Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “images”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

High-speed synchrotron X-ray imaging of directed energy deposition of titanium: effects of processing parameters on the formation of entrapped-gas pores

Laser based directed energy deposition (DED) is a competitive method for repairing and remanufacturing metallic parts used in numerous industries including aerospace and biomedical. However, the numerous dynamic phenomena associated with the DED process often result in defects such as entrapped-gas pores, lack of fusion, and undesirable anisotropic properties. The entrapped-gas pore, being one of the most common issues, not only influences melt-pool dynamics but also reduces the fabrication quality and mechanical properties of parts fabricated by the DED process. To reduce and further understand this issue, the real-time observation of the pore formation process needs to be studied first. To directly observe the phenomena in the melt pool, high-speed techniques are needed because rapid solidification leads to rapid pore formation and movement. In-situ high-speed X-ray has been proven to be an effective method in investigating the melt pool dynamics and pore formation mechanisms in the laser powder bed fusion process, in which the fabrication process is quite different from that in DED. Here, the high-speed X-ray method is extended to study the formation of entrapped-gas pores. The real-time formation and quantitative analysis of pores under each set of processing parameters (particle velocity, laser power, and spot welding dwelling time of stationary laser) in the DED process are investigated. We found that the DED with a higher particle velocity (3.19 m/s) produced a smaller average pore size of 27.8 µm and a lower pore area fraction of 0.52%. The DED under lower laser power (156 W) generated a smaller average pore size of 20.3 µm and a lower pore area fraction of 1.94%. The shorter dwelling time (10 ms) benefited the decrease of both average pore size and pore area fraction.

Defect↗

Imaging the Phase Evolution of the Li-N-H Hydrogen Storage System

Complex metal hydrides provide high-density hydrogen storage, which is essential for vehicular applications. However, the utility of these materials has been limited by thermodynamic and kinetic barriers present during the dehydrogenation and rehydrogenation processes as new phases form inside parent phases. Better understanding of the mixed-phase mesostructures and their interfaces may assist in improving cyclability. In this work, the evolution of the phases during hydrogenation of lithium nitride and dehydrogenation of lithium amide with lithium hydride are probed with scanning-transmission X-ray microscopy at the nitrogen K edge. With this technique, intriguing core-shell structures were observed in particles of both partially hydrogenated Li 3 N and partially dehydrogenated LiNH 2 + 2 LiH. The potential contributions of both internal hydrogen mobility and interfacial energies on the generation of these structures are discussed.

08 HYDROGEN↗