Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SPINELS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Morphology‐controlled synthesis of multi‐metal‐based spinel oxide nanocatalysts and their performance for oxygen reduction

Abstract We present a one‐pot colloidal synthesis method for producing monodisperse multi‐metal (Co, Mn, and Fe) spinel nanocrystals (NCs), including nanocubes, nano‐octahedra, and concave nanocubes. This study explores the mechanism of morphology control, showcasing the pivotal roles of metal precursors and capping ligands in determining the exposed crystal planes on the NC surface. The cubic spinel NCs, terminated with exclusive {100}‐facets, demonstrate superior electrocatalytic activity for the oxygen reduction reaction (ORR) in alkaline media compared to their octahedral and concave cubic counterparts. Specifically, at 0.85 V, (CoMn)Fe 2 O 4 spinel oxide nanocubes achieve a high mass activity of 23.9 A/g and exhibit excellent stability, highlighting the promising ORR performance associated with {100}‐facets of multi‐metal spinel oxides over other low‐index and high‐index facets. Motivated by exploring the correlation between ORR performance and surface atom arrangement (active sites), surface element composition, as well as other factors, this study introduces a prospective approach for shape‐controlled synthesis of advanced spinel oxide NCs. It underscores the significance of catalyst shape control and suggests potential applications as nonprecious metal ORR electrocatalysts.

Li, Can↗

Experimental Study on the Formation of V-Rich Spinel Phase in CaO-SiO{sub 2}-MgO-FeO{sub t}-Al{sub 2}O{sub 3}-V{sub 2}O{sub 3}-P{sub 2}O{sub 5} Slags at 1573 K (1300 °C)

To concentrate vanadium dissolved in steelmaking slag and to separate the obtained vanadium (V)-concentrating phase by a magnetic method, the mineral phases in a CaO-SiO{sub 2}-MgO-FeO{sub t}-Al{sub 2}O{sub 3}-V{sub 2}O{sub 3}-P{sub 2}O{sub 5} system at 1573 K (1300 °C) were characterized by scanning-electron microscopy-energy-dispersive spectroscopy and X-ray diffractometry. When the samples were equilibrated in a pure iron crucible and argon atmosphere, four phases were identified, namely, orthosilicate, V-bearing spinel, wüstite, and a glass phase. The orthosilicate, V-bearing spinel, and glass phase occurred in all samples, whereas wüstite appeared only in samples with a higher basicity or high FeO{sub t} content. The results indicate that the V-bearing spinel phase, which is analogous to Fe{sub 3}O{sub 4}, is a thermodynamically stable phase that is suitable for the enrichment of vanadium dissolved in slags. Further analysis reveals that the increases in contents of FeO{sub t} and MgO in slag favor spinel-phase formation. When the slags are saturated by the wüstite phase, almost all dissolved vanadium can be concentrated in the spinel phase.

36 MATERIALS SCIENCE↗

99Tc immobilization from off-gas waste streams using nickel-doped iron spinel

Technetium-99 (99Tc) incorporation within stable spinel phases is a novel method for 99Tc removal and immobilization from waste streams. In this study, transformation of Ni-doped Fe(OH)2(s) to spinel minerals, e.g. trevorite (NiFe2O4), is explored as a method for removing 99Tc from Hanford Waste Treatment and Immobilization Plant (WTP) primary off-gas waste stream simulant. The Fe(OH)2(s) transformation process was found to reduce 99Tc(VII) to 99Tc(IV) and incorporate reduced Tc(VI) into the produced spinel simultaneously. Nickel doping was applied in the mineral transformation to inhibit potential reoxidation of 99Tc(IV). Solid phase characterization by XRD and XANES confirmed the formation of nickel substituted ferric-spinel, and suggest incorporation of 99Tc(IV) in the final spinel. Furthermore, in the primary off-gas stream, which contains both redox-sensitive contaminants Cr(VI) and 99Tc(VII), results from solution analysis and solid digestion indicate that nearly 100% Cr and over 80% 99Tc can be simultaneously removed by adding Fe(OH)2(s) to solution with a solid to solution ratio of 5 g/L under near neutral and alkaline conditions. The 99Tc removal approach developed herein provides an alternative treatment method to eliminate the proposed recycle process of the off-gas waste stream, which ultimately can reduce WTP mission cost and operation time.

Wang, Guohui↗

First-Principles Study of Spinel MgTiS 2 as a Cathode Material

Spinel intercalation hosts are well known to to facilitate high rate capability and high voltage Li-ion batteries. A recent experimental study has shown that Mg can reversibly intercalate in spinel TiS 2 , demonstrating the viability of Li intercalation host crystal structures for Mg-ion batteries. We report on a first-principles statistical mechanics study of Mg insertion into spinel TiS 2 , accounting for occupancy on both octahedrally and tetrahedrally coordinated interstitial sites. In contrast to Li-containing spinels, we predict mixed octahedral and tetrahedral site occupancy at nondilute Mg concentrations consistent with the recent experimental study of Sun et al. The onset of mixed occupancy is correlated with an increase in the spinel volume upon Mg insertion, which is more pronounced in MgxTiS 2 than in its Li counterpart. Lastly, the results in this study suggest that the degree of mixed occupancy could be controlled through the volume of the host with addition of electrochemically inactive species.

25 ENERGY STORAGE↗

Covalency competition dominates the water oxidation structure–activity relationship on spinel oxides

Spinel oxides have attracted growing interest over the years for catalysing the oxygen evolution reaction (OER) due to their efficiency and cost-effectiveness, but fundamental understanding of their structure–property relationships remains elusive. Here we demonstrate that the OER activity on spinel oxides is intrinsically dominated by the covalency competition between tetrahedral and octahedral sites. The competition fabricates an asymmetric M$_T-O-M_O$ backbone where the bond with weaker metal–oxygen covalency determines the exposure of cation sites and therefore the activity. Driven by this finding, a dataset with more than 300 spinel oxides is computed and used to train a machine-learning model for screening the covalency competition in spinel oxides, with a mean absolute error of 0.05 eV. [Mn]$_T$[Al$_{0.5}$Mn$_{1.5}$]OO$_4$ is predicted to be a highly active OER catalyst and subsequent experimental results confirm its superior activity. This work sets mechanistic principles of spinel oxides for water oxidation, which may be extendable to other applications.

36 MATERIALS SCIENCE↗

Crystal engineering in 3D: Converting nanoscale lamellar manganese oxide to cubic spinel while affixed to a carbon architecture

Here, by applying differential pair distribution function (DPDF) analyses to the energy–storage relevant MnOx/carbon system— but in a 3D architectural rather than powder–composite configuration—we can remove contributions of the carbon nanofoam paper scaffold and quantify the multiphasic oxide speciation as the nanoscale, disordered MnOx grafted to the carbon walls (MnOx@CNF) structurally rearranges in situ from birnessite AMnOx (A = Na + ; Li + ) to tetragonal Mn 3 O 4 to spinel LiMn 2 O 4 . The first reaction step involves topotactic exchange of interlayer Na + by Li + in solution followed by thermal treatments to crystal engineer the –10–nm–thick 2D layered oxide throughout the macroscale nanofoam paper into a spinel phase. The oxide remains affixed to the walls of the nanofoam throughout the phase transformations. The DPDF fits are improved by retention of one plane of birnessite–like oxide after conversion to spinel. We support the DPDF–derived assignments by X–ray photoelectron spectroscopy and Raman spectroscopy, the latter of which tracks how crystal engineering the oxide affects the disorder of the carbon substrate. We further benchmark MnOx@CNF with nonaqueous electrochemical measurements versus lithium as the oxide converts from X–ray–amorphous birnessite to interlayer-registered LiMnOx to spinel. The lamellar AMnOx displays pseudocapacitive electrochemical behavior, with a doubling of specific capacitance for the interlayer–registered LiMnOx, while the spinel LiMn 2 O 4 @CNF displays a faradaic electrochemical response characteristic of Li–ion insertion. Our results highlight the need for holistic understanding when crystal engineering an (atomistic) charge–storing phase within the (architectural) structure of practical electrodes.

36 MATERIALS SCIENCE↗

Short Range Order in Disordered Spinel and the Impact on Cation Vacancy Transport

Spinels are important complex oxides for use in radiation damage environments and resulting from the corrosion of steels. It is known that, in these environments, normal spinels exist with some concentration of antisite cation pairs known as inversion. In this work we show that even in highly disordered states characterized by high levels of inversion, spinel still shows some short range order (SRO) that manifests itself in antisite chains. The propensity to form these antisite chains is confirmed through Monte Carlo simulations which find that the length of chains which can form depend on the spinel chemistry. We also consider the effect of antisite chains on the diffusivity of cation vacancies and find the effect strongly depends on the spinel chemistry. At the extremes, chains in FeCr2O4 significantly increase vacancy transport but in MgAl2O4 chains have the inverse effect of drastically reducing vacancy mobility. The explanation of these dramatically different effects results from the assessment of the thermodynamic stability of the antisite chains and contrasting attractive/repulsive interactions of vacancies with the chains.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Origin of spinel-rich chondrules and inclusions in carbonaceous and ordinary chondrites

The evaluation of three models of the origin of spinel-rich chondrules and inclusions presented here includes new calculations of the major-element refractory mineral condensation sequence from a gas of solar composition over a wide pressure interval. Condensation calculations show that spinel-rich chondrules did not crystallize from metastable liquid condensates, and that spinel-rich inclusions are not aggregates of refractory nebular condensates. It is proposed that spinel-rich objects are fractionated distillation residues of small aggregates of primitive dust that lost Ca, Si-rich partial melts by evaporation, ablation, or splashing during collisions. This model also explains why spinel-rich chondrules and inclusions (1) are usually smaller than melilite-rich chondrules and inclusions; (2) often have highly fractionated trace-element compositions; and (3) usually do not contain Pt-metal nuggets even when they are more enriched in the Pt-group metals than nugget-bearing melilite-rich objects.

Kornacki, A. S.↗

Distribution of Fe3+ and H in Minerals During Partial Melting and Metasomatism of Spinel Peridotite

Oxygen fugacity and water content are crucial parameters for many chemical and physical properties of the Earth's mantle, for example bearing on fluid type, melting initiation, and deformation. However, the exact behaviour of Fe3+ and H during melting and metasomatism is still under debate. Here, the Fe3+/ΣFe ratio (Mössbauer and EMP) and water content (FTIR) of peridotite minerals are examined in mantle xenoliths from Kilbourne Hole (KH), NM, and Dish Hill (DH), CA (USA). These spinel peridotites have compositions consistent with partial melting with variable degrees of metasomatism (undetectable to cryptic to modal). Pyroxenites also allow to examine melt-rock reactions. Bulk-rock Fe2O3 content of the KH peridotites correlates with indices of melting (positive with bulk-rock Al2O3 and Cpx Yb contents, and negative with spinel Cr#) confirming that Fe3+ behaves as an incompatible element during melting. Correlations of the Fe3+/ΣFe ratio of minerals with these indices, however, indicates that Fe3+ is incompatible in Cpx but compatible in Opx and spinel during melting. Water contents in olivine, Cpx and Opx from most KH peridotites can be explained by partial melting and correlate negatively with the Fe3+/ΣFe ratio of spinel and Opx but positively with that of Cpx. This indicates partial control of Fe3+ on the incorporation of H in pyroxene, but not related to a redox equilibrium in Cpx. The higher Fe3+/ΣFe ratio of spinel in the metasomatized KH and DH peridotites, and in the pyroxenites confirms that oxidation characterizes modal metasomatism. Metasomatism, however, is not necessarily accompanied by water addition.

Peslier, A. H.↗

MgAl2O4 spinel refractory as containment liner for high-temperature alkali salt containing environments

A method includes containing a high-temperature alkali salt containing environment using a refractory containment liner containing MgAl.sub.2O.sub.4 spinel. A method, includes forming a refractory brick containing MgAl.sub.2O.sub.4 spinel having an exterior chill zone defined by substantially columnar crystallization and an interior zone defined by substantially equiaxed crystallization; and removing at least a portion of the exterior chill zone from the refractory brick containing MgAl.sub.2O.sub.4 spinel by scalping the refractory brick containing MgAl.sub.2O.sub.4 spinel to define at least one outer surface having an area of substantially equiaxed crystallization. A product of manufacture includes a refractory brick containing MgAl.sub.2O.sub.4 spinel including an interior zone defined by substantially equiaxed crystallization; and at least one outer surface having an area of substantially equiaxed crystallization.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The effects of glass doping, temperature and time on the morphology, composition, and iron redox of spinel crystals

Precipitation of large crystals/agglomerates of spinel and their accumulation in the pour spout riser of a Joule-heated ceramic melter during idling can plug the melter and prevent pouring of molten glass into canisters. Thus, there is a need to understand the effects of spinel-forming components, temperature, and time on the growth of crystals in connection with an accumulation rate. In our study, crystals of spinel [Fe, Ni, Mn, Zn, Sn][Fe, Cr]₂O₄ were precipitated from simulated high-level waste borosilicate glasses containing different concentrations of Ni, Fe, and Cr by heat treating at 850 and 900°C for different times. These crystals were extracted from the glasses and analyzed with scanning electron microscopy and image analysis for size and shape, with inductively coupled plasma-atomic emission spectroscopy and atom probe tomography for concentration of spinel-forming components, and with wet colorimetry and Mössbauer spectroscopy for Fe²⁺/Fe total ratio. High concentrations of Ni, Fe, and Cr in glasses resulted in the precipitation of crystals larger than 100 µm in just two days. Crystals were a solid solution of NiFe₂O₄, NiCr₂O₄, and -Fe₂O₃ (identified only in the high-Ni-Fe glass) and also contained small concentrations of less than 1 at% of Li, Mg, Mn, and Al.

chemical analysis↗

Rationalization of Diversity in Spinel MgFe 2 O 4 Surfaces

Spinel magnesium ferrite (MgFe 2 O 4 ) is a prospective anode material for lithium ion batteries (LIBs). In this study, using density functional theory the first systematic study of diverse MgFe 2 O 4 surfaces is reported in three types of spinel structures: normal, mixed, inverse, which can have significant impact on the initial lithiation. The results show that the faceting and therefore the shape of MgFe 2 O 4 crystals strongly depend on the bulk structures. Upon going from normal, mixed to inverse spinel, the energetically preferred facets of MgFe 2 O 4 vary from the combination of (1 0 0) and (3 1 1), soly {1 0 0} to a combination of (1 0 0), (0 0 1), (1 1 1), and (3 1 1), respectively, depending on the distribution of Mg 2+ in the spinel structure. However, there is one common descriptor to the stable surfaces among all three MgFe 2 O 4 systems: high density of Mg 2+ exposed to the surface. Finally, this study rationalizes the essential effect of the substitution of Zn 2+ for Mg 2+ in ferrites and provides new insights on how to control the shape of ferrite materials and thus tune the performances of LIBs.

36 MATERIALS SCIENCE↗

Upgrading the Performance and Stability of Lithium, Manganese-Rich Layered Oxide Cathodes with Combined-Formic Acid and Spinel Coating Treatment

We report improving sluggish rate performance and cycling stability of Li, Mn-rich cathode materials (LMR) is of great importance for practical implementation. Here, dual surface modification on LMR particles with formic acid washing and spinel coating improves the electrochemical performance. Dilute formic acid can remove the Li2CO3 surface impurities and selectively reduce Ni while significantly increasing specific surface area by ~32 %, unlocking more electrochemically active surfaces. Spinel coating enhances cycle stability by suppressing detrimental side reactions at electrode-electrolyte interfaces at high voltage. Post-annealing temperature was found to significantly affect the cathode performance. Higher temperature favors diffusion of transition metal (TM)/Li ions of the spinel coating from surface to the bulk, removing the coating by possible reconstruction into the layered structure and thus degrading the performance. The spinel coating also appears to increase Co 3+ segregation on the particle surface. Compared to the original material, the optimized sample demonstrates 47 % higher capacity retention at 3C and retains 89 % of initial capacity after 150 cycles at 0.5C. Besides, the specific energy density of 523 Wh kg -1 can be attained after 150 cycles at 0.5C. Moreover, the post-cycling analysis of modified sample verifies a better structural integrity with less particle cracking. Altogether, this study portrays an alternative strategy to overcome the shortcomings of LMR cathode materials.

25 ENERGY STORAGE↗

Lewis Acid Site Engineering in Chromite Spinels Orchestrated Surface Reconstruction and Surpasses RuO 2 in Oxygen Evolution

Atomic-scale engineering of chromite spinels featuring redox-active tetrahedral A-sites and strong Cr–O covalency offers a promising route to superior platinum-group-metal-free oxygen evolution reaction (OER) catalysts. However, comprehensive studies addressing how cation substitution influences surface chemistry and governs OER activity and durability in chromite spinels remain limited. Here, in this work, a systematic investigation of the multicationic chromite series Ni x Fe y Cr 3−x−y O 4 is presented, identifying composition-dependent Lewis acidity as a descriptor of superior OER performance. It is further demonstrated that tuning surface acidity directly controls dynamic reconstruction processes and lattice-oxygen participation during spinel-based electrocatalysis. Following activation, the optimized Ni 0.8 Fe 0.3 Cr 1.9 O 4 catalyst delivers a current density of 10 mA cm −2 at an overpotential of 235 mV, surpassing RuO 2 , with excellent long-term stability. Integrating microscopic and spectroscopic analysis with operando impedance spectroscopy, it shows that activation generates an oxyhydroxide overlayer and reveals a previously unrecognized link between surface Lewis acidity and the growth kinetics and activity of these shells. Density functional theory calculations indicate that Fe incorporation at octahedral sites raises the O 2p-band center and lowers oxygen-vacancy formation energy, promoting lattice-oxygen activation and triggering reconstruction, yielding enhanced OER. This work integrates cation-driven surface-acidity modulation, acidity-governed reconstruction, and OER activity enhancement into a unified predictive framework for designing earth-abundant spinel-based catalysts.

operando impedance spectroscopy↗

Facile Synthesis of Spinel Ferrites with Enhanced Magnetic Properties from Two Intractable Metallurgical Resources: Zinc-Bearing Dust and Nickel Laterite Ore

Nickel laterite ore and zinc-bearing dust are multi-metal-associated and intractable resources. Comprehensive and cooperative utilization of zinc-bearing dust and nickel laterite ore for the preparation of spinel ferrites with enhanced magnetic properties by a facile process was proposed. The structure and magnetic properties of as-prepared spinel ferrites were characterized by X-ray diffraction (XRD), Raman spectroscopy, and Physical Property Measurement System (PPMS). The effect of mass ratios of zinc-bearing dust to nickel laterite ore, calcination temperature, and Zn substitution content on the as-prepared samples was investigated in detail. A single phase of Zn-substituted spinel ferrites (x= 0.00, 0.10, 0.20, and 0.30) could be obtained when the mass ratios were controlled at 1:0.4, 1:4:1.8, 1:2:1.5, and 1:1:1.2 after being calcined at 900 {sup ∘}C for 30 min, respectively. The magnetic property tests present that the as-prepared spinel ferrite exhibits enhanced magnetic properties with the saturation magnetization (Ms) value of 66.8 emu g{sup − 1} and the coercivity (Hc) value of 26 Oe when the mass ratio was controlled at 1:1:1.2. This research could provide an effective way to transfer two intractable resources into soft magnetic materials.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Metal Substitution on the Magnetic Properties of Spinel Ferrites Synthesized from Zinc-Bearing Dust

This paper provides a facile way for comprehensive utilization of multi-metal-associated and intractable zinc-bearing dust to synthesize multi-metal-doped spinel ferrites. The effects of preparation conditions including mass ratios of zinc-bearing dust to MgO addition and calcination temperature on the purity of as-prepared samples were investigated in detail, as well as the effect of metal substitution on the magnetic properties of as-synthesized spinel ferrites. The results show that single-phase spinel ferrite could be obtained when the mixture with the mass ratio of zinc-bearing dust to MgO addition of 1:0.20 was calcined at 1000 {sup ∘}C for 2 h. The saturation magnetization M{sub s} values for Mg-substituted, Ni-substituted, and Mn-substituted ferrites are 43.2, 47.6, and 54.3 emu g{sup − 1}, respectively, which can be explained by Neel’s two sub-lattice collinear models and the cation distribution between the tetrahedron (A) sites and octahedral (B) sites of the as-prepared samples. Notably, the heavy metals leaching from the as-prepared samples are very limited compared with zinc-bearing dust. In this way, hazardous zinc-bearing dust could be comprehensively utilized to synthesize spinel ferrites with excellent magnetic properties.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A Kinetic Model for Modification of MgAl{sub 2}O{sub 4} Spinel Inclusions During Calcium Treatment in the Ladle Furnace

A common approach in the processing of Al-killed steels is the modification of alumina inclusions by calcium treatment. A model for this process has already been developed by the current authors and validated by means of plant data. Often, magnesium aluminate spinels are also present and transformed to magnesium calcium aluminate inclusions during calcium treatment. In the current study, a fundamental kinetic model is proposed for modification of spinel inclusions considering mass transfer of solute through the boundary layer to the inclusion and diffusion within the product layer. Sensitivity analysis has been carried out to determine rate-controlling step for spinel modification. The rate of transformation of spinel inclusions is compared with alumina inclusions reported in the current authors’ prior model.

36 MATERIALS SCIENCE↗

Kinetic model for quartz and spinel dissolution during melting of high-level-waste glass batch

The dissolution of quartz particles and the growth and dissolution of crystalline phases during the conversion of batch to glass potentially affects both the glass melting process and product quality. Crystals of spinel exiting the cold cap to molten glass below can be troublesome during the vitrification of iron-containing high-level wastes. To estimate the distribution of quartz and spinel fractions within the cold cap, we used kinetic models that relate fractions of these phases to temperature and heating rate. Fitting the model equations to data showed that the heating rate, apart from affecting quartz and spinel behavior directly, also affects them indirectly via concurrent processes, such as the formation and motion of bubbles. Because of these indirect effects, it was necessary to allow one kinetic parameter (the pre-exponential factor) to vary with the heating rate. The resulting kinetic equations are sufficiently simple for the detailed modeling of batch-to-glass conversion as it occurs in glass melters. The estimated fractions and sizes of quartz and spinel particles as they leave the cold cap, determined in this study, will provide the source terms needed for modeling the behavior of these solid particles within the flow of molten glass in the melter.

Batch melting, Cold cap, Quartz, Spinel, Waste gla↗