Fracture toughness of plasma-sprayed thermal barrier ceramics: Influence of processing, microstructure, and thermal aging

Fracture toughness has become one of the dominant design parameters that dictates the selection of materials and their microstructure to obtain durable thermal barrier coatings (TBCs). Much progress has been made in characterizing the fracture toughness of relevant TBC compositions in bulk form, and it has become apparent that this property is significantly affected by process-induced microstructural defects. In this investigation, a systematic study of the influence of coating microstructure on the fracture toughness of atmospheric plasma sprayed (APS) TBCs has been carried out. Yttria partially stabilized zirconia (YSZ) coatings were fabricated under different spray process conditions inducing different levels of porosity and interfacial defects. Fracture toughness was measured on free standing coatings in as-processed and thermally aged conditions using the double torsion technique. Results indicate significant variance in fracture toughness among coatings with different microstructures including changes induced by thermal aging. Comparative studies were also conducted on an alternative TBC composition, Gd 2 Zr 2 O 7 (GDZ), which as anticipated shows significantly lower fracture toughness compared to YSZ. Furthermore, the results from these studies not only point towards a need for process and microstructure optimization for enhanced TBC performance but also a framework for establishing performance metrics for promising new TBC compositions.

36 MATERIALS SCIENCE↗

Durable aluminate toughened zirconate composite thermal barrier coating (TBC) materials for high temperature operation

Research on advanced thermal barrier coating (TBC) materials capable of operating beyond 1200°C has primarily focused on the rare earth zirconate pyrochlores, particularly gadolinium zirconate (Gd 2 Zr 2 O 7 – GZO). The drawback of this material is a significant reduction in durability due to a low fracture toughness. This study investigates utilization of a thermodynamically compatible gadolinia alumina perovskite (GdAlO 3 – GAP) toughening phase to improve the durability of GZO. Dense pellets were fabricated to assess the material properties with minimal microstructural influence. Thermal stability, elastic modulus, hardness, indentation fracture resistance and erosion durability were evaluated for GZO, GAP, and composite pellets containing 10, 30, and 50 wt.% GAP. It was demonstrated that GAP and GZO are thermodynamically compatible through 1600°C and thus capable of operating well beyond the limits of traditional 7 wt.% yttria stabilized zirconia (YSZ). Grain sizes are maintained due to a lack of diffusion, and thus microstructural stability is enhanced. The GAP fracture toughness was shown to be over 2X that of GZO while exhibiting a lower elastic modulus and similar hardness. The 50:50 GZO-GAP composite exhibited a 63% reduction in the absolute erosion rate, demonstrating the immense toughening capabilities of this system. The implications for composite TBCs utilizing this system are discussed, along with future research.

36 MATERIALS SCIENCE↗

Enhanced thermal stability by introducing TiN diffusion barrier layer between W and SiC

The combination of W and SiC has many applications such as a hot cell of a thermionic energy converter, nuclear material, and high temperature microelectronics. In this study, a 2 µm thick TiN film is introduced as a diffusion barrier between SiC and W to avoid the inter-diffusion reaction at high temperature. Additionally, the effect of annealing temperature on the surface morphology and microstructure of the TiN film is studied to explore its high temperature stability. Then 500 nm W film is sputtered on the TiN film to characterize the inter-diffusion and stability of the W/TiN/SiC multilayer at 1100°C by XRD, Raman spectroscopy and cross-sectional EDS mapping techniques. The results indicate that the W/TiN/SiC multilayer is very stable even when heated at 1100°C for 25 hours.

36 MATERIALS SCIENCE↗

In situ characterization of foreign object damage (FOD) in environmental-barrier-coated silicon carbide (SiC) ceramic

Environmental barrier coatings (EBCs) protect advanced ceramics and ceramic matrix composites (CMCs) from oxidation and corrosion in gas turbine engine environments. Foreign object damage (FOD), where debris impact the protective coatings, is a critical hazard which limits the turbine durability. Despite previous efforts to understand FOD in EBCs, a detailed understanding of the fundamental transient damage mechanisms is still lacking. In the current work, the real-time FOD behavior of a Mullite / Silicon EBC was visualized via a dynamic synchrotron X-ray source in phase contrast imaging (PCI) configuration. Prior to the in situ FOD experiments, the microstructure and composition of the coating were respectively characterized using a scanning electron microscope (SEM) and X-ray diffraction (XRD). The variation in the properties of the debris was modeled by ~ 1.5 mm diameter Partially Stabilized Zirconia (PSZ) and Silicon Nitride (Si 3 N 4 ) spheres. A modified light-gas gun setup, synchronized with the X-ray beam, was used to propel the projectiles at velocities ranging between 300 and 355 m·s -1 . Coated samples were impacted under a fully backed support configuration and at normal incidence. Coating penetration and delamination, as well as projectile deformation at the bond coat resulted for FOD by PSZ spheres. Comparatively, projectile fracture, with subsequent rebound of fragments, as well as complete coating penetration and delamination at the substrate interface occurred for FOD by Si 3 N 4 spheres. It should be noted that only cone cracking was observed for FOD by PSZ spheres while back surface cracking was present for both projectile types. Qualitative understanding of the driving forces for the observed damage mechanisms were provided.

36 MATERIALS SCIENCE↗

Steam oxidation of ytterbium disilicate environmental barrier coatings with and without a silicon bond coat

The current generation of multilayer Si/Yb 2 Si 2 O 7 environmental barrier coatings (EBCs) are temperature limited by the melting point of Si, 1414°C. To investigate higher temperature EBCs, the cyclic steam oxidation of EBCs comprised of a single layer of ytterbium disilicate (YbDS) was compared to multilayered Si/YbDS EBCs, both deposited on SiC substrates using atmospheric plasma spray. In this work, after 500 1-h cycles at 1300°C in 90 vol%H2O-10 vol%air with a gas velocity of 1.5 cm/s, both multilayer Si/YbDS and single layer YbDS grew thinner silica scales than bare SiC, with the single layer YbDS forming the thinnest scale. Both coatings remained fully adherent and showed no signs of delamination. Silica scales formed on the single layer coating were significantly more homogeneous and possessed a markedly lower degree of cracking compared to the multilayered EBC. The single layer EBC also was exposed at 1425°C in steam with a gas velocity of 14 cm/s in an alumina reaction tube. The EBC reduced specimen mass loss compared to bare SiC but formed an extensive 2nd phase aluminosilicate reaction product. A similar reaction product was observed to form on some regions of the bare SiC specimen and appeared to partially inhibit silica volatilization. The 1425°C steam exposures were repeated with a SiC reaction tube and no 2nd phase reaction product was observed to form on the single layer EBC or bare SiC.

36 MATERIALS SCIENCE↗

Evaluating steam oxidation kinetics of environmental barrier coatings

Environmental barrier coatings (EBCs) are a commercially proven means of protecting SiC-based materials in gas turbine environments. However, there are little specific data in the literature on the impact of coatings like Yb 2 Si 2 O 7 on preventing accelerated SiO 2 growth in the presence of H 2 O. Quantification of reduced rates are necessary for evaluating and comparing EBC effectiveness and incorporation of silica growth rates into future EBC lifetime models. In this study, baseline kinetics of silica formation on bare Si and chemically vapor deposited (CVD) SiC in the 1250–1425 °C range were obtained via 100 h isothermal exposures in dry air and steam environments utilizing a SiC reaction tube to mitigate specimen volatility. An Arrhenius plot of the resulting rates was constructed, representing baseline minimum and maximum rates for Si and SiC oxidation at ambient pressure. Various EBC systems on CVD SiC substrates including air plasma sprayed (APS) EBCs with and without a Si bond coating and with surface roughening to enhance Yb 2 Si 2 O 7 adhesion were subjected to 1-h furnace cycle testing in air with 90vol%H 2 O at 1250–1350°C for up to 500 cycles. After exposure, silica formation rates were measured and compared to the baseline rates to assess EBC effectiveness, where EBC effectiveness is gauged as the propensity to reduce underlying rates of silica formation. With a Si bond coating, a ~180 µm Yb 2 Si 2 O 7 (YbDS) top coating reduced rates over the entire 1250°-1350°C range. Without a Si bond coating, ~60 µm (YbDS) coatings deposited directly onto CVD SiC exhibited poor adhesion, and had to be deposited onto substrates with enhanced roughness at 1350°C. Finally, while exhibiting good adhesion at 1350°C, overall the single layer YbDS coating exhibited a decreasing effectiveness from 1250° to 1350°C.

36 MATERIALS SCIENCE↗

Holistic comparison of environmental barrier coating material candidates through design of a figure of merit

The first figure of merit for environmental barrier coating (EBC) materials was designed through a ranking system for material properties pertaining to established EBC failure modes in service. Seven past, present, and novel EBC candidate materials were used in the figure of merit design: SiO 2 , Ba 0.75 Sr 0.25 Al 2 Si 2 O 8 (BSAS), HfSiO 4 , Yb 2 Si 2 O 7 , Yb 2 SiO 5 , Yb 2 O 3 , and YbPO 4 . Utilizing compiled data from the literature, the presented figure of merit verified Yb 2 Si 2 O 7 as the state-of-the-art candidate with optimal EBC properties and inferred that YbPO 4 should be considered as a potentially viable EBC material candidate. Further, the figure of merit allows for a holistic comparison of EBC candidates and informs experimental and computational search efforts for next-generation complex EBCs. Clear knowledge gaps found through this work include CaO–MgO–Al 2 O 3 –SiO 2 (CMAS)-resistant coatings, EBC lifetimes before delamination, and oxidant diffusion rates in relevant EBC microstructures. It was shown that while some materials show promise for solving a single key failure mode for EBCs (i.e., CMAS reactivity), a community-wide goal should be placed on materials development to achieve acceptable resistance against all major failure modes, which are interconnected. Novel compositionally complex EBC materials, in addition to layered EBC architectures, show promise for the optimization of material properties for long-lifetime EBCs in combustion environments.

36 MATERIALS SCIENCE↗

The effect of environment on thermal barrier coating lifetime

While the water vapor content of the combustion gas in natural gas-fired land-based turbines is ~10%, it can be 20–85% with coal-derived (syngas or H 2 ) fuels or innovative turbine concepts for more efficient carbon capture. Additional concepts envisage working fluids with high CO 2 contents to facilitate carbon capture and sequestration. To investigate the effects of changes in the gas composition on thermal barrier coating (TBC) lifetime, furnace cycling tests (1-h and 100-h cycles) were performed in air with 10, 50, and 90 vol. % water vapor and CO 2 -10% H 2 O and compared to prior results in dry air or O 2 . Two types of TBCs were investigated: (1) diffusion bond coatings (Pt-diffusion or Pt-modified aluminide) with commercial electron-beam physical vapor-deposited yttria-stabilized zirconia (YSZ) top coatings on second-generation superalloy N5 and N515 substrates and (2) high-velocity oxygen fuel (HVOF) sprayed MCrAlYHfSi bond coatings with air plasma-sprayed YSZ top coatings on superalloys X4, 1483, or 247 substrates. For both types of coatings exposed in 1-h cycles, the addition of water vapor resulted in a decrease in coating lifetime, except for Pt-diffusion coatings which were unaffected by the environment. In 100-h cycles, environment was less critical, perhaps because coating failure was chemical (i.e., due to interdiffusion) rather than mechanical. As a result, in both 1-h and 100-h cycles, CO 2 did not appear to have any negative effect on coating lifetime.

36 MATERIALS SCIENCE↗

The Effect of Coating Composition and Geometry on Thermal Barrier Coatings Lifetime

Several factors are being investigated that affect the performance of thermal barrier coatings (TBC) for use in land-based gas turbines where coatings are mainly thermally sprayed. This study examined high velocity oxygen fuel (HVOF), air plasma-sprayed (APS), and vacuum plasma-sprayed (VPS) MCrAlYHfSi bond coatings with APS YSZ top coatings at 900–1100 °C. For superalloy 247 substrates and VPS coatings tested in 1 h cycles at 1100 °C, removing 0.6 wt %Si had no effect on average lifetime in 1 h cycles at 1100 °C, but adding 0.3%Ti had a negative effect. Rod specimens were coated with APS, HVOF, and HVOF with an outer APS layer bond coating and tested in 100 h cycles in air + 10%H 2 O at 1100 °C. With an HVOF bond coating, initial results indicate that 12.5 mm diameter rod specimens have much shorter 100 h cycle lifetimes than disk specimens. Furthermore, much longer lifetimes were obtained when the bond coating had an inner HVOF layer and outer APS layer.

36 MATERIALS SCIENCE↗

Thermally Grown Oxide Stress in PS-PVD and EB-PVD Thermal Barrier Coatings Observed at Various Lifetimes Via Synchrotron X-ray Diffraction

The current standard application method for thermal barrier coatings (TBCs) on turbine blades for jet engines is electron-beam physical vapor deposition (EB-PVD) due to its high strain tolerance and low thermal conductivity. An emerging deposition method, plasma-spray physical vapor deposition (PS-PVD), presents an opportunity for a tailorable microstructure, and non-line-of-sight deposition that is faster and less expensive. To compare the lifetime behavior of both PS-PVD and EB-PVD coatings, samples subjected to 300 and 600 thermal cycles were measured during a 1 h thermal cycle to determine the strains, which were converted to stress, in the thermally grown oxide (TGO) layer of the TBCs using synchrotron X-ray diffraction (XRD). Room temperature XRD measurements indicated among samples that PS-PVD coatings experienced greater variation in in-plane room temperature strain in the TGO after cycling than the EB-PVD coatings. In-situ XRD measurements indicated similar high-temperature strain and no spallation after 600 thermal cycles for both coatings. Further, microscopy imaging after cycling showed greater rumpling in PS-PVD coatings that led to different failure modes between the two coatings’ TGO layers. The tailorability of PS-PVD coatings allows for adjustments in the processing parameters to improve their overall performance after aging and bridge the differences between the two deposition methods.

36 MATERIALS SCIENCE↗

Understanding Environmental Barrier Coating Lifetimes and Performance for Industrial Gas Turbines

Hydrogen or hydrogen blend fuels are expected to replace natural gas in land-based industrial gas turbines (IGTs) to support a greener power economy. Silicon carbide (SiC) base ceramic matrix composites (CMCs) are considered for replacement of Ni-based superalloys to facilitate future efficiency improvements. SiC CMCs require environmental barrier coatings (EBCs) to mitigate volatilization from high-temperature steam, thus making the EBC lifetime critical information for identifying CMC component lifetimes. Here, the goal of this project is to determine the maximum bond coating temperature underneath the EBC for achieving an IGT component lifetime goal of 25,000 h, which is far greater than current CMC component lifetime requirements for aeroturbine applications. To provide data for the lifetime model, laboratory testing used atmospheric plasma-sprayed rare-earth silicate EBCs on monolithic SiC substrates with an intermediate Si bond coating. Specimens exposed to 1-h thermal cycles in flowing air–steam environments and reaction kinetics were assessed from 700 °C to 1350 °C by measuring the thickness of the thermally grown silica scales. The silica growth and phase transformation appear critical in predicting EBC lifetime and several strategies have been explored to reduce the oxide growth rate and improve EBC durability at elevated temperatures. Advanced characterization using Raman spectroscopy has helped clarify this system.

08 HYDROGEN↗

Single-chamber plasma enhanced chemical vapor deposition of transparent organic/inorganic multilayer barrier coating at low temperature

Deposition of organic/inorganic multilayers is usually carried out by two different process steps by two different deposition methods. A single-chamber process for the deposition of multilayer stacks can make the process and deposition system simpler. In this work, SiOCH and plasma-polymerized methylcyclohexane (pp-MCH) films and their multilayer stacks for application to transparent diffusion barrier coatings were deposited in a single low-temperature plasma enhanced chemical vapor deposition reactor using hexamethyldisilazane/N{sub 2}O/O{sub 2}/Ar and methylcyclohexane/Ar mixtures for SiOCH and pp-MCH layers, respectively. The deposition rates of the SiOCH and pp-MCH layers were increased with increasing the N{sub 2}O:O{sub 2} gas flow ratio and rf plasma power, respectively. Oxygen concentration in the SiOCH films was decreased and carbon and hydrogen incorporation was increased when increasing the N{sub 2}O:O{sub 2} gas flow ratio from 0:1 to 3:1. In this work, the water vapor transmission rate of polyester sulfone substrate could be reduced from a level of 50 (bare substrate) to 0.8 g/m{sup 2} day after deposition of a pp-MCH/SiOCH/pp-MCH multilayer coating.

36 MATERIALS SCIENCE↗

Surface sealing of electron beam physical vapor deposited thermal barrier coatings by high-intensity pulsed ion beam

A surface sealing technology by employing high-intensity pulsed ion beam (HIPIB) technique is developed for electron beam physical vapor deposited (EB-PVD) thermal barrier coatings (TBCs) to further improve the high temperature performance. The HIPIB irradiation can deliver a high-density energy up to 100 J/cm{sup 2} into the shallow ion range of about 0.1-10 {mu}m within a short pulse width of less than 1 {mu}s, by which a micrometer-thick bridging layer was achieved on the gap between columnar grains of EB-PVD TBCs under a single pulse of 4.5 J/cm{sup 2}. The thin bridging layer provided atmosphere shielding for the TBCs along with matching strain tolerance of the columnar top coat during thermal cycling. Cyclic oxidation tests at 1050 deg. C demonstrated that weight gain of the sealed TBC samples is decreased by about 60% from 0.8 mg/cm{sup 2} of the as-deposited ones.

36 MATERIALS SCIENCE↗

Atomic layer deposited nanocrystalline tungsten carbides thin films as a metal gate and diffusion barrier for Cu metallization

Tungsten carbides (WC{sub x}) thin films were deposited on thermally grown SiO{sub 2} substrates by atomic layer deposition (ALD) using a fluorine- and nitrogen-free W metallorganic precursor, tungsten tris(3-hexyne) carbonyl [W(CO)(CH{sub 3}CH{sub 2}C ≡ CCH{sub 2}CH{sub 3}){sub 3}], and N{sub 2} + H{sub 2} plasma as the reactant at deposition temperatures between 150 and 350 °C. The present ALD-WC{sub x} system showed an ALD temperature window between 200 and 250 °C, where the growth rate was independent of the deposition temperature. Typical ALD characteristics, such as self-limited film growth and a linear dependency of the film grown on the number of ALD cycles, were observed, with a growth rate of 0.052 nm/cycle at a deposition temperature of 250 °C. The ALD-WC{sub x} films formed a nanocrystalline structure with grains, ∼2 nm in size, which consisted of hexagonal W{sub 2}C, WC, and nonstoichiometric cubic β-WC{sub 1−x} phase. Under typical deposition conditions at 250 °C, an ALD-WC{sub x} film with a resistivity of ∼510 μΩ cm was deposited and the resistivity of the ALD-WC{sub x} film could be reduced even further to ∼285 μΩ cm by further optimizing the reactant pulsing conditions, such as the plasma power. The step coverage of ALD-WC{sub x} film was ∼80% on very small sized and dual trenched structures (bottom width of 15 nm and aspect ratio of ∼6.3). From ultraviolet photoelectron spectroscopy, the work function of the ALD-WC{sub x} film was determined to be 4.63 eV. Finally, the ultrathin (∼5 nm) ALD-WC{sub x} film blocked the diffusion of Cu, even up to 600 °C, which makes it a promising a diffusion barrier material for Cu interconnects.

36 MATERIALS SCIENCE↗

Sputtered carbon as a corrosion barrier for x-ray detector windows

Sputtered amorphous carbon thin films were explored as corrosion resistant coatings on aluminum thin films to be incorporated into x-ray detector windows. The requirements for this application include high corrosion resistance, low intrinsic stress, high strains at failure, and high x-ray transmission. Low temperature sputtering was used because of its compatibility with the rest of the window fabrication process. Corrosion resistance was tested by exposure of carbon coated and uncoated Al thin films to humidity. Substrate curvature and bulge testing measurements were used to determine intrinsic stress and ultimate strain at failure. The composition and bonding of the carbon films were further characterized by electron energy loss spectroscopy, Raman spectroscopy, and carbon, hydrogen, and nitrogen elemental analyses. Samples had low compressive stress (down to.08 GPa), a high strain at failure (3%), and a low fraction of sp{sup 3} carbon–carbon bonds (less than 5%). The high breaking strain and excellent x-ray transmission of these sputtered carbon films indicate that they will work well as corrosion barriers in this application.

36 MATERIALS SCIENCE↗

Van der Waals metal-semiconductor junction: Weak Fermi level pinning enables effective tuning of Schottky barrier

Two-dimensional (2D) semiconductors have shown great potential for electronic and optoelectronic applications. However, their development is limited by a large Schottky barrier (SB) at the metal-semiconductor junction (MSJ), which is difficult to tune by using conventional metals because of the effect of strong Fermi level pinning (FLP). We show that this problem can be overcome by using 2D metals, which are bounded with 2D semiconductors through van der Waals (vdW) interactions. This success relies on a weak FLP at the vdW MSJ, which is attributed to the suppression of metal-induced gap states. Consequently, the SB becomes tunable and can vanish with proper 2D metals (for example, H-NbS2). This work not only offers new insights into the fundamental properties of heterojunctions but also uncovers the great potential of 2D metals for device applications.

14 SOLAR ENERGY↗

Cross sections and barriers for nuclear fission induced by high-energy nucleons

The cross sections for the fission of {sup 232}Th, {sup 235,238}U, {sup 237}Np, and {sup 239}Pu target nuclei that was induced by 20- to 1000-MeV neutrons and protons were calculated. The respective calculations were based on the multiconfiguration-fission (MCFx) model, which was used to describe three basic stages of the interaction of high-energy nucleons with nuclei: direct processes (intranuclear cascade), equilibration of the emerging compound system, and the decay of the compound nucleus (statistical model). Fission barriers were calculated within the microscopic approach for isotopic chains formed by 15 to 20 nuclei of the required elements. The calculated fission cross sections were compared with available experimental data. It was shown that the input data set and the theoretical model used made it possible to predict satisfactorily cross section for nuclear fission induced by 20- to 1000-MeV nucleons.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Pellet injection into H-mode ITER plasma with the presence of internal transport barriers

The impacts of pellet injection into ITER type-1 ELMy H-mode plasma with the presence of internal transport barriers (ITBs) are investigated using self-consistent core-edge simulations of 1.5D BALDUR integrated predictive modeling code. In these simulations, the plasma core transport is predicted using a combination of a semi-empirical Mixed B/gB anomalous transport model, which can self-consistently predict the formation of ITBs, and the NCLASS neoclassical model. For simplicity, it is assumed that toroidal velocity for {omega}{sub E Multiplication-Sign B} calculation is proportional to local ion temperature. In addition, the boundary conditions are predicted using the pedestal temperature model based on magnetic and flow shear stabilization width scaling; while the density of each plasma species, including both hydrogenic and impurity species, at the boundary are assumed to be a large fraction of its line averaged density. For the pellet's behaviors in the hot plasma, the Neutral Gas Shielding (NGS) model by Milora-Foster is used. It was found that the injection of pellet could result in further improvement of fusion performance from that of the formation of ITB. However, the impact of pellet injection is quite complicated. It is also found that the pellets cannot penetrate into a deep core of the plasma. The injection of the pellet results in a formation of density peak in the region close to the plasma edge. The injection of pellet can result in an improved nuclear fusion performance depending on the properties of pellet (i.e., increase up to 5% with a speed of 1 km/s and radius of 2 mm). A sensitivity analysis is carried out to determine the impact of pellet parameters, which are: the pellet radius, the pellet velocity, and the frequency of injection. The increase in the pellet radius and frequency were found to greatly improve the performance and effectiveness of fuelling. However, changing the velocity is observed to exert small impact.