Possible Realization of Hyperbolic Plasmons in Few-Layered Rhenium Disulfide

Hyperbolic plasmons are a highly desired property in optoelectronics and biomolecular sensing. The necessary condition to realize hyperbolic plasmons is a significant anisotropy of the principal components of the dielectric function, such that at a certain frequency range, one component is negative and the other is positive, i.e., one component is metallic, and the other one is dielectric. Here, we study the effect of anisotropy in ReS 2 , and our theory shows that ReS 2 can host hyperbolic plasmons in the ultraviolet frequency range. The operating frequency range of the hyperbolic plasmons can be tuned with the number of ReS 2 layers. However, we note that the significantly large imaginary part of the macroscopic dielectric response in all layered variants of ReS 2 can result in substantial losses for the hyperbolic plasmons, as in the case with other known hyperbolic materials, with the exception of MoOCl 2 . We also note that ReS 2 hosts ultraviolet hyperbolic plasmons while ZrSiSe, WTe 2 , and CuS nanocrystals host infrared plasmons, providing a novel platform for optoelectronics in the ultraviolet range.

36 MATERIALS SCIENCE↗

Enhanced Magnetism and Anomalous Hall Transport through Two-Dimensional Tungsten Disulfide Interfaces

The magnetic proximity effect (MPE) has recently been explored to manipulate interfacial properties of two-dimensional (2D) transition metal dichalcogenide (TMD)/ferromagnet heterostructures for use in spintronics and valleytronics. However, a full understanding of the MPE and its temperature and magnetic field evolution in these systems is lacking. In this study, the MPE has been probed in Pt/WS 2 /BPIO (biphase iron oxide, Fe 3 O 4 and α-Fe 2 O 3 ) heterostructures through a comprehensive investigation of their magnetic and transport properties using magnetometry, four-probe resistivity, and anomalous Hall effect (AHE) measurements. Density functional theory (DFT) calculations are performed to complement the experimental findings. We found that the presence of monolayer WS 2 flakes reduces the magnetization of BPIO and hence the total magnetization of Pt/WS 2 /BPIO at T > ~120 K—the Verwey transition temperature of Fe 3 O 4 (T V ). However, an enhanced magnetization is achieved at T < T V . In the latter case, a comparative analysis of the transport properties of Pt/WS 2 /BPIO and Pt/BPIO from AHE measurements reveals ferromagnetic coupling at the WS 2 /BPIO interface. Our study forms the foundation for understanding MPE-mediated interfacial properties and paves a new pathway for designing 2D TMD/magnet heterostructures for applications in spintronics, opto-spincaloritronics, and valleytronics.

36 MATERIALS SCIENCE↗

Superconductivity in intercalated molybdenum disulfide.

X-ray studies show the existence of two different types of expansions of the intercalated unit cell in both Na and K compounds. Two different phases are also indicated in the superconducting behavior of the K compound. All intercalated samples studied show a superconducting transition. K and Rb compounds become superconductors in the temperature range from 6.5 to 6.0 K. The Na compounds become superconductors at about 4.5 K. In all cases, the superconductivity disappears upon a short exposure of the sample to air. This phenomenon confirms that the superconductivity is due to the presence of the alkali metal.

Somoano, R.↗

Bearing endurance tests in vacuum for sputtered molybdenum disulfide films

Angular-contact, 440C stainless steel, ball bearings with sputtered MoS2 films 0.0000006 x 10-7m (6000 A) thick were evaluated in a vacuum bearing chamber (1750 rpm, 137.9-N- (31-lbf-) thrust load) for endurance. Two types of sputtered films were evaluated: (1) MOS2 sputtered directly onto bearing components, and (2) a thin 0.0000001 x 10-7m (1000 A) underlayer of Cr3Si2 subsequently sputtered with MoS2. Bearing test evaluations in vacuum showed that endurance lives of more than 1000 hours (105,000,000 cycles) were obtained with bearings (cage, races, and balls) directly sputtered with MoS2. The same endurance lives were also obtained when only the races and cage were sputtered with an underlayer of Cr3Si2 and subsequently with MoS2.

Spalvins, T.↗

X-ray photoelectron spectroscopy study of radiofrequency sputtered chromium bromide, molybdenum disilicide, and molybdenum disulfide coatings and their friction properties

Radiofrequency sputtered coatings of CRB2, MOSI2, and MOS2 were examined by X-ray photoelectron spectroscopy. The effects of sputtering target history, deposition time, RF power level, and substrate bias on film composition were studied. Friction tests were run on RF sputtered surfaces of 440-C steel to correlate XPS data with lubricating properties. Significant deviations from stoichiometry and high oxide levels for all three compounds were related to target outgassing. The effect of biasing on these two factors depended on the compound. Improved stoichiometry correlated well with good friction and wear properties.

Wheeler, D. R.↗

Lubrication and failure mechanisms of molybdenum disulfide films. 2: Effect of substrate roughness

An optical microscope was used to study the lubrication and failure mechanisms of rubbed MoS2 films applied to three substrate surface finishes; polished, sanded, and sandblasted as a function of sliding distance. The lubrication mechanism was the plastic flow of thin films of MoS2 between flat plateaus on the rider and on the metallic substrate. If the substrate was rough, flat plateaus were created during run-in and the MoS2 flowed across them. Wear life was extended by increasing surface roughness since valleys in the roughened substrate served as reservoirs for MoS2 and as deposit sites for wear debris. In moist air the failure mechanism was the transformation of metallic colored MoS2 films to a black, powdery material that was found by X-ray diffraction to be alpha iron, MoO3, and possibly FeMoO3. In dry argon the failure mechanism was the gradual depletion of MoS2 from the contact region by transverse flow, and the wear debris on the track at failure was alpha iron, residual MoS2, and possibly FeS.

Fusaro, R. L.↗

Effect of Substrate Surface Finish on the Lubrication and Failure Mechanisms of Molybdenum Disulfide Films

An optical microscope was used to study the lubrication and failure mechanisms of rubbed (burnished) MoS2 films applied to three substrate surface finishes - polished, sanded, and sandblasted - as a function of sliding distance. The lubrication mechanism was the plastic flow of thin films of MoS2 between flat plateaus on the rider and on the metallic substrate. If the substrates were rough, flat plateaus were created during 'run in' and the MoS2 flowed across them. Wear life was extended by increasing surface roughness since valleys in the roughened substrate served as reservoirs for MoS2 and a deposit site for wear debris. In moist air, the failure mechanism was the transformation of metallic colored MoS2 films to a black, powdery material that was found by X ray diffraction to consist primarily of alpha iron and MoO3 powders. In dry argon, the failure mechanism was the gradual depletion of the MoS2 film from the contact region by transverse flow. Analysis of the wear debris on the wear track at failure showed it consisted mainly of alpha iron and some residual MoS2. No molybdenum oxides were found.

Fusaro, R. L.↗

Dynamics of solid dispersions in oil during the lubrication of point of contacts. Part 2: Molybdenum disulfide

A Hertzian contact consisting of a steel ball in contact with a glass disk is lubricated with MoS2 dispersions and observed by optical microscopy at various slide/roll conditions. In general the behavior of MoS2 and graphite are similar. That is, the solids tend to enter the contact and form a film on the contacting surfaces whenever a rolling component of motion is used, but solid particles seldom enter the contact during pure sliding. The MoS2 has more pronounced plastic flow behavior than graphite. However, the polished steel ball is more readily scratched by MoS2 than by graphite. Under the conditions of these studies, lower friction and wear are observed with pure oil rather than with the dispersions. However under other conditions (such as different contact geometry or rougher surfaces) the solid lubricant dispersions might be beneficial.

Cusano, C.↗

Effect of substrate surface finish on the lubrication and failure mechanisms of molybdenum disulfide films

An optical microscope was used to study the lubrication and failure mechanisms of rubbed (burnished) MoS2 films applied to three substrate surface finishes - polished, sanded, and sandblasted - as a function of sliding distance. The lubrication mechanism was the plastic flow of thin films of MoS2 between flat plateaus on the rider and on the metallic substrate. If the substrate was rough, flat plateaus were created during 'run-in' and the MoS2 flowed across them. Wear life was extended by increasing surface roughness since valleys in the roughened substrate served as reservoirs for MoS2 and a deposit site for wear debris. In moist air, the failure mechanism was the transformation of metallic-colored MoS2 films to a black, powdery material that was found by X-ray diffraction to consist primarily of alpha-iron and MoO3 powders. In dry argon, the failure mechanism was the gradual depletion of the MoS2 film from the contact region by transverse flow. Analysis of the wear debris on the wear track at failure showed it consisted mainly of alpha-iron and some residual MoS2. No molybdenum oxides were found.

Fusaro, R. L.↗

Picosecond coherent anti-Stokes Raman scattering (CARS) study of vibrational dephasing of carbon disulfide and benzene in solution

The vibrational dephasing of the 656/cm mode (nu1, a1g) of CS2 and the 991/cm mode (nu2, a1g) of benzene have been studied as a function of concentration in mixtures with a number of solvents using a ps time-resolved CARS technique. This technique employs two tunable synchronously-pumped mode-locked dye lasers in a stimulated Raman pump, coherent anti-Stokes Raman probe time-resolved experiment. Results are obtained for CS2 in carbon tetrachloride, benzene, nitrobenzene, and ethanol and for benzene nu2 in CS2. The dephasing rates of CS2 nu1 increase on dilution with the polar solvents and decrease or remain constant on dilution with the nonpolar solvents. The CS2/benzene solutions show a contrasting behavior, with the CS2 nu1 dephasing rate being nearly independent of concentration whereas the benzene nu2 dephasing rate decreases on dilution. These results are compared to theoretical models for vibrational dephasing of polyatomic molecules in solution.

Perry, Joseph W.↗

Performance and properties of arsenic passivated lithium-titanium disulfide cells

In order to inhibit chemical degradation associated with the lithium-electrolyte interaction in ambient temperature lithium cells, an attempt was made to synthetically passivate the anode via ion implantation of arsenic. Solvent reduction is reduced although salt reaction with lithium is still present. The performance of the Li-TiS2 cell differs from those with standard electrodes, but further work is necessary to clarify the efficacy of this mode of passivation.

Yen, S. P. S.↗

Interfacial analysis of tribological systems containing molybdenum disulfide and iron using XPS and CEMS

In the present evaluation of results from studies of the interfacial chemistry and morphology of a buried lubricant-substrate interface, specimens of increasing complexity that culminated with the effects of excess sulfur and defects were characterized by XPS and SEM, as well as conversion-electron Moessbauer spectroscopy (CEMS). In order to simulate sputtered systems, single crystals of MoS2 were damaged with Ar(+) bombardment and coated with Fe. Fe is found to react differently with MoS2 depending on surface treatments, surface defects, annealing treatments, and the presence of excess sulfur. The annealing temperature determines which compounds are formed, as well as the crystal habit and plane at the Fe-MoS2 interface.

Zabinski, J. S.↗

Disulfide-linked oligonucleotide phosphorothioates - Novel analogues of nucleic acids

The synthesis of phosphorothioate analogs of oligonucleotides by the oxidation of deoxyadenosine 3',5'-bisphosphorothioate (3) was attempted. Cyclization of 3 is much more efficient than oligomerization under all the conditions investigated. However, a preformed oligonucleotide carrying a 5'-terminal phosphorotioate group undergoes efficient chain-extension when oxidized in the presence of 3.

Wu, Taifeng↗

Electrochemical impedance spectroscopy of lithium-titanium disulfide rechargeable cells

The two-terminal alternating current impedance of Li/TiS2 rechargeable cells was studied as a function of frequency, state-of-charge, and extended cycling. Analysis based on a plausible equivalent circuit model for the Li/TiS2 cell leads to evaluation of kinetic parameters for the various physicochemical processes occurring at the electrode/electrolyte interfaces. To investigate the causes of cell degradation during extended cycling, the parameters evaluated for cells cycled 5 times were compared with the parameters of cells cycled over 600 times. The findings are that the combined ohmic resistance of the electrolyte and electrodes suffers a tenfold increase after extended cycling, while the charge-transfer resistance and diffusional impedance at the TiS2/electrolyte interface are not significantIy affected. The results reflect the morphological change and increase in area of the anode due to cycling. The study also shows that overdischarge of a cathode-limited cell causes a decrease in the diffusion coefficient of the lithium ion in the cathode.

Narayanan, S. R.↗