play in many technologies including the nuclear industry. Accelerated 1–4 MeV protons impacting on PVC in vacuum lead to the formation of polyenyl radicals as shown by EPR and to an increase in free surface energy due to functionalization of the surface of the irradiated polymer. γ-irradiation leads to the formation of unsaturated bonds, carbonyl and hydroxyl groups as shown by IR and to the release of HCl. Correlated molecular orbital theory calculations of reaction thermodynamics were used to aid in the development of a mechanism in the absence of oxygen. The formation and accumulation of chromophores and auxochromic groups during γ-radiolysis of PVC leads to a gradual change of the initial white color of the polymer to yellow and then to brown and black with high sensitivity. A mixture of powdered PVC and silicate glue was used to determine the profile of a 60 Co γ-radiation beam on targets with a complex relief. γ-irradiated polymer does not have a local irritating effect due to a single application to the skin of mice in an adhesive mixture at a concentration of up to 5000 mg/kg. γ-radiolysis of PVC powder in air with a dose of up to 1400 kGy does not affect its acute toxicity when administered intragastrically to BDF1 mice. PVC and its γ-irradiated analogs are non-toxic at doses ≤5000 mg/kg.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗