Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “TENSILE PROPERTIES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Tensile Properties of 7075-T6 and 2024-T3 Aluminum-alloy Sheet Heated at Uniform Temperature Rates Under Constant Load

Results are presented of tests to determine the effect of heating at uniform temperature rates from 0.2 degrees to 100 degrees F. per second on the tensile properties of 7075-T6 d(75s-T6) and 2024-T3 (24s-T3) aluminum-alloy sheet under constant-load conditions. Yield and rupture stresses, obtained under rapid-heating conditions, are compared with results of elevated-temperature stress-strain tests for 1/2-hour exposure. Master yield-and-rupture-stress curves based on linear temperature-rate parameter are presented. Yield and rupture stresses and temperatures may be predicted by means of master curves and the parameter.

Heimerl, George J↗

Tensile Properties of Hydrogels and of Snake Skin

Stimulus-responsive or 'smart' gels are of potential interest as sensors and actuators, in industrial separations, and as permeable delivery systems. In most applications, a certain degree of mechanical strength and toughness will be required, yet the large-strain behavior of gels has not been widely reported. Some exceptions include work on gelatin and other food gels, some characterization of soft gels applicable for in-vitro cell growth studies, and toughness determinations on commercial contact lens materials. In general, it can be anticipated that the gel stiffness will increase with increasing degree of crosslinking, but the tensile strength may go through a maximum. Gel properties can be tailored by varying not only the degree of crosslinking, but also the polymer concentration and the nature of the polymer backbone (e.g. its stiffness or solubility). Polypeptides provide an especially interesting case, where secondary structure affects trends in moduli and conformational transitions may accompany phase changes. A few papers on the tensile properties of responsive gels have begun to appear. The responsive hydrogel chosen for the present study, crosslinked hydroxypropylcellulose, shrinks over a rather narrow temperature range near 44 C. Some vertebrate skin is also subject to substantial strain. Among reptiles, the morphologies of the skin and scales show wide variations. Bauer et al. described the mechanical properties and histology of gecko skin; longitudinal tensile properties of snake skin were examined by Jayne with reference to locomotion. The present measurements focus on adaptations related to feeding, including the response of the skin to circumferential tension. Tensile properties will be related to interspecific and regional variation in skin structure and folding.

Hinkley, Jeffrey A.↗

High Temperature Tensile Properties and Fatigue Behavior of a Melt-Infiltrated SiC/SiC Composite

High temperature fatigue behavior of a woven, SiC/SiC ceramic matrix composite (CMC) was investigated in air at two temperatures. The reinforcement for the CMC consisted of 5HS Sylramic(Trademark) fabric with a [0deg/90deg]4s lay-up. The SiC matrix material was infiltrated into the fiber-preform with a slurry-cast, melt-infiltration process. Tensile and fatigue test specimens were machined from the CMC plates. Initially tensile tests were conducted to obtain the average values of tensile properties at 1038 and 1204 C. Subsequently, low-cycle fatigue (LCF) tests with zero and two-hour hold-times at the maximum stress were conducted at the same two temperatures. Fatigue life data generated in the LCF tests were used to determine the geometric mean fatigue lives. In this paper, the tensile behavior and the fatigue durability of the CMC determined under different loading conditions are documented. In addition, reductions observed in the cyclic lives of the composite due to the two hour hold-time at maximum tensile stress are discussed.

Kalluri, Sreeramesh↗

Work hardening behavior and tensile properties of a high-Mn damping steel at elevated temperatures

Highlights: • Stability of austenite and ε-martensite was varied by changing the temperature of deformation. • Work hardening behavior was affected by the effects of TRIP, TWIP, DSA and dislocation slip. • Ultimate elongation was significantly decreased when ε → α′ transformation was too hard to occur. - Abstract: An austenite/ε-martensite dual-phase high-Mn damping steel was tensile deformed at elevated temperatures to conduct a comprehensive study about the effects of transformation-induced plasticity (TRIP), twinning-induced plasticity (TWIP), dynamic strain aging (DSA) and dislocation slip (DS) on its work hardening behavior and tensile properties. The results showed that the work hardening behavior of high-Mn damping steel can be divided into two stages. In stage-I, the main factor influencing the work hardening changed from γ → ε transformation to DS as the deformation temperature was increased. In the second stage, the work hardening exponent and ultimate tensile strength were large when intense DSA occurred at 80 °C and 120 °C, although ε → α′ transformation became more difficult at elevated temperatures. Tensile deformation at 200 °C promoted ε → γ transformation, such that the work hardening exponent and ultimate elongation were significantly decreased. In the later stage of deformation at 260 °C, TWIP effect effectively enhanced the work hardening as deformation-induced ε → α′ transformation occurred at low deformation temperatures.

36 MATERIALS SCIENCE↗

Effects of HCP/BCC element ratios on the room-temperature tensile properties of Ti-Zr-Hf-Nb-Ta refractory high-entropy alloys

Equiatomic and non-equiatomic Ti-Zr-Hf-Nb-Ta refractory high-entropy alloys (RHEAs) were arc melted, homogenized, cold rolled, and recrystallized to produce single-phase, body-centered cubic (BCC), microstructures with weak texture and equiaxed grains 76–199 μm in size. Here, the non-equiatomic alloys had either a 60:40 or 80:20 atomic ratio of hexagonal close-packed (HCP) elements (Ti + Zr + Hf) to BCC elements (Nb + Ta). Alloy compositions were measured after thermomechanical processing to determine the concentrations of the major (substitutional) and minor (interstitial) elements. We investigated how elastic constants and uniaxial tensile properties were affected by changes in the relative concentrations of the constituent elements at fixed HCP:BCC ratios. Yield strengths ranged from 801 to 922 MPa and ultimate tensile strengths from 815 to 933 MPa. Good agreement is obtained between the experimental yield strengths and those predicted by a strength theory based on edge dislocations indicating that the observed compositional effects are due to their effects on shear modulus and volume misfit. Fracture occurred by dimpled rupture with fracture strains of 19.4%–25.7%, but uniform strains were an order of magnitude lower at 1.1%–3.2%, calling into question the useable ductility (prior to necking) of RHEAs considered to be ductile based on their fracture strain. Contrary to predictions in the literature that HCP elements promote ductility, our present results show that increasing the HCP:BCC ratio decreases both the total strain and the uniform strain. Similar trends were not evident in the yield or ultimate strengths; rather, strengths were affected mainly by shear modulus and volume misfit.

BCC high-entropy alloys↗

Influence of humidity, temperature, and annealing on microstructure and tensile properties of electrospun polyacrylonitrile nanofibers

This study investigates the microstructure and mechanical properties of electrospun nanofibers from polyacrylonitrile (PAN)-dimethylformamide (DMF) solution at different relative humidity (RH) in the range from 14% to 60% and two different temperatures (20 °C and 40 °C). Nanofibers produced at low RH (22% or less at 20 °C) exhibit relatively smooth surface and solid core, whereas at higher RH (30% or higher at 20 °C) rough surface and porous core are observed. The resulting morphology is explained by means of H 2 O/DMF/PAN ternary phase diagram. At higher RH, the water diffusion into polymer-solution jet brings thermodynamic instability into the system leading to separation of polymer-rich phase and polymer-lean phase, where the later contributes to porosity. Higher process temperature (40 °C) yields larger miscibility area in the ternary phase diagram leading to formation of porous structure at relatively higher RH (40%). Tensile strength of nanofibrous yarns is found to vary from 80 MPa to 130 MPa depending on the processing temperature and RH. The amount of porosity is found to affect the tensile properties of nanofibers most significantly, although diameter and crystallinity play important role. Annealing is found to alleviate surface roughness and porosity and increase crystallinity. Furthermore, tensile strength of nanofibrous yarns is found to improve by up to 25% after annealing.

36 MATERIALS SCIENCE↗

Effect of prior creep at 1365 K on the room temperature tensile properties of several oxide dispersion strengthened alloys

An experimental study was conducted to determine whether oxide dispersion-strengthened (ODS) Ni-base alloys in wrought bar form are subject to creep degradation effects similar to those found in thin-gage sheet. The bar products evaluated included ODS-Ni, ODS-NiCr, and advanced ODS-NiCrAl types; the alloys included microstructures ranging from an essentially perfect single crystal to a structure consisting of very small elongated grains. Tensile test specimens were exposed to creep at various stress levels at 1365 K and then tensile tested at room temperature. Low residual tensile properties, change in fracture mode, appearance of dispersoid free bands, grain boundary cavitation, and/or internal oxidation are interpreted as creep degradation effects. The amount of degradation depends on creep strain, and degradation appears to be due to diffusional creep which produces dispersoid free bands around grain boundaries acting as vacancy sources.

Whittenberger, J. D.↗

Effects of Intermittent Versus Continuous Heating upon the Tensile Properties of 2024-T4, 6061-T6 and 7075-T6 Alloys

In some applications, aluminum alloys are subjected to intermittent heating at elevated temperature. It is generally considered that the effects of such intermittent heating are cumulative, and therefore are the same as if the heating had been continuous for the same total length of time. The object of these tests was to determine the effects of intermittent and continuous heating at 300 and 400 F, for total periods of 100 and 200 hr, upon the tensile properties of 2024-T4 and 6061-T6 alloy rolled-and-drawn rod and 7075-T6 alloy extrusions, at room temperature and at the temperature of heating.

Stickley, G. W.↗

Experimental study of UV induced tensile properties deterioration and chemical aging of polyurea–POSS composites

Ultraviolet (UV) radiation present in natural sunlight degrades the chemical and mechanical properties of polymeric matrices in composites. Polyurea possess a unique set of chemical and mechanical properties due to its complex microstructure comprising of hard and soft segments (phases). The primary objective of the work presented here is to characterize the chemical and mechanical degradation of pure polyurea and polyurea - polyhedral oligomeric silsesquioxane (POSS) nanocomposites subjected to UV radiation exposure for 45 days. Control specimen in as-received condition (reference specimen) and UV-aged tensile test specimen are tested in the study. Analysis of Fourier transformed infrared (FTIR) spectra for UV-aged polyurea and polyurea-POSS composites reveals that the addition of POSS nanoparticles accelerate the deterioration of polyurea matrix by breaking the hard phase network and altering the mechanism of degradation for the soft phase present in polyurea microstructure. The deterioration of hard and soft segments cause a significant reduction in tensile properties of polyurea-POSS composites.

Materials Science↗

A precipitation-hardened high-entropy alloy with outstanding tensile properties

Recent studies indicated that high-entropy alloys (HEAs) possess unusual structural and thermal features, which could greatly affect dislocation motion and contribute to the mechanical performance, however, a HEA matrix alone is insufficiently strong for engineering applications and other strengthening mechanisms are urgently needed to be incorporated. In this work, we demonstrate the possibility to precipitate nanosized coherent reinforcing phase, i.e., L1 2 -Ni 3 (Ti,Al), in a fcc-FeCoNiCr HEA matrix using minor additions of Ti and Al. Through thermomechanical processing and microstructure controlling, extraordinary balanced tensile properties at room temperature were achieved, which is due to a well combination of various hardening mechanisms, particularly precipitation hardening. The applicability and validity of the conventional strengthening theories are also discussed. In conclusion, the current work is a successful demonstration of using integrated strengthening approaches to manipulate the properties of fcc-HEA systems, and the resulting findings are important not only for understanding the strengthening mechanisms of metallic materials in general, but also for the future development of high-performance HEAs for industrial applications.

3 dimensional atom probe tomography↗

Anisotropic Tensile Properties of a 14YWT Nanostructured Ferritic Alloy: On the Role of Cleavage Fracture

Two plates of nanostructured ferritic alloy NFA-1 were processed by ball milling atomized Fe-14Cr-3W-0.4Ti-0.2Y (wt.%) with FeO powders, canning, and hot-extrusion at 850 °C, followed by annealing and multipass cross-rolling at 1000 °C. This produces a severe (001) brittle cleavage texture on planes running parallel to the plate faces. In the first plate (P1), pre-existing microcracks (MCs) formed on the cleavage planes during cross-rolling. The second plate (P2) contained far fewer, if any, MCs. Here, we compare the tensile data for out-of-plane (S) and in-plane (L) tensile axis orientations, at temperatures from −196 °C to 800 °C. We also assess the tensile property differences between P1 and P2, and the effect of specimen size. The L-orientation strength and ductility were excellent; for example, the room temperature (RT) yield stress, σy ≈ 1042 ± 102 MPa, and the total elongation, εt ≈ 12.9 ± 1.5%. In contrast, the S-orientation RT σy ≈ 708 ± 57 MPa, and εt ≤ 0.2%. These differences were due to cleavage on the brittle (001) planes. Cleavage leads to beneficial delamination toughening, but is deleterious to deformation processing and through-wall heat transfer. Therefore, it is important to quantitatively characterize the pronounced NFA-1 strength anisotropy due to severe crystallographic texturing and cleavage fracture.

Crystallography↗

Tensile Properties and Fracture Characteristics of Nanostructured Copper and Cu-SiC Nanocomposite Produced by Mechanical Milling and Spark Plasma Sintering Process

The presence of large grains within nanometric and ultrafine grain matrix is an effective method in order to enhance strength while keeping the high ductility of metals. For this purpose, in this research, spark plasma sintering (SPS) was used to consolidate milled Cu and Cu-SiC powders. In SPS process, local sparks with high temperature between particles take place and locally lead to intense grain growth, and therefore, this method has the ability to produce bimodal grain structures in copper and copper-based composites. Microstructural and mechanical studies showed ≈ 185 and ≈ 437 nm matrix grain sizes, high tensile yield strength values of ≈ 188.4 and ≈ 296.9 MPa, and fracture strain values of 15.1 and 6.7% for sintered Cu and Cu-4 vol.% SiC nanocomposite materials, respectively. The presence of nanoparticles promoted the occurrence of static recrystallization and decreased the fraction of coarse grains in microstructure. The high tensile properties of the produced materials are attributed to fine grain size, homogenous dispersion of nanoparticles and retarded grain boundary migration during sintering.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Tensile properties of HA 230 and HA 188 after 400 and 2500 hour exposures to LiF-22CaF2 and vacuum at 1093 K

The solid-to-liquid phase transformation of the nominal LiF-20CaF2 eutectic at 1043 K is considered to be an ideal candidate thermal energy storage mechanism for a space based low temperature Brayton cycle solar dynamic system. Although Co, Fe, and Ni superalloys are thought to be suitable containment materials for LiF based salts, long term containment is of concern because molten fluorides are usually corrosive and Cr can be lost into space through evaporation. Two examples of commercially available superalloys in sheet form, the Ni-base material HA 230 and the Co-base material Ha 88, have been exposed to molten LiF-22CaF2, its vapor, and vacuum, at 1093 K, for 400 and 2500 hr. Triplicate tensile testing of specimens subjected to all three environments have been undertaken between 77 to 1200 K. Comparison of the weight gain data, microstructure, and tensile properties indicate that little, if any, difference in behavior can be ascribed to the exposure environment.

Whittenberger, J. Daniel↗

Incorporating historical data and past analyses for improved tensile property prediction of 9% Cr steel

Data-driven analytical clustering and visualization techniques were applied to the dataset of 9% Cr experimental alloy data generated through the eXtremeMAT project. Techniques and results were compared with the resulting clusters obtained through similar analytical techniques on previous and reduced versions of the dataset. The principal components were generated in order to reduce the dimensionality of the complex dataset and to visualize the underlying trends in the data. Partitioning around medoids was performed on the resulting principal components to determine relevant clusters. Domain knowledge labels were further applied to the principal components to compare the labels with the trends identified through the clustering methods. The resulting clusters show the addition of the new data into the dataset, and show where alignment between the domain knowledge labels and partitioning around medoids (PAM) clusters show where the labels are appropriate. The clusters can be used to compare the tensile properties of the alloys, and to reduce the variation in the dataset.

Alloy design, Mechanical Properties, data analysis↗

Microstructure-refinement–driven enhanced tensile properties of high-pressure die-cast A380 alloy through friction stir processing

This work employs friction stir processing (FSP), a well-known severe plastic deformation technique, to selectively modify the microstructure of thin-walled, high-pressure die-cast (HPDC) aluminum alloy A380, a major HPDC alloy fabricated in the die casting sector. FSP effectively breaks down Al dendrites and acicular Si particles, creating a homogenized distribution of equiaxed Si particles in the aluminum matrix. After FSP, the refined Si particles (~1.5 µm) are smaller than the eutectic Si particles (3–8 µm) in HPDC condition. In addition, interparticle distance has decreased almost 50% compared to dendritic arm spacing, and FSP has reduced the aspect ratio of Si particles to ~2. Furthermore, FSP eliminates porosity, and breaks down needle-like second-phase Fe-Mn and Cu-rich particles, yielding a refined, homogeneous distribution. The FSP-induced microstructural refinement and porosity reduction improve bulk yield strength and ductility by 23% and 66%. Tensile properties are enhanced beyond those of the die skin of the HPDC plate, and the alloy possesses lower defect density and a highly refined microstructure. This study establishes the viability of FSP as a tool for microstructure modification and mechanical property improvement for HPDC Al alloys for the light-weighting goal of the automotive industries.

36 MATERIALS SCIENCE↗

The effect of postprocessing on tensile property and microstructure evolution of friction stir welding aluminum alloy joint

Friction stir welding is an efficient manufacturing method for joining aluminum alloy and can dramatically reduce grain size conferring excellent plastic deformation properties. Consequently, friction stir welding is used to manufacture tailor welded blanks to optimize weight or performance in the final component. In the study, the microstructural evolution and mechanical properties of friction stir welding joint during plastic forming and subsequent heat treatment were investigated. The microstructural characteristics of the friction stir welding joints were studied by Electron Backscattered Diffraction and Transmission Electron Microscopy. The mechanical properties were evaluated by tensile and microhardness tests. It is found that the tensile and yield strengths of friction stir welding joints are significantly improved after severe plastic deformation due to the grain refinement. Following heat treatment, the strength of the friction stir welding joints significantly decrease due to the obvious abnormal grain growth. Careful attention must be given to the processing route of any friction stir welding joint intended for plastic forming, especially the annealing between forming passes. Severe plastic deforming of the friction stir welding joint leads to a high level of stored energy/dislocation density, which causes the abnormal grain growth during subsequent heat treatment, and consequently reduce the mechanical properties of the friction stir welding joint. - Highlights: • Great changes are observed in the microstructure of FSW joint after postprocessing. • Postprocessing shows great effect on the microstructure stability of FSW joint. • The weld shows more significant decrease in strength than the BM due to the AGG. • Attention must be given to the processing route of FSW joint for plastic forming.

36 MATERIALS SCIENCE↗

Influence of the - phase separation on the tensile properties of Fe-base ODS PM 2000 alloy

The yield and ultimate tensile strengths of an ultrafine grained, oxide dispersion strengthened (ODS) PM 2000 alloy increased during aging at 475 C. Atom probe tomography and X-ray diffraction analysis revealed that the decrease in lattice parameter and the increases in the yield and ultimate tensile strengths were correlated with phase separation into Fe-rich {alpha} and Cr-enriched {alpha}{prime} phases. The lattice misfit between the emerging {alpha} and {alpha}{prime} domains and the resulting elastic strain, and the increment of the elastic modulus with aging time due to the corresponding decrease of lattice parameter during {alpha}-{alpha}{prime} phase separation, can be regarded as the main causes of hardening.

36 MATERIALS SCIENCE↗

In-Plane Tensile Properties, Creep Behavior and Failure Mechanisms of CVI and PIP SiC/SiC Composites at Temperatures to 1,650⁰C in Air

The in-plane tensile and creep properties of 2D woven CVI and PIP SiC/SiC composites with SylramicTM-iBN SiC fibers were measured at temperatures to 16500C in air and the data compared with the literature. Batch-to-batch variations in the tensile and creep properties, influence of thermal treatment on creep, creep parameters, damage mechanisms and failure modes for these composites were studied. Under the tested conditions, the CVI SiC/SiC composites exhibited both matrix and fiber dominated creep depending on stress, whereas the PIP SiC/SiC composites displayed only fiber dominated creep. Creep durability in both composite systems is controlled by the most creep resistant phase as well as oxidation of the fibers via cracked matrix. The Larson-Miller parameter and Monkman-Grant relationship were used wherever applicable for analyzing and predicting creep durability.

SiC-SiC Composites, CVI, PIP, Creep, In-plane tens↗