Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Solid electrolyte interface”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Improved electrochemical performance of spinel LiMn 1.5 Ni 0.5 O 4 through MgF 2 nano-coating

In this paper, a spinel LiMn 1.5 Ni 0.5 O 4 (LMNO) cathode material synthesized by a sol–gel method is modified by MgF 2 nano-coating via a wet coating strategy. The results of X-ray diffraction (XRD), Raman spectroscopy, field emission scanning electron microscopy (FESEM) and high resolution transmission electron microscopy (HRTEM) showed that the MgF 2 nano-coating layers do not physically change the bulk structure of the pristine material. Compared with the pristine compound, the MgF 2 -coated LMNO electrodes display enhanced cycling stabilities. Particularly, the 5 wt% MgF 2 -coated LMNO demonstrates the best reversibility, with a capacity retention of 89.9% after 100 cycles, much higher than that of the pristine material, 69.3%. The dQ/dV analysis and apparent Li + diffusion coefficient calculation prove that the kinetic properties are enhanced after MgF 2 surface modification, which partly explains the improved electrochemical performances. Electrochemical impedance spectroscopy (EIS) and Fourier transform infrared spectroscopy (FTIR) data confirm that the MgF 2 coating layer helps in suppressing the fast growth of the solid electrolyte interface (SEI) film in repeated cycling, which effectively stabilizes the spinel structure. Finally and additionally, differential scanning calorimetry (DSC) tests show that the MgF 2 nano-coating layer also helps in enhancing the thermal stability of the LMNO cathode.

36 MATERIALS SCIENCE↗

Electroreduction of Er 3+ in nonaqueous solvents

Here, the electroreduction of Er 3+ in propylene carbonate, N,N-dimethylformamide, or a variety of quaternary ammonium ionic liquids (ILs) was investigated using [Er(OTf) 3 ] and [Er(NTf 2 ) 3 ]. Systematic variation of the ILs' cation and anion, Er 3+ salt, and electrode material revealed a disparity in electrochemical interactions not previously seen. For most ILs at a platinum electrode, cyclic voltammetry exhibits irreversible interactions between Er 3+ salts and the electrode at potentials significantly less than the theoretical reduction potential for Er 3+ . Throughout all solvent–salt systems tested, a deposit could be formed on the electrode, though obtaining a high purity, crystalline Er 0 deposit is challenging due to the extreme reactivity of the deposit and resulting chemical interactions, often resulting in the formation of a complex, amorphous solid–electrolyte interface that slowed deposition rates. Comparison of platinum, gold, nickel, and glassy carbon (GC) working electrodes revealed oxidation processes unique to the platinum surface. While no appreciable reduction current was observed on GC at the potentials investigated, deposits were seen on platinum, gold, and nickel electrodes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A three-dimensional hierarchical structure of cyclized-PAN/Si/Ni for mechanically stable silicon anodes

Here, the main challenges associated with silicon anodes are their poor conductivity and severe structural degradation during cycling. Here we design a three-dimensional sandwich hierarchical structure that tackles these problems, and we demonstrate its use in flexible, large-area silicon anode assemblies. The design of the electrode is achieved via plasma enhanced chemical vapor deposition of silicon nanoparticles onto three-dimensional nickel foam followed by conformal coating of cyclized-PAN on the silicon surface, thus forming a sandwiched cyclized-PAN/Si/Ni hierarchical structure. The three-dimensional networks provide abundant electroactive zones and conductive transport paths, the conformal coating of cyclized-PAN accommodates volume change during cycling, and the monolithic electrode configuration without additional binders or conductive agents improves the energy density of the whole electrode. Furthermore, as a result of the sandwich hierarchical arrangement, the solid-electrolyte interface of the anode remains stable and spatially confined, leading to an increased reversible capacity and improved cycling stability (910 mA h g –1 after 100 cycles at 1.0 A g –1 ).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Solvating power series of electrolyte solvents for lithium batteries

From dictating the redox potential of electrolyte solvents to shaping the stability of solid-electrolyte interfaces, solvation plays a critical role in the electrochemistry of electrolytes. To efficiently design functional electrolytes for lithium batteries, it is particularly important to understand the relative solvating ability of each individual organic solvent, because most of the electrolyte systems are comprised of two or more electrolyte solvents. Using a newly developed internally referenced diffusion-ordered spectroscopy technique and diffusion coefficient–coordination ratio ($D–α$) analysis, we successfully constructed a solvating power series for common electrolyte solvents. We demonstrated the usefulness of this solvating power series in designing more reliable electrolyte system by selecting an appropriate fluorinated electrolyte solvent for a high-voltage lithium metal battery (LMB) as an example. For a methyl(2,2,2-trifluoroethyl)carbonate-based electrolyte, we identified fluoroethylene carbonate as a more desirable cyclic carbonate co-solvent than difluoroethylene carbonate for LMB due to its significantly higher ability to solvate lithium ions.

25 ENERGY STORAGE↗

Design principles of heterointerfacial redox chemistry for highly reversible lithium metal anode

High electrochemical reversibility is required for the application of high-energy-density lithium (Li) metal batteries; however, inactive Li formation and SEI (solid electrolyte interface)-instability-induced electrolyte consumption cause low Coulombic efficiency (CE). The prior interfacial chemical designs in terms of alloying kinetics have been used to enhance the CE of Li metal anode; however, the role of its redox chemistry at heterointerfaces remains a mystery. Herein, the relationship between heterointerfacial redox chemistry and electrochemical transformation reversibility is investigated. It is demonstrated that the lower redox potential at heterointerface contributes to higher CE, and this enhancement in CE is primarily due to the regulation of redox chemistry to Li deposition behavior rather than the formation of SEI films. Low oxidation potential facilitates the formation of the surface with the highly electrochemical binding feature after Li stripping, and low reduction potential can maintain binding ability well during subsequent Li plating, both of which homogenize Li deposition and thus optimize CE. In particular, Mg hetero-metal with ultra-low redox potential enables Li metal anode with significantly improved CE (99.6%) and stable cycle life for 700 cycles at 3.0 mA cm -2 . This work provides insight into the heterointerfacial design principle of next-generation negative electrodes for highly reversible metal batteries.

25 ENERGY STORAGE↗

Exploring Electrode-Level State-of-Charge and State-of-Health Dynamics in Lithium-Ion Battery Cells: Modeling and Experimental Identification

A computationally efficient model serves as a critical prerequisite for battery performance analysis and advanced battery management algorithm design. Although battery models that capture cell-level behavior have been widely explored in existing literature, electrode-level battery models have received much lesser attention till to date. However, such electrode-level models can significantly increase battery performance and life by enabling electrode-level health-conscious control. Such electrode-level control can effectively expand usable energy and power limits of the battery cells by utilizing the knowledge of individual electrodes' charge and health. In this context, this paper presents a comprehensive battery model developed with a reference electrode insertion that captures (i) electrode-level charge/discharge dynamics, (ii) stoichiometric and temporal dependencies of electrode-level resistances, (iii) solid electrolyte interface (SEI) layer growth as key degradation phenomenon, and (iv) capacity fade and resistance rise in each electrode due to nominal battery aging. The proposed model is identified, and a preliminary validation is performed utilizing terminal voltage and negative electrode potential data collected from a pouch cell under one continuous cycling and accelerated aging conditions where the cell experienced 14% capacity loss.

aging↗

Lithium-Ion Battery Life Model with Electrode Cracking and Early-Life Break-in Processes

This paper develops a physically justified reduced-order capacity fade model from accelerated calendar- and cycle-aging data for 32 lithium-ion (Li-ion) graphite/nickel-manganese-cobalt (NMC) cells. The large data set reveals temperature-, charge C-rate-, depth-of-discharge-, and state of charge (SOC)-dependent degradation patterns that would be unobserved in a smaller test matrix. Model structure is informed by incremental capacity analysis that shows loss of lithium inventory and cathode-material loss as the dominant capacity fade mechanisms. The model includes terms attributable to solid-electrolyte interface (SEI) growth, electrode cracking, cycling-driven acceleration of SEI growth, and "break-in" mechanisms that slightly decrease or increase available Li inventory early in life. The study explores what mathematical couplings of these mechanisms best describe calendar aging, cycle aging, and mixed calendar/cycle aging. Various approaches are discussed for extracting relevant stress factors from complex cycling profiles to predict lifetime during real-world battery loads using models trained on constant-current laboratory test results. The complexity of the present human-driven model identification process motivates future work in machine learning to more widely search and statistically discern the optimal model that correctly extrapolates capacity fade based on physical knowledge.

25 ENERGY STORAGE↗

Investigation of the Electrode-Electrolyte Interphase in Ester-Based Electrolytes in NCM523/Graphite Cells

The use of methyl acetate (MA) and methyl propionate (MP) as co-solvents in carbonate/LiPF 6 electrolytes have been investigated in LiNi 0.5 Co 0.2 Mn 0.3 O 2 (NCM523)/graphite cells to improve electrochemical performance at low temperature (−20 °C). Consistent with previous investigations, improved low temperature performance was observed with all electrolyte formulations containing esters. Detailed ex situ surface analysis of the surface films generated with the ester-based electrolytes containing electrolyte additives reveal significant changes to the SEI on graphite upon cycling at moderately elevated temperature (45 °C). In the presence of vinylene carbonate (VC) lithium plating is observed upon cycling at low temperature (−20 °C) which leads to a thicker solid electrolyte interface (SEI) upon cycling at 45 °C. Incorporation of fluoroethylene carbonate (FEC) as an electrolyte additive results in the generation of a thin SEI and alters the structure of the surface film on the NCM523 cathode resulting in stable cycling over a wide temperature range.

Rodrigo, Nuwanthi D. (ORCID:0000000343129536)↗

Electrolyte Study for High-Nickel LiNi 0.9 Mn 0.05 Co 0.05 O 2 Cathodes

With an increasing demand for intermittent renewable energy and electric vehicles, it is imperative to develop lithium-ion batteries with Earth-abundant cathode materials. Cobalt (Co) is preferred to be kept at a minimum because of its high cost and limited mining options, yet it has played an essential role in the high-performance transition metal oxides (TMOs). Herein, we report work from Argonne National Laboratory, conducted under the U.S. DoE's Vehicle Technologies Office, Deep Dive consortium on Next-Generation Cathodes, to optimize electrolytes for LiNi 0.9 Mn 0.05 Co 0.05 O 2 . LiNi 0.9 Mn 0.05 Co 0.05 O 2 is a high-Ni TMO benchmark as it outperforms most other TMOs under standard cycling conditions. In this study, we use the figure-of-merit approach to optimize electrolytes for this novel cathode material. Dual-salt carbonate electrolytes containing lithium difluorooxyphosphate and hexafluorophosphates were found to be the best for capacity retention and slowing the impedance rise. Importantly, transition metal dissolution and lithium inventory losses in the solid electrolyte interface were found to be the major causes for capacity fade.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Vinylene Carbonate and Fluoroethylene Carbonate on SEI Formation on Graphitic Anodes in Li-Ion Batteries

Binder free (BF) graphite electrodes were utilized to investigate the effect of electrolyte additives fluoroethylene carbonate (FEC) and vinylene carbonate (VC) on the structure of the solid electrolyte interface (SEI). The structure of the SEI has been investigated via ex-situ surface analysis including X-ray Photoelectron spectroscopy (XPS), Hard XPS (HAXPES), Infrared spectroscopy (IR) and transmission electron microscopy (TEM). The components of the SEI have been further investigated via nuclear magnetic resonance (NMR) spectroscopy of D2O extractions. The SEI generated on the BF-graphite anode with a standard electrolyte (1.2 M LiPF6 in ethylene carbonate (EC) / ethyl methyl carbonate (EMC), 3/7 (v/v)) is composed primarily of lithium alkyl carbonates (LAC) and LiF. Incorporation of VC (3% wt) results in the generation of a thinner SEI composed of Li2CO3, poly(VC), LAC, and LiF. Incorporation of VC inhibits the generation of LAC and LiF. Incorporation of FEC (3% wt) also results in the generation of a thinner SEI composed of Li2CO3, poly(FEC), LAC, and LiF. The concentration of poly(FEC) is lower than the concentration of poly(VC) and the generation of LAC is inhibited in the presence of FEC. The SEI appears to be a homogeneous film for all electrolytes investigated.

25 ENERGY STORAGE↗

Characterizing Solid Electrolyte Interphase on Sn Anode in Lithium Ion Battery

Tin (Sn) nanoparticle electrodes have been prepared and battery cycling performance has been investigated with 1.2 M LiPF6 in ethylene carbonate (EC) / diethyl carbonate (DEC) electrolyte (1:1, w/w) with and without added vinylene carbonate (VC) or fluoroethylene carbonate (FEC). Incorporation of either VC or FEC improves the capacity retention of Sn nanoparticle electrodes although incorporation of VC also results in a significant increase in cell impedance. The best electrochemical performance was observed with electrolyte containing 10% of added FEC. In order to develop a better understanding of the role of the electrolyte in capacity retention and solid electrolyte interface (SEI) structure, ex-situ surface analysis has been performed on cycled electrodes with infrared (IR) spectroscopy, X-ray photoelectron spectroscopy (XPS), and Hard XPS (HAXPES). The ex-situ analysis reveals a correlation between electrochemical performance, electrolyte composition, and SEI structure.

25 ENERGY STORAGE↗

Ion Diffusivity through the Solid Electrolyte Interphase in Lithium-Ion Batteries

Understanding the transport properties of the solid electrolyte interface (SEI) is a critical piece in the development of lithium ion batteries (LIB) with better performance. We studied the lithium ion diffusivity in the main components of the SEI found in LIB with silicon anodes and performed classical molecular dynamics (MD) simulations on lithium fluoride (LiF), lithium oxide (Li 2 O) and lithium carbonate (Li 2 CO 3 ) in order to provide insights and to calculate the diffusion coefficients of Li-ions at temperatures in the range of 250 K to 400 K, which is within the LIB operating temperature range. We find a slight increase in the diffusivity as the temperature increases and since diffusion is noticeable at high temperatures, Li-ion diffusion in the range of 130 to 1800 K was also studied and the diffusion mechanisms involved in each SEI compound were analyzed. We observed that the predominant mechanisms of Li-ion diffusion included vacancy assisted and knock-off diffusion in LiF, direct exchange in Li 2 O, and vacancy and knock-off in Li 2 CO 3 . Moreover, we also evaluated the effect of applied electric fields in the diffusion of Li-ions at room temperature.

25 ENERGY STORAGE↗

Review—Multifunctional Materials for Enhanced Li-Ion Batteries Durability: A Brief Review of Practical Options

Transition metal (TM) ions dissolution from positive electrodes, migration to and deposition on negative electrodes, followed by Mn-catalyzed reactions of solvents and anions, with loss of Li+ ions, is a major degradation (DMDCR) mechanism in Li-ion batteries (LIBs) with spinel positive electrode materials. While the details of the DMDCR mechanism are still under debate, it is clear that HF and other acid species’ attack is the main cause in solutions with LiPF6 electrolyte. We first review the work on various mitigation measures for the DMDCR mechanism, now spanning more than two decades. We then discuss recent progress on our understanding of Mn species in electrolyte solutions and the extension of a mitigation measure first proposed by Tarascon and coworkers in 1999, namely chelation of TM cations, to Mn cation trapping, HF scavenging, and alkali metal ions dispensing multi-functional materials. We focus on practicable, drop-in technical solutions, based on placing such materials in the inter-electrode space, with significant benefits for LIBs performance: increased capacity retention during operation at room and above-ambient temperatures as well as robust (both maximally ionically conducting and electronically insulating) solid-electrolyte interfaces, having reduced charge transfer and film resistances at both negative and positive electrodes. We illustrate the multifunctional materials approach with both new and previously published data. We also discuss and offer our evaluation regarding the merits and drawbacks of the various mitigation measures, with an eye for practically relevant technical solutions capable to meet both the performance requirements and cost constraints for commercial LIBs, and end with recommendations for future work.

25 ENERGY STORAGE↗

Capacity Fading Mechanisms of Silicon Nanoparticle Negative Electrodes for Lithium Ion Batteries

A thorough analysis of the evolution of the voltage profiles of silicon nanoparticle electrodes upon cycling has been conducted. The largest changes to the voltage profiles occur at the earlier stages (> 0.16 V vs Li/Li + ) of lithiation of the silicon nanoparticles. The changes in the voltage profiles suggest that the predominant failure mechanism of the silicon electrode is related to incomplete delithiation of the silicon electrode during cycling. The incomplete delithiation is attributed to resistance increases during delithiation, which are predominantly contact and solid electrolyte interface (SEI) resistance. The capacity retention can be significantly improved by lowering delithiation cutoff voltage or by introducing electrolyte additives, which generate a superior SEI. The improved capacity retention is attributed to the reduction of the contact and SEI resistance.

25 ENERGY STORAGE↗

Effects of Carbonate Solvents and Lithium Salts on Morphology and Coulombic Efficiency of Lithium Electrode

The application of lithium (Li) metal anode in rechargeable batteries is hindered by Li dendrite growth during Li deposition and low Li Coulombic efficiency (CE), where the nonaqueous electrolyte plays a critical role. In this work, the effects of different carbonate solvents and Li salts on Li deposition morphology and CE were systematically investigated. Typically cyclic carbonates are found to favor the formation of uniform Li film and improve Li CE than linear carbonates do. Several specific cyclic carbonates that are conventionally used as solid electrolyte interface formation additives in Li ion batteries can also improve the CE of Li anode. Furthermore, among the nine electrolyte salts studied, LiAsF6 and LiBOB lead to the highest CE for Li anode. LiBOB also leads to much smoother Li morphology than other salts do. Considering the better safety of LiBOB as compared to LiAsF6, LiBOB is a promising Li salt for rechargeable Li metal batteries with high CE. By combining the best electrolyte solvent/salt that can lead to high Li CE and novel electrolyte additives that can prevent dendrite formation, it is possible to find an electrolyte that not only prevents Li dendrite formation but also lead to high CE during Li deposition/stripping processes.

Environmental Molecular Sciences Laboratory↗

Electrochemical Properties and Challenges of Type II Silicon Clathrate Anode in Sodium Ion Batteries

The development of advanced anodes for low-cost room temperature sodium-ion batteries (SIBs) with high cycling stability is of great significance. Silicon clathrates are promising intercalation anodes due to their cage-like frameworks. It is predicted that the open cages can easily accommodate alkali ions with negligible volume changes. However, the complicated surface structure and chemical reactions make it challenging to understand the electrochemical performance of clathrate anodes in SIBs. In this paper, we evaluated the performance of type II clathrate anodes in SIBs. A slightly elevated testing temperature (45 degrees C) is shown to improve the cell capacity and rate performance due to the improved ionic conductivity. However, side reactions on the solid electrolyte interface (SEI) and loss of active material during the first sodiation process contribute to the low Coulombic efficiency during the first cycle. Analysis is supported by electrode morphology, elemental mapping, and X-ray photoelectron spectroscopy (XPS) on the clathrate electrodes at different electrochemical states. Na+ ion transport behavior between clathrate cages and surface in terms of migration barriers was also computed to explain the positive effect of higher cell testing temperature, and the low Coulombic efficiency of the first cycle.

25 ENERGY STORAGE↗

Cobalt-Free Cathodes for Next Generation Li-Ion Batteries

In this U.S. Department of Energy sponsored project Nexceris, in collaboration with project partners; The Ohio State University and Navitas Advanced Systems have advanced the technical maturity of a non-cobalt containing cathode for next-generation Li-ion batteries. The cathode is based on the lithium manganese nickel-titanium oxide, LiNi 0.5 Mn 1.5 TiO 4 (LNMTO) high voltage spinel. To address limitations with poor cycle and calendar life an microstucturally hierarchical LNMO/LNMTO core-shell cathode powder has been developed that enables the formation of a solid-electrolyte interface that effectively passivates the cathode surface. The microstructural enhancements of the cathode material focus on preferentially enriching the surface with titanium. In parallel, new, optimized binder and electrolyte chemistries have been incorporated to address degradation mechanisms associated with high-voltage systems. Single-layer pouch cell and large-format 2-Ah cell testing have shown that an optimized LNMO/LNMTO core-shell powder significantly improves initial cell capacity and cycle life compared to homogeneous LNMO powder. To support development and the fabrication of 2-Ah cells a novel Hybrid Alternative Wet-Chemical Synthesis (HAWCS) process have been developed. This low-cost, synthesis approach enables the excellent compositional and particle morphology control achieved with co-precipitation without the strict process controls and associated expensive process equipment.

25 ENERGY STORAGE↗