Dielectric, ferromagnetic and maganetoelectric properties of BaTiO{sub 3}–Ni{sub 0.7}Zn{sub 0.3}Fe{sub 2}O{sub 4} composite ceramics
Graphical abstract: - Highlights: • The lead-free ME ceramic composites BaTiO{sub 3}–Ni{sub 0.7}Zn{sub 0.3}Fe{sub 2}O{sub 4} were successfully synthesized. • The composites showed high dielectric constant and low dielectric loss. • The composite with 30% NiZn ferrite presented good soft magnetic properties and ME performance. - Abstract: Lead-free magnetoelectric composite ceramics (1 − x)BaTiO{sub 3}–xNi{sub 0.7}Zn{sub 0.3}Fe{sub 2}O{sub 4} (x = 0.15, 0.3, 0.45) were successfully prepared by conventional oxide ceramic process. The tetragonal perovskite BaTiO{sub 3} and cubic spinel Ni{sub 0.7}Zn{sub 0.3}Fe{sub 2}O{sub 4} were confirmed by X-ray diffraction. The dielectric behaviors of all composite samples show a normal response to the increasing measurement frequency and Ni{sub 0.7}Zn{sub 0.3}Fe{sub 2}O{sub 4} ferrite content. Well defined ferromagnetic hysteresis loops and obvious magnetoelectric coupling effect are observed in the composite ceramics. The influence of applied dc bias magnetic field and Ni{sub 0.7}Zn{sub 0.3}Fe{sub 2}O{sub 4} ferrite content on the magnetoelectric coupling responding voltage is investigated. The strongest peak magnetoelectric coupling voltage coefficient is 124 μV/cm Oe when x = 0.3, which corresponds to the maximum magnetoelectric coupling responding voltage of 200 μV.