Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Graphite”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,621 records · Page 90

Electrochemical method of producing nano-scaled graphene platelets

A method of producing nano-scaled graphene platelets with an average thickness smaller than 30 nm from a layered graphite material. The method comprises (a) forming a carboxylic acid-intercalated graphite compound by an electrochemical reaction; (b) exposing the intercalated graphite compound to a thermal shock to produce exfoliated graphite; and (c) subjecting the exfoliated graphite to a mechanical shearing treatment to produce the nano-scaled graphene platelets. Preferred carboxylic acids are formic acid and acetic acid. The exfoliation step in the instant invention does not involve the evolution of undesirable species, such as NO.sub.x and SO.sub.x, which are common by-products of exfoliating conventional sulfuric or nitric acid-intercalated graphite compounds. The nano-scaled platelets are candidate reinforcement fillers for polymer nanocomposites. Nano-scaled graphene platelets are much lower-cost alternatives to carbon nano-tubes or carbon nano-fibers.

36 MATERIALS SCIENCE↗

AGC-4 Experiment Irradiation Monitoring Data Qualification Final Report

The Graphite Technology Development Program ran a series of six experiments to quantify the effects of irradiation on nuclear grade graphite. This report focuses on the fourth experiment, Advanced Graphite Creep 4 (AGC 4). The Advanced Reactor Development (ARD) Technology Development Office (TDO) Program for research and development activities require documentation of qualified monitoring data to design and license the first high-temperature reactor nuclear plant. Qualified data meets the requirements for use as described in the experiment planning and quality assurance documents. Failed data do not meet the requirements and provide no useable information. Trend data may not meet all requirements but still provide some useable information. Use of Trend data requires assessment of how any deficiencies affect a particular use of the data. AGC-4 began with Advanced Test Reactor (ATR) Cycle 157D on May 30, 2015. After irradiating the graphite for two cycles, the capsule was removed from the reactor after ATR Cycle 158A, which ended on January 2, 2016, due to interference with another experiment. Irradiation was resumed with Cycle 162A on October 7, 2017 after the interfering experiment was removed from the reactor. AGC-4 irradiation completed by the end of Cycle 166B on January 10, 2020. Between Cycles 162A and 166B, AGC-4 capsule was removed from the reactor core during two Powered Axial Locator Mechanism (PALM) Cycles 163A and 165A to avoid overheating. All thermocouples (TCs) have functioned throughout the AGC-4 experiment. A total of 9,256,184 out of all 11,167,213 temperature records (or 82.9%) are Qualified for use by the ARD Program and 1,911,029 missing values are Failed. Argon, helium, and total gas flow data were within expected ranges, except only eight out-of-range values occurred during outages. A total of 21,240,627 out of all 22,288,5103 gas flow rates (or 92.8%) are Qualified for use by the ARD Program and 1,644,476 are Failed records mostly due to missing values. Discharge gas line moisture values were consistently low during full ATR power, except for 162B, when moisture content was increasing to more than 200 ppmv by the end of this cycle. During outages, moisture content reached as high as 700 ppmv. 1,089,941 out of a total of 1,107,331 moisture values (or 98.4%) are within the measurement range of the instrument and are Qualified for use by the ARD Program and 17,390 missing moisture values are Failed. Graphite creep specimens were subjected to one of three loads: 393, 491, or 589 lbf. For a brief period during Cycle 157D between 12:19 on June 2, 2015, and 08:23 on June 11, 2015, the load cells were wired incorrectly, resulting in missing stack load data. Missing stack loads were estimated from measured ram pressures using regression equations developed from the existing data from Cycle 157D. Estimated stack loads during this period are considered to be an accurate representation of actual load applied to the stacks. These loads deviate slightly from the planned loads. This deviation does not prevent the data from being Qualified for use but must be taken into account when analyzing the effect of load on creep. 6,095,728 out of a total of 6,403,985 moisture values (or 95.2%) are within the measurement range of the instrument and are Qualified for use by the ARD Program and 308,257 missing load values are Failed. Stack displacement increased consistently throughout the eight cycles, with total displacement reached highest value of 2.4 in by the end of irradiation. During ATR outages, a set of pneumatic rams raised the stacks of graphite creep specimens to ensure the specimens were not stuck within the test train. This stack raising was performed seven times throughout irradiation. All stacks were raised successfully each time. 4,744,974 out of a total of 6,094,513 displacement values (or 77.9%) are within the measurement range of the instrument and are Qualified for use by the ARD Program and 1,349,539 displacement values are Failed mostly due to missing values. Analyses were conducted on correlations between TCs to look for trends and step changes that might indicate instrument degradation or failure. Correlation analysis was used to identify instances when TCs form short circuits, referred to as virtual junctions, which result in TCs reporting temperatures from some location in the capsule other than the location where they were intended to read. No evidence of virtual junctions was found. Analyses were also conducted on control charts of temperature differences of between two TCs, which are expected to behave consistently throughout the entire irradiation period. Upward or downward trend over time indicates at least one TC in the pair was drifted. Examining control charts for all 66 possible pairs out of twelve TCs installed in the AGC-4 capsules reveal no clear drift failures occurred, except unstable behavior of two TCs in Zone 3, TC-7 and TC-8, over irradiation time. In conclus

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Baseline Characterization Database Verification Report – 2114 Billet A20568

This ECAR provides the results of a validity evaluation of the physical and mechanical property data collected on a billet of nuclear-grade graphite (i.e., 2114 Billet A20568) in support of the ART Baseline Graphite Characterization Program.1,2 Millions of raw data points have been collected during testing and quantification analyses for these billets. The summary scalar property values and supplementary traceability data are collected into comprehensive spreadsheets. Data sets are composed of single billets of graphite for any given grade, organized by mechanical test-specimen type, and further subdivided into individual spreadsheet tabs according to the specific test or evaluation being performed. A direct analysis of properties was not conducted, and this report does not provide information on the validity or performance characteristics of the graphite itself. Rather, this report is intended as a verification of the completeness of actual data collected in accordance with PLN-3467, “Baseline Graphite Characterization Plan: Electromechanical Testing,”3 and their representation of the measurement and test results with sole regard to the graphite billets under evaluation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Direct recycling of lithium-ion battery scraps for manufacturing a new anode

An improved method of recycling lithium-ion battery anode scraps is provided. The method involves isolating an anode scrap including a graphite anode film adhered to a current collector foil with a polyvinylidene fluoride binder. The anode scrap is combined with deionized water to form a first mixture. The graphite anode film is delaminated from the current collector foil to form a second mixture comprising a free collector foil and a free graphite anode film. The free graphite anode film is filtered and dried from the second mixture to recover the free graphite anode film. The free graphite anode film is combined with a solvent comprising N-methyl-2-pyrrolidone (NMP) to form an anode formation slurry. The slurry is coated onto a copper current collector to produce a new anode.

Bai, Yaocai↗

HDG-1 Experiment Irradiation Monitoring Data Qualification Final Report

SUMMARY The U.S. Department of Energy (DOE) Advanced Reactor Technologies (ART) Graphite Research and Development (GRD) Program is conducting a series of six experiments to quantify the effects of irradiation on nuclear-grade graphite. This report documents the qualification of irradiation monitoring data for the fifth experiment, High Dose Graphite-1 (HDG-1). Qualified monitoring data are required by the ART program to support the design and licensing of the first high-temperature reactor (HTR) nuclear plant. Data are classified as Qualified if they meet the usage requirements described in the experiment planning and quality assurance (QA) documents, Failed if they do not meet those requirements and provide no usable information, or Trend if they do not fully meet all requirements but still provide useful information subject to an assessment of how any deficiencies may affect a particular use of the data. HDG-1 irradiation began with Advanced Test Reactor (ATR) Cycle 168B on August 24, 2020, and concluded after Cycle 173C on January 27, 2025. The HDG-1 capsule was removed from the reactor core twice—during core internal change (CIC) Cycle 170A and powered axial locator mechanism (PALM) Cycle 172A—to prevent overheating of the graphite specimens during high-power PALM cycles. The capsule was therefore irradiated during a total of seven normal ATR cycles: 168B, 169A, 171A, 171B, 173A, 173B, and 173C. Irradiation monitoring data evaluated in this report include thermocouple (TC) temperature, gas flow rate, gas moisture, gas pressure, specimen load, and graphite stack displacement. Temperature. A total of 14,508,065 TC temperature records were captured. Of these, 13,901,785 (95.8%) are Qualified and 606,280 (4.2%) are Failed. The principal source of failed temperature data was the instrument failure of TC-9 (Zone 2) on June 24, 2024, and TC-10 (Zone 1) on July 5, 2024, near the end of Cycle 173A, which resulted in 595,554 Failed readings. An additional 379 missing values and 10,347 slightly negative values from TC-13 during ATR outages are also Failed. Neither TC-9 nor TC-10 was used as a temperature-control TC, and their failures did not compromise capsule condition monitoring. Correlation analysis of all 13 TCs found no evidence of virtual junction formation. Control chart analysis revealed clear downward drift of approximately 80°C for TC-6 (Zone 3) relative to other stable TCs, and possible downward drift of approximately 60°C for TC-13 relative to the Zone 5 control TC (TC-1), though TC-13 remained consistent with the Zone 2 control TC (TC-12). Gas flow. A total of 20,088,090 gas flow rate records were captured. Of these, 19,941,463 (99.3%) are Qualified and 146,627 (0.7%) are Failed due to missing values. All argon, helium, and total gas flow data were within expected ranges throughout the irradiation. Gas moisture. A total of 1,116,005 outlet gas moisture values were captured. Of these, 1,101,421 (98.7%) are Qualified and 14,584 (1.3%) are Failed, comprising 14,556 out-of-range values and 28 missing values. The out-of-range moisture values exceeded 22,000 ppmv for approximately 1 week at the beginning of Cycle 173A, when accumulated moisture evaporated after the capsule was retrieved from water storage during PALM Cycle 172A and reinserted into the east flux trap. Moisture levels returned to below 25 ppmv for the remaining three cycles, and the transient high-moisture event did not affect the integrity of specimen irradiation. Gas pressure. A total of 7,812,035 gas pressure values were captured. Of these, 6,642,048 (85.0%) are Qualified and 1,169,987 (15.0%) outlet pressure values are Failed, comprising 718,537 zero outlet pressure values due to sensor failure from Cycle 168B through Cycle 171B, 54,550 missing values, and 396,900 too-low outlet pressure values, ranging from 1.1 to 1.6 psia after sensor replacement during Cycle 173A. Load. A total of 6,696,030 load values were captured. Of these, 6,694,580 (99.98%) are Qualified and 1,450 (0.02%) are Failed due to missing values. Applied loads to the six specimen stacks were stable throughout the irradiation. Stack displacement. A total of 6,696,030 displacement values were captured. Of these, 5,713,297 (85.32%) are Qualified and 3,781 (0.06%) are Failed due to missing values. Stack displacement increased consistently throughout the irradiation, reaching approximately 3.08 in. for Channels 5 and 6 by the end of irradiation. 978,952 (14.62%) substantially elevated displacements observed for Channel 6 beginning in Cycle 171A and for Channel 5 beginning in Cycle 173A are assigned Trend status. Raising pressure. A total of 1,115,999 raising pressure values were captured. Of these, 1,115,430 (99.95%) are Qualified and 569 (0.05%) are Failed due to missing values. Ram pressure. A total of 6,696,030 ram pressure values were captured. Of these, 6,692,249 (99.95%) are Qualified and 3,484 (0.05%) are Failed due to missing values. Stack raising was perf

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enabling fast-charging of lithium-ion batteries through printed electrodes

It has been well recognized that introducing secondary porous networks (SPNs) into the electrodes can effectively improve the electrochemical performance of lithium-ion batteries (LIBs), especially under fast-charging operations. However, the process complexity and high cost limit the commercial success of advanced electrodes with SPNs. To address this issue, we developed a facile screen-printing process to produce structured graphite electrodes with SPNs. The experimental results demonstrated that, by tuning the diameter and center-to-center (C2C) distance of emulsion dots on the stencil screen, the pore diameters and C2C pore distances of SPNs in screenprinted electrodes can be precisely controlled in the range of 100 mu m to 1 mm and 100 mu m to 3 mm respectively. In addition, the SPNs with hexagonal and square-shape pore alignments have also been imprinted onto the electrode coatings through adjusting the patterns of screen stencils. Used as anodes, the printed graphite electrodes demonstrated significantly reduced overpotential and voltage fluctuation under fast-charging operations from 2C to 6C. Coupled with LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) cathodes, the full cells with printed graphite anodes exhibited an unprecedently stable performance with almost no capacity decay up to 170 cycles when charged to 80 % SOC at 2C. Observations from electron microscopy showed plated lithium undetectable at the surface of printed graphite electrodes after numerous cycles. The electrochemical analysis on the voltage evolution during the cell rest period indicated the significantly delayed onset of lithium plating in the presence of printed graphite electrodes. In conclusion, all these results suggest that the significantly improved cell performance is associated with the shortened Li-ion diffusion distance, reduced polarization and suppressed Li plating in the printed electrodes with patterned SPNs.

25 ENERGY STORAGE↗

Gradient porosity electrodes for fast charging lithium-ion batteries

The tendency of Li plating at the surface of thick graphite electrodes greatly limits their application in electrical vehicle (EV) batteries for fast charging applications. To address this concern, we proposed an innovative gradient porosity architecture to facilitate mass transport and suppress Li plating in the thick anodes for fast charging applications. This concept was approved through a thick 3-layered graphite electrode with the highest porosity in the top layer and the lowest porosity in the bottom layer, in contact with the current collector. Here, the gradient porosity structure in the 3-layered graphite electrodes was confirmed by electron microscopy and mercury porosimetry measurements. Used as the anodes of lithium-ion batteries, 3-layered graphite electrodes demonstrated unprecedentedly rate capability and durability superior to 1-layered electrodes. The post-mortem analysis on the cycled cells shows that 3-layered electrodes can significantly suppress Li plating at a high rate up to 4C, which might be responsible for the improved performance of the derived cells. The excellent electrochemical behaviors of 3-layered graphite electrodes are associated with the favored mass transport originating from the unique gradient porosity structure. This is consistent with theoretical studies showing that gradient porosity lowers the Li-ion concentration gradient in the electrolyte in the region close to the separator and slows down the process of reaching the Li plating threshold.

25 ENERGY STORAGE↗

High temperature blackbody BB2000/40 for calibration of radiation thermometers and thermocouple

The cavity-type high temperature blackbody (HTBB) models of BB3200/3500 series are the most spread among metrological institutes worldwide as sources for radiometry and radiation thermometry, due to their ultra high working temperatures, high emissivity and stability. The materials of radiating cavities are graphite, pyrolytic graphite (PG) and their combination. The paper describes BB2000/40 blackbody with graphite-tube cavity that was developed for calibration of radiation thermometers at SCEI (Singapore). The peculiarity of BB2000/40 is a possibility to use it, besides calibration of pyrometers, as an instrument for thermocouples calibration. Operating within the temperature range from 900 °C to 2000 °C, the blackbody has a wide cavity opening of 40 mm. Emissivity of the cavity, with PG heater rings replaced partly by graphite elements, was estimated as 0.998 ± 0.0015 in the spectral range from 350 nm to 2000 nm. The uniformity along the cavity axis, accounting for 10 °C, was measured using a B-type thermocouple at 1500 °C. The BB2000/40, if necessary, can be easily modified, by replacing the graphite radiator with a set of PG rings, to be able to reach temperatures as high as 3200 °C. The HTBB utilizes an optical feedback system which allows temperature stabilization within 0.1 °C. This rear-view feedback allows the whole HTBB aperture to be used for measurements.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Synthesis and characterizations of graphene oxide and reduced graphene oxide nanosheets

Interest in graphene on its excellent mechanical, electrical, thermal and optical properties, it’s very high specific surface area, and our ability to influence these properties through chemical functionalization. Chemical reduction of graphene oxide is one of the main routes of preparation for large quantities of graphenes. Hydrazine hydrate used as reducing agent to prepare for the reduced graphene oxide (RGO). There are a number of methods for generating graphene and chemically modified graphene from natural graphite flakes, graphite derivative (such as graphite oxide) and graphite interaction compounds (i.e. expandable graphite). Here we review the use of colloidal suspensions of reduced graphene oxide (RGO) with large scalable, and is adaptable to a wide variety of applications. The graphene oxide (GO) and the reduced material (RGO) were characterized by XRD, UV-Vis spectroscopy, Thermo-gravimetric analysis (TGA), Raman spectroscopy and Field emission Scanning electron microscopy (FESEM) etc.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

RELICS OF ANCIENT POST-AGB STARS IN A PRIMITIVE METEORITE

Graphite is one of the many presolar circumstellar condensate species found in primitive meteorites. While the isotopic compositions of low-density graphite grains indicate an origin in core-collapse supernovae, some high-density grains have extreme isotopic anomalies in C, Ca, and Ti, which cannot be explained by envelope predictions of asymptotic giant branch (AGB) stars or theoretical supernova models. The Ca and Ti isotopic anomalies, however, match the predictions of He-shell abundances in AGB stars. In this study, we show that the C, Ca, and Ti isotopic anomalies are consistent with nucleosynthesis predictions of the H-ingestion phase during a very late thermal pulse (VLTP) event in post-AGB stars. The low {sup 12}C/{sup 13}C isotopic ratios in these grains are a result of abundant {sup 12}C efficiently capturing the protons that are being ingested during the VLTP. Very high neutron densities of ∼10{sup 15} cm{sup –3}, typical of the i-process, are achieved during this phase in post-AGB stars. The large {sup 42,43,44}Ca excesses in some graphite grains are indicative of neutron capture nucleosynthesis during VLTP. The comparison of VLTP nucleosynthesis calculations to the graphite data also indicate that apparent anomalies in the Ti isotopic ratios are due to large contributions from {sup 46,48}Ca, which cannot be resolved from the isobars {sup 46,48}Ti during the measurements. We conclude that presolar graphite grains with moderate to extreme Ca and Ti isotopic anomalies originate in post-AGB stars that suffer a VLTP.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Impact of corrosion test container material in molten fluorides

The effects of crucible material choice on alloy corrosion rates in immersion tests in molten LiF–NaF–KF (46.5–11.5-42 mol. %) salt held at 850 °C for 500 hrs are described. Four crucible materials were studied. Molten salt exposures of Incoloy-800H in graphite, Ni, Incoloy-800H, and pyrolytic boron nitride (PyBN) crucibles all led to weight-loss in the Incoloy-800H coupons. Alloy weight loss was ~30 times higher in the graphite and Ni crucibles in comparison to the Incoloy-800H and PyBN crucibles. It is hypothesized galvanic coupling between the alloy coupons and crucible materials contributed to the higher corrosion rates. Alloy salt immersion in graphite and Ni crucibles had similar weight-loss hypothesized to occur due to the rate limiting out diffusion of Cr in the alloys to the surface where it reacts with and dissolves into the molten salt, followed by the reduction of Cr from solution at the molten salt and graphite/Ni interfaces. As a result, both the graphite and the Ni crucibles provided sinks for the Cr, in the formation of a Ni–Cr alloy in the case of the Ni crucible, and Cr carbide in the case of the graphite crucible.

14 SOLAR ENERGY↗

Sodium Intercalation of Graphene Films on Re(101̄0)

It is shown that during low-temperature (300–500 K) intercalation of sodium atoms into thin multilayer graphene and graphite films on rhenium the first graphene layer plays the role of a trap to which atoms coming on the surface diffuse through a graphite film. The intercalation phase of the interlayer space in the graphite bulk is actively filled at a sodium atoms concentration under the first graphene layer close to the maximum possible (2 ± 0.5) × 10{sup 14} cm{sup –2}. This phase capacity is proportional to the graphite film thickness that can be varied in this work from one graphene layer to ~50 atomic layers. The diffusion energy E{sub d} of Na atoms through the graphite film was estimated to be E{sub d} ≈ 1.4 eV.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

AGR-1 Irradiated Test Train Preliminary Inspection and Disassembly First Look

The AGR-1 irradiation experiment ended on November 6, 2009, after 620 effective full power days in the Advanced Test Reactor, achieving a peak burnup of 19.6% FIMA. The test train was shipped to the Materials and Fuels Complex in March 2010 for post-irradiation examination. The first PIE activities included non-destructive examination of the test train, followed by disassembly of the test train and individual capsules and detailed inspection of the capsule contents, including the fuel compacts and the graphite fuel holders. Dimensional measurements of the compacts, graphite holders, and steel capsules shells were performed using a custom vision measurement system (for outer diameters and lengths) and conventional bore gauges (for inner diameters). Gamma spectrometry of the intact test train gave a preliminary look at the condition of the interior components. No evidence of damage to compacts or graphite components was evident from the isotopic and gross gamma scans. Neutron radiography of the intact Capsule 2 showed a high degree of detail of interior components and confirmed the observation that there was no major damage to the capsule. Disassembly of the capsules was initiated using procedures qualified during out-of-cell mockup testing. Difficulties were encountered during capsule disassembly due to irradiation-induced changes in some of the capsule components’ properties, including embrittled niobium and molybdenum parts that were susceptible to fracture and swelling of the graphite fuel holders that affected their removal from the capsule shells. This required various improvised modifications to the disassembly procedure to avoid damage to the fuel compacts. Ultimately the capsule disassembly was successful and only one compact from Capsule 4 (out of 72 total in the test train) sustained damage during the disassembly process, along with the associated graphite holder. The compacts were generally in very good condition upon removal. Only relatively minor damage or markings were visible using high resolution photographic inspection. Compact dimensional measurements indicated diametrical shrinkage of 0.9 to 1. 4%, and length shrinkage of 0.2 to 1.1%. The shrinkage was somewhat dependent on compact location within each capsule and within the test train. Compacts exhibited a maximum diametrical shrinkage at a fast neutron fluence of approximately 3×1021 n/cm2. A multivariate statistical analysis indicates that fast neutron fluence as well as compact position in the test train influence compact shrinkage.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

AGR-1, AGR-2 and AGR-3/4 Dimensional Change Data Analysis

A series of Advanced Gas Reactor (AGR) experiments have been completed in the Advanced Test Reactor at Idaho National Laboratory in support of qualification and development of tristructural isotropic fuel. Each AGR test consists of multiple independently controlled and monitored capsules containing fuel compacts placed in a graphite cylinder. These capsules are instrumented with thermocouples embedded in the graphite, enabling temperature control. The fuel compacts are composed of fuel particles surrounded by a graphitic A3 matrix material. Dimensional change in AGR fuel compacts is vital because the swelling or shrinkage affects the size of the gas gaps that are used to control temperatures. Analysis of dimensional change in the AGR fuel compacts is needed to establish the variables directly relating to compact shrinkage. The variables initially identified for consideration were matrix density, compact density, fuel packing fraction, uranium loading, fuel particle diameter, cumulative fast neutron fluence, and volume average time average fuel temperature. In addition to the data available from the AGR experiments, the analysis included specimens formed from the same A3 matrix material used in Advanced Graphite Creep (AGC) experiments, which provide graphite creep data during irradiation for design and licensing purposes. The primary purpose of including the AGC specimens was to encompass dimensional behavior at zero packing fraction, zero uranium loading, and zero particle diameter. All possible combinations of first-order variable regressions were considered in the analysis. The study focused on identifying the best regression models for percent change in diameter, length, and volume. Bootstrap analysis was used to ensure the resulting regression models were robust and well-performing. The variables identified as very significant in predicting change in one or more dimensions (diameter, length, and volume) are volume average time average temperature, fast fluence, compact density, packing fraction and fuel particle diameter. Due to the presence of confounding effects between several variables, interpretation of these results is equivocal; the use of multiple statistical tests provides additional confidence in the conclusion.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

AGR-3/4 Irradiation Test Train Disassembly and Component Metrology First Look Report

The AGR-3/4 experiment was designed to study fission product transport within graphitic matrix material and nuclear-grade graphite. To this end, this experiment consisted of 12 capsules, each fueled with 4 compacts containing UCO TRISO particles as driver fuel and 20 UCO designed-to-fail (DTF) fuel particles in each compact. The DTF fuel was fabricated with a thin pyrocarbon layer which was intended to fail during irradiation and provide a source of fission products. These fission products could then migrate through the compact and into the surrounding concentric rings of graphitic matrix material and/or nuclear graphite. Through post-irradiation examination (PIE) of the rings (including physical sampling and gamma scanning) fission product concentration profiles within the rings can be determined. These data can be used to elucidate fission product transport parameters (e.g. diffusion coefficients within the test materials) which will be used to inform and refine models of fission product transport. After irradiation in the Advanced Test Reactor (ATR) had been completed in April 2014, the AGR-3/4 experiment was shipped to the Hot Fuel Examination Facility (HFEF) at the Materials and Fuels Complex (MFC) for inspection, disassembly, and metrology. The AGR-3/4 test train was received at MFC in two separate shipments between February and April 2015. Visual examinations of the test train exterior did not indicate dimensional distortion, and only two small discolored areas were observed at the bottom of Capsules 8 and 9. No corresponding discoloration was found on the inside of these capsules, however. Prior to disassembly, the two test train sections were subject to analysis via the Precision Gamma Scanner (PGS), which did not indicate that any gross fuel relocation had occurred. A series of specialized tools (including clamps, cutters, and drills) had been designed and fabricated in order to carry out test train disassembly and recovery of capsule components (graphite rings and fuel compacts). This equipment performed well for separating each capsule in the test train and extracting the capsule components. Only a few problems were encountered. In one case, the outermost ring (the sink ring) was cracked during removal of the capsule through tubes. Although the sink ring will be analyzed in order to obtain a mass balance of fission products in the experiment, these cracks do not pose a major concern because the sink ring will not be analyzed in detail to obtain the spatial distribution of fission products. In Capsules 4 and 5, the compacts could not be removed from the inner rings. Strategies for removing the compacts are being evaluated. Sampling the inner rings with the compacts in-place is also an option. Dimensional measurements were made on the compacts, inner rings, outer rings, and sink rings. The diameters of all compacts decreased by 0.5 to 2.0 %. Generally, the extent of diametric shrinkage increased linearly with increasing neutron fluence. Most compact lengths also decreased. Compact lengths decreased with increasing fluence, reaching maximum shrinkage of about 0.9 % at a fast fluence of 4.0x1025 n/m2 E > 0.18 MeV. Above this fluence, the extent of length shrinkage appeared to decrease with fluence, and two compacts from Capsule 7 were found to have slightly increased in length (< 0.1 %) after a fluence of 5.2x1025 n/m2.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Air Ingress Analysis: Part 1 - Theoretical Approach

Idaho National Laboratory (INL), under the auspices of the U.S. Department of Energy (DOE), is performing research and development that focuses on key phenomena important during potential scenarios that may occur in very high temperature gas-cooled reactors (VHTRs). Phenomena identification and ranking studies to date have ranked an air ingress event, following on the heels of a VHTR depressurization, as important with regard to core safety. Consequently, the development of advanced air-ingress-related models and verification and validation data are a very high priority. Following a loss of coolant and system depressurization incident, air will enter the core of the VHTR through the break, possibly causing oxidation of the graphite core and reflector graphite structure. Simple core and plant models indicate that, under certain circumstances, the oxidation may proceed at an elevated rate with additional heat generated from the oxidation reaction itself. Under postulated conditions of fluid flow and temperature, excessive degradation of lower plenum graphite caused by graphite oxidation can lead to a loss of mechanical strength. Excessive oxidation of core graphite can also lead to a release of fission products into the confinement, which could be detrimental to reactor safety. Analytical models developed in this study will improve our understanding of this phenomenon. This paper presents two sets of analytical models for the qualitative assessment of the air ingress phenomena. The results from the analytical models are compared with results of the computational fluid dynamic models (CFD) in the subsequent paper. The analytical models agree well with those CFD results.

99 GENERAL AND MISCELLANEOUS↗

STUDY ON AIR INGRESS MITIGATION METHODS IN THE VERY HIGH TEMPERATURE GAS COOLED REACTOR (VHTR)

An air-ingress accident followed by a pipe break is considered as a critical event for a very high temperature gas-cooled reactor (VHTR). Following helium depressurization, it is anticipated that unless countermeasures are taken, air will enter the core through the break leading to oxidation of the in-core graphite structure. Thus, without mitigation features, this accident might lead to severe exothermic chemical reactions of graphite and oxygen. Under extreme circumstances, a loss of core structural integrity may occur along with excessive release of radiological inventory. Idaho National Laboratory under the auspices of the U.S. Department of Energy is performing research and development (R&D) that focuses on key phenomena important during challenging scenarios that may occur in the VHTR. Phenomena Identification and Ranking Table (PIRT) studies to date have identified the air ingress event, following on the heels of a VHTR depressurization, as very important (Oh et al. 2006, Schultz et al. 2006). Consequently, the development of advanced air ingress-related models and verification and validation (V&V) requirements are part of the experimental validation plan. This paper discusses about various air-ingress mitigation concepts applicable for the VHTRs. The study begins with identifying important factors (or phenomena) associated with the air-ingress accident by using a root-cause analysis. By preventing main causes of the important events identified in the root-cause diagram, the basic air-ingress mitigation ideas can be conceptually derived. The main concepts include (1) preventing structural degradation of graphite supporters; (2) preventing local stress concentration in the supporter; (3) preventing graphite oxidation; (4) preventing air ingress; (5) preventing density gradient driven flow; (4) preventing fluid density gradient; (5) preventing fluid temperature gradient; (6) preventing high temperature. Based on the basic concepts listed above, various air-ingress mitigation methods are proposed in this study. Among them, the following two mitigation ideas are extensively investigated using computational fluid dynamic codes (CFD): (1) helium injection in the lower plenum, and (2) reactor enclosure opened at the bottom. The main idea of the helium injection method is to replace air in the core and the lower plenum upper part by buoyancy force. This method reduces graphite oxidation damage in the severe locations of the reactor inside. To validate this method, CFD simulations are addressed here. A simple 2-D CFD model is developed based on the GT-MHR 600MWt design. The simulation results showed that the helium replace the air flow into the core and significantly reduce the air concentration in the core and bottom reflector potentially protecting oxidation damage. According to the simulation results, even small helium flow was sufficient to remove air in the core, mitigating the air-ingress successfully. The idea of the reactor enclosure with an opening at the bottom changes overall air-ingress mechanism from natural convection to molecular diffusion. This method can be applied to the current system by some design modification of the reactor cavity. To validate this concept, this study also uses CFD simulations based on the simplified 2-D geometry. The simulation results showed that the enclosure open at the bottom can successfully mitigate air-ingress into the reactor even after on-set natural circulation occurs.

99 GENERAL AND MISCELLANEOUS↗

Small Specimen Data from a High Temperature HFIR Irradiation Experiment

The HTV capsule is a High Flux Isotope Reactor (HFIR) target-rod capsule designed to operate at very high temperatures. The graphite containing section of the capsule (in core) is approximately 18 inches (457.2 mm) long and is separated into eight temperature zones. The specimen diameters within each zone are set to achieve the desired gas gap and hence design temperature (900 C, 1200 C or 1500 C). The capsule has five zones containing 0.400 inch (10.16 mm) diameter specimens, two zones containing 0.350 inch (8.89 mm) diameter specimens and one zone containing 0.300 inch (7.62 mm) diameter specimens. The zones have been distributed within the experiment to optimize the gamma heating from the HFIR core as well as minimize the axial heat flow in the capsule. Consequently, there are two 900 C zones, three 1200 C zones, and three 1500 C zones within the HTV capsule. Each zone contains nine specimens 0.210 0.002 inches (5.334 mm) in length. The capsule will be irradiated to a peak dose of 3.17 displacements per atom. The HTV specimens include samples of the following graphite grades: SGL Carbon s NBG-17 and NBG-18, GrafTech s PCEA, Toyo Tanso s IG-110, Mersen s 2114 and the reference grade H-451 (SGL Carbon). As part of the pre-irradiation program the specimens were characterized using ASTM Standards C559 for bulk density, and ASTM C769 for approximate Young s modulus from the sonic velocity. The probe frequency used for the determination of time of flight of the ultrasonic signal was 2.25 MHz. Marked volume (specimen diameter) effects were noted for both bulk density (increased with increasing specimen volume or diameter) and Dynamic Young s modulus (decreased with increasing specimen volume or diameter). These trends are extended by adding the property vs. diameter data for unirradiated AGC-1 creep specimens (nominally 12.5 mm-diameter x 25.4 mm-length). The relatively large reduction in Dynamic Young s Modulus was surprising given the trend for increasing density with increasing volume. The graphite-filler particle size was noted to be influential in the volume dependency data, with finer grained graphites showing the least specimen volume/diameter effect. Here the volume dependency trends are discussed in terms of the graphite s filler-particle size and texture.

graphite↗