At least 163 records · Page 9

Redox chemistry of plutonium and plutonium surrogates in vitrified nuclear wastes

Lanthanide borosilicate glasses containing Pu and the analog element, Ce, were subjects of an X-ray absorption spectroscopy investigation to quantify the +3/+4 ratio of the redox-sensitive element. The data show that the dominant oxidation states are +4 for Pu and +3 for Ce. The data also indicate that the reductive potential of glasses can be quantified, although allowances must be made for glass composition, from a solution chemistry method adapted to glass chemistry. These data can therefore be used to formulate glass compositions and processing schedules that lead to knowledge of the oxidation state of Pu in melts. Furthermore, the data show that Ce is a poor analog for Pu behavior in melt and that the suitability of surrogates can be evaluated by this method. The methods demonstrated in this paper can be used to estimate the oxidation states of a range of multi-valent elements as functions of temperature and composition with data from only a single redox couple.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

SPRUCE S1 Bog Porewater, Groundwater, and Stream Chemistry Data: 2011-2013

This data set reports the chemistry of S1 bog porewater, outlet stream water, and groundwater from upland wells from 2011 through 2013. These data provide information for studies of the biogeochemical status of the bog and surrounding groundwater aquifer. Porewater samples were collected from one nest of 6 piezometers installed in a hollow in the south end of the S1 bog to characterize solute chemistry depth profiles. Peat porewater was collected from piezometers that opened at 0, 0.3, 0.5, 1, 2, and 3 m depths below hollow surfaces. Samples were collected weekly (2011) or monthly (2012 & 2013) when the samplers were not frozen (typically June – November). Stream water was sampled weekly (2011-2013) from the outlet of the S1 bog (located on the southern edge of the bog). Four groundwater wells located in the uplands of the S1 watershed were sampled monthly in 2013. Bog water level data are also reported for the S1 bog. Water samples were analyzed for pH, specific conductivity, nutrient concentrations (ammonium, nitrate, soluble reactive phosphorus, total nitrogen, total phosphorus), cation concentrations (calcium, potassium, magnesium, sodium, aluminum, iron, manganese, silicon, strontium), anion concentrations (chloride, sulfate), and total organic carbon concentrations. The experimental work is to be conducted in a Picea mariana [black spruce] – Sphagnum spp. bog forest in northern Minnesota, 40 km north of Grand Rapids, in the USDA Forest Service Marcell Experimental Forest (MEF).

54 ENVIRONMENTAL SCIENCES↗

Gel nanostructure in alkali-activated binders based on slag and fly ash, and effects of accelerated carbonation

Binders formed through alkali-activation of slags and fly ashes, including ‘fly ash geopolymers’, provide appealing properties as binders for low-emissions concrete production. However, the changes in pH and pore solution chemistry induced during accelerated carbonation testing provide unrealistically low predictions of in-service carbonation resistance. The aluminosilicate gel remaining in an alkali-activated slag system after accelerated carbonation is highly polymerised, consistent with a decalcification mechanism, while fly ash-based binders mainly carbonate through precipitation of alkali salts (bicarbonates at elevated CO{sub 2} concentrations, or carbonates under natural exposure) from the pore solution, with little change in the binder gel identifiable by nuclear magnetic resonance spectroscopy. In activated fly ash/slag blends, two distinct gels (C–A–S–H and N–A–S–H) are formed; under accelerated carbonation, the N–A–S–H gel behaves comparably to fly ash-based systems, while the C–A–S–H gel is decalcified similarly to alkali-activated slag. This provides new scope for durability optimisation, and for developing appropriate testing methodologies. -- Highlights: •C-A-S-H gel in alkali-activated slag decalcifies during accelerated carbonation. •Alkali-activated fly ash gel changes much less under CO{sub 2} exposure. •Blended slag-fly ash binder contains two coexisting gel types. •These two gels respond differently to carbonation. •Understanding of carbonation mechanisms is essential in developing test methods.

36 MATERIALS SCIENCE↗

Uptake of aqueous heavy metal ions (Co2+, Cu2+ and Zn2+) by calcium-aluminium-silicate-hydrate gels

Highlights: • C-A-S-H gels containing metal ions (Co{sup 2+}, Cu{sup 2+} or Zn{sup 2+}) were precipitated by a sol-gel technique. • Uptake mechanism and immobilization capacity of divalent metal ions by C-A-S-H are elucidated. • Up to ~55–60 mol% of Zn can be incorporated in defective tobermorite-type C-A-S-H. • Metal uptake by C-A-S-H is controlled mainly by isomorphous substitution for Ca ions. • Crystal-chemical features of C-A-S-H gels and implications for practical application are discussed. Calcium-aluminium-silicate-hydrate (C-A-S-H) gels containing heavy metal ions (Me: Co{sup 2+}, Cu{sup 2+} or Zn{sup 2+}) were precipitated at different Me/Si molar ratios to study the uptake mechanism and immobilization capacity. Aqueous solution chemistry and solid-phase characterization using XRD, FTIR, ESEM-EDX, TEM-HAADF and TG-DSC methods reveal threshold values for ion substitution of ~55–60 mol% for Zn, ~30–40 mol% for Co and ~25–30 mol% for Cu in defective tobermorite-type C-A-S-H with (Ca + Me)/(Si + Al) molar ratios from 0.86 to 1.04. At higher aqueous Me concentrations, Me (chloride) hydroxides start to co-precipitate. The uptake mechanism of Me ions by C-A-S-H is based on (i) isomorphous substitution of Me for Ca in the CaO layer, (ii) ion exchange in the interlayer, (iii) tetrahedral substitution (Zn) within the dreierketten chains and (iv) surface adsorption onto the C-A-S-H gel structure. Systematics in crystal-chemistry of Me-bearing C-A-S-H and implications for application and performance in natural and man-made settings are discussed.

36 MATERIALS SCIENCE↗

Non-stoichiometry Governs the Pathway from Amorphous to Crystalline Calcium Carbonate

The controlled crystallization of calcium carbonate underlies the elaborate architectures of marine corals, the design of biomimetic materials, and the global carbon cycle. Despite its ubiquity, the chemical mechanisms that govern the crystallization of calcium carbonate from its amorphous precursor, amorphous calcium carbonate (ACC), remain elusive, largely due to the difficulty in resolving the structure and chemistry of this transient amorphous state. Here, we use time-lapse photography, image analysis, spatially resolved pH determination, in situ synchrotron pair distribution function (PDF) analysis, and dynamic nuclear polarization (DNP) solid-state nuclear magnetic resonance (NMR) spectroscopy to reveal pervasive compositional variability in ACC that underpins its metastability and crystallization. By evaluating the kinetics of the amorphous-to-crystalline transition across different solution chemistries, we demonstrate that ACC is non-stoichiometric and CO 3 -deficient. Counterions from the precursor (e.g., NO 3 - from Ca(NO 3 ) 2 ) substitute into the ACC network, displacing CO 3 ions and mediating both ACC stability and transformation. Crystallization proceeds through refinement of the stoichiometry toward CaCO 3 and uptake of free CO 3 2- anions. Furthermore, these findings are consistent across a wide range of concentrations and different carbonate sources, explaining the diverse behaviors observed for ACC and providing a chemical framework for controlling calcium carbonate crystallization.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Understanding and Controlling Cesium Loading on Crystalline Silicotitanate - 19601

Savannah River Remediation (SRR) contracted with Westinghouse Electric Corporation (WEC), Columbia Energy and Environmental Services (CEES), to build and deliver a modular ion exchange process that will be used to remove radioactive cesium from dissolved salt solution contained in Tank 10 at the Savannah River Site (SRS). The resulting decontaminated salt solution will be sent to Tank 11 and then to Tank 50 for final disposition in grout at the Saltstone facility. At the end of processing, the loaded ion exchange (IX) columns are drained, rinsed, and dried. The IX columns are removed from the modular unit and stored at Interim Safe Storage (ISS). This ion exchange process is called the Tank Closure Cesium Removal (TCCR) system. The TCCR system consists of several unit operations and process monitoring capability housed within three modular units. The first modular unit contains the process control computer, the second modular unit contains the main process equipment (two prefilters, four IX columns, and resin trap (post filtration)), and the third modular unit is the ventilation system. The main unit operations of the TCCR system are filtration, ion exchange, and ventilation. The ion exchange media utilized is a form of inorganic Crystalline Silicotitanate (CST), IONSIV{sup TM} R9120-B supplied by UOP Honeywell. CST has a high selectivity for cesium (Cs) and has some affinity for other Group IA alkali metals on the periodic chart (hydrogen, lithium, sodium, potassium, rubidium, and francium). CST has also been shown to have affinity for strontium and actinides. Cesium loading on the CST is dependent on many factors including chemical composition (cations and anions), temperature, and pH of the salt solution. The actual amount of Cs loaded onto an IX column is dependent on the factors above along with the salt solution volume fed to the IX column. Because of CST's high selectivity for Cs, the Cs-137 equilibrium loading can contribute enough decay heat to result in an ion exchange column boiling event under no flow conditions in the IX column. The boiling event under no flow is a safety concern that must be prevented from occurring. To prevent boiling of the column under no flow conditions, the Cs-137 equilibrium loading must be determined and understood. Several methodologies were evaluated for performing the Cs-137 equilibrium loading determination for CST. After review of available research and development (R and D), batch equilibrium contact test data, and Zheng Anthony Miller (ZAM) model predictions for the salt solution chemistry in Tank 10, a methodology for determining the Cs-137 equilibrium loading on CST was selected. The methodology selected involves an in-tank batch equilibrium contact test performed in duplicate that considers additional corrections to account for anticipated operational evolutions. The in-tank batch equilibrium contact test utilizes ∼0.1 grams of CST secured in a slotted sample vial. The slotted sample vial design allows for salt solution to be in contact with the CST. The slotted sample vials containing the CST are submerged in Tank 10 and exposed to the salt solution for ten days. After ten days, the samples are retrieved and sent to the Savannah River National Laboratory (SRNL) for analysis of the Cs-137 equilibrium loading. Additional corrections are then made to the Cs-137 results to account for anticipated operational evolutions. Anticipated operational evolutions include external additions (water/caustic) to Tank 10 that result in a change to its chemical composition, tank temperature effects, departures from the laboratory testing (mixed vs. stagnant tank conditions), and IX column flushes. A description of the methodologies considered, feasibility of methodology deployment, and the down select process (benefits vs. risks) is discussed in this paper. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Amine-Thiol/Selenol Chemistry for Efficient and Stable Perovskite Solar Cells

Controlling the crystallization of perovskites is imperative to reduce defect densities in perovskite thin films and extend device lifetimes. In this work, combinations of amine and chalcogenide ligands were introduced in the sequential deposition method to fabricate highly crystalline and orientated formamidinium lead iodide thin films with reduced defect densities and increased charge carrier lifetimes. The dual additives can tune the perovskite intermediate state and control the crystallization leading to devices with improved efficiencies and stabilities. While thiophenol failed to prevent the amine ligand from degrading the perovskite precursors, benzene selenol combinations with amine-ligands drastically changed the solution chemistry to increase the PbI 2 conversion to highly crystalline and orientated α-FAPbI 3 films with lower defect densities. X-ray photoelectron spectroscopy studies reveal benzene selenol evaporates from the thin film leaving behind a modified surface, which is associated with the amine additive. These results indicate the amine selection can be used to tune the surface properties. Lastly, we propose a highly tunable I 2 reduction strategy using chalcogenide chemistry to help enable the realization of perovskite solar cells with high performance and stability.

defects↗

Modeling of aqueous species interaction energies prior to nucleation in cement-based gel systems

Arguably the most ubiquitous construction material in modern civilization, concrete is enabling the development of megacities around the globe together with increasing living standards in developing nations. However, the exact formation mechanisms of the strength-giving calcium-rich gels remain a topic of debate. Using density functional modeling, we simulate the fundamental solution-based building blocks of cement hydrates (calcium ions and silicate and aluminate monomers) and their propensity to form pair-wise complexes with bonding environments characteristic of those found in calcium-silicate-hydrate, calcium-alumino-silicate-hydrate and sodium-containing calcium-alumino-silicate-hydrate gels, as assessed from Gibbs free energies of chemical reactions. By accurately simulating the high pH pore solution chemistry in Portland cements and related systems, along with discrete solvation of the species, we hypothesize potential early age formation routes of the gels and discuss limitations and future work associated with this approach.

36 MATERIALS SCIENCE↗

An Overview of Nanomaterials for Environmental Remediation Applications

The environmental remediation capabilities of nanoparticles were reviewed and evaluated. Nanoparticles (NPs) have been used to remediate various forms of environmental contamination. Various materials, morphologies, and conditions are required to remediate different contaminants. Nanoparticles may have benefits and/or limitations compared with traditional remediation methods. New techniques are being applied to mitigate the limitations of NPs. Nanomaterials are a promising technology for the environmental remediation. NPs have been used for the remediation of aqueous and atmospheric contaminants. Nanoparticles have been used to sequester contaminants toxic to human and environmental health. Various materials, morphologies, and conditions are necessary for the remediation of different contaminants. The remediation of heavy metals is of significant concern. Contaminants may be remediated by means of sorption or reduction. The remediation capability of nanoparticles is promising due to their high surface area and reactivity. Reaction kinetics are, therefore, notably fast. These characteristics make NPs attractive for environmental remediation. Various NPs have been used as sequestering agents for environmental contaminants. NPs have been used to remediate heavy metals as well as organic contaminants. Technical Objectives: Assess viability of nanoparticles (NPs) for environmental remediation; Review benefits and limitations of NPs; Design future experiments to test remediation capabilities of NPs. Future Plans: Create NP filters for remediation - Grow Au NPs on Stainless Steel Wool: Stainless steel wool has many defects and crevices allowing the Au NPs to grow on the surface; Stainless steel wool will not react with the heavy metal contaminants tested; NPs are embedded, so they do not have to be removed from solution. Test sorption capabilities with heavy metal contaminants in aqueous solution. Benefits of Gold NPs: Corrosion/oxidation resistant; Exhibit visible/near IR plasmon resonance; Can be synthesized by solution chemistry: cost efficient and easily scalable. Surfactants: Used to lower surface energy and prevent aggregation; Sodium citrate: anionic surfactant (-); Cetyltrimethylammonium bromide (CTAB): cationic surfactant (+); Ionic surfactants create charged NPs; Charged NPs can be used to sequester ionic contaminants (eg. heavy metals)

54 ENVIRONMENTAL SCIENCES↗

Lab-Scale Study of the Calcium Carbonate Dissolution and Deposition by Marine Cyanobacterium Phormidium subcapitatum

Suggestions that calcification in marine organisms changes in response to global variations in seawater chemistry continue to be advanced (Wilkinson, 1979; Degens et al. 1985; Kazmierczak et al. 1986; R. Riding 1992). However, the effect of [Na+] on calcification in marine cyanobacteria has not been discussed in detail although [Na+] fluctuations reflect both temperature and sea-level fluctuations. The goal of these lab-scale studies therefore was to study the effect of environmental pH and [Na+] on CaCO3 deposition and dissolution by marine cyanobacterium Phormidium subcapitatum. Marine cyanobacterium P. subcapitatum has been cultivated in ASN-III medium. [Ca2+] fluctuations were monitored with Ca(2+) probe. Na(+) concentrations were determined by the initial solution chemistry. It was found that the balance between CaCO3 dissolution and precipitation induced by P. subcapitatum grown in neutral ASN III medium is very close to zero. No CaCO3 precipitation induced by cyanobacterial growth occurred. Growth of P. subcapitatum in alkaline ASN III medium, however, was accompanied by significant oscillations in free Ca(2+) concentration within a Na(+) concentration range of 50-400 mM. Calcium carbonate precipitation occurred during the log phase of P. subcapitatum growth while carbonate dissolution was typical for the stationary phase of P. subcapitatum growth. The highest CaCO3 deposition was observed in the range of Na(+) concentrations between 200-400 mM. Alkaline pH also induced the clamping of P. subcapitatum filaments, which appeared to have a strong affinity to envelop particles of chemically deposited CaCO3 followed by enlargement of those particles size. EDS analysis revealed the presence of Mg-rich carbonate (or magnesium calcite) in the solution containing 10-100 mM Na(+); calcite in the solution containing 200 mM Na(+); and aragonite in the solution containing with 400 mM Na(+). Typical present-day seawater contains xxmM Na(+). Early (Archean) seawater was likely less saline. The division of marine cyanobacterium P. subcapitatum is associated with periodic deposition and dissolution of CaCO3, the rhythms and intensity of which are dependent on concentrations of both OH(-) and Na(+). Thus, the role of present-day marine cyanobacteria in the global carbonate cycle might be reduced to aggregation and recrystallization of available CaCO3 particles in marine water rather than long-term precipitation and accumulation of CaCO3 deposits. For lower Na(+) concentrations, precipitation of carbonates by cyanobacteria would be even less significant. These results suggest that the lack of calcified cyanobacteria in stromatalite-bearing Precambrian sequences can be explained not only by high dissolved inorganic carbon concentrations but also by lower salinity, as well as possible lower pH compared to present-day oceans.

Karakis, S. G.↗

Corrosion Assessment of Candidate Materials for the SHINE Subcritical Assembly Vessel and Components FY15 Report

In the previous report of this series, a literature review was performed to assess the potential for substantial corrosion issues associated with the proposed SHINE process conditions to produce 99 Mo. Following the initial review, substantial laboratory corrosion testing was performed emphasizing immersion and vapor-phase exposure of candidate alloys in a wide variety of solution chemistries and temperatures representative of potential exposure conditions. Stress corrosion cracking was not identified in any of the exposures up to 10 days at 80°C and 10 additional days at 93°C. Mechanical properties and specimen fracture face features resulting from slow-strain rate tests further supported a lack of sensitivity of these alloys to stress corrosion cracking. Fluid velocity was found not to be an important variable (0 to ~3 m/s) in the corrosion of candidate alloys at room temperature and 50°C. Uranium in solution was not found to adversely influence potential erosion-corrosion. Potentially intense radiolysis conditions slightly accelerated the general corrosion of candidate alloys, but no materials were observed to exhibit an annualized rate above 10 μm/y.

36 MATERIALS SCIENCE↗

Applications of SPM to Studies of Mineral–Water Interface Chemistry

The scanning probe microscope (SPM) has been utilized in studies of solid surfaces for nearly four decades. With resolution as high as the single atom level, valuable information on the structure and other properties of solid surfaces can be obtained. One of the most exciting areas of application for the SPM is in the study of mineral–water interfaces where the chemical reactions taking place are both of fundamental interest as well as important from an environmental/geochemical perspective. In this article, the basic design of one type of SPM, the atomic force microscope (AFM), is introduced followed by an examination of the different levels of resolution that may be exploited to obtain fundamental information on kink, step, and surface microtopography from mineral surfaces immersed in reactive solutions. The examples of these particular applications highlight the influence of solution chemistry on the rates and mechanisms of mineral growth and dissolution reactions that are readily followed with in-situ AFM instrumentation.

Higgins, Steven↗

Aerothermodynamic Analysis of Commercial Experiment Transporter (COMET) Reentry Capsule

An aerothermodynamic analysis of the Commercial Experiment Transporter (COMET) reentry capsule has been performed using the laminar thin-layer Navier-Stokes solver Langley Aerothermodynamic Upwind Relaxation Algorithm. Flowfield solutions were obtained at Mach numbers 1.5, 2, 5, 10, 15, 20, 25, and 27.5. Axisymmetric and 5, 10, and 20 degree angles of attack were considered across the Mach-number range, with the Mach 25 conditions taken to 90 degrees angle of attack and the Mach 27.5 cases taken to 60 degrees angle of attack. Detailed surface heat-transfer rates were computed at Mach 20 and 25, revealing that heating rates on the heat-shield shoulder ,can exceed the stagnation-point heating by 230 percent. Finite-rate chemistry solutions were performed above Mach 10, otherwise perfect gas computations were made. Drag, lift, and pitching moment coefficients are computed and details of a wake flow are presented. The effect of including the wake in the solution domain was investigated and base pressure corrections to forebody drag coefficients were numerically determined for the lower Mach numbers. Pitching moment comparisons are made with direct simulation Monte Carlo results in the more rarefied flow at the highest Mach numbers, showing agreement within two-percent. Thin-layer Navier-Stokes computations of the axial force are found to be 15 percent higher across the speed range than the empirical/Newtonian based results used during the initial trajectory analyses.

Wood, William A.↗

Contrasting Trivalent Lanthanide and Actinide Complexation by Polyoxometalates via Solution-State NMR

Deciphering the solution chemistry and speciation of actinides is inherently difficult due to radioactivity, rarity, and cost constraints, especially for transplutonium elements. In this context, the development of new chelating platforms for actinides and associated spectroscopic techniques is particularly important. In this study, we investigate a relatively overlooked class of chelators for actinide binding, namely, polyoxometalates (POMs). We provide the first NMR measurements on americium–POM and curium–POM complexes, using one-dimensional (1D) 31 P NMR, variable-temperature NMR, and spin-lattice relaxation time (T 1 ) experiments. The proposed POM–NMR approach allows for the study of trivalent f-elements even when only microgram amounts are available and in phosphate-containing solutions where f-elements are typically insoluble. The solution-state speciation of trivalent americium, curium, plus multiple lanthanide ions (La 3+ , Nd 3+ , Sm 3+ , Eu 3+ , Yb 3+ , and Lu 3+ ), in the presence of the model POM ligand PW 11 O 39 7– was elucidated and revealed the concurrent formation of two stable complexes, [M III (PW 11 O 39 )(H 2 O) x ] 4– and [M III (PW 11 O 39 ) 2 ] 11– . Interconversion reaction constants, reaction enthalpies, and reaction entropies were derived from the NMR data. The NMR results also provide experimental evidence of the weakly paramagnetic nature of the Am 3+ and Cm 3+ ions in solution. Furthermore, the study reveals a previously unnoticed periodicity break along the f-element series with the reversal of T 1 relaxation times of the 1:1 and 1:2 complexes and the preferential formation of the long T 1 species for the early lanthanides versus the short T 1 species for the late lanthanides, americium, and curium. Furthermore, given the broad variety of POM ligands that exist, with many of them containing NMR-active nuclei, the combined POM–NMR approach reported here opens a new avenue to investigate difficult-to-study elements such as heavy actinides and other radionuclides.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of Coordination Complexes by Desorption Electrospray Mass Spectrometry with a Capillary Target

Metal coordination complexes were formed directly from liquid surfaces using desorption electrospray ionization (DESI) mass spectrometry. The approach is attractive because it separates complexities of ESI spray droplet formation from delivery of the analyte solution, and thereby gets around difficulty resulting from alteration of the spray process by changes in solution chemistry. Cs+, Ba2+, and La3+ coordination complexes were formed using 18-crown-6 (18c6) and triethylphosphate (TEP) as ligands (L), that had the general formula [Mn+(NO3-)n-1(L)m]+. Formation of singly charged cation complexes was preferred, with charge reduction at the metal site accomplished by attachment of nitrate. Using TEP as a model phosphoryl ligand, alkali metals coordinate with up to three ligands, with Cs+ preferring fewer than Na+. Ba2+ and La3+ are formed as ion pair complexes [Ba(NO3)]+ and [La(NO3)2]+, and both will coordinate with up to four TEP ligands. Using 18c6, Cs+ forms a bis-ligand complex. In contrast, [Ba(NO3)]+ prefers a single 18c6 ligand, while La forms mainly [La(NO3)2(18c6)]+, for which DFT calculations suggested a structure in which the nitrate ligands occupy pseudo-axial positions on opposing sides of the crown. Lower abundances of bis-18c6 complexes were also formed together with doubly charged [La(NO3)(18c6)n]2+ complexes (n = 2 – 4). The results suggest an alternative strategy for probing metal speciation in solution that is less perturbed by the droplet formation and ionization mechanisms operating in conventional electrospray ionization mass spectrometry.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crystallization Physics in Biomacromolecular Systems

The crystals are built of molecules of protein, nucleic acid and their complexes, like viruses, approx. 5x10(exp 3)+ 3x10(exp 6) Da in weight and 2 + 20 nm in effective diameter. This size strongly exceeds action range of molecular forces and makes a big difference with inorganic crystals. Intermolecular contacts form patches on the biomacromolecular surface. Each patch may occupy only a small percent of the whole surface and vary from polymorph to polymorph of the same protein. Thus, under different conditions (pH, solution chemistry, temperature, any area on the macromolecular surface may form a contact. The crystal Young moduli, E approx. equals 0.1 + 0.5 GPa are more than 10 times lower than that of inorganics and the biomolecules themselves. Water within biocrystals (30-70%) is unable to flow unless typical deformation time is longer than approx. 10(exp -5)s. This explains the discrepancy between light scattering and static measurements of E. Nucleation and Growth requires typically concentrations exceeding the equilibrium ones up to 100 times - because of the new size scale results in 10 - 10(exp 3) times lower kinetic coefficients than that needed for inorganic solution growth. All phenomena observed in the latter occur with protein crystallization and are even better studied by AFM. Crystals are typically facetted. Among unexpected findings of general significance are - net molecular exchange flux at kinks is much lower than that expected from supersaturation, steps with low (< approx. 10(exp -2)) kink density at steps follow Gibbs-Thomson law only at very low supersaturations, step segment growth rate may be independent of step energy. Crystal perfection is a must of biocrystallization to achieve the major goal to find 3-D atomic structure of biomacromolecules by x-ray diffraction. Poor diffraction resolution (> 3Angstrom) makes crystallization a bottleneck for structural biology. All defects typical of small molecule crystals are found in biocrystals, but the defects responsible for poor resolution are not identified. Conformational changes are one of them. Biocrystallization in microgravity reportedly results in 20% cases of better crystals. The mechanism of how lack of convection can do this is still not clear. Lower supersaturation, self-purification &om preferentially trapped homologous impurities and step bunching are viable hypotheses.

Chernov, A. A.↗

Sulfide precipitation characteristics of Mn, Ni, Co, and Zn in the presence of contaminant metal ions

In this study, the effects of Al 3+ and Fe 2+ on the precipitation characteristics of four valuable metals, including Mn 2+ , Ni 2+ , Co 2+ , and Zn 2+ , were investigated by conducting solution chemistry calculations, sulfide precipitation tests, and mineralogy characterizations. It was found that the ability of the valuable metals to form sulfide precipitates followed an order of Zn 2+ > Ni 2+ > Co 2+ > Mn 2+ . The sulfide precipitate of Zn 2+ was the most stable and did not re-dissolve under the acidic condition (pH 4.00 ± 0.05). In addition, the sulfide precipitation characteristics of Zn 2+ was barely affected by the contaminant metal ions. However, in the presence of Al 3+ , the precipitation recoveries of Mn 2+ , Ni 2+ , and Co 2+ were noticeably reduced due to simultaneous hydrolysis and competitive adsorption. The precipitation recoveries of Ni 2+ and Co 2+ in solutions containing individual valuable metals also reduced when Fe 2+ was present, primarily due to competitive precipitation. However, the recovery of Mn 2+ was enhanced due to the formation of ferrous sulfide precipitate, providing abundant active adsorption sites for Mn species. Here, in the solution containing all the valuable metals, Fe 2+ promoted the recovery of the valuable metals due to the higher concentration of Na 2 S and the formation of ferrous sulfide precipitate.

58 GEOSCIENCES↗