Synergistic Computational and Microstructural Design of Next- Generation High-Temperature Austenitic Stainless Steels

The purpose of this project was to: 1) study deformation twinning, its evolution, thermal stability, and the contribution on mechanical response of the new advanced stainless steels, especially at elevated temperatures; 2) study alumina-scale formation on the surface, as an alternative for conventional chromium oxide, that shows better oxidation resistance, through alloy design; and 3) design new generation of high temperature stainless steels that form alumina scale and have thermally stable nano-twins. The work involved few baseline alloys for investigating the twin formation under tensile loading, thermal stability of these twins, and the role of deformation twins on the mechanical response of the alloys. These baseline alloys included Hadfield Steel (Fe-13Mn-1C), 316, 316L and 316N stainless steels. Another baseline alloy was studied for alumina-scale formation investigations. Hadfield steel showed twinning but undesired second phases formed at higher temperatures. 316N stainless steel did not show signs of deformation twinning. Conventional 316 stainless steel demonstrated extensive deformation twinning at room temperature. Investigations on this alloy, both in single crystalline and polycrystalline forms, showed that deformation twins evolve in a hierarchical manner, consisting of micron–sized bundles of nano-twins. The width of nano-twins stays almost constant as the extent of strain increases, but the width and number of the bundles increase with increasing strain. A systematic thermomechanical cycling study showed that the twins were stable at temperatures as high as 900°C, after the dislocations are annealed out. Using such cycles, volume fraction of the thermally stable deformation twins were increased up to 40% in 316 stainless steel. Using computational thermodynamics and kinetics calculations, we designed two generations of advanced austenitic stainless steels. In the first generation, Alloy 1, which had been proposed as an alumina-forming austenitic stainless steel, is fully austenitic, but possesses carbides that were not dissolvable and could not be controlled. This alloy also did not show deformation twinning. Alloy 2 was designed based on alloy 1, but was not fully austenitic and had significant traces of uncontrollable precipitates as well. Alloy 3, also designed based on alloy 1, was mainly austenitic with evolution of a second phase along the grain boundaries, but also had precipitates that were not controllable. Based on the knowledge gained from the first generation of the designed steels, two more steels, called PGAA1 and PGAA2, were proposed using genetic algorithms that, based on the modelling, were supposed to exhibit alumina-scale formation. PGAA1, however, did not demonstrate a fully austenitic structure. PGAA2 could achieve a mostly austenitic structure through thermo-mechanical processing, and was then used for oxidation tests. The oxidation tests of PGAA2, with and without nitrogen impurities, along with alloy 1, suggested that PGAA2 can form alumina-scale similar to alloy 1, but N impurity will prevent formation of such a scale, probably through formation of aluminum nitrides. For the above mentioned genetic algorithm framework of alloy design, separate models were developed for specific design criteria. For prediction of alumina formation in stainless steels, a model was constructed based off of two criteria – effective valence and third element effect. These criteria capture the thermodynamics and kinetics of alumina formation in steels. To test the efficacy and robustness of this model, they were tested against alloys in the literature which had been experimentally verified to exhibit alumina formation and the predictions were in excellent agreement with the experiments. Another meta-model for prediction of twinning in unknown steel compositions was developed by an informatics based machine learning/data mining approach. Stacking Fault Energy data was captured from the literature for a large number of steel compositions and then this data was used to build a classifier to predict deformation mechanisms. Here a training set-test set based analysis was performed to test performance. The above genetic algorithm based optimization framework for alloy design was exhibited to be a successful methodology for accelerated materials discovery in the context of alloy design.

36 MATERIALS SCIENCE↗

The fatigue evaluation method for a structural stainless steel using the magnetic sensor composed of three pancake coils

May metallic structural materials, such as stainless steels, are currently used in our surroundings. If external force is repeatedly added for many years, it is thought that fatigue damage accumulates in stainless steels. When excessive fatigue damage accumulates in these metals, there is a possibility that they are destroyed by fatigue damage accumulation. Therefore, it is important to know the amount of the fatigue damage they have suffered in order to prevent them from being destroyed. We are developing the fatigue evaluation method for stainless steels with a magnetic sensor composed of three pancake type coils. In this research, the inspection object is ferritic stainless steels such as SUS430. The method of fatigue evaluation for ferritic stainless steels uses the three coil type sensor, and shows a good correlation between the number of stress cycles and the output signal of the sensor, even though the correlation between the output signal and an added stress is not completely accurate. This paper describes the evaluation method of fatigue damage in ferritic stainless steel using a magnetic sensor composed of three pancake-type coils.

36 MATERIALS SCIENCE↗

Identification of the mechanism that confers superhydrophobicity on 316L stainless steel

This study develops a rapid method to confer superhydrophobicity on 316L stainless steel surfaces with an amphiphilic reagent such as dodecanoic acid. The highest contact angle (approaching 173°) was obtained after forming hierarchical structures with a non-aqueous electrolyte by an electrolytic process. Our goal was to induce superhydrophobicity directly on 316L stainless steel substrates and to establish which molecules cause the effect. The superhydrophobic behaviour is analysed by contact angle measurements, scanning electron microscopy (SEM), IR spectroscopy and atomic force microscopy (AFM). The growth mechanism is analysed using FE-SEM, TOF-SIMS and XPS in order to determine the molecules involved in the reaction and the growth. The TOF-SIMS analysis revealed that the Ni{sup 2+} ions react with lauric acid to create an ester on the stainless steel surface. - Highlights: • This study develops a rapid and facile approach to impart superhydrophobicity properties to 316L stainless steel surfaces with an amphiphilic reagent such as dodecanoic acid. Surface character changes from superhydrophilicity to superhydrophobicity. • This process changes the surface character from superhydrophilicity to superhydrophobicity. • The process based on electrolysis of a nickel salt in lauric acid provides superhydrophobic behaviour in 316L stainless steel. • The growth mechanism is proposed as a mode island (Volmert- Weber mode). • TOF-SIMS and XPS provided the identification of the molecules involved in the surface modification reaction on AISI 316L inducing superhydrophobicity.

36 MATERIALS SCIENCE↗

Stainless steel anodes for alkaline water electrolysis and methods of making

The corrosion resistance of stainless steel anodes for use in alkaline water electrolysis was increased by immersion of the stainless steel anode into a caustic solution prior to electrolysis. Also disclosed herein are electrolyzers employing the so-treated stainless steel anodes. The pre-treatment process provides a stainless steel anode that has a higher corrosion resistance than an untreated stainless steel anode of the same composition.

25 ENERGY STORAGE↗

The Effect of 17-4 PH Stainless Steel on the Lifetime of a Pennzane(Trademark) Lubricated Microwave Limb Sounder Antenna Actuator Assembly Ball Screw for the AURA Spacecraft

During ground based life testing of a Microwave Limb Sounder (MLS) Antenna Actuator Assembly (AAA) ball-screw assembly, lubricant darkening and loss were noted when approximately 10 percent of required lifetime was completed. The MLS-AAA ball screw and nut are made from 17-4 PH steel, the nut has 440C stainless steel balls, and the assembly is lubricated with a Pennzane formulation containing a three weight percent lead naphthenate additive. Life tests were done in dry nitrogen at 50 C. To investigate the MLS-AAA life test anomaly, Spiral Orbit Tribometer (SOT) accelerated tests were performed. SOT results indicated greatly reduced relative lifetimes of Pennzane formulations in contact with 17-4 PH steel compared to 440C stainless steel. Also, dry nitrogen tests yielded longer relative lifetimes than comparable ultrahigh vacuum tests. Generally, oxidized Pennzane formulations yielded shorter lifetimes than non-oxidized lubricant. This study emphasizes surface chemistry effects on the lubricated lifetime of moving mechanical assemblies.

Jones, William R., Jr.↗

Side-by-side evaluation of the outgassing rate and ultimate pressure achieved inside tubes made of low-carbon and stainless steel

The hydrogen outgassing rate of a vacuum chamber made of AISI 1020 low-carbon steel was found to be notably smaller than a similar chamber made of AISI 316L stainless steel following heat treatment at 150 °C. When the chambers were baked at 400 °C, the outgassing rate of the 1020 low-carbon steel chamber was approximately 2000 times smaller than that of the 316L stainless-steel chamber. After quantifying hydrogen outgassing rates, vacuum chambers made of 1020 low-carbon steel and 316L stainless steel were heated for a prescribed duration and then pumped with an ion pump and nonevaporable getter pump to reach “ultimate pressure.” The 1020 low-carbon steel chamber reached lower pressures than the 316L stainless-steel chamber. Monte Carlo simulation predictions using the measured hydrogen outgassing rates are in good agreement with the ultimate pressure measurements. Finally, our measurements indicate that low-carbon steel can provide pressures within the extreme high vacuum range (<7.5 × 10 -13 Torr) if care is taken to minimize the surface area contribution from stainless steel.

36 MATERIALS SCIENCE↗

Electroless Plated Nanodiamond Coating for Stainless Steel Passivation

Tritium gas sample bottles and manifold components require passivation surface treatments to minimize the interaction of the hydrogen isotopes with surface contamination on the stainless steel containment materials. This document summarizes the effort to evaluate electroless plated nanodiamond coatings as a passivation layer for stainless steel. In this work, we developed an electroless nanodiamond (ND)-copper (Cu) coating process to deposit ND on stainless steel parts with the diamond loadings of 0%, 25% and 50% v/v in a Cu matrix. The coated Conflat Flanged Vessel Assemblies (CFVAs) were evaluated on surface morphology, composition, ND distribution, residual hydrogen release, and surface reactivity with deuterium. For as-received Cu and ND-Cu coated CFVAs, hydrogen off-gassing is rapid, and the off-gas rates of H 2 was one to two orders of magnitude higher than that for both untreated and electropolished stainless steel CFVAs, and hydrogen and deuterium reacted to form HD as well. These results indicated that residual H 2 was entrapped in the Cu and ND-Cu coated CFVAs during the coating process, and moisture was adsorbed on the surface, and ND and/or Cu might facilitate catalytic isotope exchange reaction for HD formation. However, hydrocarbons (i.e., CH 3 ) did not form, and did not appear to be an issue for the Cu and ND-Cu coated CFVAs. After vacuum heating, residual H 2 and adsorbed H 2 O in the Cu and ND-Cu coated CFVAs were dramatically reduced. The H 2 off-gassing rate after the vacuum treatment of Cu and 50% ND-Cu coated CFVAs was on the level of 10 -14 l mbar/s cm 2 , while H 2 O off-gas rate was on the level of 10 -15 l mbar/s cm 2 , consistent with the untreated or electropolished stainless steel CFVA, but the HD formation remained. The Restek EP bottle was used as a reference for this work. The Restek Electro-Polished (EP) bottle and their SilTek coated bottles tested under a different research project exhibited very little hydrogen off-gassing and unmeasurable HD formation. ND and Cu were initially chosen to develop improved passivation technology, because Cu has a lower permeability of hydrogen, and diamond is more inert than other materials under a hydrogen atmosphere. However, our tests demonstrated that even after an 8-18 day vacuum extraction heat treatment, the electroless plated Cu and ND-Cu coated stainless steel CFVAs exhibited H 2 off-gassing rates that were just comparable to those for the untreated or electropolished stainless steel CFVA, and the HD formation was still observed. Thus, the Restek Electro-Polished (EP) bottle outperformed the electroless plated Cu and ND-Cu coated stainless steel CFVAs, and the electroless plated nanodiamond coating is not promising as a surface passivation technology. However, the ND-Cu coating may be beneficial to another application in which catalyzing the H 2 -D 2 exchange reaction is desired.

08 HYDROGEN↗

Investigation of annealing temperature on microstructure and texture of Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel

Highlights: • Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel was investigated. • Shear bands provided recrystallization nucleation sites. • Annealing temperature can affect microstructure and texture. • r-bar increased to a maximum value (1.69) and then decreased to 1.42. - Abstract: The evolution of microstructure and texture of Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel annealed at different temperatures was investigated using a combination of X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). EBSD investigations confirm that the in-grain shear bands provide more recrystallization nucleation sites to γ-fiber recrystallization grains with high Taylor factor orientations during cold rolling requiring further annealing for a more homogenous equiaxied grain structure. As the annealing temperatures increase, the grains in center layer are oriented towards {110}∥ND, and the recrystallization grains at 1050 °C are dominated by the uniform and equiaxial γ-fiber grains favourable for the improvement of r-values, while the occurrence of {100} <011> texture detrimental to r-values indicates that an exorbitant annealing temperature can reduce the intensity of γ-fiber textures affecting the formability, accordingly, the average plastic strain ratio of ferritic stainless steel increases sharply up to a maximum value (1.69) and then decreases to a certain value (1.42).

36 MATERIALS SCIENCE↗

Degradation of impact toughness in cast stainless steels during long-term thermal aging

Cast austenitic stainless steels (CASSs) have been extensively used for the large components of nuclear reactor primary coolant systems. Since the cast steels inevitably contain degradable metastable phases and replacement of the large coolant system components is impractical, the thermal embrittlement of CASS components has been a serious concern in the extended-term operation of nuclear power plants. This study aimed to systematically measure and analyze the effect of long-term thermal aging on the Charpy impact toughness to provide a comprehensive understanding of thermal degradation behavior and a practical aging model to predict the degree of thermal degradation in the cast stainless steels. Additionally, the materials tested in the research include eight CASS alloys (two CF3s, one CF3M, three CF8s, and two CF8Ms) and two reference wrought materials (304L and 316L), in which the nominal δ-ferrite content ranges from ~2% to 33%. These stainless steels have been thermally aged at two light water reactor (LWR) temperatures (290 and 330 °C) and at two accelerated-aging temperatures (360 and 400 °C) for up to 30,000 h; these include both under-aged and over-aged conditions relative to the extended service lifetime (80 years). Charpy impact testing was performed for aged and non-aged specimens, and the impact (absorbed) energy parameters were correlated with a new aging parameter (A). Both the reduction of impact fracture toughness and the shift of ductile-brittle transition temperature were strongly dependent on the δ-ferrite content and degree of thermal aging. A linear relationship was found between the increasing rate of the index transition temperature T 41J and aging parameter A; base on which an empirical model was proposed for prediction of the transition temperature as a simple function of the aging parameter (A) and δ-ferrite content (F). Finally, the critical aging parameter for embrittlement (AC) was evaluated and compared with the existing δ-ferrite content criteria.

36 MATERIALS SCIENCE↗

Surface integrity and fatigue behaviour of electric discharged machined and milled austenitic stainless steel

Machining of austenitic stainless steels can result in different surface integrities and different machining process parameters will have a great impact on the component fatigue life. Understanding how machining processes affect the cyclic behaviour and microstructure are of outmost importance in order to improve existing and new life estimation models. Milling and electrical discharge machining (EDM) have been used to manufacture rectangular four-point bend fatigue test samples; subjected to high cycle fatigue. Before fatigue testing, surface integrity characterisation of the two surface conditions was conducted using scanning electron microscopy, surface roughness, residual stress profiles, and hardness profiles. Differences in cyclic behaviour were observed between the two surface conditions by the fatigue testing. The milled samples exhibited a fatigue limit. EDM samples did not show the same behaviour due to ratcheting. Recrystallized nano sized grains were identified at the severely plastically deformed surface of the milled samples. Large amounts of bent mechanical twins were observed ~ 5 μm below the surface. Grain shearing and subsequent grain rotation from milling bent the mechanical twins. EDM samples showed much less plastic deformation at the surface. Surface tensile residual stresses of ~ 500 MPa and ~ 200 MPa for the milled and EDM samples respectively were measured. - Highlights: •Milled samples exhibit fatigue behaviour, but not EDM samples. •Four-point bending is not suitable for materials exhibiting pronounced ratcheting. •LAGB density can be used to quantitatively measure plastic deformation. •Grain shearing and rotation result in bent mechanical twins. •Nano sized grains evolve due to the heat of the operation.

36 MATERIALS SCIENCE↗

Brazing titanium to stainless steel

Titanium and stainless-steel members are usually joined mechanically for lack of any other effective method. New approach using different brazing alloy and plating steel member with nickel resolves problem. Process must be carried out in inert atmosphere.

Batista, R. I.↗

Stress corrosion cracking evaluation of martensitic precipitation hardening stainless steels

The resistance of the martensitic precipitation hardening stainless steels PH13-8Mo, 15-5PH, and 17-4PH to stress corrosion cracking was investigated. Round tensile and c-ring type specimens taken from several heats of the three alloys were stressed up to 100 percent of their yield strengths and exposed to alternate immersion in salt water, to salt spray, and to a seacoast environment. The results indicate that 15-5PH is highly resistant to stress corrosion cracking in conditions H1000 and H1050 and is moderately resistant in condition H900. The stress corrosion cracking resistance of PH13-8Mo and 17-4PH stainless steels in conditions H1000 and H1050 was sensitive to mill heats and ranged from low to high among the several heats included in the tests. Based on a comparison with data from seacoast environmental tests, it is apparent that alternate immersion in 3.5 percent salt water is not a suitable medium for accelerated stress corrosion testing of these pH stainless steels.

Humphries, T. S.↗

Superhard Nanocrystalline Homometallic Stainless Steel on Steel for Seamless Coatings

The objective of this work is to deposit nanocrystalline stainless steel onto steel substrates (homometallic) for enhanced wear and corrosion resistance. Homometallic coatings provide superior adhesion, and it has been shown that ultrafine-grained materials exhibit the increased hardness and decreased permeability desired for protective coatings. Nanocrystals will be produced by controlling nucleation and growth and use of an ion beam during deposition by e-beam evaporation or sputtering. Phase I is depositing 31 6L nanocrystalline stainless steel onto 31 6L stainless steel substrates. These coatings exhibit hardnesses comparable to those normally obtained for ceramic coatings such ZrO2, and possess the superior adhesion of seamless, homometallic coatings. Hardening the surface with a similar material also enhances adhesion, by avoiding problems associated with thermal and lattice mismatch. So far we have deposited nanocrystalline homometallic 316L stainless steel coatings by varying the ions and the current density of the ion beams. For all deposition conditions we have produced smooth, uniform, superhard coatings. All coatings exhibit hardness of at least 200% harder than that of bulk materials. Our measurements indicate that there is a direct relationship between nanohardness and the current density of the ion beam. Stress measurements indicate that stress in the films is increasingly proportional to current density of the ion beam. TEM, XPS, and XRD results indicate that the coated layers consist of FCC structure nanocrystallites with a dimension of about 10 to 20 nm. The Ni and Mo concentration of these coating are lower than those of bulk 316L but the concentration of Cr is higher.

Tobin, Eric J.↗

Properties of Austenitic Stainless Steels for Nuclear Reactor Applications

Austenitic stainless steels are widely used in current commercial BWR and PWR systems as in-core and surrounding structural materials. These versatile steels have also been the main materials considered and applied for many advanced reactor technologies, including fast-breeder reactors and magnetic fusion reactors. For advanced reactors for higher-temperatures or high lifetime damage levels, modified versions of the standard commercial stainless steel grades have been developed to provide improved properties performance and radiation-resistance in specific reactor environments. An overview of the unirradiated properties and a summary of some important radiation-induced properties changes are presented. Highlights of several alloys developed for more radiation-resistance or better performance in specific reactor environments are highlighted.

Maziasz, Philip J↗

THE EFFECTS OF HYDROGEN, TRITIUM, AND HEAT TREATMENT ON THE DEFORMATION AND FRACTURE TOUGHNESS PROPERTIES OF STAINLESS STEEL

The deformation and fracture toughness properties of forged stainless steels pre-charged with tritium were compared to the deformation and fracture toughness properties of the same steels heat treated at 773 K or 873 K and precharged with hydrogen. Forged stainless steels pre-charged with tritium exhibit an aging effect: Fracture toughness values decrease with aging time after precharging because of the increase in concentration of helium from tritium decay. This study shows that forged stainless steels given a prior heat treatment and then pre-charged with hydrogen also exhibit an aging effect: Fracture toughness values decrease with increasing time at temperature. A microstructural analysis showed that the fracture toughness reduction in the heat-treated steels was due to patches of recrystallized grains that form within the forged matrix during the heat treatment. The combination of hydrogen and the patches of recrystallized grains resulted in more deformation twinning. Heavy deformation twinning on multiple slip planes was typical for the hydrogen-charged samples; whereas, in the non-charged samples, less twinning was observed and was generally limited to one slip plane. Similar effects occur in tritium pre-charged steels, but the deformation twinning is brought on by the hardening associated with decay helium bubbles in the microstructure.

36 MATERIALS SCIENCE↗

Effects of scan rate on the corrosion behavior SS 304 stainless steel in the nanofluid measured by Tafel polarization methods

The Effects of scan rate on the Tafel polarization curve that is obtained to determine corrosion rate are conducted. The tafel polarization curves are obtained at different scan rates for Stainless Steel 304 in nanofluids contain 0.01 gpl nano particle ZrO{sub 2}. The corrosion stainless steel in nanofluid contains adm+0.01 gpl ZrO{sub 2} nanoparticles at different scan rate was performed by Tafel polarization. The results show that according corrosion potential examination of the stainless steel in nanofluid media 0.01gpl ZrO{sub 2} nanoparticle was actively corroded. The value of cathodic Tafel slope stainless steel in nanofluid at different scan rate relatively unchanged after polarization testing. Mean while the value of anodic Tafel slope stainless steel in nanofluid increase at different scan rate. The results of Tafel polarization technique show that corrosion rate of stainless steel in nanofluid increase with increasing scan rate. X ray diffraction examination of stainless steel after Tafel polarization depict that γ Fe phase is major phase in the surface of alloy.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Crush Strengths of Stainless Steel Honeycomb for Packaging

Honeycomb structures are used as energy absorbers to dissipate kinetic energy. Their low density to high axial strength and inexpensive cost make them ideal for the energy absorption application. Mechanical properties of lightweight materials are well known compared to more dense materials like stainless steel. Determines the viability of using 304 Stainless Steel honeycomb in future SRNL radioactive material packages. Using a combination of the material properties and testing procedures both static and dynamic crush strength of stainless steel honeycomb will be determined. Both static and dynamic crush strengths of stainless steel honeycomb need to be quantified because strain rate plays a role in the material strength. The stainless steel honeycomb being tested will be cut into sections of about 2.0 inches in width, 2.3 inches in length and 2.5 inches in height. The cell size of the material is 0.25 in and the ribbon thickness 0.003 in. The material has a yield strength of 48 ksi and an ultimate strength of 103.2 ksi, with an elastic modulus of 29,300 ksi. Compression testing to determine the static crush strength will use an Instron compression test machine. This Instron machine uses a 20 ksi capacity load cell, while recording data at varying low strain rates. Dynamic impact testing will involve dropping a 43.8 lb impactor from a height around 5 feet onto the stainless steel honeycomb. The honeycomb structure will be on a rigid surface and the impactor will be dropped via a quick release hook. Dynamic crush strength is determined from the weight of the impactor, height of the drop and difference in height of the honeycomb after the drop.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗