Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “grain boundary segregation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

High-pressure strengthening in ultrafine-grained metals

The Hall–Petch relationship, according to which the strength of a metal increases as the grain size decreases, has been reported to break down at a critical grain size of around 10 to 15 nanometres. As the grain size decreases beyond this point, the dominant mechanism of deformation switches from a dislocation-mediated process to grain boundary sliding, leading to material softening. In one previous approach, stabilization of grain boundaries through relaxation and molybdenum segregation was used to prevent this softening effect in nickel–molybdenum alloys with grain sizes below 10 nanometres. Here we track in situ the yield stress and deformation texturing of pure nickel samples of various average grain sizes using a diamond anvil cell coupled with radial X-ray diffraction. Our high-pressure experiments reveal continuous strengthening in samples with grain sizes from 200 nanometres down to 3 nanometres, with the strengthening enhanced (rather than reduced) at grain sizes smaller than 20 nanometres. Here, we achieve a yield strength of approximately 4.2 gigapascals in our 3-nanometre-grain-size samples, ten times stronger than that of a commercial nickel material. A maximum flow stress of 10.2 gigapascals is obtained in nickel of grain size 3 nanometres for the pressure range studied here. We see similar patterns of compression strengthening in gold and palladium samples down to the smallest grain sizes. Simulations and transmission electron microscopy reveal that the high strength observed in nickel of grain size 3 nanometres is caused by the superposition of strengthening mechanisms: both partial and full dislocation hardening plus suppression of grain boundary plasticity. These insights contribute the ongoing search for ultrastrong metals via materials engineering.

36 MATERIALS SCIENCE↗

Minor Elements and Solidification Cracking During Laser Powder-Bed Fusion of a High $\gamma ^{\prime }$ CoNi-Base Superalloy

Here, the cracking behavior of a high γ' volume fraction CoNi-base superalloy fabricated via laser powder bed fusion (LPBF) is studied in relation to the content of carbon and boron. Severe cracking occurred with the increase in boron content from 0.08 to 0.16 at. pct (0.015 to 0.029 wt pct), while compositions with 0.1 to 0.36 at. pct C (0.02 to 0.076 wt pct) and 0.08 at. pct B exhibited minimal cracking. Assessment of cracks in the high-boron composition shows a variation in crack density with printing parameters, and alignment of the cracks with the build direction. Scanning electron microscopy (SEM) of the crack surfaces shows evidence of a solidification cracking mode. Differential thermal analysis (DTA) reveals a decreased incipient melting temperature for the high-boron composition, and atom probe tomography (APT) is used to measure the enrichment at grain boundaries, revealing distinct boron segregation. Scheil-Gulliver solidification simulations for the different C and B levels are consistent with the incipient melting behavior observed with DTA. Evaluation of the solidification cracking susceptibility from the simulations allow for comparison of the CoNi alloy behavior to Ni-base superalloys studied for LPBF fabrication and displays how such metrics may aid in the design of new precipitation-strengthened superalloys for additive manufacturing (AM).

36 MATERIALS SCIENCE↗

Role of niobium in the high-temperature oxidation of titanium

Here, we compared the oxidation of Ti and Ti-2 at.% Nb at 800°C in Ar-20% O 2 and in sequential 16 O 2 - 18 O 2 atmospheres to clarify the role of niobium in the high-temperature oxidation of titanium. Niobium had no effect on the amount of oxygen dissolved in the metal or on oxygen diffusion in the metal. Instead, niobium enhanced oxidation resistance by segregating to TiO 2 grain boundaries, where it likely slowed outward Ti diffusion. These findings spotlight doping of TiO 2 grain boundaries as a strategy for improving the oxidation resistance of Ti alloys and, more generally, TiO 2 -forming alloys.

36 MATERIALS SCIENCE↗

Stabilizing Ni-rich layered cathode for high-voltage operation through hierarchically heterogeneous doping with concentration gradient

High-nickel LiNi x Mn y Co 1-x-y O 2 (NMC) cathodes have demonstrated superior energy density, yet their stability is compromised under high voltage conditions. To address this, here we propose a strategy of heterogeneous doping with a concentration gradient, specifically through Sr–Zr co-modification. We synthesized Ni-rich NMC particles featuring several micron-sized secondary particles composed of micron-sized primary grains. This design aims to harness the structural robustness of single-crystalline grains and the favorable diffusion kinetics of polycrystalline secondary particles. Systematic characterization using a combination of electrochemical measurements and synchrotron analytics reveals an intriguing pattern of hierarchically heterogeneous Sr–Zr co-doping. It demonstrates a depth-dependent concentration gradient at the secondary particle level and competing dopant segregation over the buried grain boundaries. This unique characteristic creates opportunities for enhancing battery performance, particularly by optimizing precursors and implementing advanced modulation techniques. We also investigate the dissolution and precipitation of the cathode's transition metal cations upon high-voltage cycling. These insights suggest that a tailored compositional variation can be a viable approach to effectively design the next-generation high-Ni NMC cathode materials for high-voltage lithium batteries.

36 MATERIALS SCIENCE↗

Impact of annealing at 1000°C in flowing He with low O 2 concentration on the room temperature tensile properties of Mo alloys

NorthStar is developing an accelerator-based technology to produce the medical isotope Mo-99. A previous ORNL report (ORNL/SPR-2022/2490) studied the oxidation behavior of Mo in flowing He with low oxygen content at 800°C and 1000°C and it was shown that an O 2 concentration lower than ~5ppm (μ1/1) is required to achieve acceptable oxidation rates for wrought or powder metallurgy (PM) Mo. Oxidation may also impact the mechanical properties of Mo and this report summarizes tensile results at room temperature on wrought and PM Mo before and after exposure at 1000°C in flowing He with O 2 concentration varying from 1 to 15 ppm O 2 . It was found that oxidation at 1000°C results in a significant decrease of Mo strength and ductility with brittle intergranular fracture surfaces, likely due to the segregation of oxygen at grain boundaries. For the PM Mo material, the decrease in strength and ductility was also observed after annealing in vacuum at 1000°C, indicating that the diffusion of the oxygen trapped in the material pores to grain boundaries after 20-100h at 1000°C is sufficient to embrittle the material. Finally, initial results on actual aMo and high-density disks provided by NorthStar revealed the lack of ductility of the materials due to the specific disk microstructure.

36 MATERIALS SCIENCE↗

Effects of Melt Convection and Solid Transport on Macrosegregation and Grain Structure in Equiaxed Al-Cu Alloys

Macrosegregation in metal casting can be caused by thermal and solutal melt convection, and the transport of unattached solid crystals resulting from nucleation in the bulk liquid or dendrite fragmentation. To develop a comprehensive numerical model for the casting of alloys, an experimental study has been conducted to generate benchmark data with which such a solidification model could be tested. The objectives were: (1) experimentally study the effects of solid transport and thermosolutal convection on macrosegregation and grain size; and (2) provide a complete set of boundary conditions temperature data, segregation data, and grain size data - to validate numerical models. Through the control of end cooling and side wall heating, radial temperature gradients in the sample and furnace were minimized. Thus the vertical crucible wall was adiabatic. Samples at room temperature were 24 cc and 95 mm long. The alloys used were Al-1 wt. pct. Cu, and Al- 10 wt. pct. Cu; the starting point for solidification was isothermal at 710 and 685 C respectively. To induce an equiaxed structure various amounts of the grain refiner TiB2 were added. Samples were either cooled from the top, or the bottom. Several trends in the data stand out. In attempting to model these experiments, concentrating on these trends or differences may be beneficial.

Rerko, Rodney S.↗

Grain boundary self-diffusion and point defect interactions in α -U via molecular dynamics

Though metallic U-Zr fuel has been used in nuclear reactors since the 1960s, many of its fundamental and thermodynamic properties are still unknown. The a-U phase, which has a highly anisotropic crystal structure and physical properties, is present in U-Zr fuel. The character and behavior of a-U grain boundaries will strongly impact fuel thermophysical performance under irradiation. Here, we study the interaction of point defects with grain boundaries, diffusion along grain boundaries, and the predicted diffusional creep behavior of a-U via molecular dynamics. We calculate the segregation energy of vacancies and interstitials to grain boundaries and quantify the biased sink strength of the grain boundaries, and observe that this sink strength is not strongly dependent on the grain boundary orientation. We also find that grain boundary diffusivity is strongly dependent on the grain boundary energy and grain boundary orientation. The presence of point defects within the grain boundary can induce diffusion in grain boundaries with low formation energies and can enhance diffusion in high-energy grain boundaries. We also find that diffusional creep of a-U at prototypical metallic fuel operation conditions is extremely high and could help explain observed metallic fuel swelling behaviors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Convection-Induced Compositional Patterning at Grain Boundaries in Irradiated Alloys

We consider the stability of precipitates formed at grain boundaries (GBs) by radiation-induced segregation in dilute alloys subjected to irradiation. Here, the effects of grain size and misorientation of symmetric-tilt GBs are quantified using phase field modeling. A novel regime is identified where, at long times, GBs are decorated by precipitate patterns that resist coarsening. Maps of the chemical Péclet number indicate that arrested coarsening takes place when solute advection dominates over thermal diffusion right up to the precipitate/matrix interface, preventing interfacial local equilibrium and overriding capillary effects. This contrasts with liquid-solid mixtures where convection always accelerates coarsening.

36 MATERIALS SCIENCE↗

Effect of Melt Convection and Solid Transport on Macrosegregation and Grain Structure in Equiaxed Al-Cu Alloys

Macrosegregation in metal casting can be caused by thermal and solutal melt convection, and the transport of unattached solid crystals. These free grains can be a result of, for example, nucleation in the bulk liquid or dendrite fragmentation. In an effort to develop a comprehensive numerical model for the casting of alloys, an experimental study has been conducted to generate benchmark data with which such a solidification model could be tested. The specific goal of the experiments was to examine equiaxed solidification in situations where sinking of grains is (and is not) expected. The objectives were: 1) experimentally study the effects of solid transport and thermosolutal convection on macrosegregation and grain size distribution patterns; and 2) provide a complete set of controlled thermal boundary conditions, temperature data, segregation data, and grain size data, to validate numerical codes. The alloys used were Al-1 wt. pct. Cu, and Al-10 wt. pct. Cu with various amounts of the grain refiner TiB2 added. Cylindrical samples were either cooled from the top, or the bottom. Several trends in the data stand out. In attempting to model these experiments, concentrating on experiments that show clear trends or differences is recommended.

Rerko, Rodney S.↗

($\mathrm{INVITED}$)Counter-ion effect on the diffusion behavior of $\mathrm{Y}$b, $\mathrm{L}$u, and $\mathrm{N}$d ions in $\mathrm{YAG}$ transparent ceramics

The ability to fabricate additively manufactured laser waveguides with sharp dopant concentration interfaces is limited by diffusion of the dopants at the temperatures required to fully densify the material. Compositional analysis of bilayer samples, where each layer was either undoped YAG or YAG doped with Yb, Lu, or Nd, were fabricated such that all combinations were available for testing. Samples were fabricated at both 1750°C and 1850°C to determine the diffusion behavior of each dopant alone and also in the presence of a second dopant. It was found that the experimental concentration profiles exhibited both intragranular (bulk) and grain boundary contributions, and thus fitting to a complementary error function equation required the use of two diffusion coefficients. Nd always diffused further along grain boundaries than the other dopants, due in part to its small segregation coefficient in YAG. It is shown that the presence of Nd as a counter dopant inhibits intragranular diffusion of other dopants while enhancing their grain boundary diffusion. All the observed trends were attributed to a combination of intragranular lattice strain due to: dopant ions replacing yttrium substitutionally, the relative driving forces for the segregation of dopant ions to grain boundaries, and the ability of one dopant to affect the diffusion of a different dopant in the other direction to maintain charge neutrality.

36 MATERIALS SCIENCE↗

Computational design of passivants for CdTe grain boundaries

CdTe is the second most-widely deployed photovoltaic (PV) material due to its high efficiency and low manufacturing costs. Currently, polycrystalline CdTe (poly-CdTe) has a record efficiency of similar to 22%, which is still well below the theoretical limit (similar to 30%). Polycrystalline CdTe films that have incorporated Cl or Se show higher efficiency, possibly due to the segregation of these ions to the grain boundaries (GBs), where they may passivate the dangling bonds. However, the efficiency enhancement mechanisms of passivants in CdTe GBs, and the feasibility of employing alternative passivants, have not been well explored. Here, we present a systematic computational study of CdTe GBs with potential passivants, namely S, P, As, Se, and Sb on Te sites, and Na, Mg, Al, Sc, Cu, and Zn on Cd sites. Density functional theory (DFT) calculations were performed on GB dislocation core structures derived from scanning transmission electron microscopy (STEM) images of a model GB (bicrystal). We computed the segregation thermodynamics, electronic density of states, and charge variations near doped CdTe GBs. We find that segregation of impurities to GBs is thermodynamically favorable. For a Te-terminated core, Se, S, and P on Te sites effectively reduce midgap states. For both Cd-and Te-terminated dislocation cores, Sc and Al reduce midgap states when substituted for Cd atoms. Overall, the greatest improvement was achieved with co-doping, i.e. simultaneously substituting Te with Se and substituting Cd with Cu or Al. The elimination of midgap states is predicted to increase the photovoltaic efficiency of CdTe by reducing the recombination at grain boundaries.

14 SOLAR ENERGY↗

Segregation behavior and phase instability of Eurofer97 after neutron irradiation to 72 dpa

Here, a reduced activation ferritic/martensitic steel, Eurofer97, was neutron irradiated in the vicinity of 300 °C in the High Flux Isotope Reactor (HFIR) up to 72 dpa. Advanced analytical scanning transmission electron microscopy and conventional transmission electron microscopy were applied to investigate the radiation-induced segregation and phase instability behavior after neutron irradiation. Amorphization was observed in M 23 C 6 carbides. Cr-rich clusters were seen within the matrix, near the lath boundaries and close to the M 23 C 6 carbides. Cr enrichment and Fe depletion were detected at both prior austenite grain boundaries and lath boundaries, despite different segregation magnitude. In addition, the enrichment of Ni, the depletion of V, and tiny cavities (presumably helium bubbles) are also found at lath boundaries. This work interrogates the evolution of microstructures after neutron irradiation, which provides detailed understanding on the microstructural aspects controlling the mechanical integrity of Eurofer97 under high-dose neutron damage.

36 MATERIALS SCIENCE↗

Heavy ion irradiation response of an additively manufactured 316LN stainless steel

Additive manufacturing has become an appealing technique to fabricate three-dimensional metallic materials and components for nuclear reactors. However, response of additively manufactured alloys to high-dose heavy ion irradiations at elevated temperatures is still not well understood. Here, an additively manufactured 316LN austenitic stainless steel with high-density solidification cells was irradiated using 3.5 MeV Fe ion to a peak dose of 220 dpa at 450 °C. Microscopy studies show a lower Frank loop density and smaller size in the additively manufactured sample compared with its cold worked counterpart, and the cellular structures may largely suppress the formation of perfect loops and dislocation networks and reduce the magnitude of solute segregations comparing with high angle grain boundaries. In conclusion, the present work advances the understanding on the high-temperature irradiation response of additively manufactured steels for nuclear reactor applications.

36 MATERIALS SCIENCE↗

Texturing of high T(sub c) superconducting polycrystalline fibers/wires by laser-driven directional solidification in an thermal gradient

This paper summarizes the technique of laser-driven directional solidification in a controlled thermal gradient of yttria stabilized zirconia core coated Y-Ba-Cu-O materials to produce textured high T(sub c) superconducting polycrystalline fibers/wires with improved critical current densities in the extended range of magnetic fields at temperatures greater than 77 K. The approach involves laser heating to minimize phase segregation by heating very rapidly through the two-phase incongruent melt region to the single phase melt region and directionally solidifying in a controlled thermal gradient to achieve highly textured grains in the fiber axis direction. The technique offers a higher grain growth rate and a lower thermal budget compared with a conventional thermal gradient and is amenable as a continuous process for improving the J(sub c) of high T(sub c) superconducting polycrystalline fibers/wires. The technique has the advantage of suppressing weak-link behavior by orientation of crystals, formation of dense structures with enhanced connectivity, formation of fewer and cleaner grain boundaries, and minimization of phase segregation in the incongruent melt region.

Varshney, Usha↗

The effect of diffusive segregation on the fracture of hydrogen charged nickel

Hydrogen charged nickel was deformed in tension at a test temperature of 208 K to study the diffusive segregation of hydrogen during straining and the dependence of embrittlement on grain boundary hydrogen concentration and deformation rate. Tests were performed on samples in the as-quenched condition at various strain rates. An increase in the degree of embrittlement at slow strain rates can be attributed to diffusive segregation of hydrogen to grain boundaries during the test period. The embrittlement of samples with equal grain boundary hydrogen concentration was found to be relatively insensitive to strain rate, bulk hydrogen concentration and the total time at the test temperature.

Lassila, D. H.↗

Vacancy-mediated transport and segregation tendencies of solutes in FCC Ni under diffusional creep

Nickel-based alloys are known for their excellent corrosion resistance and high-temperature strength. However, at high temperatures, polycrystals experience grain boundary-stress-driven vacancy diffusion leading to diffusion-driven creep. Understanding the fundamentals of defect migration is essential to predict diffusion creep behavior. In this talk, we explore the Nabarro-Herring diffusion creep and the associated solute segregation that is likely to result from the different diffusivities of the solute and solvent elements. Density functional theory calculations are performed to determine the formation, migration and binding energies of the solute and vacancy defects in stress-free and stressed states. The dilute-limit transport coefficients are then calculated using the self-consistent mean field theory as implemented in the Kinetic Cluster Expansion (KineCluE) code. Predictions of diffusion creep strain rates and solute segregation are then presented for various solutes, stress and temperatures. This work opens research avenues for exploration of diffusion creep via characterization of elemental segregation to grain boundaries.

36 MATERIALS SCIENCE↗

The Riddle of Dark LLZO: Cobalt Diffusion in Garnet Separators of Solid‐State Lithium Batteries

Abstract Solid‐state batteries (SSBs) with a Li 7 La 3 Zr 2 O 12 (LLZO) garnet electrolyte are attracting much attention as robust and safe alternative to conventional lithium‐ion batteries. Technical challenges in the practical implementation of garnet SSBs are related to the need for high‐temperature sintering, which often leads to undesirable chemical reactions with the cathode material. While these reactions are well understood for composite cathodes, very little is known about similar processes between cathode and separator during battery fabrication. This work focuses on understanding the processes between the composite LiCoO 2 ‐LLZO cathode and the LLZO separator and how they affect the battery performance. The extensive diffusion of Co‐ions within LLZO, which leads to the often‐observed LLZO darkening, is shown to have a significant impact on ionic conductivity, electronic conductivity, and dendrite stability of the separator. Experimental data coupled with large‐scale molecular dynamics simulations uncover the diffusion mechanism for Co‐ions and identify secondary phases that form during these interactions. In addition to extensive Co‐ion diffusion within the grains, a non‐uniform segregation of Co‐ions at grain boundaries is found leading to the formation of three distinct Co‐containing phases. This work offers a general approach to studying the fundamental ion diffusion processes that occur during the fabrication of oxide SSBs.

electrochemical properties↗

Microstructural characterization of cold-worked 316 stainless steel flux thimble tubes irradiated up to 100 dpa in a commercial Pressurized Water Reactor

Two flux thimble tubes (FTT) made of 15% cold-worked 316 stainless steel (SS) were harvested from Ringhals Pressurized Water Reactor (PWR) Unit 2, with peak damages of 76 and 100 displacements per atom (dpa) after 29 and 34 years’ service, respectively. Specimens sectioned from parent tubes were comprehensively characterized with nominal damage levels of ~0, ~41, ~74, 76, and 100 dpa at a nominal temperature range of 285-323 °C. Both FTTs contained helium and hydrogen gases as transmutation products. The helium follows a production rate of ~9.8 appm/dpa, while environmental factors complicate hydrogen production obscuring an exact H/dpa ratio. Irradiation-induced dislocation loops, nano-cavities, solute clusters, and microsegregation were all observed. The dislocation loops and nano-cavities indicated saturation at 41 dpa. The solute clusters continued to evolve with Ni-Si clusters formed at 41 dpa, and Ni-Si-Mn-P clusters formed at 74 and 100 dpa, but neither clusters exhibited distinct diffraction patterns at any damage levels. Solute clusters were observed to frequently be co-located with dislocation loops, but fully decorated loops were rarely detected. Significant radiation-induced segregation (RIS) was observed around grain boundaries at all damage levels. The modified inverse Kirkendall (MIK) model captured the RIS behavior of major elements. Large cavities within or around an Mn-S rich region were observed for the first time. Through all the damage levels, void swelling is always below 0.05%, making significant dimensional change unlikely in core internals when used at similar conditions. Meanwhile, the role of overwhelming nanocavities, presumably helium bubbles, should be considered in other potential degradation mechanisms, including irradiation-assisted stress corrosion cracking, embrittlement, and loss of fracture toughness, which remain the concerns for extended operation of nuclear power plants.

Post Irradiation Examination, Isotope Dilution Mas↗