Investigation of high temperature fracture of T-111 and ASTAR-811C
The high temperature deformation and fracture behavior of T-111 and ASTAR-811C were studied over the temperature range 982 to 2205 C (1800 to 4000 F). As-cast and wrought-recrystallized material as well as GTA welds in sheet and plate were evaluated using conventional tensile and creep tests. Post test examinations were performed using optical metallography, scanning electron microscopy and transmission electron microscopy. A high temperature region of reduced ductility, in terms of tensile elongation, was identified for both alloys. The reduction in tensile elongation became more severe with increase in grain size, being near catastrophic for the as-cast specimens. Optical and electron metallography indicated that even for failures at very low total strain, considerable deformation of a very localized nature had occurred prior to fracture.