At least 163 records · Page 9

Suppressed deprotonation enables a durable buried interface in tin-lead perovskite for all-perovskite tandem solar cells

Low-band-gap tin (Sn)-lead (Pb) perovskites are a critical component in all-perovskite tandem solar cells (APTSCs). Current state-of-the-art Sn-Pb perovskite devices exclusively use poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) (PEDOT:PSS) as the hole-transport layer (HTL) but suffer from undesired buried-interface degradation. Here, we show that the deprotonation of the –SO 3 H group in PSS is the root cause of the interface degradation due to its low acid dissociation constant (pK a ), leading to acidic erosion and iodine volatilization in Sn-Pb perovskites. We identify that HTL featuring the carboxyl (–COOH) group with a higher pK a , such as poly[3-(4-carboxybutyl)thiophene-2,5-diyl] (P3CT), can suppress deprotonation and strengthen the interface, mitigating the buried-interface degradation. Motivated by established P3CT modification, we introduce Pb doping to P3CT to increase its work function and reduce interfacial energy loss. Furthermore, we fabricate APTSCs with a champion efficiency of 27.8% and an operational lifetime of over 1,000 h, with 97% retaining efficiency under maximum power point tracking.

08 HYDROGEN↗

Operando Depth-Resolved Measurement of Solvation Entropy, Interfacial Transport, and Charge-Transfer Kinetics in Lithium-Ion Batteries

Understanding and improving the performance and longevity of lithium-ion batteries critically depends on insight into the dynamic processes occurring at buried electrode-electrolyte interfaces. However, direct, depth-resolved, and operando diagnosis of these interfaces remains a longstanding challenge due to their inaccessibility beneath bulk materials, the limitations of conventional surface- and bulk-sensitive characterization tools, and the difficulty of maintaining realistic cell environments during measurement. These challenges have made it nearly impossible to uniquely resolve important interfacial properties such as charge transfer resistance, SEI (solid electrolyte interphase) resistance, and solvation entropy at the individual electrode interfaces within a working cell, information that is essential for mechanistic insight and accelerated battery design. Here, in this study, we report the development of multiharmonic electro-thermal spectroscopy (METS), an operando technique that enables depth-resolved measurement of solvation entropy, interfacial transport resistance, charge-transfer resistance, and SEI resistance at individual electrode-electrolyte interfaces within practical lithium-ion batteries. By leveraging frequency-dependent, thermal-wave sensing and interface-specific modeling, METS uniquely attributes interfacial properties to specific electrodes, as validated by comparison with traditional electrochemical impedance spectroscopy (EIS). The ability to spatially and temporally resolve interfacial processes in real time provides new diagnostic capabilities that are crucial for mechanistic studies of battery degradation and for the rapid development of next-generation energy storage systems.

Chalise, Divya [University of California, Berkeley↗

Basics of the scanning electrochemical microscope and its application in the characterization of lithium-ion batteries: a brief review

A scanning electrochemical microscope (SECM) can directly monitor electrochemical processes at interfaces of electrodes and electrolytes and has been used as an analytical tool for lithium-ion battery (LIB) studies. Through SECM, we can visualize the electrochemical reactivities of active species in LIBs in-situ during cycling. This review begins with introducing SECM-based LIB research and then summarizes the working mechanism and operating modes of the technique as well as combinations of SECM with other techniques for LIB studies. We review the results with a focus on the interfacial properties, surface reactions and electrochemical activity of different electrode materials for LIBs. The investigations of battery degradation, kinetic parameters and electrolyte swelling by SECM are also discussed. Finally, the current limitations and perspectives are also described regarding future developments.

25 ENERGY STORAGE↗

Computational Modeling of Heterogeneity of Stress, Charge, and Cyclic Damage in Composite Electrodes of Li-Ion Batteries

Charge heterogeneity is a prevalent feature in many electrochemical systems. In a commercial cathode of Li-ion batteries, the composite is hierarchically structured across multiple length scales including the sub-micron single-crystal primary-particle domains up to the macroscopic particle ensembles. The redox kinetics of charge transfer and mass transport strongly couples with mechanical stresses. This interplay catalyzes substantial heterogeneity in the charge (re)distribution, stresses, and mechanical damage in the composite electrode during charging and discharging. We assess the heterogeneous electrochemistry and mechanics in a LiNi x Mn y Co z O 2 (NMC) cathode using a fully coupled electro-chemo-mechanics model at the cell level. A microstructure-resolved model is constructed based on the synchrotron X-ray tomography data. We calculate the stress field in the composite and then quantitatively evaluate the kinetics of surface charge transfer and Li transport biased by mechanical stresses. We further model the cyclic behavior of the cell. The repetitive deformation of the active particles and the weakening of the interfacial strength cause gradual increase of the interfacial debonding. The mechanical damage impedes electron transfer, incurs more charge heterogeneity, and results in the capacity degradation in batteries over cycles.

25 ENERGY STORAGE↗

Comprehensive Characterization of Multi-Phase Sulfurized Polyacrylonitrile Cathodes for Lithium-Sulfur Batteries

Sulfurized polyacrylonitrile (SPAN) is considered one of the most promising cathode materials to overcome the operational challenges that plague lithium-sulfur (Li-S) batteries. However, material properties and electrochemical performance implications of SPAN prepared under different synthesis conditions are not yet fully investigated. In this study, we show the impacts of different synthesis conditions on the formation of sulfur to PAN bonds and redox reaction mechanisms of multi-phase SPAN via comprehensive material and electrochemical characterizations. In-situ Raman analysis was first applied to study the multi-phase SPAN-based Li-S cells. We found that both elemental sulfur and chemically bonded sulfur are present under the synthesis condition of 300 degree C/3 h along with unreacted PAN. The incompletely sulfurized, multi-phase SPAN exhibited an unusually rapid capacity degradation in the resultant Li-S cells, which is attributed to polysulfide formation and continuously growing interfacial impedance in the Li-S cells. On the other hand, SPAN samples prepared under the synthesis condition of 350 degree C/3 h are found completely sulfurized with chemically bonded sulfur to the PAN backbone without the presence of free elemental sulfur. Complete sulfurization of SPAN led to exceptionally stable cycle performance due to excellent reversible redox processes of chemically bonded sulfur with Li+ in the Li-S cells.

DIRECT ENERGY CONVERSION,ENERGY STORAGE↗

Enhanced cycling stability of Ni-rich Li-metal cells enabled by dual vinylene carbonate and tris(trimethylsilyl)borate electrolyte additives

NMC811 (LiNi 0.8 Co 0.1 Mn 0.1 O 2 ) and other high-Ni chemistries are promising cathode candidates for high-performance electric vehicles, owing to their high energy density and reduced cobalt content. However, their long-term cycling stability is hindered by surface degradation, particularly when paired with conventional electrolytes and a lithium metal anode. Electrolyte additives represent a practical approach to enhance interfacial stability and improve overall battery performance by promoting the formation of a robust electrolyte–electrode interphase (EEI). In this study, we revisit the effects of vinylene carbonate (VC) and tris(trimethylsilyl)borate (TMSB) additives on single-crystal SC-NMC811||Li cells. While TMSB only increases the open-circuit voltage and initial overpotential, it delivers superior capacity retention at C/3 compared to cells containing only VC or a dual additive system (VC and TMSB). Notably, under fast-charging conditions (1C, 2C, and 5C), the dual-additive system significantly outperforms other formulations, achieving markedly enhanced long-term capacity retention. Comprehensive electrochemical and spectroscopic analyses reveal that the VC/TMSB dual-additive system suppresses surface transition in NMC811, mitigates structural degradation by forming a thin, LiF-deficient cathode-electrolyte interface (CEI) layer. Moreover, they promote smooth and dense Li deposition and generate a LiF-deficient solid-electrolyte interphase (SEI). Consequently, the synergistic stabilization of both the CEI and SEI effectively limits the overall cell impedance growth during extended cycling. These findings provide key insights into co-additive strategies for engineering stable interfaces in high-energy Ni-rich Li-metal batteries.

36 MATERIALS SCIENCE↗

Electrolyte Reactivity at the Charged Ni-Rich Cathode Interface and Degradation in Li-Ion Batteries

The chemical and electrochemical reactions at the positive electrode–electrolyte interface in Li-ion batteries are hugely influential on cycle life and safety. Ni-rich layered transition metal oxides exhibit higher interfacial reactivity than their lower Ni-content analogues, reacting via mechanisms that are poorly understood. Here, we study the pivotal role of the electrolyte solvent, specifically cyclic ethylene carbonate (EC) and linear ethyl methyl carbonate (EMC), in determining the interfacial reactivity at charged LiNi 0.33 Mn 0.33 Co 0.33 O 2 (NMC111) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes by using both single-solvent model electrolytes and the mixed solvents used in commercial cells. While NMC111 exhibits similar parasitic currents with EC-containing and EC-free electrolytes during high voltage holds in NMC/Li 4 Ti 5 O 12 (LTO) cells, this is not the case for NMC811. Online gas analysis reveals that the solvent-dependent reactivity for Ni-rich cathodes is related to the extent of lattice oxygen release and accompanying electrolyte decomposition, which is higher for EC-containing than EC-free electrolytes. Combined findings from electrochemical impedance spectroscopy (EIS), TEM, solution NMR, ICP, and XPS reveal that the electrolyte solvent has a profound impact on the degradation of the Ni-rich cathode and the electrolyte. Higher lattice oxygen release with EC-containing electrolytes is coupled with higher cathode interfacial impedance, a thicker oxygen-deficient rock-salt surface reconstruction layer, more electrolyte solvent and salt breakdown, and higher amounts of transition metal dissolution. These processes are suppressed in the EC-free electrolyte, highlighting the incompatibility between Ni-rich cathodes and conventional electrolyte solvents. Finally, new mechanistic insights into the chemical oxidation pathways of electrolyte solvents and, critically, the knock-on chemical and electrochemical reactions that further degrade the electrolyte and electrodes curtailing battery lifetime are provided.

25 ENERGY STORAGE↗

Substrate effects on phase formation and interfacial stability in superconducting vanadium silicide thin films

Thin films of vanadium silicide (V-silicide) in the A15 cubic phase (V 3 Si) are promising for superconducting quantum devices due to their high transition temperature and potential compatibility with scalable semiconductor fabrication. However, solid-phase synthesis often yields secondary silicide phases that degrade performance. Here, in this study, we investigate the influence of substrate properties using two silicon-on-insulator architectures: one with a polycrystalline HfO 2 buried layer (group A) and the other with amorphous SiO 2 (group B). Both systems exhibit superconductivity consistent with V 3 Si formation, yet structural analysis reveals mixed-phase films in both cases. Crucially, only group A maintains an atomically sharp and chemically stable interface, a prerequisite for phase purity. Prolonged annealing in group A reduces the unwanted V 5 Si 3 phase but also leads to the emergence of Si-rich VSi 2 , likely due to localized substrate degradation. Preliminary atomic-resolution imaging suggests that HfO 2 crystallinity may promote local phase-selective nucleation. These findings highlight the importance of substrate design in promoting phase control and maintaining interfacial integrity in superconducting silicides.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Enhanced Electrocatalytic and Cathode‐Electrolyte Interfacial Properties With a Pr‐Based Simple Perovskite/Ruddlesden‐Popper Nanocomposite Cathode in Protonic Ceramic Fuel Cells

The sluggish kinetics and poor stability of the oxygen reduction reaction (ORR) remain the primary bottleneck for achieving high performance in protonic ceramic fuel cells (PCFCs) at intermediate temperatures (400–650°C). In this work, a Pr-based nanocomposite cathode comprised of simple perovskite phase (PrNi 0.7 Co 0.3 O 3-δ ) and Ruddlesden-Popper phase (Co-doped Pr 4 Ni 3 O 10+δ ) is developed. Although PrNi 0.7 Co 0.3 O 3-δ solely stands as a good cathode with facile proton transfer, combining the superior catalytic activity against oxygen on the Ruddlesden-Popper phase boosts the ORR performance further. The designed nanocomposite cathode outperforms the simple perovskite cathode, attributed to enhanced oxygen absorption and surface diffusion with the Ruddlesden-Popper phase. A precursor-based cathode deposition technique is also developed to achieve cathode grain sizes of ∼100 nm. A single cell with the nanocomposite cathode delivers a peak power density of 1.38 W cm −2 at 650°C, among the highest in reported PCFCs with Pr-based cathodes, with a small degradation rate of 0.145 mV h −1 during 250 h stability test. Further investigation of cathode-electrolyte interface revealed interfacial PrO 2 phase formation, promoted by abundant Pr 6 O 11 in the nanocomposite precursor powder, thereby improving both ohmic resistance and stability. These findings highlight the effectiveness of the nanocomposite cathode and underscore its advantages on interfacial properties.

08 - HYDROGEN↗

Coherent Acoustic Interferometry during the Photodriven Oxygen Evolution Reaction Associates Strain Fields with the Reactive Oxygen Intermediate (Ti–OH*)

The oxygen evolution reaction (OER) from water requires the formation of metastable, reactive oxygen intermediates to enable oxygen–oxygen bond formation. Conversely, such reactive intermediates could also structurally modify the catalyst. Here, a descriptor for the overall catalytic activity, the first electron and proton transfer OER intermediate from water, (M–OH*), has been associated with significant distortions of the metal–oxygen bonds upon charge-trapping. Time-resolved spectroscopy of in situ, photodriven OER on transition metal oxide surfaces has characterized M–OH* for the charge trapping and the symmetry of the lattice distortions by optical and vibrational transitions, respectively, but had yet to detect an interfacial strain field arising from a surface coverage M–OH*. Here, we utilize picosecond, coherent acoustic interferometry to detect the uniaxial strain normal to the SrTiO 3 /aqueous interface directly caused by Ti–OH*. The spectral analysis applies a fairly general methodology for detecting a combination of the spatial extent, magnitude, and generation time of the interfacial strain through the coherent oscillations’ phase. For lightly n-doped SrTiO 3 , we identify the strain generation time (1.31 ps), which occurs simultaneously with Ti–OH* formation, and a tensile strain of 0.06% (upper limit 0.6%). In addition to fully characterizing this intermediate across visible, mid-infrared, and now GHz-THz probes on SrTiO 3 , we show that strain fields occur with the creation of some M–OH*, which modifies design strategies for tuning catalytic activity and provides insight into photo-induced degradation so prevalent for OER. To that end, the work put forth here provides a unique methodology to characterize intermediate-induced interfacial strain across OER catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Reactive boride infusion stabilizes Ni-rich cathodes for lithium-ion batteries

Engineered polycrystalline electrodes are critical to the cycling stability and safety of lithium-ion batteries, yet it is challenging to construct high-quality coatings at both the primary- and secondary-particle levels. Here, we present a room-temperature synthesis route to achieve full surface coverage of secondary particles and facile infusion into grain boundaries, thus offering a complete “coating-plus-infusion” strategy. Cobalt boride metallic glass is successfully applied to Ni-rich layered cathode LiNi 0.8 Co 0.1 Mn 0.1 O 2 . Here, it dramatically improves the rate capability and cycling stability, including under high-discharge-rate and elevated-temperature conditions and in pouch full cells. The superior performance originates from simultaneous suppression of microstructural degradation of intergranular cracking and side reactions with electrolyte. Atomistic simulations identified the critical role of strong selective interfacial bonding, which offers not only a large chemical driving force to ensure uniform reactive wetting and facile infusion but also lowered the surface/interface oxygen activity, contributing to the exceptional mechanical and electrochemical stabilities of the infused electrode.

25 ENERGY STORAGE↗

On Stability and Electrochemical Performance of 316 Stainless Steel in Wastewater: Implications for Resource Recovery

Electrochemical nutrient recovery systems rely on stable electrode materials capable of operating in chemically complex wastewater environments. We investigated corrosion resistance and interfacial electrochemical behavior of 316 stainless steel (SS316) in a synthetic wastewater matrix representative of centrate streams, a key knowledge gap in electrochemical phosphorus recovery. A comprehensive suite of electrochemical techniques (chronoamperometry, cyclic voltammetry, potentiodynamic polarization, and electrochemical impedance spectroscopy (EIS)) and surface characterization methods (scanning electron microscopy, X-ray diffraction) were employed. Results revealed that wastewater containing typical ionic constituents (such as PO 4 3- , NH 4 + , and divalent cations) exhibited enhanced cathodic activity and the formation of a more stable, protective surface film on SS316 that mitigated chloride-induced corrosion. In contrast, SS316 in the NaCl solution showed significant susceptibility to passive layer breakdown and localized corrosion. Time-resolved EIS further confirmed improved interfacial stability and restricted charge transfer in WW over time, in stark contrast to the progressive passive layer degradation in NaCl. Surface analyses corroborated these findings, showing limited surface attack in WW compared to distinct localized corrosion features in NaCl. These findings indicate that competing ionic species in WW effectively mitigate chloride aggressiveness, enhance SS316 stability, and demonstrate improved electrode longevity and reliability for sustainable wastewater-based electrochemical phosphorus recovery applications.

36 MATERIALS SCIENCE↗

Dependence of adhesion on degradation mechanisms of ethylene co-vinyl acetate encapsulants over the lifetime of photovoltaic modules

The long-term reliability of encapsulation has a critical impact on the overall cost and effectiveness of photovoltaic modules. An often overlooked but important element of this reliability concerns adhesive degradation of the encapsulant, which results in delamination. This work critically examines the degradation mechanisms – deacetylation, β-scission, and hydrolytic depolymerization – primarily responsible for adhesion loss in ethylene co-vinyl acetate (EVA) encapsulants to provide evidence and clarity regarding the contribution of these mechanisms to the adhesive degradation over the lifetime of a module. EVA samples obtained from mini-modules exposed in two sets of controlled, accelerated conditions – with and without ultraviolet (UV) radiation – are characterized to find specific evidence for the proposed degradation mechanisms. The mini-modules were exposed up to 10,000 h, which represents up to 15–20 years in the field. Results affirm that initially, deacetylation dominates the degradation before scission takes over, followed by hydrolytic depolymerization. Additional analysis highlights the climacteric interdependency between deacetylation and hydrolytic depolymerization as it relates to eventual delamination, where deacetylation products catalyze interfacial hydrolysis reactions. Furthermore, effects occurring at a given interface are isolated, explicitly providing evidence for how these mechanisms are nonuniform throughout the thickness of the EVA. Results demonstrate that the EVA that interfaces with the glass as opposed to the cell experiences increased levels of degradation, explaining why this initially stronger interface becomes the preferential interface for delamination after longer periods of exposure. Additionally, elevated temperatures alone are shown to induce limited migration of sodium ions across the glass/EVA interface.

36 MATERIALS SCIENCE↗

Multi-phase characterization of pitch-carbon coated nano-silicon anodes for lithium-ion batteries

Silicon (Si) is a leading next-generation Li-ion battery anode candidate that meets rigorous performance demands for portable power including enhanced power and energy density with robust cycling performance. However, a series of complex and interrelated reactions lead to reduced calendar life in Si-containing systems and therefore challenge practical adoption. In the present work, we probe the mechanisms underlying observed performance improvements by adding a pitch-carbon coating onto nano-Si material. We pair solid-phase (X-ray photoemission spectroscopy, Fourier-transform infrared), semi-volatile phase (solid-phase microextraction-gas chromatography-mass spectrometry), and gas-phase (gas chromatography-flame-ionization detector) characterization signals to comprehensively evaluate the impact of pitch-carbon coating on the evolution of the Si solid-electrolyte interphase (SEI) and the associated impacts on electrode/electrolyte reactivity. The pitch-carbon is found to serve as a physicochemical barrier, reducing the electro-active surface area for Si/electrolyte reactivity and preventing Si oxidation. Further, the pitch-carbon coating promotes the evolution of a more-favorable SEI by subsuming substantial functionality typically associated with the fluoroethylene carbonate (FEC) electrolyte additive - such as alkoxide scavenging and suppression of transesterification pathways - and by shifting the competitive electrolyte degradation pathways' favorability. The multi-phase characterization approach enables holistic end-products evaluation from complex (electro)chemical interfacial reactions, which informs a robust interpretation of the carbon coating's role in electrochemical performance improvements. The present mechanistic evaluation aids the rational design for improved nano-Si materials.

25 ENERGY STORAGE↗

How Water Attacks MXene

Two-dimensional (2D) transition metal carbides and nitrides (MXenes) have shown outstanding performances in electrochemical energy storage and many other applications. However, the stability of MXene remains a concern, especially its quick degradation in aqueous solutions under ambient conditions. Here, we report on the water/Ti 3 C 2 O 2 -MXene interfacial chemistry from first-principles molecular dynamics simulations at room temperature. Surprisingly, we find that the water molecules can attack the basal plane of Ti 3 C 2 O 2 and pull the surface Ti atoms out, thereby reconstructing the surface. Further, by tracking close encounters of water molecules and surface Ti atoms on the basal plane of Ti 3 C 2 O 2 , we show that the attack is initiated by the chemisorption of a water molecule on a surface Ti atom, followed by the breaking of Ti–C bonds and deprotonation of the water molecule, leading to the formation of Ti–OH on the Ti 3 C 2 O 2 surface and a hydronium ion in the aqueous phase. Our finding highlights the susceptibility of Ti 3 C 2 O 2 MXene to water attack, supporting recent experimental observations. Furthermore, we demonstrate that preventing close encounters of water molecules and the surface Ti atoms is key to the stability of the basal plane and can be realized by negatively charging the surface (thereby reorienting the O atoms of water away from the surface) or converting the surface O to -OH groups (thereby shifting the water layer further away from the surface). Our insights and approach highlight the importance of the reactivity of water when interfacing with 2D materials such as MXenes.

36 MATERIALS SCIENCE↗

Dynamic Bubbling Balanced Proactive CO 2 Capture and Reduction on a Triple-Phase Interface Nanoporous Electrocatalyst

The formation and preservation of the active phase of the catalysts at the triple-phase interface during CO 2 capture and reduction is essential for improving the conversion efficiency of CO 2 electroreduction toward value-added chemicals and fuels under operational conditions. Designing such ideal catalysts that can mitigate parasitic hydrogen generation and prevent active phase degradation during the CO 2 reduction reaction (CO 2 RR), however, remains a significant challenge. Herein, we developed an interfacial engineering strategy to build a new SnO x catalyst by invoking multiscale approaches. This catalyst features a hierarchically nanoporous structure coated with an organic F-monolayer that modifies the triple-phase interface in aqueous electrolytes, substantially reducing competing hydrogen generation (less than 5%) and enhancing CO 2 RR selectivity (~90%). This rationally designed triple-phase interface overcomes the issue of limited CO 2 solubility in aqueous electrolytes via proactive CO 2 capture and reduction. Concurrently, we utilized pulsed square-wave potentials to dynamically recover the active phase for the CO 2 RR to regulate the production of C1 products such as formate and carbon monoxide (CO). This protocol ensures profoundly enhanced CO 2 RR selectivity (~90%) compared with constant potential (~70%) applied at -0.8 V (V vs RHE). We further achieved a mechanistic understanding of the CO 2 capture and reduction processes under pulsed square-wave potentials via in situ Raman spectroscopy, thereby observing the potential-dependent intensity of Raman vibrational modes of the active phase and CO 2 RR intermediates. Finally, this work will inspire material design strategies by leveraging triple-phase interface engineering for emerging electrochemical processes, as technology moves toward electrification and decarbonization.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

LLNL-LDRD-Final report

The main focus of this study is the X-ray spectroscopy and complementary modeling characterization of the range of perovskite materials. Specific areas covered in this study include: • Quantitative characterization of individual (both CB and VB) band edge movement as a function of Sn concentration; • The effects of creating an interface with the charge transport layer and back contact on both the interfacial bonding and unoccupied band structure – i.e., how does the interfacial eDOS evolve when the interface is assembled; • How does this interface change (local bonding, CB edge) evolve with degradation – this includes depth profiling; • Additional insights from the spectroscopy – e.g., the pathway of degradation (Sn(II) oxide formation to a significant depth before Sn(IV) oxide formation, etc.), do different charge transport layers have distinct properties in slowing degradation, etc.

14 SOLAR ENERGY↗

Engineering ligand reactivity enables high-temperature operation of stable perovskite solar cells

Perovskite solar cells (PSCs) consisting of interfacial two- and three-dimensional heterostructures that incorporate ammonium ligand intercalation have enabled rapid progress toward the goal of uniting performance with stability. However, as the field continues to seek ever-higher durability, additional tools that avoid progressive ligand intercalation are needed to minimize degradation at high temperatures. We used ammonium ligands that are nonreactive with the bulk of perovskites and investigated a library that varies ligand molecular structure systematically. Here, we found that fluorinated aniliniums offer interfacial passivation and simultaneously minimize reactivity with perovskites. Using this approach, we report a certified quasi–steady-state power-conversion efficiency of 24.09% for inverted-structure PSCs. In an encapsulated device operating at 85°C and 50% relative humidity, we document a 1560-hour T85 at maximum power point under 1-sun illumination.

14 SOLAR ENERGY↗