Mechanical Properties of Niobium Cavities

The mechanical stability of bulk Nb cavity is an important aspect to be considered in relation to cavity material, geometry and treatments. Mechanical properties of Nb are typically obtained from uniaxial tensile tests of small samples. In this contribution we report the results of measurements of the resonant frequency and local strain along the contour of single-cell cavities made of ingot and fine-grain Nb of different purity subjected to increasing uniform differential pressure, up to 6 atm. Measurements have been done on cavities subjected to different heat treatments. Good agreement between finite element analysis simulations and experimental data in the elastic regime was obtained with a single set of values of Young’s modulus and Poisson’s ratio. The experimental results indicate that the yield strength of medium-purity ingot Nb cavities is higher than that of fine-grain, high-purity Nb.

36 MATERIALS SCIENCE↗

Nano-Composite Material Development for 3-D Printers

Graphene possesses excellent mechanical properties with a tensile strength that may exceed 130 GPa, excellent electrical conductivity, and good thermal properties. Future nano-composites can leverage many of these material properties in an attempt to build designer materials for a broad range of applications. 3-D printing has also seen vast improvements in recent years that have allowed many companies and individuals to realize rapid prototyping for relatively low capital investment. This research sought to create a graphene reinforced, polymer matrix nano-composite that is viable in commercial 3D printer technology, study the effects of ultra-high loading percentages of graphene in polymer matrices and determine the functional upper limit for loading. Loadings varied from 5 wt. % to 50 wt. % graphene nanopowder loaded in Acrylonitrile Butadiene Styrene (ABS) matrices. Loaded sample were characterized for their mechanical properties using three point bending, tensile tests, as well as dynamic mechanical analysis.

36 MATERIALS SCIENCE↗

Structural health monitoring of compression connectors for overhead transmission lines

Two-stage aluminum conductor steel-reinforced (ACSR) compression connectors are extensively used in US overhead transmission lines. The connectors are made by crimping a steel sleeve onto a steel core and an aluminum sleeve over aluminum conductive strands. The connectors are designed to operate at temperatures up to 125 C, but their performance is increasingly degrading because of overloading of lines. Currently, electric utilities conduct routine line inspections using thermal and electrical measurements. However, information about the structural integrity of connectors cannot be obtained. In this work, structural health monitoring (SHM) of compression connectors was studied using electromechanical impedance (EMI) analysis. Lead zirconate titanate (PZT)-5A was identified as a smart material for SHM. A flexible high-temperature bonding layer was used to address challenges in PZT integration due to a significant difference in the coefficients of thermal expansion of PZT and the aluminum substrate. The steel joint on the steel core was investigated because it is responsible for the ultimate tensile strength of the connector. Tensile testing was used to create structural damage to the joint, or steel core pullout, and thermal cycling introduced additional structural perturbations. EMI measurements were conducted between the tests. The root mean square deviation (RMSD) of EMI was identified as a damage index. The use of steel joints has been shown to enable SHM under simulated conditions. The EMI signature is sensitive to variations in structural conditions. RMSD can be correlated to the structural health of a connector and has potential for use in the SHM and structural integrity evaluation.

compression connectors↗

EVALUATION OF SPECIFICATION RANGES FOR CREEP STRENGTH ENHANCED FERRITIC STEELS

Creep Strength Enhanced Ferritic Steels (CSEF) such as Gr. 91, 911, 92, and 122 require a fully martensitic structure for optimum properties, mainly good creep strength. However, broad chemical compositional ranges are specified for these steel grades which can strongly influence the microstructures obtained. In this study, we have produced chemical compositions within the specification ranges for these alloys which intentionally cause the formation of ferrite or substantially alter the lower intercritical temperatures (A1) so as to affect the phase transformation behavior during tempering. Thermodynamic modeling, thermo-mechanical simulation, tensile testing, creep testing, and microstructural analysis were used to evaluate these materials. The results show the usefulness of thermodynamic calculations for setting rational chemical composition ranges for CSEF steels to control the critical temperatures, set heat-treatment temperature limits, and eliminate the formation of ferrite.

Shingledecker, John P↗

Development at ANL of a Copper-brazed Joint for the Coupling of the Niobium Cavity End Wall to the Stainless Steel Helium Vessel in the Fermilab SSR1 Resonator

In order to reduce the sensitivity of the Fermilab SSR1 resonator to helium pressure variations, it was concluded that the cavity and helium vessel end-walls needed to be structurally coupled by means of a transition ring. With the materials t o be connected being Niobium and Stainless Steel, it was decided to utilize the same technology already developed for the cavity flanges which consists of a furnace-brazed joint utilizing oxygen-free electrolytic copper. Small-scale and full-scale annular samples have been constructed at Argonne National Laboratory and subject to tensile tests, thermal cycling and visual inspections to qualify the joint. The transition ring is electron-beam welded to the cavity and TIG welded to the helium vessel, the pro cess is explained in detail.

43 PARTICLE ACCELERATORS↗

Crack Initiation Behavior of Cold-Worked Alloy 690 in Simulated PWR Primary Water - Role of Starting Microstructure, Applied Stress and Cold Work on Precursor Damage Evolution

Long-term stress corrosion crack (SCC) initiation behavior in Alloy 690 is being evaluated by constant load tensile testing in simulated pressurized water reactor primary water. Seven commercial Alloy 690 heats with different starting microstructures and cold-work levels are being tested at either 90% or 100% of the material yield stress. Previous studies have revealed grain boundary (GB) cavity formation after 7,110 to 9,220 hours of exposure in certain thermally treated (TT) Alloy 690 heats in highly cold-worked (CW) conditions, serving as precursors to intergranular cracks. This paper summarizes the new characterization results for the evolution of GB cavities in four Alloy 690TT heats in 21% and 31%CW conditions loaded at yield stress after 18,400 hours of exposure. Link-up of GB cavities has led to formation of long internal creep cracks, resulting in crack initiation detected by direct current potential drop in a highly CW Alloy 690TT heat with uniform, semi-continuous distribution of small GB carbides. In comparison, highly CW materials featuring larger and more widely spaced GB carbides did not show a significant increase in GB cavity density or size. Quantitative assessments were performed on GB cavity evolution in highly CW specimens for two Alloy 690TT heats demonstrating the strong dependence of GB cavity evolution on applied stress and starting GB microstructure.

Zhai, Ziqing↗

Ultrasonic Additive Manufacturing

Ultrasonic additive manufacturing (UAM) is a solid-state hybrid manufacturing technique that leverages the principles of ultrasonic welding, mechanized tape layering, and computer numerical control (CNC) machining operations to create three-dimensional metal parts. This article begins with a discussion on the process fundamentals and process parameters of UAM. It then describes metallurgical aspects in UAM. The article provides a detailed description of a wide range of mechanical characterization techniques of UAM, namely tensile testing, peel testing, and pushpin testing. The article ends with information on sensor embedding.

Niyanth S, Niyanth↗

Process Robustness of Friction Stir Dovetailing of AA7099 to Steel with In Situ AA6061 Interlayer Linking

Rolled homogeneous armor (RHA) steel was joined to aluminum alloy AA7099-T7451 with an interlayer of AA6061-T651 by single-pass friction stir dovetailing (FSD). The evolution of the AA7099/AA6061 and AA6061/steel interfacial microstructures and mechanical properties of the joints were examined. The AA6061 interlayer prevented Zn migration from the AA7099 to the steel during FSD and inhibited formation of brittle, Zn-rich, Fe-Al intermetallic compounds within the joint. The flow of the dissimilar aluminum alloys at the interface was controlled with a partially threaded friction stir welding pin and a dovetail geometric configuration optimized in previous work. The process robustness was explored to establish parameter windows by elucidating parametric effects on the relationship between process conditions and the joint’s microstructure and mechanical properties. Ranges of process forge force (50–70 kN) and interface temperature (475°C–515°C) consistently yielded joints with adequate performance. The load-carrying capacity in lap shear tensile tests was 2025 ? 100 N/mm.

Friction Stir Dovetailing, FSW, AA7099, AA6061, Ro↗

The Role of Interface in Additively Manufactured Interpenetrating Composites

Additively Manufactured Interpenetrating Composites (AMIPCs) are a relatively new metal-metal chain composite in development for use in high energy absorption systems. In this system, reinforcing phase of additively manufactured continuous lattice configurations 316L austenitic stainless-steel is in melt infiltrated with a matrix phase of A356 aluminum-silicon casting alloy. Measurements and observations of this material system have shown that weakly bonded or open/porous interface between the reinforcement and matrix phases exhibits dramatically different mechanical properties of AMIPCs, which is not currently well understood. In this work, Finite Element Models (FEM) are used to model the effects of interfaces between the composite phases. Mechanical tensile tests measurements of various composite volume fractions and varying degrees of casting infiltration are also examined and used to show consistency with the FEM results. The outcome provides insight into material design criteria and performance predictions for new hybrid material systems with exceptional damage tolerance.

Allen, Jason↗

Design, Creep Performance and Deformation Behavior of an Eta-Phase Strengthened Nickel-Base Alloy for A-USC Power Plant Applications

By utilizing computational thermodynamics in a Design of Experiments approach, it was possible to design and manufacture nickel-base superalloys that are strengthened by the eta phase (Ni3Ti), and that contain no gamma prime (Ni3Al,Ti). The compositions are similar to Nimonic 263, and should be cost-effective, and have more stable microstructures. By varying the aging temperature, the precipitates took on either cellular or Widmanstätten morphologies. The Widmanstätten-based microstructure is thermally stable at high temperatures, and was found to have superior ductility, so development efforts were focused on that microstructure. High temperature tensile test and creep test results indicated that the performance of the new alloys was competitive with Nimonic 263. SEM and TEM microscopy were utilized to determine the deformation mechanisms during creep.

36 MATERIALS SCIENCE↗

Design stress evaluation based on strain-rate sensitivity analysis for nickel alloys used in the very-high temperature nuclear system

Both Alloy 617 and Alloy 230 have been considered the most promising structural materials for the Very High Temperature Reactor (VHTR). In this study, mechanical properties of both alloys were examined by performing tensile tests at three different strain rates and at temperatures up to 1000 deg.C. This range covers time-dependent (plasticity) to time-independent (creep) deformations. Strain-rate sensitivity analysis for each alloy was conducted in order to approximate the long-term flow stresses. The strain-rate sensitivities for the 0.2% flow stress were found to be temperature independent (m {approx_equal} 0) at temperatures ranging from room temperature to 700 deg.C due to dynamic strain aging. At elevated temperatures (800-1000 deg.C), the strain-rate sensitivity significantly increased (m > 0.1). Compared to Alloy 617, Alloy 230 displayed higher strain-rate sensitivities at high temperatures. This leads to a lower estimated long-term flow stresses. Results of this analysis were used to evaluate current American Society of Mechanical Engineers (ASME) allowable design limits. According to the comparison with the estimated flow stresses, the allowable design stresses in ASME B and PV Code for either alloy did not provide adequate degradation estimation for the possible long-term service life in VHTR. However, rupture stresses for Alloy 617, developed in ASME code case N-47-28, can generally satisfy the safety margin estimated in the study following the strain-rate sensitivity analysis. Nevertheless, additional material development studies might be required, since the design parameters for rupture stresses are constrained such that current VHTR conceptual designs cannot satisfy the limits. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Overview of the experiments performed with Russian claddings at MTA EK

The mechanical and corrosion behavior of the Russian-type zirconium cladding alloy E110, predominantly used in VVERs, has been investigated for many decades. The recent commercialization of a new alloy E110G, produced on a sponge zirconium basis, gave the opportunity to compare the mechanical properties of the old E110 and the new E110G fuel claddings. The mechanical experiments performed with samples from both claddings in MTA EK including axial and tangential (ring) tensile tests at 20, 150 and 300 Celsius degrees. The chosen geometries for the tests were modelled using finite element method. Due to the anisotropy of the cladding tubes the axial yield strength was 6% higher than the tangential. The yield strength of the E110G alloy was 12% higher than for the E110 claddings at ambient temperature, but this difference decreased to 5% at 300 C. degrees. Some samples underwent chemical or thermal treatments and the effects of these were evaluated. These treatments were slight oxidation in steam at 800 C. degrees up to 3 ECR%, hydridation at 600 C. degrees up to 400 ppm, and heat treatment in argon atmosphere at temperatures between 600 and 1000 C. degrees. The results confirm that the heat treatment has more significant effect on the yield strength of the claddings than the chemical treatments. While the yield strength of the oxidized samples was slightly higher, when combined with the data from the heat treatment at 800 C. degrees, the oxidation itself seems to have lowered the yield strength as the thickness of the metal decreased. The hydridation of the cladding samples did not change the yield strength and the samples remained ductile even at room temperature. The thermo-mechanical creep of the two cladding alloys was also investigated. Biaxial and uniaxial creep experiments were performed with 100 mm long cladding tubes. In the biaxial test, samples of both alloys were pressurized with argon to 5, 7.5 and 10 MPa at 500 C. degrees and the test lasted till the depressurization of the tubes. The uniaxial creep was measured at 300 and 500 C. degrees in the axial direction and constant stress was applied using weights. This stress was 14.8 and 27.7 MPa at 300 C. degrees and 3.7 and 6.5 MPa at 500 C. degrees. The elongation and diametrical change of the samples were measured using different methods. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Dispersion of Nano-Sized Oxide Particles in Ni-based Alloy

High temperature materials with a good resistance to oxidation or corrosion are crucial for the Generation IV nuclear system such as VHTR (Very High Temperature Reactor). While several commercial Ni-based high temperature alloys have been among the candidate ones for the IHX (intermediate heat exchanger) or HGD (hot gas duct) of VHTR, they disclose their insufficiency for the application to the anticipated outlet temperature range such as 900 deg. C or above. Unless the operating temperature is significantly lowered and the performance of the system drops in consequence, a breakthrough in the candidate materials for the key components shall be necessary for the realization of the system. Feasibility for the oxide dispersion strengthening (ODS) of Ni-based alloys was studied by fabrication of alloy 617-base ODS alloy. Alloy 617 powders were mechanically alloyed (MA) with 0.3 wt% Y{sub 2}O{sub 3} powders of around 30 nm in diameter using a horizontal ball mill (ZoZ CM 08). After degassing and canning procedure, MA powders were hot extruded. Extruded alloy samples were tensile tested at high temperatures as well as at room temperature. Also high temperature creep rupture tests were conducted at 950 deg. C in air under 20 and 25 MPa, respectively. The behavior of oxide particles within the Ni-based alloy matrix was investigated by mechanical alloying of Ni- Cr-Fe ternary alloy powders and pure Ni powders with oxide particles, respectively. Oxide such as Y{sub 2}O{sub 3}, Cr{sub 2}O{sub 3}, HfO{sub 2}, ZrO{sub 2}, TiO{sub 2}, La{sub 2}O{sub 3} were chosen from the thermodynamic point of view as the first stable candidates from more than twenty oxides, nitrides and carbides. The behavior of oxide particle within the MA powder matrix along with the temperature was characterized by using high temperature XRD (X-ray Diffractometer) and (HR)TEM (High Resolution Transmission Electron Microscope). Creep rupture tests of the ODS alloy samples at 950 deg. C showed one order of magnitude lower creep rates than those of the corresponding alloy. (authors)

36 MATERIALS SCIENCE↗

Investigation of the Hydrogen Embrittlement of API 5L Natural Gas Pipeline Steels

Hydrogen ions produced during corrosion or through hydrogen blending into natural gas pipelines can lead to the degradation of ductility of metals used in these transmission pipelines. The effect of hydrogen on the mechanical properties of pipeline steels was studied for three grades of API 5L steels: X56, X65, and X100. These steels are either commonly used in or considered for use in natural gas transmission pipelines which are being considered for use in hydrogen blending. These steels were subjected to constant strain rate tensile testing after charging with electrochemically generated hydrogen. This presentation reports on work to extend the life of the natural gas pipeline network via understanding the effect of hydrogen embrittlement induced by corrosion processes.

Teeter, Lucas↗

INFLUENCE OF SUPPLEMENTARY ARGON GAS SHIELDING ON THE MICROSTRUCTURE AND MECHANICAL BEHAVIOR OF SS316L ADDITIVELY MANUFACTURED BY DIRECTED ENERGY DEPOSITION

The dissolution of atmospheric gases into parts additively manufactured by directed energy deposition (DED) has long been of concern, and stock shielding solutions have usually proven inadequate at fully removing atmospheric gases from weld beads. The objective of this work was to design a new supplementary argon gas shroud for a specific DED printer and evaluate its effect on microstructure and macroscopic properties of SS316L and the potential for printing more reactive metals such as Ti-6Al-4V. This was investigated by printing four SS316L sample blocks, two with and two without the shroud, each printed in two different orientations. These samples were subsequently evaluated with inert gas fusion (IGF), SEM/EDS imaging, and tensile tests. The shroud reduced oxygen content by 0.019-0.031%, and SEM imaging revealed fewer oxide inclusions. A more dramatic reduction of 0.13% oxygen and 0.171% nitrogen was observed by the inert gas fusion of Ti-6Al-4V samples. Overall, the results indicated the shroud was successful at reducing atmospheric gas uptake within the print region and may enable the printing of reactive metal powders in DED systems.

Helvie, Kyle↗

Development of Irradiation hardening of Unalloyed and ODS molybdenum during neurtron irradiation to low doses at 300C and 600C

Unalloyed molybdenum and Oxide Dispersion Strengthened (ODS) molybdenum were irradiated at 300 C and 600 C in the high flux isotope reactor (HFIR) to neutron fluences of 0.2, 2.1, and 24.3 x 10{sup 24} n/m{sup 2} (E > 0.1 MeV), producing damage levels of 0.01, 0.1 and 1.3 Mo-dpa. Hardness measurements, electrical resistivity measurements, tensile testing, and Transmission Electron Microscopy (TEM) were used to assess the defect structure. Irradiation hardening was evident even at a damage level of 0.01 dpa resulting in a significant increase in yield stress, decrease in ductility, and elevation of the Ductile-to-Brittle Transition Temperature (DBTT). The observed size and number density of voids and loops as well as the measured irradiation hardening and electrical resistivity were found to increase sub-linearly with fluence over the range of exposure investigated. This supports the idea that the formation of the extended defects that produce irradiation hardening in molybdenum are the result of a nucleation and growth process rather than the formation of sessile defects directly from the displacement damage cascades. The formation of sessile defect clusters in the displacement cascade would be expected to result in a linear fluence dependence for the number density of defects followed by saturation at fluences less than 1-dpa. This conclusion is supported by Molecular Dynamics (MD) simulations of cascade damage which do not reveal large clusters forming directly as a result of the short-term collapse of the cascade. The finer grain size for the unalloyed Mo and ODS Mo compared to Low Carbon Arc Cast molybdenum results in slightly less irradiation hardening and slightly lower DBTT values. The unalloyed molybdenum used in this work had a low impurity interstitial content that correlates with a slightly lower void size and void number density, less irradiation hardening and lower change in electrical resistivity in this fluence range than is observed for ODS Mo. Although the differences are relatively subtle, this result does suggest that high purity can result in slightly improved resistance to irradiation embrittlement in molybdenum at low fluences.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

A PROPOSED METHODOLOGY FOR STRAIN BASED FAILURE CRITERIA

This paper proposes an alternative methodology to determine the failure criteria for use in dynamic simulations of radioactive material shipping packages in the events of hypothetical accident conditions. The current stress failure criteria defined in the Nuclear Regulatory Guide 7.6 [1] and the ASME Code, Section III, Appendix F [2] for Level D Service Loads are based on the ultimate strength of uniaxial tensile test specimen rather than on the material fracture in the state of multi-axial stresses. On the other hand, the proposed strain-based failure criteria are directly related to the material failure mechanisms in multi-axial stresses. In addition, unlike the stress-based criteria, the strain-based failure criteria are applicable to the evaluation of cumulative damages caused by the sequential loads in the hypothetical accident events as required by the Nuclear Regulatory Guide 7.8 [4].

42 ENGINEERING↗