PV Module Performance After 30 Year Without Washing
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Encapsulant browning is one of the most common degradation modes found in crystalline silicon field-aged photovoltaic modules. Browning, usually undetected unless severe, reduces the short-circuit current (Isc) produced by a module. Therefore, field-aged browned modules have been subjected to accelerated UV testing to obtain true end-of-life activation energy for the encapsulant browning mechanism. A novel time- and resource-saving accelerated UV exposure testing method simultaneously allowing multiple module temperatures to be maintained in a single chamber run is presented. Six field-aged crystalline silicon modules of glass/backsheet construction (three each from BP Solar/Solarex MSX 60 and Siemens M55) with similar glass and encapsulant formulation were exposed to a UV dosage of 450 kWh/m2 . Through passive heating, the average module temperatures for the BP Solar/Solarex modules were 60 degrees C, 77 degrees C, and 85 degrees C and those of Siemens M55 were 75 degrees C, 80 degrees C, and 837 degrees C. To study UV browning, the modules were intermittently characterized through visual imaging, UV fluorescence imaging, electroluminescence imaging, quantum efficiency measurements, module, and cell-level light I-V measurements. An Isc decrease corroborated the increased extent of browning with increased module temperature. For the BP Solar/Solarex modules, the Low T, Mid T, and the High T modules showed a 1.37%, 2.48%, and 3.26% Isc drop, respectively. The Siemens modules showed a 4.11%, 5.65%, and 6.95% Isc drop. The multiple cell-level Isc data points obtained for each module temperature increased provided statistical significance. Activation energy for encapsulant browning was calculated as 0.44 and 0.72 eV for MSX 60 and M55 modules, respectively.
Initial results of application of the NREL Test-to-Failure Protocol are presented and discussed. Six commercially available multicrystalline Si-cell flat-plate modules were subjected to the protocol with controls. The samples were divided among three test sequences, (1) 1000 hours of 85C/85% relative humidity with positive or negative 600 V bias to the active layers with respect to the grounded frame, (2) -40/85C thermal cycling with electrical load at the rated module power, and (3) an alternating sequence between tests (1) and (2). Application of the protocol manifested in the acceleration of degradation mechanisms seen in the field including backsheet delamination, corrosion, bubble formation within the laminate, discoloration of the antireflective coating, and localized heating with degradation of the backsheet as a result of moisture ingress, corrosion, and concentrated current flow. Significant differences in performance after one round of the protocol are seen in damp heat depending on the polarity of the bias applied to the active layer (the short-circuited power leads of the module). The protocol is found to successfully accelerate module degradation mechanisms that have been observed in the field and will help to differentiate the performance and reliability of various module technologies.
In this manuscript, we present an overview of our module self-reference (MSR) calibration results of PV electrical performance collected for over three years on a silicon module. Analysis and comparison of the results based on measurement uncertainty analysis enable the quantification of the major sources of uncertainty and an estimate of the total uncertainty of the MSR measurements. The control charts show that the mean values are consistent with uncertainty calculations for P MAX , V OC and I SC .
The kinetics of light- and elevated temperature-induced degradation (LETID) in silicon solar cells depend on the precise operating excess carrier density (?n) of the device. This dependency causes differences in the way LETID manifests in modern, higher-efficiency devices compared to lower-efficiency, legacy devices that might have been deployed in the field in previous years. In this work we model how different vintages of devices are expected to behave in both accelerated laboratory testing, as well as field deployment. The differing excess carrier densities encountered in various module vintages has implications both for interpreting accelerated test data, as well as identifying, diagnosing, and potentially treating LETID in the field.
The purpose of the PV Service Life Prediction project is to examine and report on how solar modules are holding up after being in the field for 5 or more years. This poster presents the common problems crystalline-silicon and thin-film modules exhibit, including details of modules from three manufactures that were tested January 13-16, 2014.
An empirical method for estimating relative power losses caused by potential-induced degradation (PID) for p-type solar cells and modules using quantitative electroluminescence (EL) analysis (QELA) is presented. First, EL images are corrected for camera- and perspective distortion. The relative power loss map is then calculated from the logarithmic ratio of two EL images, taken either before and after PID degradation or at different applied currents. Only the cell average of the resulting power loss map is evaluated. The highest power loss across each string is averaged to obtain the overall power loss. Consequently, for modules with three strings, three cells are averaged. The resulting power loss depends on the current applied. The conversion to equivalent irradiance allows for comparison of measured and estimated device performance. The analysis of roughly 2000 EL images and related current-voltage (I-V) curves indicates a good agreement between flash-test-measured and performance estimated using QELA. A relative root mean square error of 1-3% can be achieved.
Various common crystalline silicon cell technologies were exposed to UVA radiation (1.24 Wm-2 nm-1 at 340 nm peak) on the front and back faces at 45 degrees Celsius for periods up to 3000 h, representing about 3 y of solar exposure in Phoenix, Arizona, USA. The resulting degradation of the open-circuit voltage and short-circuit current is presented. Of the various cell types examined, significant levels of degradation were seen in all cases. Less degradation was generally found after UV irradiation of cell fronts and older cell types, whereas a bifacial PERC type exposed on the rear showed about 25% degradation in short circuit current, attributable to lack of a diffused surface field. Selected cells were exposed to UV irradiation with the addition of long pass UV filters to replicate UV-absorbers in encapsulants. Modern cell designs are sensitive to UV-ID because of reduced or eliminated front and back surface field and increased dependence on high quality surface passivation. Single transformation of the independent variable (t, kW h/m^2) could be used to achieve a linear model of the data to extrapolate to 50 y. Solar Advisor Model (SAM) shows appropriate filtering of UV-irradiation can improve LCOE and net present value of plant. Some advanced cell types are seen to be UV-resistant (cell level solutions also exist). Solutions therefore exist on the cell, glass, and encapsulant level. Changes over time in each of these would also need to be considered (solarization, encapsulant browning...).
The presentation describes the composition of and motivation for the International PV QA Task Force, then describes the presentations and discussion that occurred at the workshop on Feb. 29th, 2012.
"This dataset includes spectral response curves for 12 commercial silicon module types that are deployed at SNL in Albuquerque. The modules chosen for evaluation were originally purchased by SNL for the PV Lifetime project (renamed to Systems Long-Term Evaluation [SLTE]). The majority of those modules are deployed outdoors for long-term evaluation, but several modules of each type were placed in storage for future comparison purposes. One stored module of each type was sent to NREL for the spectral response measurements. NREL used the recently developed Module Quantum Efficiency (QE) test bed. What makes this system unique is that it scans the entire module automatically, taking one or more measurements on each cell. Using the mean of these measurements at each wavelength leads to improvements in spectral mismatch correction and module power measurements but having the individual measurements also makes it possible to identify outlier cells, which could be useful for investigating underperforming modules. All measurements were performed nominally at 25°C"
Analysis discussing the cost models and supply chains of various PV technologies.
Over the past decade, there have been observations of module degradation and power loss because of the stress that system voltage bias exerts. This results in part from qualification tests and standards note adequately evaluating for the durability of modules to the long-term effects of high voltage bias that they experience in fielded arrays. This talk deals with factors for consideration,progress, and information still needed for a standardized test for degradation due to system voltage stress.
The economic viability of photovoltaic (PV) technologies is inextricably tied to both the electrical performance and degradation rate of the PV systems, which are the generators of electrical power in PV systems. Over the past 15 years, performance data have been collected on numerous PV systems installed throughout the state of Florida and will be presented.
This poster presents an overview of a study of the impact on PV system cost and performance imposed by electrical connectors used to connect PV system components.
The presentation describes the value of adding DC converters and other power electronics to modules to improve their output even when shading or bad cells would otherwise decrease the module output. The presentation was part of a workshop sponsored by ARPA-E exploring the opportunities for power electronics to support PV applications.
Explore the source record for details and available documents.