At least 1,621 records · Page 90

Evaluation of a Fluorochlorozirconate Glass-Ceramic Storage Phosphor Plate for Gamma-Ray Computed Radiography

In this paper, a fluorochlorozirconate (FCZ) glass-ceramic containing orthorhombic barium chloride crystals doped with divalent europium was evaluated for use as a storage phosphor in gamma-ray imaging. X-ray diffraction and phosphorimetry of the glass-ceramic sample showed the presence of a significant amount of orthorhombic barium chloride crystals in the glass matrix. Transmission electron microscopy and scanning electron microscopy were used to identify crystal size, structure, and morphology. The size of the orthorhombic barium chloride crystals in the FCZ glass matrix was very large, ~0.5–0.7 μm, which can limit image resolution. The FCZ glass-ceramic sample was exposed to 1 MeV gamma rays to determine its photostimulated emission characteristics at high energies, which were found to be suitable for imaging applications. Test images were made at 2 MeV energies using gap and step wedge phantoms. Gaps as small as 101.6 μm in a 440 stainless steel phantom were imaged using the sample imaging plate. Analysis of an image created using a depleted uranium step wedge phantom showed that emission is proportional to incident energy at the sample and the estimated absorbed dose. Finally, the results showed that the sample imaging plate has potential for gamma-ray-computed radiography and dosimetry applications.

36 MATERIALS SCIENCE↗

Effects of heating rate, quartz particle size, viscosity, and form of glass additives on high‐level waste melter feed volume expansion

Abstract Nuclear waste can be vitrified by mixing it with glass‐forming and ‐modifying additives. The resulting feed is charged into an electric glass melter. To comprehend melting behavior of a high‐alumina melter feed, we monitored the volume expansion of pellets in response to heating at different heating rates. The feeds were prepared with different particle sizes of quartz (the major additive component) and with varied silica‐to‐fluxes ratio to investigate the glass melt viscosity effects. Also, we used additional melter feeds with additives premelted into glass frit. The volume of pellets was nearly constant at temperatures <600°C. After a short period of volume shrinkage at ~600°C‐700°C, foam generation produced massive volume expansion. The low heat conductivity of foam hinders the transfer of heat from molten glass to the reacting feed. The extent of foaming increased with faster heating and higher melt viscosity, and decreased with increasing size of quartz particles and fritting of the additives. Volume expansion data are needed for the mathematical modeling of the cold cap.

Lee, SeungMin↗

Topological controls on aluminosilicate glass dissolution: Complexities induced in hyperalkaline aqueous environments

Abstract Fly ash, an aluminosilicate composite consisting of disordered (major) and crystalline (minor) compounds, is a low‐carbon alternative that can partially replace ordinary portland cement (OPC) in the binder fraction of concrete. Therefore, understanding the reactivity of fly ash in the hyperalkaline conditions prevalent in concrete is critical to predicting concrete's performance; including setting and strength gain. Herein, temporal measurements of the solution composition (using inductively coupled plasma‐optical emission spectrometry: ICP‐OES) are used to assess the aqueous dissolution rate of monophasic synthetic aluminosilicate glasses analogous to those present in technical fly ashes, under hyperalkaline conditions (10 ≤ pH ≤ 13) across a range of temperatures (25°C ≤ T≤45°C). The dissolution rate is shown to depend on the average number of topological constraints per atom within the glass network (n c , unitless), but this dependence weakens with increasing pH (>10). This is postulated to be on account of: (a) time‐dependent changes in the glass’ surface structure, that is, the number of topological constraints; and/or (b) a change in the dissolution mechanism (eg from network hydrolysis to transport control). The results indicate that the topological description of glass dissolution is most rigorously valid only at very short reaction times (ie at high undersaturations), especially under conditions of hyperalkalinity. These findings provide an improved basis to understand the underlying factors that affect the initial and ongoing reactivity of aluminosilicate glasses such as fly ash in changing chemical environments, for example, when such materials are utilized in cementitious composites.

Oey, Tandré↗

Accelerated discovery of metallic glasses through iteration of machine learning and high-throughput experiments

With more than a hundred elements in the periodic table, a large number of potential new materials exist to address the technological and societal challenges we face today; however, without some guidance, searching through this vast combinatorial space is frustratingly slow and expensive, especially for materials strongly influenced by processing. We train a machine learning (ML) model on previously reported observations, parameters from physiochemical theories, and make it synthesis method–dependent to guide high-throughput (HiTp) experiments to find a new system of metallic glasses in the Co-V-Zr ternary. Experimental observations are in good agreement with the predictions of the model, but there are quantitative discrepancies in the precise compositions predicted. We use these discrepancies to retrain the ML model. The refined model has significantly improved accuracy not only for the Co-V-Zr system but also across all other available validation data. We then use the refined model to guide the discovery of metallic glasses in two additional previously unreported ternaries. Although our approach of iterative use of ML and HiTp experiments has guided us to rapid discovery of three new glass-forming systems, it has also provided us with a quantitatively accurate, synthesis method–sensitive predictor for metallic glasses that improves performance with use and thus promises to greatly accelerate discovery of many new metallic glasses. We believe that this discovery paradigm is applicable to a wider range of materials and should prove equally powerful for other materials and properties that are synthesis path–dependent and that current physiochemical theories find challenging to predict.

36 MATERIALS SCIENCE↗

Emergent Halperin–Saslow mode, gauge glass and quenched disorders in quantum Ising magnet TmMgGaO 4

Quenched disorders could bring novel quantum excitations and models to certain quantum magnets. Motivated by recent experiments on the quantum Ising magnet TmMgGaO 4 , we explore the effects of the quenched disorder and the interlayer coupling in this triangular lattice Ising antiferromagnet. It is pointed out that the weak quenched (nonmagnetic) disorder would convert the emergent 2D Berezinskii–Kosterlitz–Thouless (BKT) phase and the critical region into a U(1) gauge glass. There will be an emergent Halperin–Saslow mode associated with this gauge glass. Using the Imry-Ma’s renormalization group result, we explain the fate of the finite-field [Formula: see text] symmetry breaking transition at the low temperatures. The ferromagnetic interlayer coupling would suppress the BKT phase and generate a tiny ferromagnetism. With quenched disorders, this interlayer coupling changes the 2D gauge glass into a 3D gauge glass, and the Halperin–Saslow mode persists. This work merely focuses on addressing a phase regime in terms of emergent U(1) gauge glass behaviors and hope to inspire future works and thoughts in weakly disordered frustrated magnets in general.

Physics↗

Photostability can be significantly modulated by molecular packing in glasses

While previous work has demonstrated that molecular packing in organic crystals can strongly influence photochemical stability, efforts to tune photostability in amorphous materials have shown much smaller effects. Here we show that physical vapor deposition can substantially improve the photostability of organic glasses. Disperse Orange 37 (DO37), an azobenzene derivative, is studied as a model system. Photostability is assessed through changes in the density and molecular orientation of glassy thin films during light irradiation. By optimizing the substrate temperature used for deposition, we can increase photostability by a factor of 50 relative to the liquid-cooled glass. Photostability correlates with glass density, with density increases of up to 1.3%. Coarse-grained molecular simulations, which mimic glass preparation and the photoisomerization reaction, also indicate that glasses with higher density have substantially increased photostability. These results provide insights that may assist in the design of organic photovoltaics and light emission devices with longer lifetimes.

36 MATERIALS SCIENCE↗

Enhanced laser-induced damage performance of all-glass metasurfaces for energetic pulsed laser applications

To fabricate optical components with surface layers compatible with high power laser applications that may operate as antireflective coatings, polarization rotators, or harness physical anisotropy for other uses, metasurfaces are becoming an appealing candidate. In this study, a large-beam (1.05 cm diameter) 351-nm laser-induced damage testing was done on an all-glass metasurface structure composed of cone-like features with a subwavelength spacing of adjacent features. These structures were fabricated on untreated fused silica glass and damage tested, as were structures that were fabricated on fused silica glass that experienced a preliminary etching process to remove the surface Beilby layer that is characteristic of polished fused silica. The laser-induced damage onset for structures on untreated fused silica glass was 19.3 J∙cm -2 , while the sample that saw an initial pretreatment etch exhibited an improved damage onset of 20.4 J∙cm -2 , only 6% short of the reference pretreated glass damage onset of 21.7 J∙cm -2 . For perspective, the National Ignition Facility (NIF) operational average fluence at this wavelength and pulse length is about 10 J/cm2. At a fluence of 25.5 J∙cm -2 , the reference (pretreated) fused silica initiated 5.2 damage sites per mm 2 , while the antireflective metasurface sample with a preliminary etching process treatment initiated 9.8 damage sites per mm 2 . In conclusion, these findings demonstrate that substrate-engraved metasurfaces are compatible with high energy and power laser applications, further broadening their application space.

36 MATERIALS SCIENCE↗

Melt Rate Enhancement for High Aluminum HLW Glass Formulation (Final Report)

The principal objective of the work reported here was to develop and identify HLW glass compositions that maximize waste processing rates for the aluminum limted waste composition specified by ORP while maintaining high waste loadings and acceptable glass properties. This was accomplished through a combination of crucible-scale tests, confirmation tests on the DM100 melter system, and demonstration at pilot scale (DM1200). The DM100-BL unit was selected for these tests since it was used previously with the HLW waste streams evaluated in this study, was used for tests on HLW glass compositions to support subsequent tests on the HLW Pilot Melter, conduct tests to determine the effect of various glass properties (viscosity and conductivity) and oxide concentrations on glass production rates with HLW feed streams, and to assess the volatility of cesium and technetium during the vitrification of an HLW AZ-102 composition.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Enhanced LAW Glass Formulation Testing (Final Report)

The principal objective of this work was to extend the glass formulation methodology developed in the earlier work for Envelope A, B and C waste compositions for development of compliant glass compositions targeting five high sodium-sulfur waste loading regions. This was accomplished through a combination of crucible-scale tests, and tests on the DM10 melter system. The DM10 was used for several previous tests on LAW compositions to determine the maximum feed sulfur concentrations that can be processed without forming secondary sulfate phases on the surface of the melt pool. This melter is the most efficient melter platform for screening glass compositions over a wide range of sulfate concentrations and therefore was selected for the present tests. The tests were conducted to provide information on melter processing characteristics and off-gas data, including sulfur incorporation and partitioning. As described above, the main objective was to identify the limits of waste loading in compliant glass formulations spanning the range of expected Na 2 O and SO 3 concentrations in the LAW glasses.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Micro-Continuum Modeling of Nuclear Waste Glass Corrosion

The purpose of this contribution is to report on preliminary nano-continuum scale modeling of nuclear waste glass corrosion. The focus of the modeling is an experiment involving a French glass SON68 specimen leached for 25 years in a granitic environment (Guittonneau et al., 2011; Gin et al., 2011; Gin et al., 2013). The 25 year experiment carried out by French scientists offers a unique opportunity to examine the controls on the rate of nuclear glass corrosion under controlled experimental conditions using a borosilicate glass of the kind widely considered for nuclear waste storage. The long term experiment makes it possible to move beyond the initial rate stage, with direct measurements of the longer term, residual rates of corrosion. Important in this regard is whether the rate of corrosion shows a parabolic dependence on time, as would be expected from a conventional diffusion model in which the reaction products (amorphous silica-rich gel) create a diffusion barrier that grows in width over time, or whether the time dependence is linear (Guittonneau et al., 2011). A linear dependence on time would call into question the model of a Passive Reactive Interface (PRI) presented by Cailleteau et al. (2008), although it does not entirely preclude such a model if the interface maintains a constant width over time (forming at the leading edge next to the pristine glass and dissolving at the trailing edge). The leachate concentration measurements collected every 56 days over 25 years by Guittonneau et al. (2011) provide data to constrain the long term corrosion rate and its time dependence.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enhanced LAW Glass Correlation - Phase 1

About 50 million gallons of high-level mixed waste is currently stored in underground tanks at the United States Department of Energy’s (DOE’s) Hanford site in the State of Washington. The Hanford Tank Waste Treatment and Immobilization Plant (WTP) will provide DOE’s Office of River Protection (ORP) with a means of treating this waste by vitrification for subsequent disposal. The tank waste will be separated into low- and high-activity waste fractions, which will then be vitrified respectively into Immobilized Low Activity Waste (ILAW) and Immobilized High Level Waste (IHLW) products. The ILAW product will be disposed in an engineered facility on the Hanford site while the IHLW product is designed for acceptance into a national deep geological disposal facility for high-level nuclear waste. The ILAW and IHLW products must meet a variety of requirements with respect to protection of the environment before they can be accepted for disposal. Acceptable glass formulations for vitrification of Hanford low activity waste (LAW) must meet a variety of product quality, processability, and waste loading requirements. To this end, The Vitreous State Laboratory (VSL) at The Catholic University of America (CUA) developed and tested a number of glass formulations during Part A, Part B1 and Part B2 of the WTP development program. The testing resulted in the selection of target glass compositions for the processing of eight of the Phase I LAW tanks. The selected glass compositions were tested at the crucible scale to confirm their compliance with ILAW performance requirements. Duramelter 100 (DM100) and LAW Pilot Melter tests were then conducted to demonstrate the viability of these glass compositions for LAW vitrification at high processing rates.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Measurements of Sulfur Concentration with Lower Detection Limits in Simulated LAW Glasses

This report provides sulfur concentration measurements for several simulated low-activity waste glass compositions. The Pacific Northwest National Laboratory (PNNL) selected and fabricated these glasses as part of a study on sulfur retention in glass. Methods were selected to achieve a lower detection limit for SO 3 than previously reported. The measured SO 3 concentrations of the glasses range from 0.036 to 0.130 wt %. These results will be used by PNNL in the development of improved property/composition models for LAW glass production at Hanford

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Effect of Aging on the Delamination Fracture Energy of Glass Solar Reflectors

Thin metal and metal oxide films deposited on glass or polymer substrates have been widely applied to manufacture front surfaced solar reflectors such as those used in the concentrated solar power (CSP) systems due to the facts that they are highly transparent, resistant to ultraviolet (UV) light and abrasion, and chemically inert. However, the reliable operation over long periods of outdoor exposure of such solar reflectors depends on the adequate adhesion between each layer to prevent delamination and subsequent failure. We report results from measurements of the delamination fracture energy (DFE) of the weakest interface in both as-deposited and aged reflectors, where the reflector construction consists of a glass/copper/silver/oxide stack. In this study, DFE was measured using a width-tapered beam method and the test results showed that the weakest interface of this solar reflector is the copper-glass interface, with a delamination fracture energy of approximately 4.4 J/m 2 . In order to verify the test results, finite element (FE) simulations were run using the commercial software package ABAQUS 6.14 based on the cohesive zone model (CZM). In the simulations, the DFE derived from the delamination measurement was treated as an input and the delamination forces from the FE simulations were compared to the experimental results. The good agreement between the tested and simulated delamination force indicated that this width-tapered beam method is accurate even for very small DFE, making it appropriate to test the DFE of front surfaced glass solar reflectors. Additionally, in order to study the aging effect on the DFE, accelerated aging tests were conducted using samples with different protective coatings, one group of samples with alumina ( Al 2 O 3 ) protective coating and the other group with titania ( TiO 2 ) protective coating. The DFE after 50 and 100 hours of accelerated aging were measured. The test results showed that the copper-glass interface would still be the weakest interface for all samples after aging, and the DFE for samples with Al 2 O 3 protective coating was unchanged whereas the copper-glass interface was found to undergo statistically significant change after both 50 and 100 hours of aging for samples with TiO 2 protective coating. We found that DFE at the copper/glass interface decreased after 50 hours of aging then increased after 100 hours of aging. The origin of this non-monotonic response of TiO 2 coated reflectors under accelerated aging conditions is unknown.

36 MATERIALS SCIENCE↗

DFLAW Glass and Feed Qualifications to Support WTP Start-Up and Flow-Sheet Development (Final Report, Rev. 0)

In each test, a distinct feed composition was used to determine the effects of feed composition changes on the retention of technetium and other species as detailed in the Test Plan for this work. Key operating parameters such as the glass temperature (nominally 1150°C) were held constant to investigate the effect of each new feed composition on the retention of technetium. The processing rate was maintained at ≈2,250 kg/m 2 /day of glass, which corresponds to the “stretch-goal” rate of 22.5 MT/day specified by ORP for the WTP LAW melter, or ≈2,000 kg/m 2 /day of glass, which corresponds to the enhanced baseline specified by ORP for the WTP LAW melter (as compared to the nominal 1500 kg/m 2 /day). The bubbling rate was adjusted to achieve a near-complete cold-cap (90-100% of melt surface covered with feed). Quantitative measurements of glass production rates, melter operating conditions (temperatures, pressures, power, flows, etc.), gaseous emissions by Fourier Transform Infrared Spectroscopy (FTIR), and particulate emissions using Environmental Protection Agency (EPA) methods were made for each test. Discharged and melt pool glass samples were inspected for formation of any salt phases and analyzed for chemical composition, including technetium content. Samples of the process fluids from each of the off-gas treatment system components were collected and analyzed. Following each test, the off-gas system was partially disassembled and extensively sampled for any residual feed components residing within the off-gas system. Sampling and analysis during and subsequent to each test was intended to be sufficient for supporting a mass balance for all constituents of interest and particularly technetium, rhenium, iodine, sulfur, chlorine, and fluorine. Additional sampling and analysis of evaporator concentrates and condensates was conducted for various organic compounds.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Selection of Glasses in Support of the Sludge Batch 9 Sulfate Solubility Limit for Coupled Operation with the Salt Waste Processing Facility

For Sludge Batches 3 through 8, the sulfate (SO 4 2- )solubility limit for the Defense Waste Processing Facility (DWPF) has been determined by laboratory-scale crucible testing. In preparation for Sludge Batch 9 (SB9) processing, a comparison demonstrated that minor compositional differences existed between the Sludge Batch 8 (SB8)-Frit 803 and SB9-Frit 803 glass composition regions for sludge-only and coupled operations with the Actinide Removal Process (ARP) and Modular Caustic Side Solvent Extraction Unit (MCU). Thus, no experimental testing was necessary and the SB8 SO 4 2- limit of 0.65 wt.% was recommended for SB9 processing. This previous SB9 assessment did not address coupled processing with streams from the Salt Waste Processing Facility (SWPF), which is anticipated to start operations in November 2019. These high activity streams will include monosodium titanate (MST) and sludge solids from the Sludge Solids Receipt Tank (SSRT) as well as Cs-containing strip effluent (SE). The incorporation of these SWPF streams is expected to reach TiO 2 concentrations in glass greater than 2 wt.% based on single and double MST strike scenarios. In support of coupled operation with SWPF, the DWPF Product Composition Control System was revised and allows a TiO 2 concentration of up to 6 wt.% (minus measurement uncertainty) in glass. For the SB8-Frit 803 SO 4 2- solubility study, the maximum TiO 2 concentration evaluated was 0.94 wt.%. Since the influence of increased TiO 2 on the retention of SO 4 2- in the SB9 glass region is unknown, a test matrix of ten glass compositions has been proposed to determine whether the 0.65 wt.% SO 4 2- limit is still appropriate for SB9 coupled operation with SWPF. This report documents the development of a test matrix that will support this study.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Liquidus Temperature: Assessing Standard Glasses for Furnace Calibration

Standard glasses are used to ensure accurate liquidus temperature measurements and furnace temperatures. The supply of the standard glasses used at Pacific Northwest National Laboratory (Standard Reference Material 773 [SRM-773]) has been depleted. Replacement standard glasses for furnace temperature verification and liquidus temperature measurement validation were fabricated and tested. Two glasses-ARG-1 and AmCm2-19-were fabricated in roughly 5 kg batches. The liquidus temperature of the glasses was measured and found to be consistent with those reported in literature.

36 MATERIALS SCIENCE↗

Glass-Ceramic Material Modeling

Glass-ceramics are a unique class of materials in which the growth of a ceramic phase(s) may be induced in an inorganic glass resulting in a microstructurally heterogeneous material with both glass and ceramic phases. This specialized processing is often referred to as "ceramming''. A wide variety of such materials have been developed through the use of different initial glass compositions and thermomechanical processing routes and that have enabled applications in dentistry, consumer kitchenware, and telescopes mirrors. These materials may also exhibit large apparent coefficients of thermal expansion making them attractive for consideration in glass-ceramic seals. These large apparent coefficients of thermal expansion often arise from silica polymorphs, such as cristobalite, undergoing a solid-to-solid phase transformations producing additional non-linearity in the effective material response.

36 MATERIALS SCIENCE↗

The Precision of Product Consistency Tests with Reference Glasses ARM-1 and SRM 623

An interlaboratory study (ILS) was conducted in 2014 to measure the precision with which the ASTM-International product consistency test method A (PCT-A) can be performed using properly prepared samples of reference glass ARM-1 or SRM 623 and test parameter values near the centers of ranges specified in procedure ASTM C1285. The ILS did not evaluate the full range of test parameter values allowed in the PCT-A method and the results do not represent the precision that should be expected if extreme values of the ranges are used. However, the precision measured in the ILS quantified the precision of tests conducted with mean parameters that were used to estimate the effects of individual parameters. Follow-on tests were conducted to assess the effects of several individual test parameter values on the test response and uncertainties in the derived glass dissolution rates. The effects of particle size distributions in glass samples prepared by wet- and dry-sieving methods, methods to remove fines, and the limiting parameter values for the water-to-glass (w/g) mass ratio and test duration allowed in PCT-A were measured. Test responses for all variations except test duration exceeded the precision measured in the ILS for conducting triplicate PCT-A tests within a single laboratory. The accuracy of glass dissolution rates derived from PCT results benefits from using a tighter control of these test variables than required in ASTM C1285. Comparison with previous analyses of the method shows how use of the relative standard deviation to represent the test precision can be misleading, and that the mean response and standard deviation should both be considered.

36 MATERIALS SCIENCE↗