Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solder”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Fluid Dynamics and Solidification of Molten Solder Droplets Impacting on a Substrate in Microgravity

This program investigates the fluid dynamics and simultaneous solidification of molten solder droplets impacting on a flat smooth substrate. The problem of interest is directly relevant to the printing of microscopic solder droplets in surface mounting of microelectronic devices. The study consists of a theoretical and an experimental component. The theoretical work uses axisymmetric Navier-Stokes models based on finite element techniques. The experimental work will be ultimately performed in microgravity in order to allow for the use of larger solder droplets which make feasible the performance of accurate measurements, while maintaining similitude of the relevant fluid dynamics groups (Re, We).

Megardis, C. M.↗

Investigation of Dynamic Oxygen Adsorption in Molten Solder Jetting Technology

Surface tension forces play a critical role in fluid dynamic phenomena that are important in materials processing. The surface tension of liquid metals has been shown to be very susceptible to small amounts of adsorbed oxygen. Consequently, the kinetics of oxygen adsorption can influence the capillary breakup of liquid-metal jets targeted for use in electronics assembly applications, where low-melting-point metals (such as tin-containing solders) are utilized as an attachment material for mounting of electronic components to substrates. By interpreting values of surface tension measured at various surface ages, adsorption and diffusion rates of oxygen on the surface of the melt can be estimated. This research program investigates the adsorption kinetics of oxygen on the surface of an atomizing molten-metal jet. A novel oscillating capillary jet method has been developed for the measurement of dynamic surface tension of liquids, and in particular, metal melts which are susceptible to rapid surface degradation caused by oxygen adsorption. The experimental technique captures the evolution of jet swells and necks continuously along the jet propagation axis and is used in conjunction with an existing linear, axisymmetric, constant-property model to determine the variation of the instability growth rate, and, in turn, surface tension of the liquid as a function of surface age measured from the exit orifice. The conditions investigated so far focus on a time window of 2-4ms from the jet orifice. The surface properties of the eutectic 63%Sn-37%Pb solder alloy have been investigated in terms of their variation due to O2 adsorption from a N2 atmosphere containing controlled amounts of oxygen (from 8 ppm to 1000 ppm). The method performed well for situations where the oxygen adsorption was low in that time window. The value of surface tension for the 63Sn-37Pb solder in pure nitrogen was found to be 0.49 N/m, in good agreement with previously published work. A characteristic time of O(1ms) or less was determined for the molten-metal surface to be saturated by oxygen at 1000 ppm concentration in N2.

Megaridis, Constantine M.↗

Mechanical Properties and Microstructure Investigation of Lead Free Solder

While the electronics industry appears to be focusing on Sn-Ag-Cu as the alloy of choice for lead free electronics assembly, ,the exact composition varies by geographic region, supplier and user. Add to that dissolved copper and silver from the printed circuit board traces and surface finish, and there can be significant variation in the final solder joint composition. A systematic study of the mechanical and microstructural properties of Sn-Ag-Cu alloys with Ag varying from 2wt% to 4wt% and Cu varying from 0.5wt% to lSwt%, was undertaken in this research study. Different sample preparation techniques (water quenched, oil quenched and water quenched followed by reflow) were explored and the resulting microstructure compared to that of a typical reflowed lead free chip scale package (CSP) solder joint. Tensile properties (modulus, 0.2% yield strength and the ultimate tensile strength) and creep behavior of selected alloy compositions (Sn-4Ag-1 X u , Sn-4Ag-OSCu, Sn- 2Ag-1 X u , Sn-2Ag-OSCu, Sn-3.5Ag-O.SCu) were determined for three conditions: as- cast; aged for 100 hours at 125OC; and aged for 250 hours at 125OC. There was no significant difference in Young's Modulus as a function of alloy composition. After an initial decrease in modulus after 100 hours at 125"C, there was an insignificant change with further aging. The distribution of 0.2% strain yield stress and ultimate tensile strength as a function of alloy composition was more significant and decreased with aging time and temperature. The microstructures of these alloys were examined using light and scanning electron microscopy (LM and SEM) respectively and SEM based energy dispersive x-ray spectroscopy (EDS). Fracture surface and cross-section analysis were performed on the specimens after creep testing. The creep testing results and the effect of high temperature aging on mechanical properties is presented for the oil quenched samples. In general the microstructure of oil quenched specimen exhibited a eutectic region of Sn with moderately dispersed Ag3Sn intermetallic, surrounded by a dendritic Sn-rich phase. The SEM images of the fracture surface indicated the presence of a tough shear surface at the initial cavity break area and a break line in the middle of specimen along the failure direction. A hyperbolic-sine creep model was adopted and used to fit the creep experiment data. The effect on the mechanical properties by adding the quaternary element bismuth to the Sn-3.5Ag-0.8Cu alloy was measured and compared with the mechanical properties of the ternary alloys. The results of this research study provide necessary data for the modeling of solder joint reliability for a range of Sn-Ag-Cu compositions and a baseline for evaluating the effects of subsequent quaternary additions.

Wang, Qing↗

Solder Creep-Fatigue Interactions with Flexible Leaded Part

In most electronic packaging applications it is not a single high stress event that breaks a component solder joint; rather it is repeated or prolonged load applications that result in fatigue or creep failure of the solder. The principal strain in solder joints is caused by differential expansion between the part and its mounting environment due to hanges in temperature (thermal cycles) and/or due to temperature gradients between the part and the board.

creep effects↗

Solder dross removal apparatus

An automatic dross removal apparatus (10) is disclosed for removing dross from the surface of a solder bath (22) in an automated electric component handling system. A rotatable wiper blade (14) is positioned adjacent the solder bath (22) which skims the dross off of the surface prior to the dipping of a robot conveyed component into the bath. An electronic control circuit (34) causes a motor (32) to rotate the wiper arm (14) one full rotational cycle each time a pulse is received from a robot controller (44) as a component approaches the solder bath (22).

Webb, Winston S.↗

Solder Joint Health Monitoring Testbed System

The density and pin count for Field Programmable Gate Arrays (FPGAs) has been increasing, and has exceeded current methods of solder joint inspection, making early detection of failures more problematic. These failures are a concern for both flight safety and maintenance in commercial aviation. Ridgetop Group, Inc. has developed a method for detecting solder joint failures in real time. The NASA Dryden Flight Research Center is developing a set of boards to test this method in ground environmental and accelerated testing as well as flight test on a Dryden F-15 or F-18 research aircraft. In addition to detecting intermittent and total solder joint failures, environmental data on the boards, such as temperature and vibration, will be collected and time-correlated to aircraft state data. This paper details the technical approach involved in the detection process, and describes the design process and products to date for Dryden s FPGA failure detection boards.

Delaney, Michael M.↗

Reliability of Sn/Pb and Lead-Free (SnAgCu) Solders of Surface Mounted Miniaturized Passive Components for Extreme Temperature (-185 C to +125 C) Space Missions

Surface mount electronic package test boards have been assembled using tin/lead (Sn/Pb) and lead-free (Pb-free or SnAgCu or SAC305) solders. The soldered surface mount packages include ball grid arrays (BGA), flat packs, various sizes of passive chip components, etc. They have been optically inspected after assembly and subsequently subjected to extreme temperature thermal cycling to assess their reliability or future deep space, long-term, extreme temperature environmental missions. In this study, the employed temperature range (-185oC to +125oC) covers military specifications (-55oC to +100oC), extreme old Martian (-120oC to +115oC), asteroid Nereus (-180oC to +25oC) and JUNO (-150oC to +120oC) environments. The boards were inspected at room temperature and at various intervals as a function of extreme temperature thermal cycling and bake duration. Electrical resistance measurements made at room temperature are reported and the tests to date have shown some change in resistance as a function of extreme temperature thermal cycling and some showed increase in resistance. However, the change in interconnect resistance becomes more noticeable with increasing number of thermal cycles. Further research work will be carried out to understand the reliability of packages under extreme temperature applications (-185oC to +125oC) via continuously monitoring the daisy chain resistance for BGA, Flat-packs, lead less chip packages, etc. This paper will describe the experimental reliability results of miniaturized passive components (01005, 0201, 0402, 0603, 0805, and 1206) assembled using surface mounting processes with tin-lead and lead-free solder alloys under extreme temperature environments.

extreme temperatures,↗

Microstructure and Sn crystal orientation evolution in Sn-3.5Ag lead-free solders in high temperature packaging applications

Understanding the reliability of eutectic Sn-3.5Ag lead-free solders in high temperature packaging applications is of significant interest in power electronics for the next generation electric grid. Large area (2.5mm 2.5mm) Sn-3.5Ag solder joints between silicon dies and direct bonded copper substrates were thermally cycled between 5 C and 200 C. Sn crystal orientation and microstructure evolution during thermal cycling were characterized by electron backscatter diffraction (EBSD) in scanning electron microscope (SEM). Comparisons are made between observed initial texture and microstructure and its evolution during thermal cycling. Gradual lattice rotation and grain boundary misorientation evolution suggested the continuous recrystallization mechanism. Recrystallization behavior was correlated with dislocation slip activities.

high temperature packaging↗

Microstructure and interfacial reactions of soldering magnesium alloy AZ31B

In this paper, economic and innoxious solder alloys with low melting temperature were designed for AZ31B. Their chemical composition and relevant parameters were investigated for a high-performance structure of bonding region. Results of microstructure observation showed that Zn-enriched phases disappeared and {alpha}-Mg existed in the joints in the form of coarse dendrites by increasing the concentration of Mg in the solder alloys. Water cooling with a high cooling rate was adopted in experiments. Experimental research showed that high cooling rate restricted the grains of {alpha}-Mg as the equiaxed dendrites, which was about 1/5 of the coarse dendrite but their number was more than 40-50 times. Both morphology with typical fracture and the analysis on X-ray diffraction fracture indicated that equiaxed dendrites significantly improved the mechanical property of the joints. Necking phenomenon occurred in the bonding region was in favor of the improvement of joint shear strength.

36 MATERIALS SCIENCE↗

Soldering mask laser removal from printed circuit boards aiming copper recycling

Highlights: • Use of laser as a tool for recycling of electronic waste is proposed. • Laser stripping removes varnishes from circuit boards exposing the copper underneath allowing electrochemical copper recover. •Good removal is achieved with nanosecond pulsed irradiation at 1064 nm. • Waste generated by the process is mainly solid, macroscopic and easy to handle. - Abstract: Management of waste of electric and electronic equipment (WEEE) is a key issue for modern societies; furthermore, it contains valuable materials that can be recycled, especially in printed circuit boards (PCB), which have approximately one-third of their weight in copper. In this study we demonstrated the use of laser to strip the covering soldering mask on PCB’s, thus exposing the copper underneath so that extraction techniques may take place. Using a Q-Switched Nd:YAG laser operating at 1064 nm and 532 nm we tested the procedure under different energy conditions. The laser stripping of the soldering mask was achieved with satisfactory results by irradiation with 225 mJ at 1064 nm. However, when using similar parameters at 532 nm the process of the coating ejection was not promoted properly, leading to a faulty detachment. Infrared laser PCB stripping presents itself to be technically viable and environmental friendly, since it uses no chemicals inputs, offering one more option to WEEE treatment and recycling.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Solder Bond Fatigue is Insensitive to Module Size

In this article, we explore the influence of module size on the rate of interconnecting solder bond thermomechanical fatigue (TMF) damage. Structural mechanics models of crystalline silicon PV models are created to solve with the finite-element method. Results conclusively demonstrate that the rate of solder bond TMF damage is independent of module size, interconnect location across the cell and cell location across the module.

14 SOLAR ENERGY↗

Breakthrough: Lead-free Solder

Ames Laboratory senior metallurgist Iver Anderson explains the importance of lead-free solder in taking hazardous lead out of the environment by eliminating it from discarded computers and electronics that wind up in landfills. Anderson led a team that developed a tin-silver-copper replacement for traditional lead-tin solder that has been adopted by more than 50 companies worldwide.

36 MATERIALS SCIENCE↗

Methodology for analyzing stress states during in-situ thermomechanical cycling in individual lead free solder joints using synchrotron radiation

To examine how a lead-free solder joint deforms in a thermal cycling environment, both the elastic and plastic stress and strain behavior must be understood. Methods to identify evolution of the internal strain (stress) state during thermal cycling are described. A slice of a package containing a single row of solder joints was thermally cycled from 0 C to 100 C with a period of about 1 h with concurrent acquisition of transmission Laue patterns using synchrotron radiation. These results indicated that most joints are single crystals, with some being multicrystals with no more than a few Sn grain orientations. Laue patterns were analyzed to estimate local strains in different crystal directions at different temperatures during a thermal cycle. While the strains perpendicular to various crystal planes all vary in a similar way, the magnitude of strain varies. The specimens were subsequently given several hundred additional thermal cycles and measured again to assess changes in the crystal orientations. These results show that modest changes in crystal orientations occur during thermal cycling.

43 PARTICLE ACCELERATORS↗

The Role of Elastic and Plastic Anisotropy of Sn in Recrystallization and Damage Evolution During Thermal Cycling in SAC305 Solder Joints

Because failures in lead-free solder joints occur at locations other than the most highly shear-strained regions, reliability prediction is challenging. To gain physical understanding of this phenomenon, physically based understanding of how elastic and plastic deformation anisotropy affect microstructural evolution during thermomechanical cycling is necessary. Upon solidification, SAC305 (Sn-3.0Ag-0.5Cu) solder joints are usually single or tricrystals. The evolution of microstructures and properties is characterized statistically using optical and orientation imaging microscopy. In situ synchrotron x-ray measurements during thermal cycling are used to examine how crystal orientation and thermal cycling history change strain history. Extensive characterization of a low-stress plastic ball grid array (PBGA) package design at different stages of cycling history is compared with preliminary experiments using higher-stress package designs. With time and thermal history, microstructural evolution occurs mostly from continuous recrystallization and particle coarsening that is unique to each joint, because of the specific interaction between local thermal and displacement boundary conditions and the strong anisotropic elastic, plastic, expansion, and diffusional properties of Sn crystals. The rate of development of recrystallized microstructures is a strong function of strain and aging. Cracks form at recrystallized (random) boundaries, and then percolate through recrystallized regions. Complications arising from electromigration and corrosion are also considered.

36 MATERIALS SCIENCE↗

The use of a directional solidification technique to investigate the interrelationship of thermal parameters, microstructure and microhardness of Bi–Ag solder alloys

Bi–Ag alloys have been stressed as possible alternatives to replace Pb-based solder alloys. Although acceptable melting temperatures and suitable mechanical properties may characterize such alloys, as referenced in literature, there is a lack of comprehension regarding their microstructures (morphologies and sizes of the phases) considering a composition range from 1.5 to 4.0 wt.%Ag. In order to better comprehend such aspects and their correlations with solidification thermal parameters (growth rate, v and cooling rate, T-dot), directional solidification experiments were carried out under transient heat flow conditions. The effects of Ag content on both cooling rate and growth rate during solidification are examined. Microstructure parameters such as eutectic/dendritic spacing, interphase spacing and diameter of the Ag-rich phase were determined by optical microscopy and scanning electron microscopy. The competition between eutectic cells and dendrites in the range from 1.5 to 4.0 wt.%Ag is explained by the coupled zone concept. Microhardness was determined for different microstructures and alloy Ag contents with a view to permitting correlations with microstructure parameters to be established. Hardness is shown to be directly affected by both solute macrosegregation and morphologies of the phases forming the Bi–Ag alloys, with higher hardness being associated with the cellular morphology of the Bi-2.5 and 4.0 wt.%Ag alloys. - Highlights: • Asymmetric zone of coupled growth for Bi–Ag is demonstrated. • Faceted Bi-rich dendrites have been characterized for Bi–1.5 wt.%Ag alloy. • Eutectic cells were shown for the Bi-2.5 and 4.0 wt.%Ag solder alloys. • Interphase spacing relations with G × v are able to represent the experimental scatters. • Hall-Petch type equations are proposed relating microstructural spacings to hardness.

36 MATERIALS SCIENCE↗

Optimization of Structurally Enhanced Solder Transient Liquid Phase Bonding

High temperature packaging technologies are a necessity for high temperature capable devices. SAC305 solder has an operational limit of 174°C imposed by creep effects which aligns well with current junction temperature limits of 175°C. Wide band gap semiconductor materials have the potential to reach junction temperatures of up to 800°C that are not currently attainable with significant reliability. Capitalizing on this potential will requires substrates and attachments that can operate well beyond the current 175°C standard. Silver sintering pastes have received widespread interest as a high temperature attachment alternative. However, the process requires high pressure bonding in an inert environment to achieve acceptable bond quality. Transient liquid phase (TLP) sintering is capable of good bond quality without pressure requirements but suffers from low thermal conductivity and only slightly reduced cost compared to silver sintering. SAC305 solder contains the same constituent materials for TLP as available copper-tin TLP sintering paste. By introducing engineered surface structures into the bond, intermetallic formation can be accelerated producing a bond similar to TLP sintering but in an ambient environment and for reduced cost. While this process has been demonstrated, it has not yet been optimized. Currently bonds are formed using a 75 μm stencil on substrate surface structures 24 μm tall, covering 19% of the bonding area. The process takes about 4 hours not including the formation of surface structures. Here, this study will center on the effects of stencil thickness and coating methods. Samples will be analyzed by scanning acoustic microscopy, die shear testing and cross sectional scanning acoustic microscopy.

42 ENGINEERING↗

Metal-Insulation REBCO Pancake Coil With Solder Surface Shunt: Testing and Modeling

Rare-earth barium copper oxide (REBCO) high-temperature superconducting (HTS) magnets can generate very high magnetic fields with superior engineering current density and robust mechanical integrity. The no-insulation (NI) winding technique, including its metal-insulation (MI) variant, enables “self-protection” against localized overheating through inter-turn current sharing, improving defect tolerance and allowing temporary current overloads. In REBCO pancake coils, the current-sharing path is predominantly confined to the edges of the REBCO tapes due to insulating buffer layers. Applying a surface shunt using solder can effectively enhance current sharing in NI/MI coils via the REBCO tape edges. Here, in this paper, we present both experimental and numerical research on the current distribution in surface-shunt metal-insulation (SSMI) REBCO pancake coils. We tested a stainless steel co-wound MI REBCO double-pancake coil, before and after applying a soldered surface shunt, in a saturated liquid nitrogen bath. The SSMI coil was modeled using the H-formulation and rotated anisotropic resistivity to study its dynamic behavior, including inter-turn current sharing and intra-turn screening currents. Benchmarked by experimental data, the numerical model is able to study the defect tolerance of the SSMI coil during energization.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗