Experimental Determination of the Effect of the Ratio of B/Al on Glass Dissolution along the Nepheline (NaAlSiO 4 ) – Malinkoite (NaBSiO 4 ) Join
The dissolution kinetics of five glasses along the NaAlSiO 4 -NaBSiO 4 join were used to evaluate how the structural variations associated with boron-aluminum substitution affect the rate of dissolution. The composition of each glass varied inversely in mol% of Al 2 O 3 (5 to 25 mol%) and B 2 O 3 (20 to 0 mol%) with Na 2 O (25 mol%) and SiO 2 (50 mol%) making up the remaining amount, in every case Na/(Al+B) = 1.0. Single-pass flow-through experiments (SPFT) were conducted under dilute conditions as a function of solution pH (from 7.0 to 12.0) and temperature (from 23° to 90°C). Analysis by 27 Al and 29 Si MAS-NMR suggests Al (~98% [4] Al) and Si atoms (~100% [4] Si) occupy a tetrahedral coordination whereas, B atoms occupy both tetrahedral ([4]B) and trigonal ( [3] B) coordination. The distribution of [3]B fractionated between [3] B(ring) and [3] B(non-ring) moieties, with the [3] B(ring)/ [3] B(non-ring) ratio increases with the B/Al ratio. The MAS-NMR results also indicated an increase in the fraction of [4] B with an increase in the B/Al ratio. But despite the changes in the B/Al ratio and B coordination, the 29 Si spectra maintain a chemical shift between -88 to -84 ppm for each glass. Unlike the 29 Si spectra, the 27 Al resonances shift to more positive values with an increase in the B/Al ratio which suggests mixing between the [4] Al and [3] B sites, assuming avoidance between tetrahedral trivalent cations ( [4] Al-O- [4] B avoidance). Raman spectroscopy was use to augment the results collected from MAS-NMR and demonstrated that NeB4 (glass sample with the highest B content) was glass-glass phase separated (e.g., heterogeneous glass). Results from SPFT experiments suggest a forward rate of reaction and pH power law coefficients,η, that are independent of B/Al under these neutral to alkaline test conditions for all homogeneous glasses. The temperature dependence shows an order of magnitude increase in the dissolution rate with a 67°C increase in temperature and suggests dissolution is controlled by a surface-mediated reaction, evident by the activation energy, E a , being between 44±8 and 48±7 kJ/mol. Forward dissolution rates, based on Na and Si release, for homogeneous glasses are independent of the B/Al ratio, whereas dissolution rates based on Al and B release are not. Dissolution rates based on B release increase with an increase in the fraction of [3] B(ring). Finally in accord with previous studies, the data discussed in this manuscript suggest rupture of the Al-O and Si-O bond as the rate-limiting step controlling the dissolution of these glasses.