At least 1,639 records · Page 91

Kinetic Investigations of SiMn Slags From Different Mn Sources

The kinetics of MnO and SiO 2 reduction were investigated for Silicomanganese (SiMn) slags using a Thermogravimetric analysis (TGA) between 1773 K and 1923 K (1500 °C and 1650 °C) under CO atmospheric pressure. The charge materials were based on Assmang ore and HC FeMn Slag. Rate models for MnO and SiO 2 reduction were applied to describe the metal-producing rates, as shown by the following equations: r MnO =k MnO ×A×(a MnO -((a Mn )/(K{sub T})))r SiO 2 =k SiO 2 ×A×(a SiO 2 -((a Si )/(K T ))).The results show that the choice of raw materials in the charge considerably affected the reduction rate of MnO and SiO 2 . The highest reduction rate was found to be from charges using HC FeMn slag. The difference in the driving forces was insignificant among the SiMn slags, and the similar slag viscosities could not explain the different reduction rates. Instead, the difference is attributed to small amounts of sulfur and the amount of iron in the charge. In addition, the rate models were applicable to describe the reduction of MnO and SiO 2 in SiMn slags.

36 MATERIALS SCIENCE↗

Manufacturing of Dysprosium-Iron Alloys by Electrolysis in Fluoride-Based Electrolytes. Electrolysis in a Laboratory-Scale Cell

Electrolytic production of light rare earth elements and rare earth alloys with transition elements takes place in a fluoride-based electrolyte using rare earth oxides as raw material. The optimization of this method, mainly in terms of the energy efficiency and environmental impact control, is rather challenging. Anode effects, evolution of fluorine-containing compounds and side cathode reactions could largely be minimized by good control of the amount of rare earth oxide species dissolved in the fluoride-based electrolyte and their dissolution rate. The Dy{sub 2}O{sub 3} feed rate needed for stable cell operation was studied by following up the anode voltage and gas analysis. On-line analysis of the cell off-gases by FTIR showed that the electrochemical reaction for the formation of Dy-Fe alloy gives mainly CO gas and that CF{sub 4} is starting to evolve gradually at anode voltages of ca. 3.25 V. The limiting current density for the discharge of the oxide ions at the graphite anode was in the range of 0.1 to 0.18 A cm{sup −2} at dissolved Dy{sub 2}O{sub 3} contents of ca. 1 wt pct. Modeling of the laboratory cell reactor was also carried out by implementing two models, i.e., an electrical model simulating the current density distribution at the electrodes and a laminal bubbly flow model that explains the electrolyte velocity induced by gas bubble production at the anode.

36 MATERIALS SCIENCE↗

Viscosity of TiO{sub 2}-FeO-Ti{sub 2}O{sub 3}-SiO{sub 2}-MgO-CaO-Al{sub 2}O{sub 3} for High-Titania Slag Smelting Process

The present study demonstrates the dependence of viscosity on chemical composition and temperature of high-titania slag, a very important raw material for producing titanium dioxide. The results indicated that completely molten high-titania slag exhibits a viscosity of less than 1 dPa s with negligible dependence on temperature. However, it increases dramatically with decreasing temperature slightly below the critical temperature, i.e., the solidus temperature of the slag. Above the critical temperature, the slag samples displayed the same order of viscosity at 0.6 dPa s, regardless of their compositional variation. However, the FeO, CaO, and MgO were confirmed to decrease viscosity, while SiO{sub 2} and Ti{sub 2}O{sub 3} increase it. The apparent activation energy for viscosity-temperature relation and liquidus temperature based on experiments and thermodynamic calculations are also presented. Conclusively, the critical temperatures of the slags are on average 15 K below their corresponding calculated liquidus temperatures. The increase in FeO content was found to considerably lower the critical temperature, while the increase in both Ti{sub 2}O{sub 3} and TiO{sub 2} contents increases it. The main phases of the slag in solid state, as indicated by X-ray diffraction, are (Fe, Mg){sub x}Ti{sub y}O{sub 5} (x + y = 3, pseudobrookite) and rutile.

36 MATERIALS SCIENCE↗

Zinc Removal from Basic Oxygen Steelmaking Filter Cake by Leaching with Organic Acids

The dust generated from the basic oxygen steelmaking (BOS) process is a waste material mainly containing iron that cannot be recycled owing to its high zinc content. In this study, the leaching effects of different organic acids are compared, with the aim of determining an acid that selectively leaches and removes zinc from BOS dust, so that the waste material can be recycled into ironmaking and steelmaking processes in order to substitute part of the raw materials of steelmaking. The dust used in this study was scrubbed and collected in the form of a filter cake. The acids tested were oxalic, citric, acetic, propionic, butyric, and valeric acids. Butyric acid was found to be the most effective, with a high zinc extraction level of 49.7 pct and a low iron level of only 2.5 pct. Oxalic acid was the least effective leaching reagent for both zinc and iron extractions, owing to the formation of zinc and iron oxalate precipitates following metal dissolution. The filter cake and leached residues were characterized by chemical analysis, X-ray diffraction, X-ray photoelectron spectroscopy, and scanning electron microscopy with energy dispersive spectroscpopy.

36 MATERIALS SCIENCE↗

Influence of Iron Ore Addition on Metallurgical Reaction Behavior of Iron Coke Hot Briquette

Utilization of iron coke hot briquette (ICHB) has been considered to be one effective countermeasure to achieve low-carbon blast furnace. Before its actual application, a series of extensive fundamental investigations on the ICHB are required. In this study, the influence of iron ore addition on the metallurgical reaction behavior of ICHB made from carbonizing coal–iron ore composite agglomeration were investigated based on Chinese raw material conditions, and the corresponding mechanisms were revealed. The results show that the addition of iron ore concentrate leads to the degradation of the compressive strength and drum strength of ICHB, but they are maintained at a relatively high level. Furthermore, by increasing the addition ratio of iron ore from 0 to 20 pct, the density of ICHB is enhanced from 1413 to 1637 kg/m{sup 3}, and the porosity is increased from 8.03 to 12.84 pct, and the optical texture index (OTI) is reduced from 58.1 to 25.3. The phase composition of ICHB mainly consists of C, Fe, SiO{sub 2}, Fe{sub 3}O{sub 4}, and FeO after the addition of the iron ore concentrate. Moreover, the reactivity of ICHB is accelerated from 46.74 to 69.54 pct due to the catalytic effects of metallic iron and iron oxide, which worked as oxygen transfer carriers, while the post-reaction strength is reduced from 74.08 to 36.81 pct. In addition, the starting temperature of the ICHB gasification reaction is decreased remarkably from 919 °C to 839 °C. The activation energy (E{sub a}) for the gasification reaction under nonisothermal conditions is reduced from 312.78 to 249.83 kJ/mol, and the preexponential factor (A) shows a decreasing trend as well. Simultaneously, E{sub a} and A display the kinetic compensation effect and present a good linear relationship.

36 MATERIALS SCIENCE↗

Mechanism of Ball Milling Effect on Carbothermic Reduction of Industrial Magnesia by Coke

Mechanical milling always improves the chemical reaction rate in the metallurgy process. The experiment proved that ball milling treatment on raw materials, including industrial magnesia, metallurgical coke, and fluoride calcium, could increase greatly the reaction rate of magnesia. The reaction samples and residues were analyzed by particle size measurement, X-ray diffraction (XRD) analysis, Raman spectroscopy analysis, scanning electron microscope (SEM), and transmission electron microscope (TEM). The results suggested that the positive effect of ball milling on the reaction rate came from three aspects. Ball milling could decrease magnesia particle size and peel coke into graphite sheets to enlarge their contact surface. Meanwhile, ball milling could slightly destroy the crystal grain surface of magnesia and decrease the crystallization of graphite. The nanometer-scale magnesia particles and graphite sheets would stably and strongly attract together after a longer time ball milling. The possible evolution of the particles during ball milling was given, which explained the mechanism of the ball milling effect on the carbothermic reduction of industrial magnesia by coke.

36 MATERIALS SCIENCE↗

Low-Temperature Synthesis of VB{sub 2} Nanopowders by a Molten-Salt-Assisted Borothermal Reduction Process

Vanadium diboride (VB{sub 2}) powders with low oxygen content are prepared via a molten-salt-assisted borothermal reduction reaction at 1123 K to 1273 K (850 °C to 1000 °C) using V{sub 2}O{sub 3} and boron powders as the raw materials. The effects of the amount of molten salt and reaction temperature on the phase transition and morphology of the final products are investigated. The results reveal that the addition of molten salt is beneficial for decreasing both the synthesis temperature and particle size of the final products. When the mass ratio of NaCl to reactants is 0.75:1, the VB{sub 2} powders prepared at 1173 K (900 °C) have a particle size lower than 100 nm. Too little or too high molten salt addition has a negative impact on the preparation of the VB{sub 2} powders. Furthermore, the reaction temperature has an important impact on the morphology and purity of the VB{sub 2} particles. An appropriate reaction temperature (1173 K (900 °C)) is beneficial for controlling the size of the VB{sub 2} particles in the order of nanoscale and improving the quality of the VB{sub 2} powders.

36 MATERIALS SCIENCE↗

A Thermodynamic Model Toward the Comprehension of Ferrous Burden Softening and Melting Using FactSage Macro-Processing

The softening and melting properties of iron-bearing materials play a decisive role in the formation of the cohesive zone, which greatly affects blast furnace gas flow distribution and heat-transfer efficiency. To improve the understanding regarding the evolution of condensed phases during reduction, softening, and melting, a thermodynamic model has been developed using FactSage™ thermodynamic software and macro-processing. The model was constructed using a series of equilibrium stages and splitters to determine flow directions of streams and to consider kinetic inhibitions. For all iron-bearing materials studied, the methodology proposed for modeling was capable of obtaining reduction degrees in very good agreement to its experimental data. The evolution of solid phases was qualitatively comparable to the available literature, with Fayalite, Kirschsteinite, Melilite, and FeO as the main solid phases in equilibrium before slag formation. The comparison between the profiles of the calculated slag mass fraction and the experimental pressure drop showed a close relation between these properties. Moreover, the level of heterogeneity of each raw material may play a significant role in the interpretation of its results.

36 MATERIALS SCIENCE↗

Vacuum Pressureless Sintering of Ti-6Al-4V Alloy with Full Densification and Forged-Like Mechanical Properties

Ti-6Al-4V ingots with a nearly 100% density, fine and homogeneous basket-weave microstructure, and better comprehensive mechanical properties (UTS = 935 MPa, Y.S. = 865 MPa, El. = 15.8%), have been manufactured by vacuum pressureless sintering of blended elemental powders. Coarse TiH{sub 2} powder, Al powder (2, 20 μm), V powder, and Al-V master alloy powder were used as raw materials to produce different powder mixtures (D{sub 50} = 10 μm). Then, the compacts made by cold isostatic pressing were consolidated by different sintering curves. A detailed investigation of different as-sintered samples revealed that a higher density can be obtained by generating transient molten Al in the sintering process. Coarse Al powder and a rapid heating rate under the melting point of Al contribute to molten Al formation. The presence of temporary liquid phase changes the sintering mechanism, accelerating the sintering neck formation, improving sinterability of the powder mixtures. Density of 99.5% was achieved at 1150 °C, which is markedly lower than the sintering temperatures reported for conventional blended elemental powder metallurgy routes. In addition, low interstitial content, especially for oxygen (0.17 wt.%), is obtained by strict process control.

36 MATERIALS SCIENCE↗

Synthesis and Tribological Performance of Different Particle-Sized Nickel-Ion-Exchanged α-Zirconium Phosphates

Nickel-ion-exchanged α-zirconium phosphate (Ni-α-ZrP) was synthesized by a mild hydrothermal synthesis method. Different raw material ratios (NaF/H{sub 3}PO{sub 4}/Ni(CH{sub 3}COO){sub 2}·4H{sub 2}O) influence the particle size of the Ni-α-ZrP samples. The grain size could be controlled and distributed from 20 to 600 nm. Ni-α-ZrP was evaluated as an additive in lithium grease in a four-ball test. A 3.0 wt.% addition of Ni-α-ZrP to lithium grease yielded maximum non-seizure load values of 1235 N, and the wear scar diameter on the lower balls is 0.42 mm at 294 N. Compared with smaller particles, the addition of Ni-α-ZrP with a larger particle size to grease yields a better load-carrying capacity.

36 MATERIALS SCIENCE↗

Microstructural and Property Evolution of Continuous Columnar-Grained Polycrystalline Copper during Extreme Plastic Deformation at Room Temperature

An extreme extensibility with a true strain of 11.12 has been obtained for continuous columnar-grained (CCG) polycrystalline copper at room temperature, which was cold-drawn from a 10-mm-diameter as-cast rod into a 38.5-μm-diameter ultra-fine wire without any intermediate softening heat treatment. During the extreme plastic deformation, the ultimate tensile stress increased from 140 MPa for as-cast CCG copper to 525 MPa for the deformed sample at a true stain of 11.12, while the relative electrical conductivity maintained a high value of 97.6% IACS. On this basis, CCG copper is an excellent raw material for the fabrication of ultra-fine wires with both high strength and high electrical conductivity. The original columnar grains experienced grain subdivision and formed fibrous grains along the drawing direction with a fibrous longitudinal morphology and curly transverse microstructure at medium to high strain. The subdivision of the fibrous grains then went on as the extreme plastic deformation continued. Large amounts of strain-induced boundaries and microstructural refinement facilitated the storage of abundant glide dislocations created by extreme plastic deformation. Thus, extreme plastic extensibility can be achieved through continuous work hardening of CCG copper.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of a Multiphase FeCrCuMnNi High-Entropy Alloy

A FeCrCuMnNi high-entropy alloy was produced using vacuum induction melting, starting from high-purity raw materials. The microstructure and mechanical properties of the as-cast FeCrCuMnNi alloy were studied, considering x-ray diffraction (XRD), scanning electron microscopy, and hardness and tensile tests. XRD results revealed the existence of two FCC phases and one BCC phase. Microstructural evaluation illustrated that the as-cast alloy has a typical cast dendritic structure, where dendrite regions (BCC) were enriched in Cr and Fe. Interdendritic regions were saturated with Cu and Ni and revealed G/B(T) {110} 〈111〉 and Brass {110} 〈112〉 as the major texture components. The produced alloy revealed an excellent compromise in mechanical properties due to the mixture of solid solution phases with different structures: 300 HV hardness, 950 MPa ultimate tensile strength and 14% elongation. Microhardness test results also revealed that the BCC phase was the hardest phase. The fracture surface evidenced a typical ductile failure. Furthermore, heat treatment results revealed that phase composition remained stable after annealing up to 650 °C. Phase transformation occurred at higher temperatures in order to form more stable phases; therefore, FCC2 phase grew at the expense of the BCC phase.

36 MATERIALS SCIENCE↗

New waste based clinkers: Belite and lime formulations

This work describes the formulation of new belite-based (CR2) and lime-based (CR3) cementitious materials derived from industrial wastes, such as sludges (generated in the Al-anodising and surface coating industrial processes, potable water filtration/cleaning operations and in marble sawing processes) and foundry sand. Powder mixtures were prepared and fired at different temperatures. For comparison, similar formulations were prepared with pre-treated and commercially available natural raw materials and processed in similar conditions. The thermal process was followed by differential scanning calorimetry (DSC) and high-temperature powder X-ray diffraction (HT-XRD) studies. The CR2 clinker was found to contain belite as the main cementitious phase, the main polymorph being identified by NMR. The CR3 clinker contained common cementitious phases, such as C{sub 3}A and C{sub 3}S, but free lime and calcium aluminium oxide sulphates were also identified by high temperature XRD and NMR. Then the corresponding cement was prepared and the evolution of the mechanical strength with time was evaluated. The lime-based cement obtained from wastes shows a stronger hardening character than the standard material, which tends to show dusting phenomena due to the presence of a reasonable amount of free lime (as the result of its expansive reaction with ambient moisture). Some fluxing impurities (e.g. alkalis) present in the waste materials improve the overall reactivity of the mixture and induces the combination of the lime in CR3. Raman, XPS and FIB techniques were used to fully characterise the aged cements.

36 MATERIALS SCIENCE↗

Sustainable cement production-present and future

Cement will remain the key material to satisfy global housing and modern infrastructure needs. As a consequence, the cement industry worldwide is facing growing challenges in conserving material and energy resources, as well as reducing its CO{sub 2} emissions. According to the International Energy Agency, the main levers for cement producers are the increase in energy efficiency and the use of alternative materials, be it as fuel or raw materials. Accordingly, the use of alternative fuels has already increased significantly in recent years, but potential for further increases still exists. In cement, the reduction of the clinker factor remains a key priority: tremendous progress has already been made. Nevertheless, appropriate materials are limited in their regional availability. New materials might be able to play a role as cement constituents in the future. It remains to be seen to what extent they could substitute Portland cement clinker to a significant degree.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Microstructural and compositional change of NaOH-activated high calcium fly ash by incorporating Na-aluminate and co-existence of geopolymeric gel and C-S-H(I)

This study explores the reaction products of alkali-activated Class C fly ash-based aluminosilicate samples by means of high-resolution synchrotron X-ray diffraction (HSXRD), scanning electron microscope (SEM), and compressive strength tests to investigate how the readily available aluminum affects the reaction. Class C fly ash-based aluminosilicate raw materials were prepared by incorporating Na-aluminate into the original fly ashes, then alkali-activated by 10 M NaOH solution. Incorporating Na-aluminate reduced the compressive strength of samples, with the reduction magnitude relatively constant regardless of length of curing period. The HSXRD provides evidence of the co-existence of C-S-H with geopolymeric gels and strongly suggests that the C-S-H formed in the current system is C-S-H(I). The back-scattered electron images suggest that the C-S-H(I) phase exists as small grains in a finely intermixed form with geopolymeric gels. Despite providing extra source of aluminum, adding Na-aluminate to the mixes did not decrease the Si/Al ratio of the geopolymeric gel.

36 MATERIALS SCIENCE↗

Binding and leaching of trace elements in Portland cement pastes

Portland cement contains trace elements originating from the raw materials and the fuels used for cement production. The trace elements are bound to some extent during cement hydration. A small fraction remains dissolved in the pore solution. The dissolved fractions of antimony, barium, chromium, lead, molybdenum and vanadium were quantified in the course of hydration of four different Portland cements. The development of heavy metal concentrations signifies the relevant hydration products for the binding of heavy metals. For chromate and molybdate a substitution for sulfate in ettringite was found. Vanadium and antimony are most likely not bound in ettringite. Barium precipitates as barium sulfate. For lead no clear trends could be observed. Leaching experiments were carried out and the concentrations of the leachates were compared to pore solution concentrations to check if the solubility of the heavy metals is relevant or if the leaching process is controlled by diffusion.

36 MATERIALS SCIENCE↗

Alkali-activated materials

This paper, which forms part of the UNEP White Papers series on Eco-Efficient Cements, provides a brief discussion of the class of cementing materials known as ‘alkali-activated binders’, which are identified to have potential for utilization as a key component of a sustainable future global construction materials industry. These cements are not expected to offer a like-for-like replacement of Portland cement across its full range of applications, for reasons related to supply chain limitations, practical challenges in some modes of application, and the need for careful control of formulation and curing. However, when produced using locally-available raw materials, with well-formulated mix designs (including in particular consideration of the environmental footprint of the alkaline activator) and production under adequate levels of quality control, alkali-activated binders are potentially an important and cost-effective component of the future toolkit of sustainable construction materials.

36 MATERIALS SCIENCE↗

Eco-efficient cements: Potential economically viable solutions for a low-CO2 cement-based materials industry

The main conclusions of an analysis of low-CO{sub 2}, eco-efficient cement-based materials, carried out by a multi-stakeholder working group initiated by the United Nations Environment Program Sustainable Building and Climate Initiative (UNEP-SBCI) are presented, based on the white papers published in this special issue. We believe that Portland-based cement approaches will dominate in the near future due to economies of scale, levels of process optimisation, availability of raw materials and market confidence. Two product-based approaches can deliver substantial additional reductions in their global CO{sub 2} emissions, reducing the need for costly investment in carbon capture and storage (CCS) over the next 20–30 years:1.Increased use of low-CO{sub 2} supplements (SCMs) as partial replacements for Portland cement clinker. 2.More efficient use of Portland cement clinker in mortars and concretes. However, other emerging technologies could also play an important role in emissions mitigation in the longer term, and thus merit further investigation.

36 MATERIALS SCIENCE↗