Preparation of particle-dispersion alloys (M-6)

A particle dispersion alloy is one type of metal-ceramic composite material, and is used as heat resistance material, wear resistance material, and electrical material. This material consists of a metal matrix and dispersed particles, and for its unique structure it has both tenacity as a metal and hardness as a ceramic. Its properties improve when the particles become finer and disperse more uniformly. Most of the particle dispersion alloys are produced by the powder metallurgical process. This process is favorable for uniform dispersion of particles, but it consists of complicated techniques such as mechanical alloying and hot extrusion, and has the following drawbacks: (1) it is difficult to fabricate large-sized products; (2) the amount of particles is limited to a few percent; and (3) the process is complicated and expensive. To overcome these drawbacks, recently special attention has been paid to conventional melting process. However, under terrestrial conditions, dispersions separate immediately due to the different specific gravities of the metal matrix and the particles and thermal convection effects. The microgravity environment is, therefore, considered to be an attractive place for fabricating the dispersion alloy. This space experiment is carried out to clarify the influence of microgravity on the properties of the particle dispersion alloy and to obtain a deeper understanding of the experiment under the microgravity environment.

Muramatsu, Yuji↗

Surface films and metallurgy related to lubrication and wear

The nature of the tribological surface is identified and characterized with respect to adhesion, friction, wear, and lubricating properties. Surface analysis is used to identify the role of environmental constituents on tribological behavior. The effect of solid to solid interactions for metals in contact with metals, ceramics, semiconductors, carbons, and polymers is discussed. The data presented indicate that the tribological surface is markedly different than an ideal solid surface. The environment is shown to affect strongly the behavior of two solids in contact. Results also show that small amounts of alloying elements in base metals can alter markedly adhesion, friction, and wear by segregating to the solid surface.

Buckley, D. H.↗

Plasticity analysis of wear phenomena as an aid in the development of abradable materials

Plastic deformation accompanying the wear process in fully dense and porous metals was studied in order to develop more abradable gas path seal material systems for turbine engine applications. The finite element method was used to model high-rate viscoplastic deformation in the vicinity of a moving contact. Techniques were developed for studying such deformation in both solid (fully dense) and porous metals. Results of the analysis were verified by comparison with experimental data obtained using a pendulum-type rub test apparatus and a pin-on-disk sliding wear tester. It was found that the near-surface plastic deformation in fully dense solids was different from that for porous materials because of the compressibility of the latter. Both types of materials exhibit deformation features which can be taken advantage of in the design of more abradable material systems.

Kennedy, F. E., Jr.↗

Metal DiSulfide thin films synthesized by pulsed ion beam ablation: Self-assembled structures with improved mechanical properties in humid conditions

Thin films composed of transition metal dichalcogenides such as molybdenum disulfide (MoS 2 ) or tungsten disulfide (WS 2 ) are well known for their solid lubricating behavior in dry environments such as space, but deteriorate rapidly in environments where oxygen is present. There have been many attempts over recent decades to improve MoS 2 lubricating performance in humid environments by addition of metals such as titanium to the film. The additions have come in the form of co-sputtering with the MoS 2 , or formation of nano multilayer coatings. We have previously reported on the synthesis of MoS 2 films by high-power ion beam ablation [Prasad et al, Matls. Lett. 65 (2010) 4–6]. The resulting films are observed to contain spheres of pure Mo of 10–100 nm size evenly dispersed throughout the ~1 μm-thick film, a form of self-assembly not before seen in films produced by sputtering or by pulsed laser deposition (PLD). The remaining Mosingle bondS matrix was observed to crystalize in situ under frictional contact into MoS 2 with the basal planes orienting themselves in the direction of sliding underneath the wear surface. The present study concerns metal additions in the form of alternating layers with MoS 2 deposited in between from an ablation target. The addition of Ti resulted in the extension of good tribological performance to humid air conditions, but the path to good performance appears to be relatively narrow. The same distributed Mo spheres were present in the new film, and similar self-assembled morphologies when V was substituted for the Ti, and when multilayers were formed of WS 2 with Zr additions. Furthermore, it appears that addition of Ti resulted in improvements in mechanical film strength that contributed to the wear ability in humid conditions.

Intense ion beams↗

Friction and wear characteristics of iron-chromium alloys in contact with themselves and silicon carbide

Sliding friction experiments were conducted with various iron-chromium alloys in contact with (1) themselves, (2) single crystal silicon carbide disks, and (3) single crystal abrasive grit of silicon carbide. Results indicate the coefficients of friction for the alloys sliding against themselves are between those for pure iron and pure chromium, and are only slightly different with 1, 5, 9, 14, and 19 weight percent chromium in iron. The wear is due, primarily, to shearing, or tearing fracture, of the cohesive bonds in the bulk metal and plowing of the bulk by lumps of wear debris. There are only slight differences in the coefficients of friction for the various alloys when sliding on silicon carbide. The coefficient of friction for the alloys are higher than those for pure iron and pure chromium. Alloy hardening observed in the alloys plays a dominant role in controlling the abrasive friction and wear behavior of the alloys.

Miyoshi, K.↗

Alkali metal propellants for MPD thrusters

Experiments performed in the United States in the 1960s and early 1970s and in the Soviet Union with alkali metal-fuelled MPD thrusters indicate performance levels substantially better than those achieved with gaseous propellants. Cathode wear appears to be less in engines with alkali metal propellants also. A critical review of the available data indicates that the data are consistent and reliable. An analysis of testing and systems-level considerations shows that pumping requirements for testing are substantially decreased and reductions in tankage fraction can be expected. In addition, while care must be exercised in handling the alkali metals, it is not prohibitively difficult or hazardous. The greatest disadvantage seems to be the potential for spacecraft contamination, but there appear to be viable strategies for minimizing the impact of propellant deposition on spacecraft surfaces. Renewed examination of alkali metal-fuelled MPD thrusters for ambitious SEI missions is recommended.

Polk, J. E.↗

Characterization of lubricated bearing surfaces operated under high loads

The composition and surface profiles of M-50 steel surfaces were measured after operation at high loads in a bearing contact simulator. An ester lubricant (trimethyolpropane triheptanoate) was used with and without various additives. Optical profiles were obtained + or - to 30 depth resolution with a phase-locked interference microscope in 10 micron diameter areas within and outside the wear tracks. Optical constants and surface film thickness were measured in the same areas with an electronic scanning ellipsometer. Film composition was measured with a scanning Auger electron spectrometer. It is concluded that metal oxide formation is accelerated within the wear tracks.

Lauer, J. L.↗

Ignition of a Combustible Atmosphere by Incandescent Carbon Wear Particles

A study was made to determine whether carbon wear particles from carbon elements in sliding contact with a metal surface were sufficiently hot to cause ignition of a combustible atmosphere. In some machinery, electric potential differences and currents may appear at the carbon-metal interface. For this reason the effect of these voltages and currents on the ability of carbon wear particles to cause ignition was evaluated. The test specimens used in the investigation were carbon vanes taken from a fuel pump and flat 21-inch-diameter 2 metal disks (440-C stainless steel) representing the pump housing. During each experiment a vane was loaded against a disk with a 0.5-pound force, and the disk was rotated to give a surface speed of 3140 feet per minute. The chamber of the apparatus that housed the vane and the disk was filled with a combustible mixture of air and propane. Various voltages and amperages were applied across the vane-disk interface. Experiments were conducted at temperatures of 75, 350, 400, and 450 F. Fires were produced by incandescent carbon wear particles obtained at conditions of electric potential as low as 106 volts and 0.3 ampere at 400 F. Ignitions were obtained only with carbon wear particles produced with an electric potential across the carbon-vane-disk interface. No ignitions were obtained with carbon wear particles produced in the absence of this potential; also, the potential difference produced no ignitions in the absence of carbon wear particles. A film supplement showing ignition by incandescent wear particles is available.

Buckley, Donald H.↗

Rapid and Efficient Deposition of Metal Oxide Coatings for Bearings and Gears in Harsh Environments

The objective of this project is to develop Tribocoating; an innovative, rapid, low-cost, energy-efficient, and environmentally friendly coating technology designed to enhance the performance and durability of bearings and gears operating under harsh conditions. Tribocoating creates protective metal-oxide tribofilms through in-situ tribosintering of nanocrystals (NCs). Components are simply run in a nano-enabled Tribocoating fluid prior to deployment; no surface pretreatment, coating equipment, or external energy input is required.

17 WIND ENERGY↗

Friction and wear behavior of glasses and ceramics.

Adhesion, friction and wear behavior of glasses and ionic solids are reviewed. These materials are shown to behave in a manner similar to other solids with respect to adhesion. Their friction characteristics are shown to be sensitive to environmental constituents and surface films. This sensitivity can be related to a reduction in adhesive bonding and the changes in surficial mechanical behavior associated with Rehbinder and Joffe effects. Both friction and wear properties of ionic crystalline solids are highly anisotropic. With metals in contact with ionic solids, the fracture strength of the ionic solid, the shear strength in the metal, and those properties that determine these will dictate which of the materials undergoes adhesive wear.

Buckley, D. H.↗

Dynamic-scanning-electron-microscope study of friction and wear

A friction and wear apparatus was built into a real time scanning electron microscope (SEM). The apparatus and SEM comprise a system which provides the capability of performing dynamic friction and wear experiments in situ. When the system is used in conjunction with dispersive X-ray analysis, a wide range of information on the wearing process can be obtained. The type of wear and variation with speed, load, and time can be investigated. The source, size, and distribution of wear particles can be determined and metallic transferal observed. Some typical results obtained with aluminum, copper, and iron specimens are given.

Brainard, W. A.↗

Friction and wear of single-crystal and polycrystalline maganese-zinc ferrite in contact with various metals

Sliding friction experiments were conducted with single-crystal (SCF) and hot-pressed polycrystalline (HPF) manganese-zinc ferrite in contact with various metals. Results indicate that the coefficients of friction for SCF and HPF are related to the relative chemical activity of those metals in high vacuum. The more active the metal, the higher the coefficient of friction. The coefficients of friction for both SCF and HPF were the same and much higher in vacuum than in argon at atmospheric pressure. All the metals tested transferred to the surface of both SCF and HPF in sliding. Both SCF and HPF exhibited cracking and fracture with sliding. Cracking in SCF is dependent on crystallographic characteristics. In HPF, cracking depends on the orientation of the individual crystallites.

Miyoshi, K.↗

Tribological properties of surfaces

The real area of contact between two solid surfaces is only a small portion of the apparent area. Deformation of these areas can result in solid state contact through surface films. For clean solid to solid contact strong adhesive bonding occurs across the interface. Under these conditions many properties of the solid such as the metallurgical and chemical nature of metals can influence adhesion, friction, and wear behavior. The presence of gases, liquids, and solid films on the surface of solids alter markedly tribological characteristics. These surface films can also considerably change the mechanical effects of solid state contact on bulk material behavior.

Buckley, D. H.↗

Tribological properties of surfaces

The real area of contact between two solid surfaces is only a small portion of the apparent area. Deformation of these areas can result in solid state contact through surface films. For clean solid to solid contact strong adhesive bonding occurs across the interface. Under these conditions many properties of the solid such as the metallurgical and chemical nature of metals can influence adhesion, friction, and wear behavior. The presence of gases, liquids, and solid films on the surface of solids alter markedly tribological characteristics. These surface films can also considerably change the mechanical effects of solid state contact on bulk material behavior.

Buckley, D. H.↗

Ceramic coating effect on liner metal temperatures of film-cooled annular combustor

An experimental and analytical investigation was conducted to determine the effect of a ceramic coating on the average metal temperatures of full annular, film cooled combustion chamber liner. The investigation was conducted at pressures from 0.50 to 0.062. At all test conditions, experimental results indicate that application of a ceramic coating will result in significantly lower wall temperatures. In a simplified heat transfer analysis, agreement between experimental and calculated liner temperatures was achieved. Simulated spalling of a small portion of the ceramic coating resulted in only small increases in liner temperature because of the thermal conduction of heat from the hotter, uncoated liner metal.

Claus, R. W.↗

Metallic Environmentally Resistant Coatings Rapid Innovation Initiative (MERCRII) Mechanism Development and Testing

This project seeks to address the high friction and low wea resistance of lightweight aluminum (Al) and titanium (Ti) alloys to extend the lifetime and sustainability of both lunar and Martian assets missions by developing advanced wear-and radiation-resistant. MERCRII started with 6 candidate coating materials and 3 candidate application methods that were down-selected through pathfinder and 2 phases of testing to one coating configuration: Ti64 with 2%hBN Vacuum Plasma Spray.

dust mitigation↗

Friction and wear of ceramics

The adhesion, friction, wear, and lubricated behaviors of both oxide and non-oxide ceramics are reviewed. Ceramics are examined in contact with themselves, other harder materials, and metals. Elastic, plastic, and fracture behavior of ceramics in solid state contact is discussed. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Grit size effects in two and three body abrasive wear are observed for ceramics. Both the free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Surface contaminants affect friction and adhesive wear. For example, carbon on silicon carbide and chlorine on aluminum oxide reduce friction while oxygen on metal surfaces in contact with ceramics increases friction. Lubrication increases the critical load necessary to initiate fracture of ceramics both in indentation and with sliding or rubbing.

Buckley, Donald H.↗