The compressive failure of graphite/epoxy plates with circular holes
The results of an experimental investigation of the compressive behavior of T300/5203 graphite/epoxy laminated plates measuring 127.0 by 254.0 mm and containing circular holes ranging to 38.1 mm are reported. Two thicknesses, 24-ply and 48-ply, were chosen to differentiate between stability failures resulting from buckling and strength failures caused by the hole. Both quasi-isotropic and orthotropic stacking arrangements were used. The critical buckling load of the 24-ply panels was independent of hole size. Bifurcation occurred in the two half-wave mode longitudinally and one half-wave mode laterally in the quasi-isotropic panels. For the orthotropic 24-ply panels, bifurcation began in the one half-wave mode shape in each direction, but changed to the two half-wave mode before failure. Consistent post-buckling strength was exhibited by both laminated configurations. Panels with hole diameters below 3.175 mm displayed buckling before failure; those with holes larger than 6.35 mm experienced material failure around the hole before panel collapse.