Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MARTENSITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,621 records · Page 90

Microstructural evolution of P92 ferritic/martensitic steel under Ar{sup +} ion irradiation at elevated temperature

Irradiation damage in P92 ferritic/martensitic steel irradiated by Ar{sup +} ion beams to 7 and 12 dpa at elevated temperatures of 290 Degree-Sign C, 390 Degree-Sign C and 550 Degree-Sign C has been investigated by transmission electron microscopy, scanning electron microscopy and atomic force microscopy. The precipitate periphery (the matrix/carbide interface) was amorphized only at 290 Degree-Sign C, while higher irradiation temperature could prevent the amorphization. The formation of the small re-precipitates occurred at 290 Degree-Sign C after irradiation to 12 dpa. With the increase of irradiation temperature and dose, the phenomenon of re-precipitation became more severe. The voids induced by irradiation were observed after irradiation to 7 dpa at 550 Degree-Sign C, showing that high irradiation temperature ({>=} 550 Degree-Sign C) was a crucial factor which promoted the irradiation swelling. Energy dispersive X-ray analysis revealed that segregation of Cr and W in the voids occurred under irradiation, which may influence mechanical properties of P92 F/M steel. - Graphical Abstract: High density of small voids, about 2.5 nm in diameter, was observed after irradiation to 12 dpa at 550 Degree-Sign C, which was shown in panel a (TEM micrograph). As shown in panel b (SEM image), a large number of nanometer-sized hillocks were formed in the surface irradiated at 550 Degree-Sign C, and the mean size was {approx} 30 nm. The formation of the nanometer-sized hillocks might be due to the voids that appeared as shown in TEM images (panel a). High irradiation temperature ({>=} 550 Degree-Sign C) was a crucial factor for the formation of void swelling. Highlights: Black-Right-Pointing-Pointer Small carbides re-precipitated in P92 matrix irradiated to 12 dpa at 290 Degree-Sign C. Black-Right-Pointing-Pointer High density of voids was observed at 550 Degree-Sign C. Black-Right-Pointing-Pointer Segregation of Cr and W in voids occurred under irradiation.

36 MATERIALS SCIENCE↗

Effect of V and Ta on the precipitation behavior of 12%Cr reduced activation ferrite/martensite steel

12%Cr reduced activation ferrite/martensite steels are promising candidate materials for good corrosion and irradiation resistance used for supercritical water-cooled reactor cladding and in-core components. V and Ta are considered to have improved the creep strength of high Cr steels by precipitating as MX phase. In this paper, a series of trial products microalloyed with V and V–Ta are produced, and the microstructure is characterized after quenching at 1050 °C and tempering at 780 °C by using TEM method to investigate the effect of these elements on the precipitation behavior of 12%Cr reduced activation ferrite/martensite steel. The results from both the experimental observations and thermodynamic and kinetic calculations reveal that V and V–Ta can promote the stable MX precipitation instead of M{sub 2}X, thus increasing the volume fraction of M{sub 23}C{sub 6}. Two-phase separation behavior of the (Ta, V)(C, N) carbonitride into a Ta(V)C(N) phase and a V(Ta)N(C) phase in 12Cr3WVTa steel is observed and further discussed. - Highlights: • Microalloyed with V and V-Ta can promote the precipitation of MX instead of M{sub 2}X. • The presence of delta-ferrite in microstructure affects the morphology of MX. • Two-phase separation of MX carbonitride was observed in 12Cr3WVTa steel.

36 MATERIALS SCIENCE↗

Evolution of the substructure of a novel 12% Cr steel under creep conditions

In this work we study the microstruture evolution of a newly developed 12% Cr martensitic/ferritic steel in as-received condition and after creep at 650 °C under 130 MPa and 80 MPa. The microstructure is described as consisting of mobile dislocations, dipole dislocations, boundary dislocations, precipitates, lath boundaries, block boundaries, packet boundaries and prior austenitic grain boundaries. The material is characterized employing light optical microscopy (LOM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). TEM is used to characterize the dislocations (mobile + dipole) inside the subgrains and XRD measurements are used to the characterize mobile dislocations. Based on the subgrain boundary misorientations obtained from EBSD measurements, the boundary dislocation density is estimated. The total dislocation density is estimated for the as-received and crept conditions adding the mobile, boundary and dipole dislocation densities. Additionally, the subgrain size is estimated from the EBSD measurements. In this publication we propose the use of three characterization techniques TEM, XRD and EBSD as necessary to characterize all type of dislocations and quantify the total dislocation densty in martensitic/ferritic steels. - Highlights: • Creep properties of a novel 12% Cr steel alloyed with Ta • Experimental characterization of different types of dislocations: mobile, dipole and boundary • Characterization and interpretation of the substructure evolution using unique combination of TEM, XRD and EBSD.

36 MATERIALS SCIENCE↗

The nature of nano-sized precipitates in ferritic/martensitic steel P92 produced by thermomechanical treatment

Thermomechanical treatment (TMT) can effectively improve the mechanical properties of high-Cr ferritic/martensitic (F/M) steels, which has been mainly attributed to a dense dispersion of nano-sized precipitates. Precipitate phases in high-Cr F/M steels produced by TMT require further investigations. Precipitates in commercial F/M steel P92 produced by a TMT process, warm-rolled at 650 °C plus tempered at 650 °C for 1 h, were investigated by transmission electron microscopy. Nano-sized precipitates with a high number density in the steel after the TMT were found to be Cr-rich M{sub 2}(C,N) carbonitride, rather than MX or M{sub 23}C{sub 6} phase. The M{sub 2}(C,N) carbonitride has a hexagonal lattice with the lattice parameters about a/c = 0.299/0.463 nm. These M{sub 2}(C,N) carbonitrides with a typical composition of (Cr{sub 0.85}V{sub 0.06}Fe{sub 0.06}Mo{sub 0.03}){sub 2}(C,N) have an average diameter smaller than 30 nm, and mainly distribute on dislocations and at the boundaries of equiaxed ferrite grains in the TMT steel. The TMT process inhibits the precipitation of M{sub 23}C{sub 6} and M{sub 5}C{sub 2} phases. Enhanced creep properties of the P92 steel after the TMT, as reported previously, were considered to be mainly attributed to plenty of nano-sized Cr-rich M{sub 2}(C,N) carbonitrides produced by the TMT rather than to MX and M{sub 23}C{sub 6} precipitates. - Graphical abstract: TEM micrographs of precipitates on extraction carbon replicas prepared from ferritic/martensitic (F/M) steel P92. (a) After conventional heat treatment, normalized at 1050 °C for 30 min plus tempered at 765 °C for 1 h. (b) After a thermomechanical treatment (TMT), warm-rolled at 650 °C plus tempered at 650 °C for 1 h. Nano-sized precipitates with a high number density in the steel produced by the TMT were found to be Cr-rich M{sub 2}(C,N) carbonitride, rather than MX or M{sub 23}C{sub 6} phase. The TMT process inhibits the precipitation of M{sub 23}C{sub 6} and M{sub 5}C{sub 2} phases. Enhanced creep properties of the steel by the TMT are mainly attributed to plenty of nano-sized Cr-rich M{sub 2}(C,N) carbonitrides, rather than to MX and M{sub 23}C{sub 6} precipitates. It is suggested that plenty of nano-sized Cr-rich M{sub 2}(C,N) carbonitrides produced by the TMT are more helpful to improve the creep properties of the steel than M{sub 23}C{sub 6} plus MX precipitates obtained by the conventional heat treatment. - Highlights: •Carbon replicas were used for precisely identifying nano-sized phases in steel produced by TMT. •Densely nano-sized precipitates in P92 steel after TMT were found to be Cr-rich M{sub 2}(C,N) phase. •Fine precipitates produced by TMT can be M{sub 2}X phase instead of MX and/or M{sub 23}C{sub 6} phase. •Enhanced creep properties of P92 steel by TMT is attributed to fine M{sub 2}X, rather than to MX and M{sub 23}C{sub 6}. •TMT involving a tempering at 650 °C inhibits the formation of M{sub 23}C{sub 6}/M{sub 5}C{sub 2} phases in high-Cr steels.

36 MATERIALS SCIENCE↗

Radiation-induced swelling and radiation-induced segregation & precipitation in dual beam irradiated Ferritic/Martensitic HT9 steel

Highlights: • The depth-dependence of radiation-induced cavities was characterized in self-ion irradiated HT9 co-implanted with He. • The injected interstitial effect was revealed to suppress cavity swelling in the vicinity of the damage peak. • ChemiSTEM elemental maps revealed the segregation of Ni at cavity surfaces and its possible synergistic influence on swelling was discussed. - Abstract: Ferritic/Martensitic HT9 steel was irradiated at 432 °C to 16.6 displacements per atom (dpa) (at the depth of 600 nm) using a defocused beam of 5 MeV Fe{sup ++} ions, while co-implanted with 3.22 appm He at the same depth. The helium concentration profile was designed so to follow the damage curve with a 0.22 appm He/dpa ratio at the depth from 300 to 1000 nm in the material. The depth-dependence of the cavity size and number density were characterized by both transmission electron microscopy (TEM) and scanning transmission electron microscopy (STEM) imaging methods. A comparison between the two techniques was done showing good agreement. Cavity number density and the resulting swelling were found to be suppressed by the injected interstitial effect in the vicinity of the ion induced damage peak. The region between 300 and 750 nm depth which excludes the injected interstitial effect was thus proposed for improved cavity swelling analysis. The swelling ratio in this region was found to be ~(0.86–1.02) × 10{sup − 2}%/dpa. In addition, ChemiSTEM characterization revealed radiation-induced segregation occurring throughout the irradiated region and precipitation of G-phase particles. Segregation of Ni to cavity surfaces was also observed and its possible synergistic influence on swelling was discussed.

36 MATERIALS SCIENCE↗

Formation of Ti-Al intermetallics on a surface of titanium by non-vacuum electron beam treatment

Highlights: • Electron beam cladding allows fabricating thick intermetallic coatings on Ti surface. • By variation of Ti:Al ratio the phase composition of the coatings can be controlled. • Oxidation resistance of clads increase with increase of Al content. • Single-phase Ti{sub 3}Al coating provides the highest microhardness and wear resistance. - Abstract: Titanium and titanium alloys are highly important structural materials for many industries where low density in combination with high mechanical strength and corrosion resistance are required. However, titanium is not applicable for tribological or high temperatures purposes due to its interaction with atmospheric gases and friction seizure during the contact with most metallic materials. To protect the surface of titanium and improve its wear resistance intermetallic coatings can be applied. In this study, the Ti-Al intermetallic layers were fabricated on Ti surface by electron beam melting of Al and Ti powders. By variation of Al/Ti ratio in the initial powders it was possible to control elemental and phase composition of the layers. The formation of TiAl, Al{sub 2}Ti and Ti{sub 3}Al phases was observed in the layers. Independently on Al content the layers had lamellar type of structure. Microhardness, wear resistance and oxidation resistance were measured to evaluate the quality of the layers. The microhardness and wear resistance were in good agreement with each other. The coating, consisted of pure Ti{sub 3}Al phase, demonstrated the highest level of these properties. Oxidation resistance of the coatings increased proportionally to the aluminium content due to formation of alumina in oxide scale.

36 MATERIALS SCIENCE↗

Effect of Ni content on the microstructure and mechanical properties of weld metal with both-side submerged arc welding technique

Highlights: • This manuscript primarily studied the effects of Ni content on the K65 weld metals; • Increase Ni content could significantly improve the strength and low temperature impact toughness of the weld metal. • The beneficial effect of Ni is attributed to its positive effect on phase transformation. • GBF keeps K-S or N-W relations only with one austenite and the variants belong to the same bain group are two reasons. • The M/A islands are considered to be another reason for the reduced toughness. - Abstract: The effects of nickel (Ni) content on the mechanical properties and microstructure evolution in the weld metals of commercial K65 oil and gas pipeline steel were studied. Increase Ni content could significantly improve the strength and low temperature impact toughness (−40 °C and −60 °C) of the weld metal. The above influences of Ni were attributed to the formation of predominant acicular ferrite (AF), at the expense of grain boundary ferrite (GBF), ferrite side plates (FSP) and martensite/austenite (M/A) constituent in weld metal. EBSD results indicated that GBF keeps K-S or N-W relations only with the prior austensite grain that belongs to one side of the grain boundary and the variants belong to the same bain group which always forms low angle boundary. Moreover, the retained austenite as one part of M/A constituent was mainly found in the weld metal with lower Ni content. It indicated that the transformation process could be promoted more completely by the increase of Ni content. The mechanism of the toughness improvement brought by Ni increasing was ascribed to the relatively uniform transformation to final microstructure, which reduces the appearance of GBF and M/A constituents.

36 MATERIALS SCIENCE↗

Electron-irradiation-induced Cr segregation in Fe-Cr model alloy pre-implanted with hydrogen ions

Highlights: • Streaks appeared in the diffraction patterns of hydrogen-implanted Fe-Cr alloy after electron irradiation in an HVEM. • A kind of needle-like Cr precipitates give rise to the streaks. • The streaks are explained reasonably by shape effect of precipitates. - Abstract: Reduced activation ferritic/martensitic (RAFM) steels are widely accepted as the candidate structural materials for fusion reactors. To gain knowledge about Cr behaviour of these steels in such environments, Fe-Cr binary alloys have to be investigated. In this study, Fe-10 at.% Cr ferritic model alloy pre-implanted with hydrogen ions was electron-irradiated in a high voltage electron microscope (HVEM) at the temperature ranging from 300 °C to 600 °C. Streaks were observed in the diffraction patterns in the model alloy after electron irradiation at 450–550 °C and explained reasonably by shape effect. The analysis of transmission electron microscopy (TEM) reveals that the observed streaks are induced by a kind of needle-like precipitates with the directions along <100>. The dependence of the length and density of the precipitates on the temperature were studied. In addition, contrast experiments were conducted with pure Fe and Fe-10 at.% Cr alloy with and without hydrogen ion implantation, respectively. After electron irradiation, no streak was observed in the hydrogen-implanted pure Fe and Fe-10 at.% Cr alloy without the hydrogen implantation. Therefore, it is assumed that the needle-like precipitates could be the complex of Cr and H, which segregate and precipitate along <100> direction.

36 MATERIALS SCIENCE↗

Microstructure and tensile properties of laser engineered net shaped reduced activation ferritic/martensitic steel

Highlights: • A RAFM steel has been successfully manufactured by laser engineered net shaping (LENS), which is one of laser additive manufacturing technologies. • Columnar dendrites in vertical section and a mixture of equiaxed and columnar grains in horizontal section have been observed. • The anisotropic tensile properties are induced by LENS process, which can be eliminated well through the heat treatment. - Abstract: A laser additive manufacturing technique, laser engineered net shaping (LENS), was successfully applied to manufacture a reduced activation ferritic/martensitic (RAFM) steel with nominal composition of Fe-9Cr-0.11C-1.5W-0.4Mn-0.2V-0.12Ta (wt%). The as-deposited LENS-RAFM steels were normalized and tempered. The microstructures of as-deposited and heat treated LENS-RAFM steels were characterized by using optical microscope (OM), scanning electron microscope (SEM) and transmission electron microscope (TEM). The tensile tests of as-deposited and heat treated samples in different directions were carried out at room temperature and 873 K. The results showed that columnar dendrites grow epitaxially along the direction of deposition in vertical section (YOZ) and a mixture of equiaxed and columnar grains appears in horizontal section (XOY). No precipitates are observed in the as-deposited sample while Cr-rich M{sub 23}C{sub 6} and Ta-rich MX type carbides appear in the heat treated sample. The as-deposited sample showed anisotropic tensile properties which could be eliminated by heat treatment. The tensile strength of the LENS-RAFM steel is similar to conventional RAFM steels such as EUROFER 97 and CLAM.

36 MATERIALS SCIENCE↗

Hydrogen induced cracking susceptibility of API 5L X70 pipeline steel in relation to microstructure and crystallographic texture developed after different thermomechanical treatments

Highlights: • crack propagated mainly along deformed-banded microstructure. • Lower failure strength manifested at pipeline steel surface compared to the mid-thickness. • Greater fraction of martensite/austenite constituents featured in specimen WG relative to specimen WH. • Early onset of cracking in specimen WH showed no preference to specific crystallographic orientation. • Multi-component inclusion particle was revealed along crack propagation path. - Abstract: Thermomechanical treatments offer an innovative means of controlling microstructure development and improving resistance to hydrogen induced cracking (HIC) in pipeline steel. This study was conducted on two X70 pipeline steels (labelled WG and WH) of the same chemical composition, but processed with different thermomechanical parameters. Specimen WG was hot rolled at a higher temperature range of 880–820 {sup °}C, while specimen WH was hot rolled between 830 and 760 {sup °}C before cooling at a rate of 25 {sup °}C/s. Early onset of HIC was observed in specimen WH after electrochemical hydrogen charging for 12 h in a solution of 0.2 M H{sub 2}SO{sub 4} and 3 g/l NH{sub 4}SCN, without any applied stress. Also, test pieces from the surface and mid-thickness layers of each pipeline steel were subjected to slow strain rate tensile (SSRT) test with in-situ hydrogen charging. Characterization techniques such as Optical Microscopy, Scanning Electron Microscopy, Electron Backscattered Diffraction and X-ray Diffraction were used to investigate the structure pipeline steel specimens. The role of inclusions on HIC was studied by Energy Dispersive X-ray Spectroscopy. Although the microstructure of both specimens were predominantly ferritic, more martensite/retained austenite (M/A) constituents featured in WG. Further crystallographic texture analysis indicates that grain orientation at the surfaces of both test specimens were similar with deviations towards <111> on the inverse pole figure (IPF); whereas, pole intensity at the mid-thickness deviated towards the <001> direction. Considering the increased fraction of banded-deformed grains with high stored energy, the lower HIC resistance of specimen WH in comparison to specimen WG was justified.

36 MATERIALS SCIENCE↗

Comparison of cracking behavior of nanocrystalline Cu film on substrates of different plastic deformation mechanisms

Nanocrystalline (NC) metallic thin films on metal substrates usually undergo substantial cracking at applied strains of a few percent due to strain concentration at the film/substrate interfaces. In this work, we show that the cracking of a nanocrystalline Cu film can be significantly inhibited by a NiTi substrate. NC Cu films are deposited on 304 stainless steel, Kapton and NiTi substrates, in which plastic deformation occurs via dislocation slip, molecule chain disentanglement and collective lattice shear, respectively. NC Cu film on NiTi substrate starts to show observable cracks at an applied strain of 24%, in contrast to 6% for that on steel and 15% for that on Kapton. Further, the crack density in the film on NiTi substrate is two to three orders lower than the counterparts. The discrepancy is suggested to attribute to the reduced local strain concentration enabled by the uniform lattice shear and high strain hardening of the NiTi substrate.

36 MATERIALS SCIENCE↗

High temperature materials for heavy duty diesel engines: Historical and future trends

We report that heavy duty (HD) vehicles are projected to be the largest fuel-use subsector in transportation, with current demand for diesel fuel projected to grow 30% by 2040. Historically, a primary strategy for increasing diesel engine efficiency has been to increase peak cylinder pressure (PCP). However, increasing PCP imparts greater mechanical and thermal loads on engine components and materials. In recent years, the material property limits for many components have been reached and further increases in PCP above ~20 MPa have been difficult, while still maintaining the necessary affordability and longevity of on-road HD diesel engines. This paper reviews the historical evolution and major metallurgical advancements of high temperature materials in HD on road diesel engines (10–15 L displacement) up to the current state of the art, focusing on materials in the engine block, cylinder heads, pistons, valves, and exhaust components. These components cover a wide range of material classes, including cast iron, ferritic steel, austenitic steel, titanium alloys, nickel based super-alloys, and high temperature coatings. Finally, the microstructural degradation and failure mechanisms of the materials associated with the complex mechanical and thermal loading during service are discussed and key areas for future materials research are suggested that overcome technical barriers.

36 MATERIALS SCIENCE↗

The influence of impurities on the crystal structure and mechanical properties of additive manufactured U–14at.% Nb

Uranium-niobium alloys can exist with significantly different microstructures and mechanical properties, heavily influenced by thermomechanical processing history and impurities. In this study, the influence of Ti and other impurities is studied on uranium-14 at.% niobium additively manufactured using laser powder bed fusion. In two different metallic impurity levels were investigated and a Nb equivalent (Nbeq) composition is defined to represent the impurities. Furthermore, in-situ neutron diffraction during compression loading shows that increased Nbeq promotes the formation of γ°-tetragonal phase at the expense of α''-monoclinic phase, resulting in 2 × higher yield strength than water quenched α'' and a strain induced transformation to α'' with superelastic strains to 4.5%.

36 MATERIALS SCIENCE↗

Large thermal hysteresis in a single-phase NiTiNb shape memory alloy

Large thermal hysteresis ($T$ hys ) is favorable in shape memory alloys (SMAs) because it renders wide service and storage temperature range of the SMA-made parts. In this letter, we show that large intrinsic $T$ hys up to 100 K is achieved in a low Nb content (2 at.%), β-Nb-free and single-phase NiTiNb SMA fabricated by casting, forging, wire-drawing and annealing. Such a large $T$ hys is comparable to that of the widely used dual-phase NiTiNb SMAs in which high Nb content and β-Nb are required. By exploiting the grain-size-dependence of $T$ hys in our single-phase NiTiNb SMA and that in an equiatomic NiTi SMA, we attribute the large $T$ hys to the enhanced kinetic resistance of transformation by the small grains. In conclusion, the connection between the $T$ hys and the kinetic resistance is demonstrated by a modified dislocation-based kinetic model.

36 MATERIALS SCIENCE↗

Core/shell structures of oxygen-rich nanofeatures in oxide-dispersion strengthened Fe-Cr alloys

With the significant improvement in high temperature creep properties and resistance to radiation damage by addition of nanoscale oxide features, oxide-dispersion strengthened (ODS) ferritic/martensitic alloys are potential candidates for structural applications in nuclear fusion reactors. The structure of the oxygen-rich nanofeatures was analyzed by atom-probe tomography in three ODS alloys: MA957, ODS Fe-12 wt %Cr, and ODS Eurofer-97. Although field evaporation and reconstruction of the precipitates suffer from artefacts, a core/shell structure is found even for very small precipitates. Precipitate cores are Y rich while shell regions are enriched in Ti, Cr, or V depending on alloy composition.

36 MATERIALS SCIENCE↗

Irradiation-induced grain growth in nanocrystalline reduced activation ferrite/martensite steel

In this work, we investigate the microstructure evolution of surface-nanocrystallized reduced activation ferrite/martensite steels upon high-dose helium ion irradiation (24.3 dpa). We report a significant irradiation-induced grain growth in the irradiated buried layer at a depth of 300–500 nm, rather than at the peak damage region (at a depth of ∼840 nm). This phenomenon can be explained by the thermal spike model: minimization of the grain boundary (GB) curvature resulting from atomic diffusion in the cascade center near GBs.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Large reversible magnetocaloric effect in a Ni-Co-Mn-In magnetic shape memory alloy

Reversibility of the magnetocaloric effect in materials with first-order magnetostructural transformation is of vital significance for practical magnetic refrigeration applications. Here, we report a large reversible magnetocaloric effect in a Ni 49.8 Co 1.2 Mn 33.5 In 15.5 magnetic shape memory alloy. A large reversible magnetic entropy change of 14.6 J/(kg K) and a broad operating temperature window of 18 K under 5 T were simultaneously achieved, correlated with the low thermal hysteresis (-8 K) and large magnetic-field-induced shift of transformation temperatures (4.9 K/T) that lead to a narrow magnetic hysteresis (1.1 T) and small average magnetic hysteresis loss (48.4 J/kg under 5 T) as well. Furthermore, a large reversible effective refrigeration capacity (76.6 J/kg under 5 T) was obtained, as a result of the large reversible magnetic entropy change, broad operating temperature window, and small magnetic hysteresis loss. We conclude the large reversible magnetic entropy change and large reversible effective refrigeration capacity are important for improving the magnetocaloric performance, and the small magnetic hysteresis loss is beneficial to reducing energy dissipation during magnetic field cycle in potential applications.

36 MATERIALS SCIENCE↗

Giant field-induced adiabatic temperature changes in In-based off-stoichiometric Heusler alloys

In this paper, direct measurements of the adiabatic temperature change (ΔT AD ) of Ni 50 Mn 35 In 14.5 B 0.5 have been done using an adiabatic magnetocalorimeter in a temperature range of 250–350 K, and with magnetic field changes up to ΔH = 1.8 T. The initial susceptibility in the low magnetic field region drastically increases with temperature starting at about 300 K. Magnetocaloric effects parameters, adiabatic temperature changes, and magnetic entropy changes were found to be a linear function of H 2/3 in the vicinity of the second order transitions (SOT), whereas the first order transitions do not obey the H 2/3 law due to the discontinuity of the transition. The relative cooling power based on the adiabatic temperature change for a magnetic field change of 1.8 T has been estimated. Maximum values of ΔT AD = -2.6 K and 1.7 K were observed at the magnetostructural transition (MST) and SOT for ΔH = 1.8 T, respectively. Finally, the observed ΔT AD at the MST exceeds the ΔT AD for Ni 50 Mn 35 In 14 X with X = In, Al, and Ge by more than 20% and is larger than the Gd based Heusler alloys.

36 MATERIALS SCIENCE↗