Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FIBER STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Development of Ceramic Fibers for Reinforcement in Composite Materials

Refinements of the vertical arc fiberizing apparatus resulted in its ability to fiberize very different refractory glasses having wide ranges of properties. Although the apparatus, was originally designed as a laboratory research tool for the evaluation of many compositions daily, up to one quarter pound of fibers of a single composition could be produced in an 8-hour day. Fibers up to six and a half feet long were produced with the apparatus. Studies were conducted of two methods of fiberizing refractory glasses requiring rapid freezing from the melt. The first method consisted of fiberizing droplets of molten glass passing through an annular nozzle. The second method consisted of reconstructing the annular nozzle in. the shape of a horseshoe to achieve a shorter delay in blasting a molten droplet from the tip of a rod. Both methods were judged feasible for producing fibers of glasses requiring rapid freezing. The first method would be more amenable to volume fiber production. Studies of induction heating for fiber formation did not lead to its designation as a very efficient heating method. Problems. remain to be solved, in the design of a suitable susceptor for a higher heating rate, in protecting the susceptor from oxidation with an inert gas, in contamination of the melt from a refractory crucible, and in the protective radiation shielding of the induction concentrator coil. It is not considered practical to continue studies of this heating method. In the course of this program 151 refractory glass compositions were evaluated for fiber, forming characteristics. Of the various types of materials studied, the following showed promise in producing acceptable refractory fibers: sIlica- spinel (magnesium aluminate), silica- spinel-zirconia, silica-zirconia, silica-zinc spinel, aluminum phosphate glasses, and fluoride glasses. Compositions which did not produce acceptable fibers were high zirconia materials, barium spinels, and calcium aluminates. Improvements in the. testing apparatus for single fiber tensile strength increased the precision. of tests conducted on nine fibers. The highest mean tensile strength, a value of 295,000 pounds per square inch, was obtained with R-141 fibers. Treatment of R-74 fibers with anhydrous Linde A-1100 silane finish improved its mean fiber tensile strength by 25 percent. The lapse of time after fiber formation had no measurable effect on tensile strength. A static heating test conducted with various high melting fibers indicated that Fiberfrax and R-108 underwent no significant changes in bulk volume or resiliency on exposure to 2750 degrees Fahrenheit (1510 degrees Centigrade) in an oxidizing atmosphere. For fiber-resin composition fabrication, ten fiber materials were selected on the bases of high fiber yield, fusion temperature, and type of composition. Fiberfrax, a commercial ceramic fiber, was included for comparison. A new, more effective method of removing pellets from blown fibers was developed. The de-pelletized fibers were treated with a silane finish and felted into ten-inch diameter felts prior to resin impregnation. Composites containing 30 percent by weight of CTL 91-LD phenolic resin were molded under high pressure from the impregnated felts and post-cured to achieve optimum properties. Flexural strength, flexural modules of elasticity, and punch shear strength tests were conducted on the composite specimens. The highest average flexural strength obtained was 19,958 pounds per square inch with the R-74-fiber-resin composite. This compares very favorably with the military specification of 13,000 pounds per square inch flexural strength for randomly oriented fiber reinforced composites. The highest punch shear strength (11,509 pounds per square inch) was obtained with the R-89 fiber-resin composite. The effects of anhydrous fiber finishes on composite strength were not clearly indicated. Plasma arc tests at a heat flux of 550 British Thermal Units per square foot per second on eight composite materials indicated ablation rates generally equivalent to Fiberglas-Micarta No. 259-2. The composite reinforced with R-99 fibers had an average ablation rate of 0.008 inch per second and appears quite promising on the basis of these tests. Preliminary studies for processing fibers into yarn and fabric were conducted with R-99 fibers. The use of certain organic gums aided in 2 fabricating by hand several relatively strong yarns and a crude fabric swatch. This indicated the practicality of developing techniques for processing these fibers into yarn and fabric without significant damage to the fibers.

Gates, L. E.↗

Microstructural and strength stability of CVD SiC fibers in argon environment

The room temperature tensile strength and microstructure of three types of commercially available chemically vapor deposited silicon carbide fibers were measured after 1, 10, and 100 hour heat treatments under argon pressures of 0.1 to 310 MPa at temperatures to 2100 C. Two types of fiber had carbon-rich surface coatings and the other contained no coating. All three fiber types showed strength degradation beyond 1400 C. Time and temperature of exposure had greater influence on strength degradation than argon pressure. Recrystallization and growth of near stoichiometric SiC grains appears to be the dominant mechanism for the strength degradation.

Bhatt, Ramakrishna T.↗

Microstructural and strength stability of CVD SiC fibers in argon environments

The room temperature tensile strength and microstructure of three types of commercially available chemically vapor deposited silicon carbide fibers were measured after 1, 10, and 100 hour heat treatments under argon pressures of 0.1 to 310 MPa at temperatures to 2100 C. Two types of fiber had carbon-rich surface coatings and the other contained no coating. All three fiber types showed strength degradation beyond 1400 C. Time and temperature of exposure had greater influence on strength degradation than argon pressure. Recrystallization and growth of near stoichiometric SiC grains appears to be the dominant mechanism for the strength degradation.

Bhatt, Ramakrishna T.↗

Tensile failure of fibrous composites.

Failure of composite consisting of matrix stiffened by uniaxially oriented fibers, when subjected to uniaxial tensile load parallel to fiber direction

COMPOSITE MATERIAL↗

Creep and Rupture Strength of an Advanced CVD SiC Fiber

In the as-produced condition the room temperature strength (approx. 6 GPa) of Textron Specialty Materials' 50 microns CVD SiC fiber represents the highest value thus far obtained for commercially produced polycrystalline SiC fibers. To understand whether this strength can be maintained after composite processing conditions, high temperature studies were performed on the effects of time, stress, and environment on 1400 deg. C tensile creep strain and stress rupture on as-produced, chemically vapor deposited SiC fibers. Creep strain results were consistent, allowing an evaluation of time and stress effects. Test environment had no influence on creep strain but I hour annealing at 1600 deg. C in argon gas significantly reduced the total creep strain and increased the stress dependence. This is attributed to changes in the free carbon morphology and its distribution within the CVD SiC fiber. For the as-produced and annealed fibers, strength at 1400 deg. C was found to decrease from a fast fracture value of 2 GPa to a 100-hr rupture strength value of 0. 8 GPa. In addition a loss of fast fracture strength from 6 GPa is attributed to thermally induced changes in the outer carbon coating and microstructure. Scatter in rupture times made a definitive analysis of environmental and annealing effects on creep strength difficult.

Goldsby, J. C.↗

Oxidation Kinetics and Strength Degradation of Carbon Fibers in a Cracked Ceramic Matrix Composite

Experimental results and oxidation modeling will be presented to discuss carbon fiber susceptibility to oxidation, the oxidation kinetics regimes and composite strength degradation and failure due to oxidation. Thermogravimetric Analysis (TGA) was used to study the oxidation rates of carbon fiber and of a pyro-carbon interphase. The analysis was used to separately obtain activation energies for the carbon constituents within a C/SiC composite. TGA was also conducted on C/SiC composite material to study carbon oxidation and crack closure as a function of temperature. In order to more closely match applications conditions C/SiC tensile coupons were also tested under stressed oxidation conditions. The stressed oxidation tests show that C/SiC is much more susceptible to oxidation when the material is under an applied load where the cracks are open and allow for oxygen ingress. The results help correlate carbon oxidation with composite strength reduction and failure.

Halbig, Michael C.↗

Interfacial Strength in Hierarchical Carbon Fiber Composites: Interplay of Interphase Modulus and Roughness

A facile, direct deposition approach that exploits van der Waals interactions between carbonaceous materials is utilized to create unidirectional hybrid carbon fiber composites. Two small molecule crosslinkers, a trifunctional aromatic (TL) and a difunctional aliphatic (DL) acyl chloride, are first utilized to create a crosslinked interphase with a softer and stiffer modulus respectively. TL crosslinked interphase with a higher modulus improved the tensile strength by 50%, despite non-covalent linking between fiber and matrix, elucidating the critical role of the interphase in alleviating modulus mismatch between the high modulus carbon fiber and the rubbery matrix. Fractional quantities of carbon nanotubes are additionally dispersed in the small molecule crosslinkers which behaved as a dispersant, helping introduce nanoasperities on the carbon fiber surface. Strong “pi-pi” interactions between CNTs and CF contributed to tensile properties, which are increased by 66% compared to the control. A cohesive zone model suggests that a stiffer interphase is better able to exploit surface heterogeneities and roughness on the fiber, synergistically enhancing interfacial strength.

36 MATERIALS SCIENCE↗

Effect of the Ionic Liquid Structure on the Melt Processability of Polyacrylonitrile Fibers

The production of high-strength carbon fibers is an energy-intensive process, where a significant cost involves the wet or dry-spinning of polyacrylonitrile (PAN) fiber precursors. Melt-spinning PAN fibers would allow for significant reduction in the production cost and production hazards. Ionic liquids (ILs) are an attractive fiber-processing medium because of their negligible vapor pressure and low toxicity. In addition, they are carbon-forming precursors; upon carbonization, residual ILs can enhance the carbon yield, although primarily useful for plasticized melt-spinning of PAN precursor fibers. Here, we investigated the influence of the molecular structure of ILs and the control of plasticizing interactions with PAN during melt-spinning. The structural, thermal, and mechanical properties of the melt-spun PAN fibers were obtained by a combination of various characterization methods, such as differential scanning calorimetry, thermogravimetric analysis, Fourier transform infrared spectroscopy, scanning electron microscopy, X-ray diffraction, and mechanical testing. These results demonstrated that the IL structure and counteranions influence the PAN fiber formation. More specifically, ILs containing bromide counteranions produced PAN precursor fibers with increased mechanical properties compared to ILs containing chloride anions. Our research can provide a foundation to understand the influence of ILs on melt-spinning of PAN fibers and provides us the guidelines for a higher cost-/energy-efficient production of PAN-based carbon fibers.

36 MATERIALS SCIENCE↗

Properties of thermo-chemically surface treated carbon fibers and of their epoxy and vinyl ester composites

High strength carbon fibers were surface treated by a continuous gas phase thermo-chemical surface treatment. The surface and the mechanical properties of the fibers were investigated before and after treatment and compared to the properties obtained with a conventional industrial electro-chemical surface treatment. An increase of the oxygen atomic content from 3 % to 20 % with a preferential generation of carboxylic acid functionalities and hydroxyl groups was highlighted after the thermo-chemical surface treatment, compared to an oxygen atomic content of 7 % and a wide variety of oxygen moieties with the electro-chemical surface treatment. The tensile strength of the fibers increased slightly after the thermo-chemical surface treatment and remained the same after the electro-chemical surface treatment. Short beam shear and 90 flexural tests of composites revealed that the improvement of interfacial adhesion with a vinyl ester matrix was limited, revealing that oxidation of the carbon fiber surface alone cannot tremendously improve the mechanical properties of carbon fiber-vinyl ester composites. Atomic force microscopy showed that the creation of roughness with both surface treatments at a nanometric scale. Although the surface is slightly rougher after the electro-chemical surface treatment and is expected to lead to higher adhesion due to mechanical interlocking between the fiber surface and the matrix, the effect of covalent bonding coming from the high concentration of chemical groups on the surface results in higher adhesion strength, as obtained with the thermo-chemical surface treatment.

36 MATERIALS SCIENCE↗

Composite strengthening

The mechanical behavior of unidirectionally reinforced metals is examined, with particular attention to fabrication techniques for artificial composites and eutectic alloys and to principles of fiber reinforcement. The properties of artificial composites are discussed in terms of strength of fiber composites, strength of ribbon-reinforced composites, crack initiation, crack propagation, and creep behavior. The properties of eutectic composites are examined relative to tensile strength, compressive strength, fracture, high-temperature strength, and fatigue. In the case of artificial composites, parallelism of fibers, good bonding between fibers and matrix, and freedom of fibers from damage are all necessary to ensure superior performance. For many eutectic systems there are stringent boundary conditions relative to melt purity and superheat, atmosphere control, temperature gradient, and growth rate in order to provide near-perfect alignment of the reinforcements with a minimum of growth defects.

Stoloff, N. S.↗

Measurement System Analysis of a Novel Phase-Based Ultrasonic NDE Technique for Bond Strength Measurement

Fiber reinforced polymer parts have shown tremendous benefits in aerospace structural applications, but their qualification and certification for use in safety critical areas are currently hindered by the lack of a capable non-destructive evaluation (NDE) method or technique for the inspection of these adhesively bonded parts. Conventional NDE methods and techniques typically detect gross bond defects in a qualitative (Pass/Fail) manner. These techniques struggle to detect weak or kissing bonds. Also, there are no widely adopted NDE methods or techniques for measuring interfacial bond strength or detecting kissing bonds. Bond strength is currently ensured by process control and semi-destructive testing. Results from recent research from other authors, including but not limited to mechanical testing, have shown an excellent correlation between interfacial stiffness of an adhesively bonded joint and the adhesive bond strength of that joint. In this paper, a measurement system analysis (MSA) of a novel phase-based ultrasonic NDE Technique, developed at NASA Langley Research Center, is presented for bond strength measurement to assess at an increased level the measurement process and identify components of variation in that measurement process.

Ultrasound↗

Compressive strength improvements from noncircular carbon fibers: A numerical study

The benefits of high-performance unidirectional carbon fiber composites are limited in many cost-driven industries due to the high cost relative to alternative reinforcement fibers. Low-cost carbon fibers have been previously proposed, but the longitudinal compressive strength continues to be a limiting factor or studies are based on simplifications that warrant further analysis. A micromechanical model is used to (1) determine if the longitudinal compressive strength of composites can be improved with noncircular carbon fiber shapes and (2) characterize why some shapes are stronger than others in compression. In comparison to circular fibers, the results suggest that the strength can be increased by 10%–13% by using a specific six-lobe fiber shape and by 6%–9% for a three-lobe fiber shape. A slight increase is predicted in the compressive strength of the study two-lobe fiber but has the highest uncertainty and sensitivity to fiber orientation and misalignment direction. The underlying mechanism governing the compressive failure of the composites was linked to the unique stress fields created by the lobes, particularly the pressure stress in the matrix. Importantly, this work provides mechanics-based evidence of strength improvements from noncircular fiber shapes and insight on how matrix yielding is altered with alternative fiber shapes.

36 MATERIALS SCIENCE↗

Closing the Loop on Automotive Carbon Fiber Prepreg Manufacturing Scrap

The project demonstrated how to “close the loop” on carbon fiber by integrating industrial carbon fiber scrap into new functional components in an automotive lightweighting application. The project serves as a validation of discontinuous recycled carbon fiber in a commercial context, while generating comprehensive material data throughout the production chain. To this end, the project exhibited increasing complexity as material evaluation progressed from benchtop to commercial scale through full-scale part production, with key material properties thoroughly characterized throughout the process. Of particular focus was the form of the fiber that was fed into compounding, as recycled fiber has historically been problematic to feed at commercial-scale. Carbon fiber is energy-intensive to manufacture, so reuse of existing fiber material can reduce costs and increase sustainability. Additionally, by integrating recovered short fiber into a thermoplastic, regrind processes can be used to provide feedstock for later generations of product. While regrind plastics are not “infinitely recyclable”, reusing the manufacturing scrap over several generations of products can greatly increase material sustainability and lower the fractional embodied energy of each successive product. As such, this project supports the IACMI technical goals of (1) 25% lower carbon fiber-reinforced polymer (CFRP) cost, (2) 50% reduction in CFRP embodied energy, and (3) 80% composite recyclability into useful products. The initial stage of the project involved down selecting surface treatment (sizing) chemistries. Sizing evaluations were performed on Vartega’s chemically recycled intermediate modulus fiber along with standard modulus dry scrap which was oversized with sizing provided by Michelman. More dramatic improvements from sizing were found on the standard rather than the intermediate modulus fibers. The strength of the chemically recycled individual fibers were evaluated by Michelman and ORNL through single fiber testing and found to be comparable to similarly evaluated virgin fibers. UDRI’s mechanical testing on injection molded test specimens identified similar mechanical properties and fiber distribution relative to benchmark specimens. Additional surface chemistry tests and visualizations were performed by the Colorado School of Mines to confirm close conformance between the benchmark and recycled-fiber specimens. As the mechanical test results exceeded the 80% threshold established as the go/no-go(GNG), the project scale was increased to use commercial-scale equipment that would both better characterize the manufacturing utility of the target product format and allow qualitative assessment of a complex commercial part. An upscaled compounding evaluation was performed with a 27 mm twin-screw compounding extruding using oversized standard modulus fibers that were formatted to improve bulk solids transfer. The project team anticipated that milestone mechanical benchmarks could be achieved given the favorable performance of the sized standard modulus material identified in the initial micro-compounding trials. While the mechanical performance did meet the milestone target for that phase of the project, mechanical properties for this standard modulus-based compound were still less than those of the Ford specification. To compare the performance, the project team oversized intermediate modulus dry fibers and compounded them with the project resin at BASF using a 40 mm compounder. Test specimen mechanical performance exceeded the targets laid out in both the project milestone and the Ford specification. A series of prototype parts were successfully molded, albeit with instances of short shot components due to the high thermal conductivity of the carbon fiber compared to glass fiber for which the prototype tool was designed for. The project demonstrated that recycled carbon fiber is a viable option in fiber reinforced compound, providing greatly increased strength and modulus for applications that require them. The “agglomerated” format that facilitated effective bulk solids transfer of recovered fiber showed promise for industrial application.

36 MATERIALS SCIENCE↗

A study of void effects on the interlaminar shear strength of unidirectional graphite fiber reinforced composites

A study was conducted to evaluate the effect of voids on the interlaminar shear strength (ILSS) of a polyimide matrix composite system. The graphite/PRM-15 composite was chosen for study because of the extensive amount of experience that has been amassed in the processing of this material. Composite densities and fiber contents of more than thirty different laminates were measured along with ILSS. Void contents were calculated and the void geometry and distribution were noted using microscopic techniques such as those used in metallography. It was found that there was a good empirical correlation between ILSS and composite density. The most acceptable relationship between the ILSS and density was found to be a power equation which closely resembles theoretically derived expressions. An increase in scatter in the strength data was observed as the void content increased. In laminates with low void content, the void appears to be more segregated in one area of the laminate. It was found that void free composites could be processed in matched metal die molds at pressures greater than 1.4 and less than 6.9 MPa.

Bowles, Kenneth J.↗

Sapphire reinforced alumina matrix composites

Unidirectionally reinforced A1203 matrix composites have been fabricated by hot pressing. Approximately 30 volume % of either coated or uncoated sapphire fiber was used as reinforcement. Unstabilized ZrO2 was applied as the fiber coating. Composite mechanical behavior was analyzed both after fabrication and after additional heat treatment. The results of composite tensile tests were correlated with fiber-matrix interfacial shear strengths determined from fiber push-out tests. Substantially higher strength and greater fiber pull-out were observed for the coated fiber composites for all processing conditions studied. The coated fiber composites retained up to 95% and 87% of their as-fabricated strength when heat treated at 14000C for 8 or 24 hours, respectively. Electron microscopy analysis of the fracture surfaces revealed extensive fiber pull-out both before and after heat treatment.

Jaskowiak, Martha H.↗

Influence of Cr and W alloying on the fiber-matrix interfacial shear strength in cast and directionally solidified sapphire NiAl composites

Sapphire-reinforced NiAl matrix composites with chromium or tungsten as alloying additions were synthesized using casting and zone directional solidification (DS) techniques and characterized by a fiber pushout test as well as by microhardness measurements. The sapphire-NiAl(Cr) specimens exhibited an interlayer of Cr rich eutectic at the fiber-matrix interface and a higher interfacial shear strength compared to unalloyed sapphire-NiAl specimens processed under identical conditions. In contrast, the sapphire-NiAl(W) specimens did not show interfacial excess of tungsten rich phases, although the interfacial shear strength was high and comparable to that of sapphire-NiAl(Cr). The postdebond sliding stress was higher in sapphire-NiAl(Cr) than in sapphire-NiAl(W) due to interface enrichment with chromium particles. The matrix microhardness progressively decreased with increasing distance from the interface in both DS NiAl and NiAl(Cr) specimens. The study highlights the potential of casting and DS techniques to improve the toughness and strength of NiAl by designing dual-phase microstructures in NiAl alloys reinforced with sapphire fibers.

Asthana, R.↗

An inexpensive and effective method for calculating the strength of randomly reinforced fiber composites

Planar randomly reinforced fiber composites (PRRFC) is pseudoisotropic laminate with large number of ply orientation combinations where strength is function of these ply orientation combinations. Laminate theory can be applied to determine strength of PRRFC, and in conjunction with composite micro- and macromechanics can predict mechanical properties of PRRFC's with any fiber/matrix combination.

Chamis, C. C.↗